Application of Spray Pyrolysis Process for Production of Ultra Pure and Fine Powder. (고순도 초미립 분체제조를 위한 분무열분해법의 응용)

  • Yu, Jae-Keun;Park, Hee-Beom;Park, Joo-Ill;Han, Jung-Soo;Han, Jin-A;Nam, Yung-Hyeon
    • Proceedings of the KAIS Fall Conference
    • /
    • 2000.10a
    • /
    • pp.39-41
    • /
    • 2000
  • Newly modified spray Pyrolysis system was developed to Produce ultra Pure and fine Powder by spray Pyrolysis Process. In this system, raw material solution was effectively atomized and sprayed into the reaction furnace. Also, thermal decomposition process fully completed in the three zone reaction furnace, and produced powder was effectively collected. A technology to reduce impurities in complex acid solution below 20ppm was also developed. The characteristics of produced powder were studied by changing the reaction conditions such as reaction temperature, the injection velocity of the solution and air, nozzle tip size and concentration of solution. The morphology of powder had spherical shape under the most experimental conditions, and the composition and the particle size distribution were almost uniform. Under the most experimental conditions average particle size of most produced powder was below 100nm.

Preparation of $BaTiO_3$ Fine Powders by Spray Pyrolysis Using Ultrasonic Atomization Technique (초음파 분무 열분해법에 의한 $BaTiO_3$ 미분말의 제조)

  • 조형진;이종흔;박순자
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.11
    • /
    • pp.851-858
    • /
    • 1991
  • Spherical fine BaTiO3 powders with an average diameter of 0.3${\mu}{\textrm}{m}$ to 0.9${\mu}{\textrm}{m}$ are prepared at 100$0^{\circ}C$ by the ultrasonic spray pyrolysis of solutions containing Ba(NO3)2 and TiCl4. Experimental variables are adjusted to produce BaTiO3 powders and its effect on the phase, the size and the morphology of the particles are investigated by XRD, SEM, TEM. Each particle consists of small primary particles and has a hollow around its center. The dependence of particle diameters on the concentrations of source solutions indicates that metal salt precursors are dried to precipitate solid particles and decompose to form BaTiO3 phase without gas phase reactions.

  • PDF

Preparation of Ultrafine $SnO_2$ Powders by Spray-ICP Technique

  • Kim, Jung-Hwan;Kim, Young-Do;Shin, Kun-Chul;Park, Jong-Hyun
    • Proceedings of the Korea Association of Crystal Growth Conference
    • /
    • 1998.06a
    • /
    • pp.65-70
    • /
    • 1998
  • The Spray-ICP technique uses the ICP(Inductively Coupled Plasma) of ultra-high temperature which is produced by r.f power. The ICP is well-kwown as a clean heat source for the preparation of pure ceramic particles because the ICP is a electrodeless-thermal plasma without contamination. In this study,{{{{ { SnO}_{2 } }}}} particles were sythesized from metal salt solution by Spray-ICP technique. The effects of concentration of solution, collecting location of powders were investicated. The prepared {{{{ { SnO}_{2 } }}}} particles from each concentration of solution had same crystalline phase(tetragonal {{{{ { SnO}_{2 } }}}}) a nd the mean size decreased in proportion to the increase of solution concentration. Each {{{{ { SnO}_{2 } }}}} p owders collector in reactor and electrostatic collector had same crystalline phase and morphologies. The mean size of {{{{ { SnO}_{2 } }}}} p articles prepared by Spray-ICP technique was below 30nm.

  • PDF

Preparation of Multicomponent Ceramic Powders by Ultrasonic Spray Pyrolysis

  • Youn, Jeong-Han;Chung, Byung-Joo;Sim, Soo-Man
    • The Korean Journal of Ceramics
    • /
    • v.6 no.1
    • /
    • pp.58-63
    • /
    • 2000
  • The preparation of Y-doped $SrZrO_3$powder by ultrasonic spray pyrolysis was investigated as a representative system, in order to produce fine, single phase multicomponent oxide powders. A precursor solution containing metal nitrates, citric acid and ethylene glycol was atomized glycol was atomized with an ultrasonic spray nozzle. Gel particles formed by organic functional groups were pyrolyzed and subsequently calcined at $800^{\circ}C$ to obtain well-crystallized, single perovskite phase. Most of large particles exhibited macroscopic pores and weak agglomeration between primary particles. However, strong agglomeration was observed in the surfaces of large particles. The effect of the microstructures of these particles on size reduction to submicron particles was described.

  • PDF

Atomization Characteristics of Intermittent Multi-Hole Diesel Spray Using Time-Resolved PDPA Data

  • Lee, Jeekuen;Shinjae Kang;Park, Byungjoon
    • Journal of Mechanical Science and Technology
    • /
    • v.17 no.5
    • /
    • pp.766-775
    • /
    • 2003
  • The intermittent spray characteristics of a multi-hole diesel nozzle with a 2-spring nozzle holder were investigated experimentally. Without changing the total orifice exit area, the hole number of the multi-hole nozzle varied from 3 (d$\_$n/=0.42 mm) to 5 (d$\_$n/=0.32 mm). The time-resolved droplet diameters of the spray including the SMD (Saute. mean diameter) and the AMD (arithmetic mean diameter), injected intormittently from the multi-hole nozzles into still ambient ai., were measured by using a 2-D PDPA (phase Doppler particle analyze.). The 5-hole nozzle spray shows the smaller spray cone angle, the decreased SMD distributions and the small difference between the SMD and the AMD, compared with that of the 3-hole nozzle spray. From the SMD distributions with the radial distance, the spray structure can be classified into the three regions : (a) the inner region showing the high SMD distribution , (b) the mixing flow region where the shea. flow structure would be constructed : and (c) the outer region formed through the disintegration processes of the spray inner region and composed of fine droplets. Through the SMD distributions along the spray centerline, it reveals that the SMD decreases rapidly after showing the maximum value in the vicinity of the nozzle tip. The SMD remains the constant value near the Z/d$\_$n/=166 and 156.3 for the 3-hole and 5-hole nozzles, which illustrate that the disintegration processes of the 5-hole nozzle spray proceed more rapidly than that of the 3-hole nozzle spray.

Fine Size YAG:Tb Phosphor Particles Prepared by Spray Pyrolysis (분무 열분해 공정에 의해 합성된 미세 YAG:Tb 형광체)

  • Lee, Hyo Jin;Hong, Seung Kwon;Jung, Dae Soo;Kang, Yun Chan;Jung, Kyeong Youl
    • Korean Chemical Engineering Research
    • /
    • v.43 no.3
    • /
    • pp.407-411
    • /
    • 2005
  • YAG:Tb($Y_3Al_5O_{12}:Tb$) phosphor particles were prepared by spray pyrolysis from spray solution containing various types of flux materials. The effects of type of flux, organic material and post-treatment temperature on the characteristics of morphology, crystallinity and photoluminescence of YAG:Tb phosphor particles were investigated. Citric acid and ethylene glycol used as organic additive improved the photoluminescence intensity of the YAG:Tb phosphor particles without destruction of the morphology after post-treatment at high temperature. However, the spherical shape of the precursor particles obtained by spray pyrolysis from spray solution containing high amount of flux material disappeared after post-treatment at $1300^{\circ}C$. YAG:Tb phosphor particles prepared from spray solution containing lithium carbonate flux had fine size and regular morphology after post-treatment. Lithium carbonate used as flux material was also efficient in improvement of the photoluminescence intensity of the YAG:Tb phosphor particles. The optimum photoluminescence intensity of the YAG:Tb phosphor particles prepared from spray solution containing lithium carbonate flux was 189% of that of the phosphor particles prepared from spray solution without flux material.

Ultrasonic Spray Nozzle System with Piezoelectric Device for Chemicals Dispersion (압전체를 이용한 약품 분사용 초음파 분사 노즐 시스템)

  • 고재석;김용현;김형수;조순행;최승철
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.10 no.4
    • /
    • pp.65-71
    • /
    • 2003
  • A new type of ultrasonic spray nozzle was fabricated employing a piezoelectric device. The spray nozzle was designed to disperse chemicals in a water treatment mixing tank. The piezoelectric properties in ultrasonic spray nozzles were optimized to improve the dispersion of chemicals. The piezoelectrics were packaged in an aluminum case with silicone resin for the aqueous solution proof packaging. Chemicals were dispersed with high efficiency and the chemicals consumption was reduced by the ultrasonic fine particle spraying. The concentration of Escherichia coli in mixing tank was decreased remarkably using ultrasonic spray nozzle dispersion compared to the conventional methods.

  • PDF

Thermal Characteristics of Foams and Discharge of Fire-Protection Foam Spray Nozzle (폼 분무 노즐 방사 분포 및 폼의 열적 특성 연구)

  • Kim, Hong-Sik;Kim, Youn-Jea
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.29 no.1 s.232
    • /
    • pp.151-158
    • /
    • 2005
  • A characteristic of discharge for a foam spray nozzle with various parameters was investigated. The discharge patterns from a fire foam spray nozzle are important to evenly spray over a maximum possible floor area. Two parameters of a foam spray nozzle were chosen, and compared with those from the standard one. Also, in order to evaluate the performance of discharged foam agents used to protect structures from heat and fire damages, the thermal characteristics of fire-protection foams were experimentally investigated. A simple repeatable test for fire-protection foams subjected to fire radiation was developed. This test involves foam generation equipment, a fire source for heat generation, and data acquisition techniques. Results show that the bubble size of foam is increased by large inside diameter of orifice or closed air hole, but phenomenon of discharge angle and expansion ratio is opposite. For the case of the open air hole, liquid film of a circular cone discharges with formation, growth, split and fine grain. In case of the closed air hole, a pillar of foam solution discharges with that. Though the temperature gradient in the foam increases with increased foam expansion ratio. it is not change with increased intensity of heat flux.

Intralesional steroid infusion using a spray tube to prevent stenosis after endoscopic submucosal dissection of esophageal cancer

  • Atsushi Goto;Takeshi Okamoto;Ryo Ogawa;Kouichi Hamabe;Shinichi Hashimoto;Jun Nishikawa;Taro Takami
    • Clinical Endoscopy
    • /
    • v.55 no.4
    • /
    • pp.520-524
    • /
    • 2022
  • Background/Aims: Intralesional steroid injections have been administered as prophylaxis for stenosis after esophageal endoscopic submucosal dissection. However, this method carries a risk of potential complications such as perforation because a fine needle is used to directly puncture the postoperative ulcer. We devised a new method of steroid intralesional infusion using a spray tube and evaluated its efficacy and safety. Methods: Intralesional steroid infusion using a spray tube was performed on 27 patients who underwent endoscopic submucosal dissection for superficial esophageal cancer with three-quarters or more of the lumen circumference resected. The presence or absence of stenosis, complications, and the number of endoscopic balloon dilations (EBDs) performed were evaluated after treatment. Results: Although stenosis was not observed in 22 of the 27 patients, five patients had stenosis and dysphagia requiring EBD. The stenosis in these five patients was relieved after four EBDs. No complications related to intralesional steroid infusion using the spray tube were observed. Conclusions: Intralesional steroid infusion using a spray tube is a simple and safe technique that is adequately effective in preventing stenosis (clinical trial number, UMIN000037567).

Preparation of Spherical (Zr, Sn)TiO4 Powders by Ultrasonic Spray Pyrolysis (초음파 분무 열분해법에 의한 $(Zr, SN)TiO_4$ 구형 미분말의 합성)

  • 조서용;이종흔;김명철;박순자
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.5
    • /
    • pp.465-470
    • /
    • 1994
  • Fine, spherical (Zr, SN)TiO4 powders were prepared from the aqueous solution of metal chlorides by ultrasonic spray pyrolysis. Single phase (Zr, SN)TiO4 powders could be obtained above $700^{\circ}C$ (=temperature of the reactor) and all powders exhibited sizes in the range of 0.1 to 2.0 ${\mu}{\textrm}{m}$ and a narrow size distribution. The sintering properties of the prepared powders were better than those of the powders from solid-state reaction.

  • PDF