The Experimental Study on the Fluidity Properties of Mortar Using Basalt Fiber and High Volume Fly Ash (바잘트 섬유 및 하이볼륨 플라이애시를 사용한 모르타르의 유동특성에 관한 실험적 연구)

  • Choi, Yun-Wang;Oh, Sung-Rok;Park, Man-Seok;Choi, Byung-Keol
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.2 no.4
    • /
    • pp.345-353
    • /
    • 2014
  • This study was evaluated influence of fluidity properties according to basalt fiber and high volume fly ash in the mortar level, as part of a basic study for development of fiber reinforced concrete using basalt fiber and high volume fly ash. In the first step, it was evaluated that fluidity properties of mortar according to replacement ratio 6 level of fly ash(10, 20, 30, 40, 50 and 60mass%) and fluidity properties of mortar according to content 5 levels of SP(1.3, 1.5, 1.7, 1.9 and 2.1%) and content 5 levels of VA(0.2, 0.4, 0.6, 0.8 and 1.0%) for dispersion of the basalt fiber, in the second step, it was evaluated that fluidity properties of mortar using High-volume fly ash (50mass%) on 3 levels of basalt fiber length (6, 20 and 30mm). Results of assessment, if after a fiber mixed, it showed that viscosity agent is more effective to improve the fluidity and fiber dispersion than superplasticizer, high volume fly ash (50%) applying the mixing, due to three properties of fly ash, showed that the improved fiber dispersibility and flow improvement.

Suggestion of an Fiber Channel-Embedded IPTV STB for Optical Fiber-based IPTV Networks (광섬유 기반 IPTV 네트워크를 위한 FC 내장형 IPTV STB 제안)

  • Chung, Sung-Wook
    • The Journal of Korea Institute of Information, Electronics, and Communication Technology
    • /
    • v.10 no.3
    • /
    • pp.213-219
    • /
    • 2017
  • Recently, the Internet Protocol Television (IPTV) services have become very common, enabling various Internet-based services as well as watching TV. In the IPTV system, a Set-Top box (STB) plays a key role as a network terminal device that transmits and receives realtime multimedia contents. In addition, the IPTV networks are usually supported by broadband optical fiber-base network such as fiber-to-the-home (FTTH), However, a general IPTV STB is regarded as one of the local area network (LAN)-attached devices while sharing the bandwidth of the LAN (e.g., Ethernet). In order to overcome the limited bandwidth utilization by fully facilitating the broadband bandwidth (e.g., 1 Gbps) of the optical fiber-based network, we propose a new FC (Fiber Channel)-embedded IPTV STB which can be directly attached to the optical fiber network. Then, we verify that the impacts of the proposed FC-embedded IPTV STB by organizing the the FC-AL (Fiber Channel-Arbitration Loop) network equipped with the FC-embedded IPTV We measures the average Start-up Delay, Average Reject Ratio and the Number of Concurrent Users through extensive simulations to investigate the performances of the suggested FC-AL-based IPTV network. Surprisingly, the IPTV network architecture with the proposed FC-embedded IPTV STBs has an excellent average start-up delay of less than 10 msec, an acceptable average reject ratio of less than 3 % as well as a linear increase of the number of concurrent users when extending the architecture. This reveals that the proposed FC embedded STB has a superior impacts on the performance of the entire IPTV network by effectively utilizing the broadband bandwidth of the fiber optic-based network.

The Study on the Material Behavior of Hybrid Composites (Hybrid 열가소성 복합재료의 재료거동에 관한 연구)

  • 조현철;이중희
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2000.11a
    • /
    • pp.67-70
    • /
    • 2000
  • This study was performed to investigate the material behavior of hybrid thermoplastic composites contained glass fiber and calcium carbonate. The composite was prepared with each combination ratio of calcium carbonate, and the content of glass fiber was fixed with 10% by weight. In order to investigate the material behavior for various combination ratio, tension test, flexural test, and impact test were performed. Microscopic observation were conducted to examine the fractured surface of specimen for tension test. And the material behavior of the hybrid thermoplastic composite immersed in salt water with definite time was investigated.

  • PDF

Mechanical behavior and chloride resistance of cementitious composites with PE and steel fiber

  • Liao, Qiao;Guo, Zhen-wen;Duan, Xin-zhi;Yu, Jiang-tao;Liu, Ke-ke;Dong, Fang-yuan
    • Advances in concrete construction
    • /
    • v.12 no.6
    • /
    • pp.451-459
    • /
    • 2021
  • The mechanical behaviors and chloride resistance performance of fiber reinforced cementitious composites (FRCC) with hybrid polyethylene (PE) and steel fiber (in total 2% by volume) were investigated. Based on micro-mechanics and fracture mechanics, the reason why the tensile strain capacity of FRCC changed obviously was obtained. Besides, the effects of the total surface area of fiber in FRCC on compressive strength and chloride content were clarified. It is found that the improvement of the tensile strain capacity of FRCC with hybrid fiber is attributed to the growth of strain-hardening performance index (the ratio of complementary energy to crack tip toughness). As the total surface area of fiber related with the interfacial transition zone (ITZ) between fiber and matrix increases, compressive strength decreases obviously. Since the total surface area of fiber is small, the chloride resistance performance of FRCC with hybrid PE and steel fiber is better than that of FRCC containing only PE fiber.

Steel Fiber Reinforcement for Shear Capacity Enhancement of High Strength RC Columns (고강도 RC 기둥의 전단능력 증진을 위한 강섬유 보강)

  • 장극관;이현호;문상덕
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.05a
    • /
    • pp.469-474
    • /
    • 2002
  • This study was to define the strengthening effect of steel fibers in high strength RC columns. For this, ten specimens of columns were tested under cyclic lateral load and constant axial load. The testing parameters are steel fiber volume fraction of concrete and shear reinforcement ratio of hoop bars. Finally, the optimal content of steel fibers was evaluated as 1.0 - 1.5 % volume fraction of concrete.

  • PDF

Preparation and Properties of Thermoplastic Polyurethane Copolymers (열가소성 폴리우레탄의 합성 및 성질)

  • Heo, Jae-Ho;Kim, Eun-Yeong;Kim, Han-Do
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 1996.10a
    • /
    • pp.465-467
    • /
    • 1996
  • A series of thermoplastic polyurethane copolymers were prepared from polypropyleneglycol(PPG, MW 3000), 1,4-butanediol, Isophorone diisocyanate(IPDI) and dibutyltin dilaurate(BBT) as catalyst. Studies have been made on the effects of molar ratio of isocyanate /polyol/chain extender on the properties such as tensile and thermal properties. By varying the ration of hard to soft segments, TPU ranging from soft elastomeric polymer to relatively hard elastoplastics and be obtained. The storage modulus and glass transition temperature of TPU increased with increasing the hard segment content.

  • PDF

Analysis of Insoluble(IDF) and Soluble Dietary Fiber(SDF) Content of Koran Male College Students (한국인 남자대학생의 주요 상용식품의 불용성 및 수용성 식이섬유 함량 분석)

  • 황선희
    • Journal of Nutrition and Health
    • /
    • v.29 no.3
    • /
    • pp.278-285
    • /
    • 1996
  • Contents of insoluble(IDF), soluble dietary fiber (SDF), and total dietary fiber(TDF) of 30 foods which are consumed commonly by 80 Koeran male college students were determined by Prosky and colleagues' enzymatic-gravimentric method. Foods with highest intake frequency were rice, Kimch'i, and red pepper powder. TDF, IDF, and SDF contents of rice were 0.96, 0.59 and 0.37g/100g wet wt., respectively and tose of Kimch'i were 3.07, 2.19 and 0.88g/100g wet wt., respectively. Red pepper powder contained high amount of TDF(39.37) and IDF (33.13g/100g wet wt.). The TDF content of the 30 foods ranged from 0.70 to 39.37g/100g wet wt. Red pepper (39.37), dried laver(31.36), and dried sea mustard (37.77g/100g wet wt.) contained high amounts of TDF. The IDF content of the 30 foods ranged from 0.13 to 33.13g/100g wet wt. Red pepper powder (33.13), dried laver(15.55) and sesame(15.43g/100g wet wt.) contained high amounts of IDF. SDF of the 30 foods ranged from 0.01 to 25.66g/100g wet wt. Dried sea mustard(25.66), dried laver(15.81), coffee powder (13.17), and garlic(8.72g/100g wet wt.) were good sources of SDF. % ratio of SDF to TDF of the 30 foods was lower than 50% except soybean curd(94.27%), coffee powder (88.93%), garlic(86.17%), dried sea mustard(67.94%), and dried laver(50.41%). It is recommended to increase intake of seaweeds in order to supply TDF adn SDF properly.

  • PDF

Fabrication of silk nanofibril-embedded regenerated silk fibroin composite fiber by wet spinning

  • Chang Hyun, Bae;In Chul, Um
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.45 no.2
    • /
    • pp.70-77
    • /
    • 2022
  • Wet-spun regenerated silk fibroin (RSF) fibers have been extensively studied owing to their 1) useful properties as biomaterials, including good blood compatibility and cyto-compatibility; 2) the various methods available to control the structural characteristics and morphology of the fiber, and 3) the possibility of fabricating blended fibers and new material-embedded fibers. In this study, silk nanofibrils prepared using a new method were embedded in RSF to fabricate wet-spun silk nanofibril/RSF composite fibers. Up to 2% addition of silk nanofibril, the silk nanofibril/RSF dope solution showed slight shear thinning, and the G' and G" of the dope solution were similar. However, above 3% silk nanofibril content, the viscosity of the dope solution significantly increased. In addition, shear thinning was remarkably evident, and the G' of the dope solution was much higher than the G", indicating a very elastic state. As the silk nanofibril content was increased, the wet-spun silk nanofibril/RSF composite fiber became uneven, with a rough surface, and more beaded fibers were produced. Scanning electron microscopy observations revealed that the beaded fibers were attributed to the inhomogeneous dispersion and presence of agglomerates of the silk nanofibrils. As the silk nanofibril content and RSF concentration increased, the maximum draw ratio decreased, indicating the deterioration of the wet spinnability and post-drawing performance of silk nanofibril/RSF.

A Study on Dynamic Properties of Short-fiber Reinforced Chloroprene Rubber (단섬유 강화 Chloroprene 고무의 동적특성 연구)

  • 이동주;류상렬
    • Composites Research
    • /
    • v.17 no.3
    • /
    • pp.45-50
    • /
    • 2004
  • The dynamic properties of short-fiber reinforced chloroprene rubber with different interphase conditions and fiber contents have been studied as functions of frequency, amplitude and temperature. The loss factor(LF) slightly increased more than 1.33% of strain and the dynamic ratio(DR) rapidly decreased with increasing strain amplitude. The LF rapidly decreased with increasing frequency especially more than 50Hz. The DR showed the lower when it compared to virgin material with increasing frequency. The LF showed the maximum at $65^{\circ}$ and rapidly decreased after that temperature. The DR showed the lower when it compared with virgin rubber with increasing temperature. Generally, the better interphase condition showed the lower LF and DR at the same testing condition. Therefore, the short-fiber reinforced rubber could have the better isolation when the frequency ratio is more than $\sqrt{2}$ compared with frequency ratio less than $\sqrt{2}$.

The Studies on Hydrolysis of the Silk Fibroin by Proteolytie Enzyme, Bombyx mori II. Relation between the Fibroin Hydrolysis of Different Cocoon Layers and Physical Property of Silk Fiber (견 Fibroin의 효소분해에 관한 연구 II-견층부위별 Fibroin 분해율 차이와 견사물성과의 관계-)

  • 이용우;최병희;송기언;남중희
    • Journal of Sericultural and Entomological Science
    • /
    • v.18 no.1
    • /
    • pp.21-26
    • /
    • 1976
  • The study was carried out to investigate the variations in the fibroin hydrolysis of different cocoon shell layers, and the relationship between the hydrolysis and silk physical property. The obtained results are as follows: 1. The fibroin hydrolyzing ratio was highest at the inner layer of cocoon shell and. next in order. at the middle layer and at the outer layer. 2. The fibroin hydrolyzing ratio of abnormal cocoons was higher than normal cocoon and it was different among them, tile highest was double coroon, thin shell cocoon and perforated cocoon in order. 3. The sericin content and fibroin hydrolyzing ratio of Jam 111 and Jam 112 was higher than that of Jam 111 $\times$ Jam 112. 4. The fibroin hydroiyzing ratio of the cocoons fed with the artificial diets was increased at the inner layer. The sericin content of those lessened at the inner layer, however, it slightly increased at the most inner layer more than at the inner layer. 5. The breaking strength of the degummed silk fiber of different cocoon layers was reduced at the inner layer. The breaking Strength of abnormal silk fiber was less than that of normal silk fiber. 6. A negative correlation (r= -0.8) )was approved between fibroin hydrolyzing ratio and breaking strength of silk fiber, and the regression line was Y=-0.29x+5.07.

  • PDF