• Title/Summary/Keyword: Fire flame

Search Result 833, Processing Time 0.024 seconds

Combustive Properties of Medium Density Fibreboards (MDF) Treated with Bis-(Dimethylaminomethyl) Phosphinic Acid and Alkylenediaminoalkyl-Bis-Phosphonic Acids (비스-디메틸아미노메틸 포스핀산과 알킬렌디아미노알킬-비스-포스폰산 유도체에 의해 처리된 중밀도 섬유판의 연소특성)

  • Park, Myung-Ho;Chung, Yeong-Jin
    • Fire Science and Engineering
    • /
    • v.28 no.5
    • /
    • pp.71-79
    • /
    • 2014
  • This study was performed to test the combustive properties of Medium Density Fibreboards (MDFs) treated with chemicals of the bis-(dimethylaminomethyl) phosphinic acid (DMDAP), N,N-dimethylethylenediaminomethyl-bis-phosphonic acid (DMDEDAP), piperazinomethyl-bis-phosphonic acid (PIPEABP), and methylpiperazinomethyl-bis-phosphonic acid (MPIPEABP). MDFs were painted in three times with 15 wt% solution of the bis-(dimethylaminomethyl) phosphinic acid and alkylenediaminoalkyl-bis-phosphonic acids at the room temperature, respectively. After drying MDF treated with chemicals, combustive properties and volatile organic compounds (VOCs) contents were examined by the cone calorimeter (ISO 5660-1), test for flame retardant (NEMA Notice No. 2012034), and gas chromatography (KS M ISO 11890-2), respectively. It was indicated that the MDFs treated with chemicals showed the longer time to combustion time (CT) = (442~492) s than that of virgin plate by reducing the burning rate except for CT treated with DMDAP. In adition, the MDFs treated with chemicals showed both of the higher char area (44.33~61.33) kg/kg and char length (10.33~11.67) cm than those of virgin plate. Especially, the MDFs treated with chemicals showed the higher mean volatile organic compounds (VOCs) (0.188~0.333) g/L than that of virgin plate within the prescribed limits. Thus, It is supposed that the combustion- retardation properties were improved by the partial due to the treated chemicals in the virgin MDF.

Experimental Study on the Self-extinguishing Performance of Extruded Polystyrene Insulation for Buildings and Suggestions on Institutional Management (건축용 압출법 단열판(XPS)의 자기소화성에 대한 실험적 연구 및 제도적 관리에 관한 제언)

  • Kang, Jung Ki;Choi, Don Mook
    • Fire Science and Engineering
    • /
    • v.34 no.3
    • /
    • pp.141-149
    • /
    • 2020
  • The Korea Industrial Standards (KS) stipulates methods and test procedures for measuring the horizontal combustibility of cellular plastics exposed to small flames (KS M ISO 9772:2018) and recommendations regarding the magnetic digestion of extruded polystyrene insulation (XPS) for measurement results (KS M 3808:2020). Although products that are certified to conform to KS standards must have burning characteristics (self-extinguishing), they are incinerated and spread by welds at construction sites, causing significant human and property damages. In this study, XPS produced by five companies, certified by KS, and sold in the market were purchased and tested for ignition and diffusion caused by a weld bullion at a construction site. The results showed that the five products had differences in performance. Three out of the five products were found to be self-saturated, but the other two were easily ignited and diffused, making it difficult for them to be self-extinguishing. Based on the result of this experimental investigation in line with the KS regulations, all the three types of products, including two types of products that were incinerated through weld defects, were found to be non-self-extinguishing, as specified in KS M 3808.

Evaluation of the Burning Properties of Various Carpet Samples by using the Cone Calorimeter and Gas Toxicity Test (콘칼로리미터와 가스유해성 시험법을 이용한 카페트류의 연소특성 평가)

  • Lee, Bong-Woo;Kwon, Seong-Pil;Lee, Jang-Won;Lee, Byoung-Ho;Kim, Hee-Soo;Kim, Hyun-Joong
    • Fire Science and Engineering
    • /
    • v.23 no.6
    • /
    • pp.1-9
    • /
    • 2009
  • In this study, the burning behaviours of five different kinds of carpet samples covered with nylon, PP (polypropylene), PTT (poly(trimethylene terephthalate)), wool fabric and NW (nylon and wool) were evaluated by using the cone calorimeter having a radiant flux of 50kW/$m^2$. And the combustion gas toxicity was evaluated according to KS F 2271 test method. As a result of the cone calorimeter test (KS F ISO 5660-1), nylon carpet samples were ignited most easily. In ignition ability or initial flammability, NW carpet samples showed the highest value. In heat release rate (HRR), fire intensity, PP carpet samples were larger than any other samples. Nylon carpet samples were the highest smoke production rate, while N/W carpet samples the lowest. The following were in mass loss rates: NW > wool > nylon > PP > PTT. CO (carbon monoxide) was one of the most toxic gases released from the combustion. PTT carpet samples gave rise to the highest CO concentration, while NW carpet samples the lowest. In addition, PP carpet samples caused the highest $CO_2$ (carbon dioxide) concentration, while NW carpet samples the lowest. Toxicity of the gas produced from carpet samples was determined by the mouse stop motion, and it resulted in the fact that the combustion gas of PTT carpet samples was more toxic than that of any other samples.

Study on the Shortening Effect of the Egress Travel Time Based on an Escape Scenarios by Using Shuttle Elevators for Lotte Tall Building's Evacuation Plan (초고층건물 피난계획시 피난용 엘리베이터 이용에 의한 피난소요시간의 단축효과 연구)

  • Park, Hyung-Joo;Lee, Young-Jae
    • Fire Science and Engineering
    • /
    • v.32 no.6
    • /
    • pp.46-54
    • /
    • 2018
  • A total of 19 elevators for evacuation were installed in the Lotte World Tower and it is planned to operate the shuttle using the manual key from five refuge floors to the 1st floor in an emergency. In the event of a fire or other disaster, it is necessary to conduct intensive analysis to determine how much RSET reduction could be achieved using the evacuation elevator compared to the existing evacuation plans. When the optimal transportation sharing ratio by the evacuation elevators was 40% at the Lotte World Tower, the RSET of the evacuation scenario in parallel with the elevators in the entire building was calculated to be 1 hour and 2 minutes. The RSET of a conventional evacuation scenario (Walking along the stairs without using the elevators) was calculated to be 1 hour 29 minutes, therefore, the former evacuation scenario were found to have a shortening effect of approximately 27 minutes compared to the latter. On the other hand, to maintain this effect, each part of the evacuation route using the elevator must have the capability to protect the evacuee from any hazards caused by fires, such as smoke, flame, and radiant heat during the evacuation. Moreover, the evacuation route should be continuous from the residence position of the elevator user to the final evacuation site, and be recognized easily.

Numerical analysis study on the concentration change at hydrogen gas release in semi-closed space (수치해석을 통한 반밀폐공간 내 수소가스 누출 시 농도변화에 관한 연구)

  • Baek, Doo-San;Kim, Hyo-Gyu;Park, Jin-Yuk;Yoo, Yong-Ho
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.23 no.1
    • /
    • pp.25-36
    • /
    • 2021
  • Hydrogen in hydrogen-electric vehicles has a wide range of combustion and explosion ranges, and is a combustible gas with a very fast flame propagation speed, so it has the risk of leakage, diffusion, ignition, and explosion. The fuel tank has a Thermally active Pressure Relief Device (TPRD) to reduce the risk of explosion and other explosions, and in the event of an accident, hydrogen inside the tank is released outside before an explosion or fire occurs. However, if an accident occurs in a semi-closed space such as an underground parking lot, the flow of air flow is smaller than the open space, which can cause the concentration of hydrogen gas emitted from the TPRD to accumulate above the explosion limit. Therefore, in this study, the leakage rate and concentration of hydrogen over time were analyzed according to the diameter of the nozzle of the TPRD. The diameter of the nozzle was considered to be 1 mm, 2.5 mm and 5 mm, and ccording to the diameter of the nozzle, the concentration of hydrogen in the underground parking lot increases in a faster time with the diameter of the nozzle, and the maximum value is also analyzed to be larger with the diameter of the nozzle. In underground parking lots where air currents are stagnant, hydrogen concentrations above LFL (Lowe Flammability Limit) were analyzed to be distributed around the nozzle, and it was analyzed that they did not exceed UFL (Upper Flammability Limit).

The Characteristics of Firefighter Burn Injuries in a Burn Center: A Retrospective Epidemiological Study (소방관 화상 환자의 화상수상특징에 대한 1개 화상전문병원에서의 예비조사)

  • Kim, Hyeongtae;Kang, Gu Hyun;Jang, Yong Soo;Kim, Wonhee;Choi, Hyun Young;Kim, Jae Guk;Kim, Minji;You, Ki Cheol;Kim, Dohern;Yim, Haejun;Bang, Sung Hwan;Lee, Chang Sub
    • Journal of the Korean Burn Society
    • /
    • v.19 no.1
    • /
    • pp.12-15
    • /
    • 2016
  • Purpose: Firefighters are vulnerable to burn injury during firefighting. In extensive fires, conducted heat and radiant heat can cause burn injury even though firefighters are not directly exposed to fire. There has been increasing interest in the health problems of firefighters considerably since Hongje-dong fire of 2001, which claimed the lives of six fireman. However, there have been no studies done on the characteristics of firefighter burn injuries in South Korea. Therefore, we investigated the characteristics of firefighter burn injuries in a burn center. Methods: A retrospective, single-center research was performed between Jan 2006 to Dec 2015. 24 firefighters came to the burn center. The electronic medical records of patients were reviewed. Results: Flame burns (87.5%) were the major cause of burn in firefighter. All the patients suffered second-degree or third-degree burns. Mean burn size was 6.1±6.7%. 22 of 24 patients were hospitalized and 2 of 22 hospitalized patients admitted to intensive care unit. Mean length of hospitalization was 29.1±23.7 days and mean length of intensive care unit hospitalization was 6.0±1.4 days. The face was the site most commonly burned, representing 25.8% of injuries. The hand/wrist, upper extremity, and neck were the next largest groups, with 19.4, 12.9, 11.3% of the injuries, respectively. Conclusion: Firefighter burn injuries occur to predictable anatomic sites with common injury patterns. The burn size was small but, admitted patients need about 30 days of hospitalization.

A Study on the Confirmation of non-flammabikity of the Cast Resin Mold Transformer in Subway Substation (지하철 변전실용 진공주형형 몰드변압기의 난연성 확인에 관한 연구)

  • 정용기;장성규;곽희로
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.12 no.2
    • /
    • pp.99-107
    • /
    • 1998
  • This dissertationhas confirmed the non-flam mability of cast mold transformer that is increasingly used lately. As a research progress, the investigation has been performed on the installation status and each line of the subway system which have the most mold transformer accidents, and the impediment status of the transformer for rectifier and the high-voltage distribution transformer per each manufacturer. Then, a high voltage mold of the actual mold transformer has been installed in the horiwntal heating furnace and the heat has been applied by the standard heating temperature curve of KSF 2257(Fireproof testing meth od of the construction structures: 1993). Accordingly, the combustibility of the mold transformer based on the test results has been found that 78 minutes has been required for the complete burning per the KSF 2257 combustion test curve and that, after stopping the heat application of the horizontal furnace after ignition, the flame progress has not been made but shown as the self-extinguishing characteristics when the flame progress has been checked. Thus, the non-flammability and self-extinguishability of the mold transformer have been confirmed. The result of this dissertation has indicated that the accident involving mold transformer has been progressed and expanded by the dielectric breakdown or void due to the crack in the mold rather than a fire accident caused by a short-circuit or an overload.r an overload.

  • PDF

Combustion Characteristics of Bamboo Charcoal Boards (대나무숯 성형보드의 연소특성)

  • Park, Sang-Bum;Park, Joo-Saeng
    • Journal of the Korean Wood Science and Technology
    • /
    • v.40 no.1
    • /
    • pp.19-25
    • /
    • 2012
  • The fire retardant bamboo charcoal (BC) boards were manufactured for interior building materials in this study, The BC boards were manufactured by mixing and pressing of the bamboo charcoal, expanded vermiculite, and inorganic binder. The combustion behaviors of the BC boards were investigated using a cone calorimeter at an incident heat flux of 50 kW/$m^2$. Three building materials (plywood, BC board of Japan, and gypsum board) were used to observe the burning behaviors of weight loss, total heat release rate, and maximum heat release rate. Surface test and toxicity evaluation of the BC board were also conducted. The weight loss of the BC board (12.0%) was lower than the nonflammable gypsum board (15.6%) after burning of 10 min. Total heat release of the BC was 3 MJ/$m^2$ (KS standard 8 MJ/$m^2$) and total heat release rate of the BC was 20 kW/$m^2$ (KS standard 200 kW/$m^2$). Therefore, the BC boards were adjustable for the third-grade flame retardant building materials. External appearance change and mouse toxicity were not found in the BC boards after the combustion test.

Studies on Press Drying of Fire-Retardant Treated Plywood (내화처리합판(耐火處理合板)의 열판건조(熱板乾燥)에 관(關)한 연구(硏究))

  • Kim, Jong Man
    • Journal of Korean Society of Forest Science
    • /
    • v.56 no.1
    • /
    • pp.1-25
    • /
    • 1982
  • Plywood used for construction as a decorative inner material is inflammable and can cause fire accidents. causing destruction of human life and property. To diminish the fire disaster, fire retardant plywood is indeed required. In the methods of manufacturing the fire retardant plywood, a soaking method is occasionally used. However after soaking plywood into fire retardant chemical solutions redrying of soaked plywood is of the utmost importance. In this study 3.5mm and 5.0mm thickness plywoods were selected for fire retardant treatment. Treating solutions were prepared for 20% dilute solutions of ammonium sulfate, monoammonium phosphate, diammonium phosphate, borax-boric acid minalith, and water solution, 1-, 3-, 6-, and 9 hour-soaking treatments in borax-boric acid and minalith, and 6- and 9 hours in the other chemicals were applied and after the treatment hot drying was applied to treated plywoods at $90^{\circ}C$, $120^{\circ}C$ and $150^{\circ}C$ of press temperature. Drying rates, drying curves, water absorption rates of fire retardant chemicals, weight per volume and fire retardant degree of plywood were investigated. The results may be summarized as follows: 1) In the 9 hours-soaking treatment of fire retardants by hot and cold bath method, the chemical retentions of 3.5mm thickness plywood could be attained within the range ($1.125-2.25kg/(30cm)^3$) of minimum retention specification as follows: $1.353kg/(30cm)^3$ in monoammonium phosphate, $1.331kg/(30cm)^3$ in diammonium phosphate, $1.263kg/(30cm)^3$ in ammonium sulfate, $1.226kg/(30cm)^3$ in borax-boric acid. But the chemical retention, $0.906kg/(30cm)^3$, in minalith could not be attained within the range of minimum retention specification. And also in case of 5.0mm thickness plywood, chemical retentions, as $1.356kg/(30cm)^3$ and $1.166kg/(30cm)^3$ respectively, of ammonium sulfate and diammonium phosphate could be attained within the range minimum retention specification, but the other fire retardant chemicals could not. 2) In the 6- and - hours-soaking treatments of 3.5mm and 5.0mm thickness plywood, the drying curve sloped of chemical treated plywood was smaller than that of water treated. The drying rate related to thickness of treated plywood, was about three times as fast in 3.5mm thickness plywood compared with 5.0mm thickness plywood. 3) In the treatment at $120^{\circ}C$ of hot platen temperature, the drying rates of chemical-treated plywood showed the highest quantity in diammonium phosphate of 3.5mm and 5.0mm thickness plywood. But the drying rate of water treated plywood was highest during the 6- and 9 hours-soaking treatments. 4) The drying rate remarkably increased with proportion to increase of the platen temperature, and the values were respectively 1.23%/min., 6.54%/min., 25.75%/min. in hot platen temperature of $90^{\circ}C$, $120^{\circ}C$, $150^{\circ}C$ in 3.5mm thickness plywood and 0.55%.min., 2.49%/min., 8.19%/min. in hot platen temperature of $90^{\circ}C$, $120^{\circ}C$, $150^{\circ}C$ in 5.0mm thickness plywood. 5) In the fire retardant degree of chemical treated plywood, the loss in weight was the smallest in diammonium phosphate, next was in monoammonium phosphate and ammonium sulfate, and the greatest was in borax-boric acid and minalith. And the fire-retardant effect in burning time, flame-exhausted time and carbonized area were greatest in diammouniun phosphate, next were in monoammonium phosphate and ammonium sulfate, and the weakest were in borax-boric acid and minalith.

  • PDF

Studies on Fire-Retardant-Treatment and Press Drying of Plywood (합판(合板)의 내화처리(耐火處理)와 열판건조(熱板乾燥)에 관(關)한 연구(硏究))

  • Lee, Phil-Woo;Kim, Jong-Man
    • Journal of the Korean Wood Science and Technology
    • /
    • v.10 no.1
    • /
    • pp.5-37
    • /
    • 1982
  • Plywood used for construction as a decorative inner material is inflammable to bring large fire accidents and burn out human life and their properties. To diminish the fire disaster, fire retardant plywood has been required indeed. In the methods of manufacturing the fire retardant plywood the soaking method is occasionally used. However after soaking plywood into fire retardant chemical solutions, redrying of soaked plywood is the most important. In this study, 3.5mm thin and 5.0mm thick plywoods were selected for fire retardant treatment. Treating solutions were prepared for 20% dilute solutions of ammonium sulfate, monoammonium phosphate, diammonium phosphate, borax-boric acid and minalith, and water solution. 1-, 3-, 6-, and 9 hour-soaking treatments were applied and after treatments hot plate drying was applied to those treated plywoods at $90^{\circ}C$, $120^{\circ}C$ and $150^{\circ}C$, of press temperature. Drying rates, drying curves, water absorption rates of fire retardant chemicals, weight per volume and fire retardant degree of plywood were investigated. The results may be summarized as follows: 1. The plywoods treated with ammonium sulfate, monoammonium phosphate and diammonium phosphate and diammonium phosphate showed increase of chemical absorption rate with proportion to increase of treating time, but not in case of the plywood treated with borax-boric acid and minalith. 2. In the treatment of definite time, the absorption rate per unit of volume of plywood showed higher in thin plywood (thickness of 3.5mm) than in thick plywood (thickness of 5.0mm). In both thin and thick plywoods, the highest absorption rate was observed in 9 hour-treatment of ammonium sulfate. The value was 1.353kg/$(30cm)^3$ in thin plywood and 1.356kg/$(30cm)^3$ in thick plywood. 3. The volume per weight of plywood after chemical treatment increased remarkably and. after hot plate drying, the values were to a little extent higher than before chemical treatment. 4. The swelling rates of thickness in chemical-treated plywoods increased similarly with that of water-treated plywood in 1- and 3 hour-treatment of both thin and thick plywoods. But in 6- and 9 hour-treatment, the greater increased value showed in water-treated ply wood than any other chemical, especially in thick plywood. 5. The shrinkage rates after hot plate drying showed the same tendency as the swelling rate, and the rate showed the increasing tendency with proportion to increase of treating time in thick plywood of both chemical and water treatments. 6. Among drying curves, the curves of water-treated plywood placed more highly than chemical-treated plywood without-relation to thickness in 6- and 9 hour-treatment except in 1- and 3 hour-treatment. 7. The drying rate related to thickness of treated plywood, was twice above in thin plywood compared with thick plywood. 8. The drying rate remarkably increased with proportion to increase of the plate temperature and, the values were respectively 1.226%/min., 6.540%/min., 25.752%/min. in hot plate temperature of $90^{\circ}C$, $120^{\circ}C$, $150^{\circ}C$ in thin plywood and 0.550%/min., 2.490%/min, 8.187%/min, in hot plate temperature of $90^{\circ}C$, $120^{\circ}C$, $150^{\circ}C$ in thick plywood. 9. In the treatment at $120^{\circ}C$ of hot plate temperature, the drying rates of chemical-treated plywood showed the highest value in monoammonium phosphate of thin plywood and in diammonium phosphate of thick plywood. But the drying rate of water-treated plywood was highest in 6- and 9 hour-treatment. 10. The fire retardant degree of chemical-treated plywood was higher than that of the untreated plywood as shown in loss of weight, burning time, flame-exhausted time and carbonized area. 11. The fire-retardant effect among fire retardant chemicals were the greatest in diammonium phosphate, the next were in monoammonium phosphate and ammonium sulfate, and the weakest were in borax-boric and minalith.

  • PDF