Determination of CTOD & CTOA Curve for Structural Steel Hot-Rolled Thin Plates (일반 구조용강 열간압연 박판에 대한 CTOD와 CTOA 곡선 결정)

  • 이계승;이억섭
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.729-732
    • /
    • 2003
  • The K-R design curve is an engineering method of linear-elastic fracture analysis under plane-stress loading conditions. By the way, linear-elastic fracture mechanics (LEFM) is valid only as long as nonlinear material deformation is confined to a small region surrounding the crack tip. Like general steels, it is virtually impossible to characterize the fracture behavior with LEFM, in many materials. Critical values of J contour integral or crack tip opening displacement (CTOD) give nearly size independent measures of fracture toughness, even for relatively large amounts of crack tip plasticity. Furthermore, the crack tip opening displacement is the only parameter that can be directly measured in the fracture test. On the other. the crack tip opening angle (CTOA) test is similar to CTOD experimentally. Moreover, the test is easier to measure the fracture toughness than other method. The shape of the CTOA curve depends on material fracture behavior and, on the opening configuration of the cracked structure. CTOA parameter describes crack tip conditions in elastic-plastic materials, and it can be used as a fracture criterion effectively. In this paper, CTOA test is performed for steel JS-SS400 hot-rolled thin plates under plane-stress loading conditions. Special experimental apparatuses are used to prevent specimens from buckling and to measure crack tip opening angle for thin compact tension (CT) specimens.

  • PDF

Rock Fracture Centerline Extraction based on Hessian Matrix and Steger algorithm

  • Wang, Weixing;Liang, Yanjie
    • KSII Transactions on Internet and Information Systems (TIIS)
    • /
    • v.9 no.12
    • /
    • pp.5073-5086
    • /
    • 2015
  • The rock fracture detection by image analysis is significant for fracture measurement and assessment engineering. The paper proposes a novel image segmentation algorithm for the centerline tracing of a rock fracture based on Hessian Matrix at Multi-scales and Steger algorithm. A traditional fracture detection method, which does edge detection first, then makes image binarization, and finally performs noise removal and fracture gap linking, is difficult for images of rough rock surfaces. To overcome the problem, the new algorithm extracts the centerlines directly from a gray level image. It includes three steps: (1) Hessian Matrix and Frangi filter are adopted to enhance the curvilinear structures, then after image binarization, the spurious-fractures and noise are removed by synthesizing the area, circularity and rectangularity; (2) On the binary image, Steger algorithm is used to detect fracture centerline points, then the centerline points or segments are linked according to the gap distance and the angle differences; and (3) Based on the above centerline detection roughly, the centerline points are searched in the original image in a local window along the direction perpendicular to the normal of the centerline, then these points are linked. A number of rock fracture images have been tested, and the testing results show that compared to other traditional algorithms, the proposed algorithm can extract rock fracture centerlines accurately.

COMPLICATIONS ASSOCIATED WITH OPEN REDUCTION OF MANDIBULAR FRACTURES (관혈적 정복술로 치료한 하악골 골절에서의 합병증)

  • Park, Young-Ah;Sohn, Woo-Ill;Chang, Ic-Jun;Song, Jae-Chul;Chin, Byung-Rho
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.27 no.5
    • /
    • pp.474-480
    • /
    • 2001
  • Purpose: The aim of this study was to evaluate the complications of open reduction and internal fixation of mandibular fracture with miniplates. Patients and Methods: A total of 134 patients who presented with 196 fractures were analyzed retrospectively. Complications were evaluated for factors such as age, the site of fracture, the severity of fracture, delayed operation, preoperative wound contamination, the site and disposition of teeth in the fracture line and midfacial fractures. Statistical analysis was used to compare complications to risk factors. Results: Of the 134 patients, 20 patients had some form of postoperative complications and complication rate was 14.9%. These complications included infection, plate fracture, malocclusion, wound dehiscence, nerve injury and nonunion. There was a significant correlation between complication rate and the severity of fracture, preoperative wound contamination and the site of the fracture and disposition of teeth(p<0.05). Conclusion: The occurrence of postoperative complications in the treatment of mandibular fractures was related to the severity of fracture, preoperative wound contamination and the site of the fracture and disposition of teeth.

  • PDF

MODELING THE HYDRAULIC CHARACTERISTICS OF A FRACTURED ROCK MASS WITH CORRELATED FRACTURE LENGTH AND APERTURE: APPLICATION IN THE UNDERGROUND RESEARCH TUNNEL AT KAERI

  • Bang, Sang-Hyuk;Jeon, Seok-Won;Kwon, Sang-Ki
    • Nuclear Engineering and Technology
    • /
    • v.44 no.6
    • /
    • pp.639-652
    • /
    • 2012
  • A three-dimensional discrete fracture network model was developed in order to simulate the hydraulic characteristics of a granitic rock mass at Korea Atomic Energy Research Institute (KAERI) Underground Research Tunnel (KURT). The model used a three-dimensional discrete fracture network (DFN), assuming a correlation between the length and aperture of the fractures, and a trapezoid flow path in the fractures. These assumptions that previous studies have not considered could make the developed model more practical and reasonable. The geologic and hydraulic data of the fractures were obtained in the rock mass at the KURT. Then, these data were applied to the developed fracture discrete network model. The model was applied in estimating the representative elementary volume (REV), the equivalent hydraulic conductivity tensors, and the amount of groundwater inflow into the tunnel. The developed discrete fracture network model can determine the REV size for the rock mass with respect to the hydraulic behavior and estimate the groundwater flow into the tunnel at the KURT. Therefore, the assumptions that the fracture length is correlated to the fracture aperture and the flow in a fracture occurs in a trapezoid shape appear to be effective in the DFN analysis used to estimate the hydraulic behavior of the fractured rock mass.

Effect of medium coarse aggregate on fracture properties of ultra high strength concrete

  • Karthick, B.;Muthuraj, M.P.
    • Structural Engineering and Mechanics
    • /
    • v.77 no.1
    • /
    • pp.103-114
    • /
    • 2021
  • Ultra high strength concrete (UHSC) originally proposed by Richards and Cheyrezy (1995) composed of cement, silica fume, quartz sand, quartz powder, steel fibers, superplasticizer etc. Later, other ingredients such as fly ash, GGBS, metakaoline, copper slag, fine aggregate of different sizes have been added to original UHSC. In the present investigation, the combined effect of coarse aggregate (6mm - 10mm) and steel fibers (0.50%, 1.0% and 1.5%) has been studied on UHSC mixes to evaluate mechanical and fracture properties. Compressive strength, split tensile strength and modulus of elasticity were determined for the three UHSC mixes. Size dependent fracture energy was evaluated by using RILEM work of fracture and size independent fracture energy was evaluated by using (i) RILEM work of fracture with tail correction to load - deflection plot (ii) boundary effect method. The constitutive relationship between the residual stress carrying capacity (σ) and the corresponding crack opening (w) has been constructed in an inverse manner based on the concept of a non-linear hinge from the load-crack mouth opening plots of notched three-point bend beams. It was found that (i) the size independent fracture energy obtained by using above two approaches yielded similar value and (ii) tensile stress increases with the increase of % of fibers. These two fracture properties will be very much useful for the analysis of cracked concrete structural components.

Analysis of Discontinuity Distribution Property to Predict Rock Slope Failure (암반 사면의 파괴 예측을 위한 불연속면 분포 특성 분석)

  • 윤운상;김정환;배기훈
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 1999.10a
    • /
    • pp.147-152
    • /
    • 1999
  • Distribution of fracture system is an important factor to analyse instability of jointed rock slope. In the most case of rock slopes, joint distribution properties are related to potential, shape, size and locality of slope failure. The purpose of this paper is to present an application of fracture characterization related to rock slope failure. Fracture data used in this study are collected by scanline survey. Two aspects of fracture characterization for rock slope are handled in this study First, In order to determine the potential and shape of slope failure, trace length of joints is considered as the weighting factor about collected orientation data. Second, Relationship between trace length and spacing is analysed to estimate failure location and size. The distribution of fracture system is directly influenced on wedge failure. It is effective to analyse the orientation of fractures by using weighting factors associated with the trace length of fractures rather than to analyse only that of fractures. It gives a conclusion that the wedge failure occurred along the peak of fracture density(or intensity) cycles.

  • PDF

Notch Radius Effect for Static Fracture Toughness of Al 7175 Alloys (Al 7175 합금의 정적 파괴인성에 미치는 노치반경 영향)

  • 김재훈;김덕회;박성욱;문순일
    • Proceedings of the Korean Society of Propulsion Engineers Conference
    • /
    • 2002.04a
    • /
    • pp.84-87
    • /
    • 2002
  • In this study, intrinsic fracture toughness of Al 7175-T74 is evaluated from the apparent toughness of notched specimen. Modified average stress model is used to establish the relationship to predict the intrinsic fracture toughness from the apparent fracture toughness of a notched-cracked specimen. The modified average stress model is established the relation between notch radius and effective distance calculated by FEM analysis. The results show that fracture toughness decreases with decreasing of notch root radius. The true fracture toughness can be predicted from test results of apparent fracture toughness measured by using notched specimen.

  • PDF

Prediction of Ductile Fracture in Metal Forming Processes (금속성형공정에서 연성파괴예측)

  • 고대철;이진희;김병민;최재찬
    • Transactions of Materials Processing
    • /
    • v.3 no.2
    • /
    • pp.167-177
    • /
    • 1994
  • Most of bulk metal forming processes may be limited by ductile fracture such as surface or internal cracks developing in the workpiece. It is important to identify the conditions within the deforming workpiece which may lead to fracture, and then it is possible to modify the forming processes to produce sound and reliable product. This paper suggests the scheme to simultaneously accomplish prediction of fracture initiation and analysis of deformation in metal forming processes. The Cockcroft-Latham criterion which is successfully applied to a variety of loading situations is used in the present investigation to estimate whether fracture occurs during the deformation process. The numerical predictions and experimental results of two types of metal forming process are compared, axisymmetric extrusion and simple upsetting. The proposed scheme has successfully predicted the fracture initiation found experimentally.

  • PDF

Dynamic Fracture Toughness of Chevron-notch Ceramic Specimens measured in Split Hopkinson Pressure Bar

  • Lee, Yeon-Soo;Yoon, Young-Ki;Yoon, Hi-Seak
    • International Journal of Precision Engineering and Manufacturing
    • /
    • v.3 no.3
    • /
    • pp.69-75
    • /
    • 2002
  • Measuring dynamic fracture toughness of brittle and small ceramic specimen is very difficult in a SHPB (Split Hopkinson Pressure Bar). As a countermeasure to this difficulty, a dynamic fracture toughness measuring method by the Chevron-notch ceramic specimen was proposed. Tested chevron specimens were of Chevron notch angles of 90$^{\circ}$, 100$^{\circ}$ and 110$^{\circ}$. Through finite element analysis, shape parameters of the Chevron-notch specimens according to notch angles were calculated. And the static fracture tough1ess of the Chevron-notch alumina specimen was measured as 3.8MPa√m similar to that of CT specimen with a precrack. Dynamic fracture toughness was 4.5MPa√m slightly higher than the static one. It was shown in this study that the proposed Chevron-notch specimens are valid to measure dynamic fracture toughness of extremely brittle materials such as ceramic.

A study on the J-integral and the fracture behavior of concrete (J-적분과 콘크리트 파괴거동에 관한 연구)

  • 최신호;윤요현;계해주;전철송;김화중
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10a
    • /
    • pp.185-190
    • /
    • 2000
  • The effect of specimen thickness and notch's depth and the validity of J-integral analysis were studied on the fracture behavior of concrete. Through the 3-point bending test, the stress-deformation curves were experimentally measured. Concrete fracture toughness is calculated from stress-displacement curves. Concrete fracture toughness decreases when notch's depth is longer. So, Gf is less sensitive than JIc and Gf is more useful factor as concrete fracture toughness parameter. The values of J-integral and fracture energy increase when the breadth of concrete specimen get longer from 75mm to 150mm. Therefore, the breadth effect of specimen has to be considered in determining the concrete fracture toughness.

  • PDF