층상 및 섬유상 $Al_2O_3$ 거시복합체의 파괴거동 (Fracture Behavior of $Al_2O_3$ Macro-composites with Layered and Fibrous Structure)

  • 신동우;윤대현;박삼식;김해두
    • 한국세라믹학회지
    • /
    • 제34권7호
    • /
    • pp.758-766
    • /
    • 1997
  • Non-brittle fracture behaviour of the two composite structures made of two different brittle materials was investigated using 3-point bending test. First, the layered and fibrous macro-composites were fabricated using the material easily formed, yet showing a brittle fracture behaviour similar to ceramics. The layered and fibrous Al2O3 /Al2O3 composites with weak interface were also fabricated using plate of 2 mm thickness and rod of 3 mm diameter respectively. Comparison of the mechanical properties between these two structures was performed in the lights of flexural strength and work of fracture for the composites consisting of Al2O3 and simulated materials respectively. The strength ratio of layered structure to the monolith of same volume was 0.6 and the ratio of fibrous one was about 0.2 for the composites made of simulated brittle material. The ratio of the work of fracture of the fibrous to the layered was 0.47. For Al2O3/Al2O3 composites, the strength ratio of layered and fibrous structures to the monolith with same volume were about 0.6 and 0.2 respectively. The ratio of work of fracture of the fibrous to the layered was 0.6. These confirmed that the layered structure was superior to the fibrous one in terms of flexural strength and work of fracture.

  • PDF

Evaluation of Fracture Strength and Material Degradation for Weldment of High Temperature Service Steel Using Advanced Small Punch Test

  • Lee, Dong-Hwan
    • Journal of Mechanical Science and Technology
    • /
    • 제18권9호
    • /
    • pp.1604-1613
    • /
    • 2004
  • This paper presents an effective and reliable evaluation method for fracture strength and material degradation of the micro-structure of high temperature service steel weldment using advanced small punch (ASP) test developed from conventional small punch (CSP) test. For the purpose of the ASP test, a lower die with a minimized ${\Phi}$1.5 mm diameter loading ball and an optimized deformation guide hole of ${\Phi}$3 mm diameter were designed. The behaviors of fracture energy (E$\_$sp/), ductile-brittle transition temperature (DBTT) and material degradation from the ASP test showed a definite dependency on the micro-structure of weldment. Results obtained from ASP test were compared and reviewed with results from CSP test, Charpy impact test, and hardness test. The utility and reliability of the proposed ASP test were verified by investigating fracture strength, behavior of DBTT, and fracture location of each micro-structure of steel weldment for test specimen in ASP test. It was observed that the fracture toughness in the micro-structure of FL+CGHAZ and ICHAZ decreased remarkably with increasing aging time. From studies of all micro-structures, it was observed that FGHAZ microstructure has the most excellent fracture toughness, and it showed absence of material degradation.

Application of a mesh-free method to modelling brittle fracture and fragmentation of a concrete column during projectile impact

  • Das, Raj;Cleary, Paul W.
    • Computers and Concrete
    • /
    • 제16권6호
    • /
    • pp.933-961
    • /
    • 2015
  • Damage by high-speed impact fracture is a dominant mode of failure in several applications of concrete structures. Numerical modelling can play a crucial role in understanding and predicting complex fracture processes. The commonly used mesh-based Finite Element Method has difficulties in accurately modelling the high deformation and disintegration associated with fracture, as this often distorts the mesh. Even with careful re-meshing FEM often fails to handle extreme deformations and results in poor accuracy. Moreover, simulating the mechanism of fragmentation requires detachment of elements along their boundaries, and this needs a fine mesh to allow the natural propagation of damage/cracks. Smoothed Particle Hydrodynamics (SPH) is an alternative particle based (mesh-less) Lagrangian method that is particularly suitable for analysing fracture because of its capability to model large deformation and to track free surfaces generated due to fracturing. Here we demonstrate the capabilities of SPH for predicting brittle fracture by studying a slender concrete structure (column) under the impact of a high-speed projectile. To explore the effect of the projectile material behaviour on the fracture process, the projectile is assumed to be either perfectly-elastic or elastoplastic in two separate cases. The transient stress field and the resulting evolution of damage under impact are investigated. The nature of the collision and the constitutive behaviour are found to considerably affect the fracture process for the structure including the crack propagation rates, and the size and motion of the fragments. The progress of fracture is tracked by measuring the average damage level of the structure and the extent of energy dissipation, which depend strongly on the type of collision. The effect of fracture property (failure strain) of the concrete due to its various compositions is found to have a profound effect on the damage and fragmentation pattern of the structure.

구조강(構造鋼) 용접부(鎔接部)의 국부인성분포(局部靭性分布)에 관한 연구(研究) (A Study on Local Distribution of Fracture Toughness for Welded Joints of Steel Structure)

  • 장동일;용환선;김동희
    • 대한토목학회논문집
    • /
    • 제4권3호
    • /
    • pp.19-25
    • /
    • 1984
  • 용접구조에 있어서 가장 위험한 단면은 용접부이며 대부분의 파괴가 용접부로부터 발생하였다. 따라서 용접부의 파괴거동을 확인하는 것은 파괴방지를 위하여 중요한 요소라 할 수 있다. 본 연구는 용접부의 파괴거동에 관한 기초적인 연구로서 용접부의 국부적인 인성분포와 다층용접의 효과 및 잔류응력제거풀림의 효과를 조사하였다. 연구에 사용된 기본소재로서는 피로이력을 갖고 있는 강재와 피로이력이 없는 강재를 선택하였다. 용접부에서 미사용강재(피로이력이 없는 강재)모재, 열영향부 용착금속의 파괴인성이 각각 차이가 있었고 용착금속은 균열저지능력으로서 파괴인성이 가장 작아서 파괴발생원이 될수 있음을 확인하였다. 특히 본연구의 대상강재인 기사용강재(피로이력을 갖고 있는 강재)는 파괴인성이 용착금속 보다 작아서 균열이 존재하는 경우 가장 취약한 단면이 될수 있다는 것을 확인하였다. 다충용접은 용접부에 결합이 존재하지 않는다면 안정개선에 효과가 있음을 확인하였고 또한 잔류응력제거 풀림은 본연구에 관한 한은 효과가 없는 것으로 밝혀졌다.

  • PDF

적층한 콘크리트 복합구조체의 파괴역학적 거동 (Fracture Behavior of a Stacked Concrete Structure Based on the Fracture Mechanics)

  • 김상철;김연태
    • 콘크리트학회지
    • /
    • 제11권1호
    • /
    • pp.119-127
    • /
    • 1999
  • 본 연구는 시멘트를 기초로 하는 준 취성재료를 2개 결합시킨 복합구조체의 파괴거동을 시뮬레이션 하는 데 그 목적이 있다. 이를 위해 작용하중방향에 직각으로 콘크리트와 시멘트를 적층하여 시편을 제작하였고, 비선형파괴해석에서 사용되는 각 구성재료별 파괴계수들을 구하기 위해 콘크리트와 시멘트 각각에 대해 3점휨시험 및 간접인장강도시험을 실시하였다. 시험을 통해 산정한 계수들을 도출한 이론식에 적용하여 복합체로 제작한 시편의 실험 결과치와 비교한 결과, 가상균열이론에 입각한 이론치와 실험결과치는 거의 유사한 경향을 나타내었다. 또한, 파괴에너지와 강도의 향상은 복합체를 구성하는 구성재료의 적층순서에 크게 의존하는 것으로 나타났다. 따라서 구조물의 목적에 맞게 복합체를 적절히 배열하므로써 구조물의 취성과 연성을 상승시킬 수 있음을 본 연구를 통해 알 수 있었다.

안와파열골절 급성기의 CT영상을 이용한 계측학적인 연구 (Measurement Analytical Study of Computed Tomography of the Orbital Structure in Acute Blow-out Fracture)

  • 정성호;신승한;박승하;구상환
    • Archives of Plastic Surgery
    • /
    • 제34권1호
    • /
    • pp.44-51
    • /
    • 2007
  • Purpose: Blow-out fracture is one of the most common fractures in facial trauma. It is diagnosed by Computed Tomography(CT) scan, which is considered as the most effective diagnostic tool. Since, the Picture Archiving Communication System(PACS) has been provided recently to many hospitals, doctors are more familiar with imaging software of PACS. Because this software has many useful measuring tools, doctors can measure orbital structure easily and make a plan for treatment with its data. Therefore, authors intended to analyze the data of orbital structure measured with PACS imaging software and evaluate its usefulness. Methods: The charts and CT images of 100 patients, which were 50 patients with medial wall fracture and 50 patients with floor fracture, were reviewed. Patients were selected by pre-determined criteria and their CT images were measured with image software of PACS. 'Extraocular muscle thickness', 'Defect ratio'(ratio of defect area to normal area) and 'Globe position index' were measured and analyzed statistically. Results: The thickness of inferior rectus muscle and medial rectus muscle was simultaneously increased in acute-stage of blow-out fracture. The medial rectus muscle was more thickened in medial wall fracture and inferior rectus was more thickened in floor fracture, respectively. In acute blow-out fracture, globe position is exophthalmic rather than enophthalmic. Especially in floor fracture, numerical value summed up thickness of all extraocular muscle is correlated to the defect ratio and globe position index. Conclusion: Clinicians can decide globe position or presume defect ratio in inferior wall fracture by measurement of CT image in acute blow-out fracture using PACS.

초저온 액화질소 저장탱크 오스트나이트계 스테인리스강의 용접부의 파괴인성 연구 (A Study on the Weld Part Fracture Toughness of Austenite Type Stainless Steel for Cryogenic Liquid Nitrogen Storage Tank)

  • 김영득;최동준;박형욱;조종래;배원병
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제35권6호
    • /
    • pp.802-808
    • /
    • 2011
  • 극저온 온도 구조 재료의 중요한 기계적 성질 중 하나는 파괴 인성이다. 파괴 인성 시험 방법의 규격화에 대한 연구는 극저온 구조 요소의 개발과 함께 매우 중요한 문제가 되고 있다. 특히 용접부의 경우 극저온 환경 하에서 사용할 때 불안정파괴를 유발할 수 있기 때문에 용접부의 각 미세조직에 따른 기계적 성질 평가가 중요하다. 본 연구에서는 STS-316L 모재와 용접재를 대상으로 액체질소(77K), 액체헬륨(4K), 293K 온도에서 제하컴플라이언스법과 예민화 열처리한 소형화된 시험편 대상으로 파괴인성평가 실험을 수행하였다.

VC 첨가가 Ti(CN)계 써메트의 미세구조 및 기계적 성질에 미치는 영향 (Effect of VC Addition on the Microstructure & Mechanical Properties of Ti(CN)-based Cermet)

  • 안성용;강신후
    • 한국세라믹학회지
    • /
    • 제35권12호
    • /
    • pp.1316-1322
    • /
    • 1998
  • The amount of VC and C/N ratio in Ti(CN) was varied to investigate the effect of VC addition on the mi-crostructural change in Ti(CN)-Ni system. As the amount of VC addition increases in Ti(C0.7N0.3)-20Ni sys-tem a complete solid solution was observed in Ti(C0.7N0.3)-20Ni-25VC system. It implies that the ratio of the dissolution rates of Ti(C0.7N0.3)to that of VC is nearly 2:1 at the sintering conditions used in this study. It was found from the experiments that the system composed of the Ti(C0.7N0.3) phase exhibits a rimless structure and relatively small amount of solid solution. That is among Ti(C0.7N0.3) phase exhibits a rimless structure and relatively small amount of solid solution. This is among Ti(C1-xNx) phases the dissolution rate of Ti(C0.3N0.7) is the lowest. Also fracture toughness(KIC) of the cermet was measured by indentation method. Attentions were paid to crack propagation path to look for a dominant fracture mode and to cor-relate it with fracture toughness values. The fracture toughness was relatively high with the addition of VC content. But the addition of a large VC content reduced the overall toughness of the cermet. This result is explained with the difference in fracture mode.

  • PDF

해저환경에 따른 두께가 두꺼운 탄소섬유/에폭시 복합재의 파괴인성에 대한 실험적 연구 (An experimental study on the fracture toughness of thick carbon/epoxy composite in the deep-sea environment)

  • 하성록;이경엽
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 추계학술대회 논문집
    • /
    • pp.1037-1041
    • /
    • 2005
  • It is well-known that the corrosive behavior of PMC (polymer matrix composite) structure is much better than the metal structure in the marine environment. The understanding of fracture behavior of PMC in the deep-sea environment is essential to expand its use in the marine industry. For a present study, fracture tests have been performed under four different pressure levels such as 0.1 MPa, 100 MPa, 200 MPa, and 270 MPa using the seawater-absorbed carbon/epoxy composite samples. Fracture toughness was determined from the work factor approach as a function of hydrostatic pressure. It was found that fracture behavior was a linear elastic for all pressure levels. The fracture toughness increased with increasing pressure.

  • PDF

Cr-Mo강 용접열영향부의 파괴인성과 용접입열량에 관한 연구(I) (HAZ 고유조직을 중심으로) (Study on Fracture Toughness and Heat Input in Weld HAZ of Cr-Mo Steel (I) (welding structure))

  • 임재규;정세희
    • Journal of Welding and Joining
    • /
    • 제2권2호
    • /
    • pp.54-61
    • /
    • 1984
  • Construction of welding structure is greatly dependent upon welding heat cycle. Fracture toughness is decreased remarkablely due to coarse grained HAZ and inequal residual stress of three dimensions to originate in welding. Post weld heat treatment(PWHT) is carried out to increase the fracture toughness of HAZ and to remove the residual stress. There occur some problem such as toughness decrement and stress relief cracking(SRC) in the coarse grained HAZ subject to the effect of tempering treatment. Therefore, in this paper, the effect of heat inputs affecting cooling rate and PWHT under the no stress on fracture toughness were evaluated by crack opening displacement (COD), SEM and micro-hardness test. Experimental results are as follows; 1. Fracture toughness of weld HAZ is dependent upon weld heat cycle and it is decreased with increment of heat input, but the degree of improvement of fracture toughness after PWHT was linearly increased with heat input. 2. Hardness of the parent metal is not changed, but the softening of coarse grained HAZ is remarkable due to PWHT. 3. Fracture surface of as-weld show the perfect brittle fracture with the cleavage fracture, but after PWHT they appear the ductile fracture surface with dimple.