Effect of Heterogeneous Microstructure on the Fracture Toughness of Weld Metal (용착금속의 파괴인성에 미치는 불균일 미세조직의 영향)

  • 정현호;김철만;김형식;김우식;홍성호
    • Journal of Welding and Joining
    • /
    • v.17 no.2
    • /
    • pp.36-43
    • /
    • 1999
  • The effect of microstructure on the fracture toughness of multi pass weld metal has been investigated. The micromechanisms of fracture process are identified by in-situ scanning electron microscopy(SEM) fracture observation using single edge notched specimen. The notches of the in-situ fracture specimens were carefully located such that the ends of the notches were in the as-deposited top bead and the reheated weld metal respectively. The observation of in-situ fracture process for as-deposited top bead indicated that as strains are applied, microcracks are formed at the interfaces between soft proeutectoid ferrite and acicular ferrite under relatively low stress intensity factor. Then, the microcracks propagate easily along the proeutectoid ferrite phase, leading to final fracture. These findings suggest that proeutectoid ferrite plays an important role in reducing the toughness of the weld metal. On the other hand, reheated regions showed that the microcrack initiated at the notch tip grows along the localized shear bands under relatively high stress intensity factor, confirming that reheated area showing momogeneous and fine microstructure would be beneficial to the fracture resistance of weld metal.

  • PDF

Brittle fracture analysis of the offset-crack DCDC specimen

  • Ayatollahi, M.R.;Bagherifard, S.
    • Structural Engineering and Mechanics
    • /
    • v.29 no.3
    • /
    • pp.301-310
    • /
    • 2008
  • Applications of fracture mechanics in the strength analysis of ceramic materials have been lately studied by many researchers. Various test specimens have been proposed in order to investigate the fracture resistance of cracked bodies under mixed mode conditions. Double Cleavage Drilled Compression (DCDC) specimen, with a hole offset from the centerline is a configuration that is frequently used in subcritical crack growth studies of ceramics and glasses. This specimen exhibits a strong crack path stability that is due to the strongly negative T-stress term. In this paper the maximum tensile stress (MTS) criterion is employed for investigating theoretically the initiation of brittle fracture in the DCDC specimen under mixed mode conditions. It is shown that the T-stress has a significant influence on the predicted fracture load and the crack initiation angle. The theoretical results suggest that brittle fracture in the DCDC specimen is controlled by a combination of the singular stresses (characterized by KI and KII) and the non-singular stress term, T-stress.

Evaluation of cyclic fracture in perforated beams using micromechanical fatigue model

  • Erfani, Saeed;Akrami, Vahid
    • Steel and Composite Structures
    • /
    • v.20 no.4
    • /
    • pp.913-930
    • /
    • 2016
  • It is common practice to use Reduced Web Beam Sections (RWBS) in steel moment resisting frames. Perforation of beam web in these members may cause stress and strain concentration around the opening area and facilitate ductile fracture under cyclic loading. This paper presents a numerical study on the cyclic fracture of these structural components. The considered connections are configured as T-shaped assemblies with beams of elongated circular perforations. The failure of specimens under Ultra Low Cycle Fatigue (ULCF) condition is simulated using Cyclic Void Growth Model (CVGM) which is a micromechanics based fracture model. In each model, CVGM fracture index is calculated based on the stress and strain time histories and then models with different opening configurations are compared based on the calculated fracture index. In addition to the global models, sub-models with refined mesh are used to evaluate fracture index around the beam to column weldment. Modeling techniques are validated using data from previous experiments. Results show that as the perforation size increases, opening corners experience greater fracture index. This is while as the opening size increases the maximum observed fracture index at the connection welds decreases. However, the initiation of fracture at connection welds occurs at lower drift angles compared to opening corners. Finally, a probabilistic framework is applied to CVGM in order to account for the uncertainties existing in the prediction of ductile fracture and results are discussed.

Televiewer에서 관찰되는 단열특성과 수리전도도와의 상관관계 분석

  • Park Gyeong-U;Bae Dae-Seok;Kim Gyeong-Su;Go Yong-Gwon
    • Proceedings of the Korean Society of Soil and Groundwater Environment Conference
    • /
    • 2005.04a
    • /
    • pp.284-287
    • /
    • 2005
  • The flow of groundwater in fractured medium is related to the geometric characteristics of the fracture system. And a fracture aperture and a fracture density are considered as important factor concerning the permeability. Data acquisition of the properties of fracture such as aperture and density is so difficult and has uncertainty. We also cannot know the fracture characteristics through the in-situ tests. We usually obtain the fracture information from a ultrasonic scan logging or borehole television indirectly. Using the deduced results, we can make the fracture system and simulate the groundwater flow and solute transport in the crystalline rock. This study aimed to analyze the correlation between the properties of fracture and hydraulic conductivities obtained at the same interval. The properties of fracture are examined by acoustic televiwer and hydraulic conductivities are obtained by constant Pressure injection test. The distributioin of fracture width and fracture frequency shows the log-normal probability plot. And, Results of correlation analysis explain that opened type fractures have proper relation with hydraulic conductivity. But, as though there are semi-opened type fractures or closed type fractures, those have the permeable structure.

  • PDF

Evaluation of fracture density distribution for the design of grouting works in fractured rocks (그라우팅 설계를 위한 절리밀도분포 산출법 개발)

  • 김중열;김유성
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2002.03a
    • /
    • pp.627-634
    • /
    • 2002
  • To facilitate a drilling plan for grouting in fractured rock, an algorithm of practical use associated with a new term “fracture density distribution”or“fracture tomogram”is developed. It is well known that Televiewer data(amplitude and traveltime image) provide detailed information about not only dip and dip direction of each fracture but also its aperture size estimated by an appropriate evaluation algorithm. A selected plane section of medium around a borehole or the cross section between two boreholes is discretized into a two dimensional grid of cells(rectangular elements). As each elongated(straight) fracture passes through the cells, the corresponding aperture size value is successively summed up in each cell, depending on the fracture length segment. In this, the fracture lines can be determined by intersecting of each fracture plane with the selected plane section. If the fracture line does not pass through a particular grid element, the segment length is set to zero. The final value(aperture size value of each cell) derived from all the detected fractures constitutes the fracture density distribution of the selected plane section, Field examples are illustrated, which will prove the benefit of the suggested algorithm for several kinds of grouting works.

  • PDF

Effects of Fine Contents on the Fracture Characteristics of Frozen Sand (세립분 함유량이 동결 사질토의 파괴특성에 미치는 영향)

  • Hwang, Bumsik;Cho, Wanjei
    • Journal of the Korean Geotechnical Society
    • /
    • v.36 no.3
    • /
    • pp.25-36
    • /
    • 2020
  • In this research, three-point bending tests were performed using a rectangular frozen specimen with various fine contents and notch offset distance from the center of the specimen to investigate the fracture characteristic of the frozen sand. Based on the test results, mode I fracture toughness was calculated, and mixed-mode (mode I + II) fracture characteristics were investigated using the fracture energy which was calculated until the maximum point of the load-displacement curve. As the fine contents increase, the peak load and mode I fracture toughness increase until 10% fine contents. Furthermore, as the notch offset distance increases, the fracture energy required for crack start also increases due to the increase in mode II load at the crack tip.

Design of Shear Fracture Specimens for Sheet Metals Using Finite Element Analyses (유한요소해석을 이용한 금속 판재용 전단 파단 시편 설계)

  • C. Kim;H.J. Bong;M.G. Lee
    • Transactions of Materials Processing
    • /
    • v.32 no.2
    • /
    • pp.92-99
    • /
    • 2023
  • In this study, shear fracture specimens are designed using finite element analyses for the characterization of ductile fracture criteria of metal sheets. Many recently suggested ductile fracture criteria require experimental fracture data at the shear stress states in the model parameter identification. However, it is challenging to maintain shear stress states in tension-based specimens from the initial yield to the final fracture, and the loading path can be different for the different materials even with the same shear specimen geometries. To account for this issue, two different shear fracture specimens for low ductility/high ductility metal sheets are designed using the sensitivity tests conducted by finite element simulations. Priorly mechanical properties including the Hosford-Coulomb fracture criterion of the aluminum alloy 7075-T6 and DP590 steel sheets are used in the simulations. The results show that shear stress states are well-maintained until the fracture at the fracture initiation points by optimizing the notch geometries of the shear fracture specimens.

Study on the Burr Formation and Fracture at the Exit Stage in Orthogonal Cutting (2차원절삭에서 공구이탈시 발생하는 버(Burr)와 파단에 관한 연구)

  • 고성림
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.5
    • /
    • pp.1172-1182
    • /
    • 1993
  • In orthogonal machining a quantitative model for burr formation process and fracture when tool exits workpiece is proposed. When no fracture during burr formation burr formation process is divided by three parts; Initiation, Development and Final burr formation. According to the properties of workpiece fracture will happen or not after initiation of burr formation. Considering the fact that fracture depends on the ductility of workpiece, the fracture strain obtained from ductile fracture criterion is used for prediction. It is verified that the fracture strain from tension test can be used as fracture criterion in burr formation without large error. For detailed observation of burr formation an experimental stage for micro orthogonal cutting inside SEM (Scanning Electron Microscope) is built. Through the comparison between model prediction and experimental result from orthogonal machining in milling machine the model is verified.

The Clinical Study of Ankle Fracture and Dislocation (족관절의 골절-탈구에 대한 임상적 고찰)

  • Kim, Ji Hoon;Song, Jae Gwang;Suh, Jin Soo
    • Journal of Korean Foot and Ankle Society
    • /
    • v.17 no.3
    • /
    • pp.182-188
    • /
    • 2013
  • Purpose: We evaluate clinical manifestations and radiologic features of ankle fracture & dislocation, as well as the usefulness of computed tomography on posterior ankle fracture & dislocation to study factors contributing to ankle fracture & dislocation. Material and Methods: Ankle dislocation was defined as the center of talar body being translated over the cortex of tibia on AP or lateral view on simple X-ray. Surgical treatments of 30 patients from January 2007 to March 2012 were categorized according to the injury mechanism, the direction of dislocation and fracture site. Joint involvement of posterior malleoalr fracture was evaluated through simple x-ray and computed tomography. We treated surgically if posterior malleolus fracture involves more than 25% of dital tibial articular surface. Thereafter, clinical outcomes were identified through radiographs and by using the AOFAS score. Results: The mean age was 42(13-78) years old, and slip down was the most common injury mechanism (13 cases). Car accident (6 cases) and fall accident (4 cases) were the next frequently found injury mechanisms. As for the types of ankle fracture, posterior fracture and dislocation (21 cases, 43.3%) was most commonly found. Out of these 21 cases, 15 cases involved trimalleolar fracture, and 19 cases were associated with posterior malleolar fracture. Danis-weber type B and C patients were 11 cases and 10 cases respectively. Articular involvement of posterior malleolar fracture turned out to be average 27.9%(5.1%~49.1%) on simple x-ray. The rate was evaluated as average 31.7%(12.6%~55.3%) on computed tomography which was conducted 15 times, and led us to more meaningful data. Conclusion: Anterolateral fracture and dislocation often accompanied open dislocation. Posterior fracture dislocation was most commonly found. Posterior malleolus was an important factor that ensures posterior stability of the ankle joint. Computed tomograph is useful to evaluate the articular involvement of posterior malleolar fracture.

Two Part Triplane Fracture with Extention through Medial Malleolus (Four Cases Report) (족관절 내과를 침범한 두 부분 삼면 골절(4예 보고))

  • Cha, Seung-Do;Kim, Hyung-Soo;Chung, Soo-Tae;Yoo, Jeong-Hyun;Park, Jai-Hyung;Kim, Joo-Hak;Kim, Yong-Hoon
    • Journal of Korean Foot and Ankle Society
    • /
    • v.13 no.2
    • /
    • pp.179-183
    • /
    • 2009
  • The triplane fracture has been described as a fracture of the distal tibial epiphysis occurring across three planes-sagittal, transverse and coronal. The characteristic pattern of fusion of distal tibial epiphysis explains the special configuration of the fragments in the triplane fracture. According to Dias-Tachdjian classification, triplane fracture is classified two part fracture, three part fracture, four part fracture and two part fracture with extension to the medial malleolus. Among four types, two part triplane fracture with extension to the medial malleolus is a relatively rare injury and generally is not treated by closed reduction. Such fractures should have an anatomic reduction and adequate fixation to restore the joint congruity and obtain an anatomic reduction of the growth plate to prevent a future growth deformity. This is usually best accomplished with an open reduction and screw fixation or k-wire fixation. We experienced two part triplane fracture with extension to medial malleolus and check the CT to define the extent of the injury completely. And then we underwent open reduction and screw fixation for the fracture. As a result, we present four cases of two part triplane fracture with extension with review of related literatures.

  • PDF