The Effect of Piezoelectric Ceramic for Properties Improvement at Electrostriction Ceramic (Actuator용 전왜재료의 특성개선을 위한 압전재료의 첨가효과)

  • 이수호;조현철;김한근;손무현;사공건
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1997.11a
    • /
    • pp.206-210
    • /
    • 1997
  • In the fields of the optics, precise machine, semiconductors, the micro-positioning actuators are required for the control of position in the submicron range. PNN-P2N-PZT ceramics were fabricated with various mole ratio of the PZT[Pb(Zr$_{1}$2//Ti$_{1}$2)O$_3$]. PNN (Pb(Ni$_{1}$3/Nb$_{2}$3/)O$_3$]and PZN[Pb(Zn$_{1}$3//Nb/sbu 2/3/)O$_3$] powders prepared by double calcination and PZT powders prepared by molten- salt synthesis method. The relative permittivity of specimen with PZT 0.3 mole ratio was shown 5,320 and appeared the relaxor ferroelectric feature. The maximum Piezoelectric coefficient d$_{31}$ to be used for evaluation the displacement of piezoceramics in PNN-PZN-PZT ceramics was 324$\times$10$^{-12}$ (C/V) at the vicinity of morphotropic phase boundary and was larger than that of solid PZT ceramics(120$\times$10$^{-12}$ C/V).

  • PDF

$BaTiO_3-(Bi_{1/2}Na_{1/2})TiO_3$ system for PTC Thermistor (PTC 써미스터를 위한 $BaTiO_3-(Bi_{1/2}Na_{1/2})TiO_3$)

  • Park, Yong-Jun;Lee, Young-Jin;Paik, Jong-Hoo;Kim, Dae-Joon;Lee, Woo-Young
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.91-92
    • /
    • 2007
  • An anomalous positive temperature coefficient of electrical resistivity (PTCR) was investigated in a ferroelectric lead-free perovskite-type compound $(Bi_{0.5}Na_{0.5})TiO_3$ within $BaTiO_3$-based solid solution ceramics. The effect of $Nb_2O_5$ content on the electrical properties and the microstructure of (1 - x) $BaTiO_3-x\;(Bi_{0.5}Na_{0.5})TiO_3$ (BNT) ceramics made using a conventional mixed oxide process also has been studied. The Curie temperature was obviously increased with the increasing of $(Bi_{0.5}Na_{0.5})TIO_3$ content. The Nb - doped BNT ceramics (x=0.01) display low resistivity values of $10^{1{\circ}}C-10^{2{\circ}}C$ ohm.cm at room temperature and the Curie Temperature of $T_c=160^{\circ}C$.

  • PDF

Dielectrical and Pyroelectrical Properties of $Pb(Zn_{1/3}Nb_{2/3})O_3-Pb(Zr_xTi_{1-x})O_3$ Compound Ceramics ($Pb(Zn_{1/3}Nb_{2/3})O_3-Pb(Zr_xTi_{1-x})O_3$세라믹의 유전 및 초전 특성)

  • 이성갑;조현무
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.10
    • /
    • pp.796-801
    • /
    • 2001
  • Ferroelectric 0.05PZN-xPZT(90/10)-(0.95-x)PZT(10/90) (x=0.65, 0.85) specimens were fabricated by the solid-state reaction method, and especially PZT(90/10) and PZT(10/90) powders were derived by the sol-gel method. All specimens showed a uniform ferroelectric grain without the presence of the pyrocholre phase. Average grain size increased with an increased in sintering temperature, the values for the x=0.65 and x=0.85 specimens sintered at 125$0^{\circ}C$ were 14.4$\mu$m and 9.8$\mu$m, respectively. The dielectric constant and dielectric loss of the x=0.65 specimen sintered at 125$0^{\circ}C$ were 1247. 2.06%, respectively. The coercive field and the remanent polarization of x=0.65 and x=0.85 specimens sintered at 125$0^{\circ}C$ were 8.5kV/cm, 13$\mu$C/$\textrm{cm}^2$ and 17.2kV/cm, 28 $\mu$C/$\textrm{cm}^2$, respectively. The pyroelectric coefficient of the x=0.65 and x=0.85 specimens sintered at 125$0^{\circ}C$ were 5.64$\times$10$^{-8}$ C/$\textrm{cm}^2$K and 2.76$\times$10$^{-8}$ C/$\textrm{cm}^2$K, respectively.

  • PDF

The Electrical Properties of $(SrPb)(CaMg)TiO_3$ Ceramics with Contents of $Bi_2O_3{\cdot}3TiO_2$ ($Bi_2O_3{\cdot}3TiO_2$의 첨가량에 따른 $(SrPb)(CaMg)TiO_3$ 세라믹의 전기적 특성)

  • Kim, Chung-Hyeok
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.2
    • /
    • pp.111-120
    • /
    • 1998
  • In this paper, the $(SrPb)(CaMg)TiO_3$ ceramics with paraelectric properties were fabricated by the mixed oxide method. It was investigated that which the variation of contents of $Bi_2O_3{\cdot}3TiO_2$ effects on structural, dielectrical and electrical properties of specimens. As a result, the grain size were grown with increasing the contents of $Bi_2O_3{\cdot}3TiO_2$. The relative dielectric constants were increased up to 4[mol%] of $Bi_2O_3{\cdot}3TiO_2$, and decreased more or less at a low temperature in the specimens which had more than. But the temperature coefficient. of capacitance were showed ${\pm}25$[%]. The dielectric loss were less than 0.05 in all specimens which had more than 4[mol%] of $Bi_2O_3{\cdot}3TiO_2$. In order to investigate the behavior of charged particles, the characteristics of electrical conduction were measured. As a result, the conduction current was divided into the three steps as a function of DC electric field. The first step was Ohmic region due to ionic conduction, below 15[kV/cm]. The second step was showed a saturation which seems to be related to a depolarizing field occuring in field-enforced ferroelectric phase, between 15[kV/cm] and 40[kV/cm]. The third step was attributed to Child's law related to space charge which injected from electrode, above 40[kV/cm].

  • PDF

A Study on the Behavior of Charged Particles of $(1-x)(SrPb)(CaMg)TiO_3-Bi_2O_3{\cdot}3TiO_2$ Ceramics ($(1-x)(SrPb)(CaMg)TiO_3-xBi_2O_3{\cdot}3TiO_2$ 세라믹의 하전입자 거동에 관한 연구)

  • Kim, Chung-Hyeok;Choi, Woon-Shik;Jung, Il-Hyung;Chung, Kue-Hye;Lee, Joon-Ung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1992.11a
    • /
    • pp.34-37
    • /
    • 1992
  • In this paper, the $(SrPb)(CaMg)TiO_3$-xBi_2O_3{\cdot}3TiO_2$ ceramics with paraelectric properties were fabricated by the mixed oxide method. In order to investigate the behavior of charged particles, the characteristics of electrical conduction and thermally stimulated current were measured respectively. As a result on characteristics of the electrical conduction, the leakage current was increased as measuring temperature was increased. At room temperature, the conduction current was divided into the three steps as a function of DC electric field. The first step was Ohmic region due to ionic conduction, below 15[kV/cm]. The second step was showed a saturation which seems to be related to a depolarizing field occuring in field-enforced ferroelectric phase, between 15[kV/cm] and 40[kV/cm]. The third step was attributed to Child's law related to spare charge which injected from electrode, above 40[kV/cm]. Thermally stimulated currents(TSC) spectra with various biasing fields exhibited three distinguished peaks that were denoted as ${\alpha}$, ${\alpha}'$ and ${\beta}$ peak, each of which appeared at nearby -30, 20 and 95[$^{\circ}C$] respectively. It is confirmed that the a peak was due to trap electron trapped in the grainboundary, and ${\alpha}'$ peak that was observed above only 1.5[kV/mm] was attributed to field-enforced ferroelectric polarization. The origin of ${\beta}$ peak was identified as ion migration which caused the degradation.

  • PDF

Ionic Doping Effect in Bi-layered Perovskite SrBi2Nb2O9 Ferroelectrics (비스무스 층구조형 페로브스카이트 SrBi2Nb2O9 강유전체의 이온 치환 효과)

  • Park, S.E.;Cho, J.A.;Song, T.K.;Kim, M.H.;Kim, S.S.;Lee, H.S.
    • Korean Journal of Materials Research
    • /
    • v.13 no.12
    • /
    • pp.846-849
    • /
    • 2003
  • Doping effect of various ions in Bi-layered ferroelectric $SrBi_2$$Nb_2$$O_{9}$ (SBN) ceramics was studied. Undoped SBN ceramic and SBN ceramics doped with $Ba^{2+}$, $Pb^{2+}$,$ Ca^{2+}$ , $Bi^{3+}$ , $La^{3+}$ , $Ti^{4+}$ , $Mo^{6+}$ , and $W^{6+}$ ions were made by a solid state reaction. Dielectric constants were measured with temperature. Ferroelectric transition temperature decreased with $Pb^{2+}$ , $Ba^{2+}$ , $La^{3+}$ doping, but the transition temperature increased with $Ca^{2+}$ , $Bi^{3+}$ , $Ti^{4+}$, $Mo^{6+}$ , or$ W^{6+}$ ionic doping. These results show that the ion size plays an important role in the ferroelectricity of SBN ceramic.

The study of ferroelectric properties for Pb(Mg1/3Ta2/3)O3-PbTiO3 solid solution modified with ZrO2 (ZrO2 첨가에 따른 Pb(Mg1/3Ta2/3)O3-PbTiO3 고용체의 강유전 특성 연구)

  • Kim, B.G.
    • Journal of the Korean Vacuum Society
    • /
    • v.17 no.4
    • /
    • pp.317-321
    • /
    • 2008
  • The $0.65Pb(Mg_{1/3}Ta_{2/3})O_3-0.35PbTiO_3$ (PMT-PT)ceramics were near morphotropic phase boundary. The dielectric constant, the loss, and pyroelectric coefficient of the ceramics were measured as a function of temperature ($25^{\circ}C\;{\sim}\;250^{\circ}C$). The dielectric constant, the loss, and the pyroelectric coefficient could be improved with the addition of small amounts of $ZrO_2$ up to 0.2 mol%. The dielectric and pyroelectric peak temperature are slightly shifted to lower temperatrues with the addition of amount of $ZrO_2$.

A Study on the Ferroelectic and Electrooptical Properties of the Transparent Ba(LaS11/2TNbS11/2T)OS13T-PbZrOS13T-PbTiOS13T Ceramics (투광성 Ba(La1/2Nb1/2)O3-PbZrO3-PbTiO3세라믹의 강유전 및 전기광학특성에 관한 연구)

  • 김준수;류기원;박영희;박창엽
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.41 no.8
    • /
    • pp.858-868
    • /
    • 1992
  • 0.085Ba(LaS11/2TNbS11/2T)OS13T-0.915Pb(ZrS1yTTiS11-yT)OS13T (0.45$\leq$y$\leq$0.65) transparent electrooptic ceramics were fabricated by two-stage sintering method. The structural, ferroelectric and electrooptic properties were investigated varying composition and second sintering time. Also the possibility of application to electrooptic device was studied. If we increase the PbZrOS13T contents, dielectric constants were increased and Curie temperature was decreased. In the composition of 0.55[mol] PbZrOS13T, electromechanical coupling factor and piezoelectric charge constant were the highest values of 43[%] and 173x10S0-12T[C/N], respectively. Mechanical quality factors were decreased with the increasing PbZrOS13T contents. Light transmittance was increased with wavelength when measured from 300[nm] to 900[nm], and with PbZrOS13T contents in the range of 0.50[mol]-0.65[mol], and had the highest value of 67[%] in the composition of 0.65[mol] PbZrOS13T. From the results of ferroelectric hysteresis loop and transmitted light intensity with electric field, the specimens with compositions of 0.65,0.60,0.55[mol] PbZrOS13T were applicable to electrooptic memory device and those with compositions of 0.50,0.45[mol] PbZrOS13T were applicable to linear electrooptic device.

Effects of High-Energy Ball Milling and Sintering Time on the Electric-Field-Induced Strain Properties of Lead-Free BNT-Based Ceramic Composites

  • Nga-Linh Vu;Nga-Linh Vu;Dae-Jun Heo;Thi Hinh Dinh;Chang Won Ahn;Chang Won Ahn;Hyoung-Su Han;Jae-Shin Lee
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.36 no.5
    • /
    • pp.505-512
    • /
    • 2023
  • This study investigated crystal structures, microstructures, and electric-field-induced strain (EFIS) properties of Bi-based lead-free ferroelectric/relaxor composites. Bi1/2Na0.82K0.18)1/2TiO3 (BNKT) as a ferroelectric material and 0.78Bi1/2(Na0.78K0.22)1/2TiO3-0.02LaFeO3 (BNKT2LF) as a relaxor material were synthesized using a conventional solid-state reaction method, and the resulting BNKT2LF powders were subjected to high-energy ball milling (HEBM) after calcination. As a result, HEBM proved a larger average grain size of sintered samples compared to conventional ball milling (CBM). In addition, the increased sintering time led to grain growth. Furthermore, HEBM treatment and sintering time demonstrated a significant effect on EFIS of BNKT/BNKT2LF composites. At 6 kV/mm, 0.35% of the maximum strain (Smax) was observed in the HEBM sample sintered for 12 h. The unipolar strain curves of CBM samples were almost linear, indicating almost no phase transitions, while HEBM samples displayed phase transitions at 5~6 kV/mm for all sintering time levels, showing the highest Smax/Emax value of 700 pm/V. These results indicated that HEBM treatment with a long sintering time might significantly enhance the electromechanical strain properties of BNT-based ceramics.

A-site Non-stoichiometric Effects of Bi0.5(Na0.78K0.22)0.5TiO3 Ceramics on the Dielectric and Electrical Properties (Bi0.5(Na0.78K0.22)0.5TiO3 세라믹스의 A-site 비화학양론이 유전 및 전기적 특성에 미치는 영향)

  • Park, Jung Soo;Lee, Ku Tak;Yun, Ji Sun;Cho, Jeong Ho;Jeong, Young Hun;Paik, Jong Hoo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.12
    • /
    • pp.803-808
    • /
    • 2014
  • $Bi_{0.5+x}(Na_{0.78}K_{0.22})_{0.5-3x}TiO_3$ ceramics with an excess $Bi^{3+}$ and a deficiency of $Na^+$ and $K^+$ were synthesized by a conventional solid state reaction method. The structure and morphology of $Bi_{0.5+x}(Na_{0.78}K_{0.22})_{0.5-3x}TiO_3$ ceramics were characterized by X-ray diffraction and field emission scanning electron microscopy. The electric polarization and mechanical strain induced by external electric field, and the temperature dependence of dielectric constant were investigated. These results demonstrated that an ergodic relaxor phase can be induced by controls of the mole ratio of $Bi^{3+}$, $Na^+$ and $K^+$. A phase boundary between non-ergodic and ergodic relaxor phases can be observed at ambient temperature. The ergodic relaxor phase can be transferred to the ferroelectric phase by application of the electric field. The stability of the induced ferroelectric phases strongly depends on the mole ratio of $Bi^{3+}$, $Na^+$ and $K^+$. The maximum strain of 0.31% was observed in $Bi_{0.51}(Na_{0.78}K_{0.22})_{0.47}TiO_3$ ceramics sintered at $1,150^{\circ}C$ for 2 h.