Shehab, Hamdy K.;Eisa, Ahmed S.;El-Awady, Kareem A.
International Journal of Concrete Structures and Materials
/
제11권2호
/
pp.327-341
/
2017
Openings in slabs are usually required for many different applications such as aeriation ducts and air conditioning. Opening in concrete slabs due to cutouts significantly decrease the member stiffness. There are different techniques to strengthen slabs with opening cutouts. This study presents experimental and numerical investigations on the use of Carbon Fiber Reinforced Polymers (CFRP) as strengthening material to strengthen and restore the load carrying capacity of R.C. slabs after having cutout in the hogging moment region. The experimental program consisted of testing five (oneway spanning R.C. flat slabs) with overhang. All slabs were prismatic, rectangular in cross-section and nominally 2000 mm long, 1000 mm width, and 100 mm thickness with a clear span (distance between supports) of 1200 mm and the overhang length is 700 mm. All slabs were loaded up to 30 kN (45% of ultimate load for reference slab, before yielding of the longitudinal reinforcement), then the load was kept constant during cutting concrete and steel bars (producing cut out). After that operation, slabs were loaded till failure. An analytical study using finite element analysis (FEA) is performed using the commercial software ANSYS. The FEA has been validated and calibrated using the experimental results. The FE model was found to be in a good agreement with the experimental results. The investigated key parameters were slab aspect ratio for the opening ratios of [1:1, 2:1], CFRP layers and the laminates widths, positions for cutouts and the CFRP configurations around cutouts.
Upgrading or strengthening of existing reinforced concrete (RC) infrastructure is an emerging demand nowadays. Near Surface Mounted (NSM) technique is very promising approach for flexural strengthening of RC members. However, premature failure such as concrete cover separation failure have been a main concern in utilizing this technique. In this study, U-wrap end anchorage with carbon fiber reinforced polymer (CFRP) fabrics is proposed to eliminate the concrete cover separation failure. Experimental programs were conducted to the consequence of U-wrap end anchorage on the flexurally strengthened RC beams with NSM-steel. A total of eight RC rectangular beam specimens were tested. One specimen was kept unstrengthened as a reference; three specimens were strengthened with NSM-steel bars and the remaining four specimens were strengthened with NSM-steel bars and U-wrap end anchorage using CFRP fabrics. A 3D non-linear finite element model (FEM) was developed to simulate the flexural response of the tested specimens. It is revealed that NSM-steel (with and without end-anchors) significantly improved the flexural strength; moreover decreased deflection and strains compared with reference specimen. Furthermore, NSM-steel with end anchorage strengthened specimens revealed the greater flexural strength and improve failure modes (premature to flexure) compared with the NSM-steel without end anchorage specimens. The results also ensured that the U-wrap end anchorage completely eliminate the concrete cover separation failure.
본 논문에서는 비접촉 손상검출기법으로 관심의 대상이 되고 있는 열화상 기법의 기본 원리, 활용 예, 제한 사항 등을 국내외 주요 연구성과를 분석하고 정리하였다. 콘크리트 구조물의 내부 결함 진단, 내부 철근 부식 측정과 콘크리트 구조물 표면과 섬유 보강 시트 사이의 비부착 검출, 포장도로의 표면 결함 검출, 오래된 건물의 표면 누수 측정, 철도 트랙 자갈의 상태 측정 등을 최근 연구결과 중심으로 광범위하게 검토하였고 최근에 보고된 실험결과도 제시하였다. 검토 결과, 열화상 기법은 광범위한 형태의 토목 구조물의 넓은 표면을 빠르게 정성적으로 검사할 수 있는 장점을 가지고 있는 것으로 확인되었다. 반면, 정량적 기법은 주변 온도 등 환경 요인에 민감하게 영향을 받는 것으로 판단되었으며, 다른 정밀계측장비와 혼용시 좋은 성과를 기대할 수 있을 것으로 예측된다.
Recently, fiber reinforced polymers(FRP) composite materials are used extensively in the rehabilitation of concrete structural members. A main application is to wrap beams and columns using the continuous fibers sheets to improve their strength and ductility. The corner chamfering affects significantly the performance of the continuous fibers sheets, and could lead to environmental problem with waste and dust. The main purpose of this paper is to verify the effect of corner conditions on the strength of the continuous fiber sheets, and to introduce new attached components which can avoid environmental problem. A total of 15 specimens were tested and carefully checked for three types of continuous fiber sheets(carbon, glass, and aramid) and three types of corner conditions(non-chamfering, chamfering, and device attaching). It is proved that the devices proposed in this research have some capabilities to use for RC member. But additional research will be needed for commercializing.
혹독한 자연환경하에서의 구조물의 내구성이 주요한 관심사도 대두되면서 건설분야에서 섬유강화폴리머의 사용이 점차 증가하고 있는 추세이다. 본 연구에서는 FRP bar를 휨부재의 휨보강근으로서의 적용가능성을 평가하기 위하여 휨실험을 수행하였다. 탄소섬유, 유리섬유 및 탄소와 유리섬유를 혼합한 hybrid 섬유 보강근을 사용하여 보강량을 변화시킨 12개의 실험체를 제작하여 실험을 수행하였으며, 그결과는 파괴형태, 모멘트-변위, 휨강도, 연성지수 및 단면에서의 변형율분포 등에 대하여 분석하였다. 실험결과는 ACI 기준에 제시된 모델과 비교하였으며, 전체적으로 보의 휨강도는 강도설계이론에 의한 결과와 거의 유사한 것으로 나타났다. 그러나 처짐의 경우에는 유리섬유의 경우는 이론이 과대평가 되었으며, 탄소섬유는 과소평가되는 것으로 나타났다.
최근에 복합재료는 콘크리트, 집성보와 같은 기존의 구조재를 보강하여 성능을 향상시킬 목적으로 적용되고 있다. 특히, 대규모의 집성보 구조물은 춤이 큰 부재를 필요로 하는데 섬유보강판을 이용하여 보의 상하부를 보강하면 춤을 크게 하지 않고도 보의 강도와 강성을 증가시킬 수 있다. 본 연구에서는 집성보에 유리섬유보강 플라스틱판(GFRP)을 붙여 스팬 중앙에 집중하중을 가한 휨실험을 수행하였고 실험결과를 층간이론을 이용한 수치해석법과 비교하였다.
섬유복합재료의 우수한 인장 성능은 섬유가 매트릭스의 균열 면에서 가교작용을 함으로써 발현되기 때문에 섬유의 분산성이 복합재료의 성능에 결정적인 영향을 미치게 된다. 그러나 PVA(Polyvinyl alcohol) 섬유를 보강 섬유로 사용하는 섬유복합재료의 경우 PVA 섬유와 매트릭스 사이의 낮은 명암비와 PVA의 비전도성 특징으로 인하여 섬유의 위치 및 분포 특성을 정량적으로 평가히는 방법은 연구가 미흡한 실정이다. 이 연구에서는 PVA 섬유를 보강 섬유로 사용하는 섬유 복합재료의 섬유 분포 특성 등을 평가할 때 가장 중요한 과정인 섬유의 검출에 대하여 검출 성능을 향상 시킬 수 있는 알고리즘을 제시하였다. 제안한 알고리즘은 형광 현미경을 사용하여 얻은 섬유 이미지를 유형별로 분류하고, 분류된 분류된 섬유 이미지의 특성에 따라 분수령 알고리즘(watershed algorithm)과 형태학적 재구성(morphological reconstruction)을 이용하여 보다 정확히 섬유를 검출하는 과정으로 구성된다. 이 과정에서 섬유 이미지를 총 5가지 유형으로 분류하였으며, 인공신경회로망을 분류기로 구축하였다. 또한 구축한 분류기를 통해 분류된 5가지 섬유 이미지 유형 중에서 잘못 검출된 섬유이미지를 분수령 알고리즘과 형태학적 재구성을 통하여 섬유를 정확히 검출할 수 있는 기법을 제안하였다.
본 논문은 분사식 FRP의 압축 구속효과와 휨 보강 효과 및 분사식 FRP의 반발률에 대한 실험적 연구이다. 분사식 FRP란 레진과 짧게 잘려진 섬유를 고압의 공기에 의해 적용면에 분사하여 보강하는 기법이다. 분사식 FRP의 구속 및 휨 보강 효과를 알아보기 위하여 원주형 공시체와 휨 공시체를 제작하여 FRP를 분사하여 보강하였고, 보강 재료로 유리섬유와 폴리에스테르 수지를 사용하였다. 최적의 보강 조건을 알기 위해 섬유 길이, 보강 두께, 섬유 혼입비, 콘크리트 강도에 따른 실험을 실시하였고, 분사식 FRP 보강법을 섬유 매트에 의한 보강법과 비교하였다. 또한, 분사식 FRP의 반발률 역시 평가하였다. 실험을 통하여 분사식 FRP의 최적 조건을 결정하였다. 본 연구의 분사식 FRP 보강은 유리 섬유 매트에 의한 보강법 이상의 성능을 발휘하였다.
The analysis of interfacial stresses in structural component has been the subject of several investigations but it still requires more effort and studies. In this study a general three-dimensional interface element has been formulated for stress and displacement analyses in the interfacial area between two adjacent plate bending element and brick element. Interface element has 16 nodes with 5 degrees of freedom (DOF) in each node adjacent to plate bending element and 3 DOF in each node adjacent to brick element. The interface element has ability to transfer three translations from each side of interface element and two rotations in the side adjacent to the plate element. Stiffness matrix of this element was formulated and implemented in three-dimensional finite element code. Application of this element to the reinforced concrete (RC) beam strengthened with fiber reinforced polymer (FRP) including variation of deflection, slip between plate and concrete, normal and shear stresses distributions in FRP plates have been verified using experimental and numerical work of strengthened RC beams carried out by some researchers. The results show that this interface element is effective and can be used for structural component with these types of interface elements.
Strengthening of reinforced concrete (RC) members against shear that is one of the failure modes especially avoided by using carbon fiber reinforced polymer (CFRP) is widely used technique, which is studied at many experimental studies. However, conducting experimental studies are required more financial resources and laboratory facilities. In addition, along with financial resources, more time is needed in order to carry out comprehensive experimental studies. For these reasons, a verified finite element model that is tested with previous experimental studies can be used for reaching generalized results and investigating parameters that are not studied. For this purpose, previous experimental study results are used and "T" cross-sectioned RC beams strengthened with CFRP strips with insufficient shear strength are modeled by using ANSYS software. First, finite elements modeling of the previously tested RC beams are done, and then the computed results are compared with the experimental ones whether they are matched or not. As a result, the finite element model is verified. Later, analyses of the cases without any test results are done by using the verified model. Optimum CFRP strip spacing is determined with this verified finite element model, and compared with the experimental findings.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.