• 제목/요약/키워드: Fracture surface

검색결과 1,856건 처리시간 0.026초

구조용 세라믹스의 연삭특성에 관한 연구(I) (Grinding Characteristics of Structural Ceramics-I)

  • 하상백;정재극;이종찬
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1995년도 추계학술대회 논문집
    • /
    • pp.14-18
    • /
    • 1995
  • Although structural ceramics have excellent mectanical properties, it is very difficult to grind with high efficiency and high quality because of their high strength, hardness, and brittleness. Unfortunately machined ceramics often contain surface damages such as micro fracture and crack on account of brittle fracture. Therefore, is is important to minimize the brittle fracture. The present paper examines grinding characteristics of representative structural ceramics,such as Al /sab 2/O /sab 3/, SiC, Si /sab 3/ N /sab 4/. Effects of grinding variables including table speed and depth of cut on the grinding performance were investigated. Experimental results show that the surface quality is related to the specific grindings energy. The higher specific energy results in the better surface quality.

  • PDF

표면적분법을 이용한 콘크리트 댐의 균열 해석 (Crack Analysis of Concrete Gravity Dam Using Surface Integral Method)

  • 진치섭;이영호;손기석
    • 콘크리트학회논문집
    • /
    • 제12권3호
    • /
    • pp.31-37
    • /
    • 2000
  • When a crack is produced in a concrete structure, a micro crack zone of fracture process zone (FPZ) appears at the crack tip. To investigate the behaviour of this the micro crack zone, nonlinear fracture mechanics (NLFM) must be applied. However, when a massive concrete structure such as a concrete gravity dam is considered, the micro crack zone can be neglected and the structure can be assumed to have linear elastic fracture mechanics (LEFM) behaviour. This study is divided into two main topics : (1) Calculating stress intensity factor (SIF) at the crack tip by surface integral method and (2) Investigating the propagation of the initial crack. If the initial crack propagates, the angle of the propagation is calculated by using maximum circumferential tensile strength theory. This study, also, contains the effects of body forces and water pressures on the crack face.

유한평판 및 필렛 용접부에 있어서 표면균열의 피로 파괴거동에 관한 연구 (A Study on Fatigue Fracture Behaviour of Surface Crack in Finite Plates and Fillet Weldment)

  • 한문식
    • 한국자동차공학회논문집
    • /
    • 제12권4호
    • /
    • pp.65-73
    • /
    • 2004
  • Fatigue crack growth from surface defects is one of the most important subjects for the evaluation and the assurance of safety in pressure vessels, piping systems, LPG/LNG fuel tank and other various structures. This paper attempts to analysis some practical or general problems such as the estimation of crack growth life to penetrate the plate thickness, based on fatigue crack growth a single surface flaw and the interaction of multiple flaws. An experiment on the coalescence of multiple undercuts was carried out under cyclic tension condition as a attempt to the analysis of multiple crack problems. It is noted that the fracture strength is characterized by the analogy to that in a single crack growth.

스폿용접된 자동차 차체용 알루미늄 박판의 피로균열진전의 파괴역학적 평가 (A fracture mechanics evaluation on the fatigue crack propagation at spot welded aluminum joint in passenger car body)

  • 박인덕;남기우;강석봉
    • 한국해양공학회지
    • /
    • 제11권3호
    • /
    • pp.20-28
    • /
    • 1997
  • The fatigue crack propagation properties and fatigue life of two kinds of Al body panel for automobile were examined experimentally by using the plate specimen and the single spot welding specimen. The fatigue limit of spot welding specimens was lower than that of a plate specimen. The fatigue limit was similar in two kinds of spot welding specimen. The shape and size of crack propagation were observed and measured on beach mark of fracture surface. The crack propagation of surface crack specimen showed almost same tendency to that of a thick plate as almost semi-elliptical. In spot welding specimen, the fatigue crack occurred in inside surface of nugget area was almost semi-elliptical. The crack growth rate can be explained using equation of stress intensity factors.

  • PDF

Influence of pre-existing surface defects on NiTi rotary instrument failure: A SEM study

  • Shin, Yu-Mi;Kim, Wu-Sung;Kum, Kee-Yeon
    • 대한치과보존학회:학술대회논문집
    • /
    • 대한치과보존학회 2003년도 제120회 추계학술대회 제 5차 한ㆍ일 치과보존학회 공동학술대회
    • /
    • pp.594-594
    • /
    • 2003
  • I. Objectives The purpose of this study is to determine if propagation of pre-existing manufacturing defects results in brittle fracture of NiTi rotary files by examining the fracture surface of the instrument by SEM, and to compare the fracture time of NiTi rotary files with different flute designs under cyclic loading. II. Materials and Methods This study examined three groups of rotary NiTi instruments (K3, ProFile, Hero). Of each group, 04 taper, size 30 and 06 taper, size 25 were selected.:120 in total. Surface defects were created by simulating the machining process of NiTi rotaries.(omitted)

  • PDF

Detection of near surface rock fractures using ultrasonic diffraction techniques

  • Selcuk, Levent
    • Geomechanics and Engineering
    • /
    • 제17권6호
    • /
    • pp.597-606
    • /
    • 2019
  • Ultrasonic Time-of-Flight Diffraction (TOFD) techniques are useful methods for non-destructive evaluation of fracture characteristics. This study focuses on the reliability and accuracy of ultrasonic diffraction methods to estimate the depth of rock fractures. The study material includes three different rock types; andesite, basalt and ignimbrite. Four different ultrasonic techniques were performed on these intact rocks. Artificial near-surface fracture depths were created in the laboratory by sawing. The reliability and accuracy of each technique was assessed by comparison of the repeated measurements at different path lengths along the rock surface. The standard error associated with the predictive equations is very small and their reliability and accuracy seem to be high enough to be utilized in estimating the depth of rock fractures. The performances of these techniques were re-evaluated after filling the artificial fractures with another material to simulate natural infills.

Effect of initial coating crack on the mechanical performance of surface-coated zircaloy cladding

  • Xu, Ze;Liu, Yulan;Wang, Biao
    • Nuclear Engineering and Technology
    • /
    • 제53권4호
    • /
    • pp.1250-1258
    • /
    • 2021
  • In this paper, the mechanical performance of cracked surface-coated Zircaloy cladding, which has different coating materials, coating thicknesses and initial crack lengths, has been investigated. By analyzing the stress field near the crack tip, the safety zone range of initial crack length has been decided. In order to determine whether the crack can propagate along the radial (r) or axial (z) directions, the energy release rate has been calculated. By comparing the energy release rate with fracture toughness of materials, we can divide the initial crack lengths into three zones: safety zone, discussion zone and danger zone. The results show that Cr is suitable coating material for the cladding with a thin coating while Fe-Cr-Al have a better fracture mechanical performance in the cladding with thick coating. The Si-coated and SiC-coated claddings are suitable for reactors with low power fuel elements. Conclusions in this paper can provide reference and guidance for the cladding design of nuclear fuel elements.

자기적 비파괴 방법으로서의 Barkhausen Noise를 이용한 강자성체의 파괴인성 및 응력분포해석 (The evaluation of fracture characteristics and the analysis of stress distribution of ferromagnetic materials by Barkhausen noise method)

  • 김동원;권동일
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 D
    • /
    • pp.1864-1866
    • /
    • 1999
  • The magnetic nondestructive test can be applied to evaluate the magnetic material characteristics and the fracture properties through the internal defects of SA-508 used in the pressure vessels of the nuclear power plants as the direct and accurate in-situ testing methods. The fracture toughness, yield strength and the stress distribution around the defects in the surface and sub-surface of magnetic materials can be directly estimated by Bark-hausen noise(BN) methods as NDT. The testing process of SA-508 by Barkhausen noise method was advanced by controlling the austenizing peak temperature and the time of maintenance at a constant austenizing peak temperature, therefore causing the variation of fracture toughness. Through above process. we can evaluate the variations of effective grain size and the correlation of effective grain size and FATT at each situation. And the stress distribution around the defects can be quantified nondestructively through Barkhausen method.

  • PDF

세라믹 접합부재에 대한 파괴역학인자 및 파면 해석 (Analysis of Fracture Mechanics Parameter and Fracture Surface in Bonded Ceramic Joints)

  • 김기성
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 1997년도 춘계학술대회 논문집
    • /
    • pp.156-163
    • /
    • 1997
  • Recently, attempts have been made to be join ceramics to metals in order to make up for the brittleness of ceramics. The difference in the coefficients of linear expansion of the two materials joined at high temperature will cause residual stress, which has a strong influence on the strength of the bonded joints. In this paper, the residual stress distribution and stress intensity factors of the ceramic/metal bonded joints were analyzed by 2-dimensional elastic boundary element method. Fracture toughness tests of ceramic/metal bonded joints with an interface crack were carried out. So the advanced method of quantitative strength evaluation for ceramic/metal bonded joints is to be suggested. Fracture surface and crack propagation path were observed using scanning electron microscope.

  • PDF

STS304강의 비틀림 피로파괴 확률특성 (Fracture Probability Properties of Torsion Fatigue of STS304 Steel)

  • 박대현;정순억
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.201-206
    • /
    • 2003
  • This study is test for STS304 specimen using bending and torsion state. Rounded specimen and notched specimen including fracture surface investigation was comparatively experimented, fatigue life according to degree of surface finishing was examined. Fatigue fracture probability of notched canilever specimens were predicted by P-S-N curve, median rank and Weibull distribution. And at the relation with the rotational speed and stress, the fatigue life of the test specimen was higher at high speed than low speed If summarize STS304 torsion result of fatigue test, is as following. Fatigue life prediction was available by Weibull statistics distribution, and 50% breakdown probability correlation equation was appeared as following.

  • PDF