고규소철 합금의 유황분위기중 열처리의 영향 (Effect of high Si-Fe alloy annealed in the sulfur atmosphere)

  • 구자명
    • 열처리공학회지
    • /
    • 제7권2호
    • /
    • pp.111-117
    • /
    • 1994
  • Effect of rapidly solidfid 6.5wt%Si-Fe alloy annealed in the sulfur atmosphere were studied. The ribbons Which were showed with random structure at the received state, were developed into(110) texture in the heat treatment of the vacuum atmosphere, into (100)texture in the sulfur atmosphere. After the ribbon was continuously annealed in the vacuum atmosphere for 3 min. at $1100^{\circ}C$, and sulfur atmosphere for 1hr at $1175^{\circ}C$, grain size of (100)plane was grew to 4-8mm and the coercive force was decreased to 2-4A/m remarkably.

  • PDF

Rheo-compocasting법에 의한 SiC입자분산 복합재료의 마모특성에 관한 연구 (A Study on the Wear Characteristics of SiC Particle Dispersed Composites by Rheo-Compocasting Method)

  • 곽현만;최창옥
    • 한국주조공학회지
    • /
    • 제13권3호
    • /
    • pp.238-247
    • /
    • 1993
  • Microstructure, hardness and wear characteristics of $SiC_p/Al-6.5wt%Si-1.7wt%Mg$ alloy composites fabricated by the method of rheo-compocasting and hot pressing are investigated in this study. The dispersion of SiC particles in the composites is homogeneous and the hardness improves as additional amount increases. The wear amount of the matrix metal increases highly as wear rates increase, for the wear mechanism changes from adhesive wear to melt wear, and the matrix metal was coated on the surface of revolving disc and its weight increases. In the 5vol% composites, Fe is adhered on the surface of specimen by the projection of the dispersed hard SiC particles which have net-work structure and the coating layer is about $300{\mu}m$. But in the composite more than 20vol%, the wear amount of composite decreases because the SiC particles which have superior hardness, wear resistance and heat resistance properties resist wear, the abrasive wear turn out predominant wear mechanism and so the wear amount of revolving disc increases.

  • PDF

반응표면분석법을 활용한 Fe-18Cr 스테인리스강의 부식 및 산화 저항성에 미치는 Ti, Si, Mo의 영향 분석 (Analysis of the Effects of Ti, Si, and Mo on the Resistance to Corrosion and Oxidation of Fe-18Cr Stainless Steels by Response Surface Methodology)

  • 장희진;윤귀섭;박찬진
    • 대한금속재료학회지
    • /
    • 제48권8호
    • /
    • pp.741-748
    • /
    • 2010
  • We studied the corrosion and oxidation properties of Fe-18Cr-0.4Nb-(0.1~0.6)Ti-(1~3)Si-(0.5~2)Mo stainless steel. The resistance to general and pitting corrosion was evaluated and the results were analyzed by Response Surface Methodology (RSM) as a function of alloy composition. The effects of alloy composition and heat treatment on the oxidation resistance were also examined. Mo increased both general corrosion resistance and pitting corrosion resistance. Si improved the resistance of the alloys to pitting corrosion. Si was also beneficial for general corrosion resistance of the alloys containing Mo at more than 1 wt.%. However, Mo was detrimental when its content was lower. Effects of Ti on general corrosion properties appeared to be weak and a high concentration of Ti appeared to deteriorate pitting resistance. The thickness of the oxidation scale increased and adhesion of the scale worsened as the temperature increased from $800^{\circ}C$ to $900^{\circ}C$. Weight gain of the alloys due to oxidation at $900^{\circ}C$ clearly showed that the resistance to oxidation is improved by annealing at $860^{\circ}C$ and an increase of Si content.

고강도 인바계 합금의 열팽창 및 인장 특성에 미치는 바나듐과 탄소 원소 첨가 영향 (Effects of V and C additions on the Thermal Expansion and Tensile Properties of a High Strength Invar Base Alloy)

  • 윤애천;윤신천;하태권;송진화;이기안
    • 소성∙가공
    • /
    • 제24권1호
    • /
    • pp.44-51
    • /
    • 2015
  • The current study seeks to examine the effects of V and C additions on the mechanical and low thermal expansion properties of a high strength invar base alloy. The base alloy (Fe-36%Ni-0.9%Co-2.75%Mo-0.7Cr-0.23Mn-0.17Si-0.3%C, wt.%) contains $Mo_2C$ carbides, which form as the main precipitate. In contrast, alloys with additions of 0.4%V+0.3%C (alloy A) or 0.4%V+0.45%C (alloy B) contain $Mo_2C$+[V, Mo]C carbides. The average thermal expansion coefficients of these high strength invar based alloys were measured in the range of $5.16{\sim}5.43{\mu}m/m{\cdot}^{\circ}C$ for temperatures of $15{\sim}230^{\circ}C$. Moreover, alloy B showed lower thermal expansion coefficient than the other alloys in this temperature range. For the mechanical properties, the [V, Mo]C improved hardness and strengths(Y.S. and T.S.) of the high strength invar base alloy. T.S.(tensile strength) and Y.S.(yield strength) of hot forged alloy B specimen were measured at 844.6MPa and 518.0MPa, respectively. The tensile fractography of alloy B exhibited a ductile transgranular fracture mode and voids were initiated between the [V, Mo]C particles and the matrix. Superior properties of high strength and low thermal expansion coefficient can be obtained by [V, Mo]C precipitation in alloy B with the addition of 0.4%V and 0.45%C.

Electromagnetic Wave Absorption Properties in Fe-based Nanocrystalline P/M Sheets with Carbon Black and BaTiO3 Additives

  • Kim, Mi-Rae;Park, Won-Wook
    • 한국분말재료학회지
    • /
    • 제16권1호
    • /
    • pp.33-36
    • /
    • 2009
  • In order to increase the magnetic loss for electromagnetic(EM) wave absorption, the soft magnetic $Fe_{73}Si_{16}B_7Nb_3Cu_1$(at%) alloy strip was used as the basic material in this study. The melt-spun strip was pulverized using an attrition mill, and the pulverized flake-shaped powder was crystallized at $540^{\circ}C$ for 1h to obtain the optimum grain size. The Fe-based powder was mixed with 2 wt% $BaTiO_3$, $0.3{\sim}0.6$ wt% carbon black, and polymer-based binders for the improvement of electromagnetic wave absorption properties. The mixture powders were tape-cast and dried to form the absorption sheets. After drying at $100^{\circ}C$ for 1h, the sheets of 0.5 mm in thickness were made by rolling at $60^{\circ}C$, and cut into toroidal shape to measure the absorption properties of samples. The characteristics including permittivity, permeability and power loss were measured using a Network Analyzer(N5230A). Consequently, the properties of electromagnetic wave absorber were improved with the addition of both $BaTiO_3$ and carbon black powder, which was caused by the increased dielectric loss of the additive powders.

반응소결법으로 제조한 Al기 복합재용 Fe-Al합금 예비성형체의 특성평가 (Characteristic Evaluation of the Fe-Al Alloy Preform Fabrication by Reactive Sintering Process for the Al Matrix Composites.)

  • 최답천;박성혁;주형곤
    • 한국주조공학회지
    • /
    • 제19권6호
    • /
    • pp.493-500
    • /
    • 1999
  • Squeeze casting was used for fabricating a light metal base composite having high strength and wearresistance. Reactive sintering was used to prepare the preform of Squeeze casting. To utilize Fe-Al intermetallic compounds and SiC particle as a reinforcement, there needs to prepare Fe-Al mixed powder at 50, 60, 70at.%Al, and add SiC powder to the above mixture at 4, 7, 16, 24wt.%. The prepared mixture with SiC was reactive sintered in a tube furnace at $660^{\circ}C$ to get a porous hybrid preform of intermetallic compound and SiC. The preform prepared above was placed in a metal mold, preheated at $660^{\circ}C$ AC4C matrix was injected into the mold with the temperature of the melt at $610^{\circ}C$ After these processes, 66MPa was applied to the mold for 5 minute to finish the whole procedure. The maximum reaction temperature was increased with the increased Al amount, but decreased with the increased SiC amount. The density of the preform was decreased with SiC amount increase in the compacts due to swelling of the preform. An optical microscope was applied to observe the micro structure and the dispersion of the reinforcements. To analyze phases, We utilized XRD, EDS. Hardness test were chosen to get the information of mechanical properties. There were no significant changes in micro structure between the composite and preform. However, it was shown that uniform dispersion of the reinforcers and complete infiltration of the melt into the preform were achieved through the procedure of the squeeze casting. It was observed that the hardness of the composite is decreased with increased SiC amount, resulting from the volumetric expansion of the preform.

  • PDF

590 MPa TRIP강의 선택적 표면산화 거동과 표면 산화막이 도금특성에 미치는 영향 (Selective Surface Oxidation of 590MPa TRIP Steel and Its Effect on Hot-Dip Galvanizability)

  • 김성환;임준모;허주열;이석규;박노범;김종상
    • 대한금속재료학회지
    • /
    • 제49권4호
    • /
    • pp.281-290
    • /
    • 2011
  • In order to gain better understanding of the selective surface oxidation and its influence on the galvanizability of a transformation-induced plasticity (TRIP) assisted steel containing 1.5 wt.% Si and 1.6 wt.% Mn, a model experiment has been carried out by depositing Si and Mn (each with a nominal thickness of 10 nm) in either monolayers or bilayers on a low-alloy interstitial-free (IF) steel sheet. After intercritical annealing at $800^{\circ}C$ in a $N_2$ ambient with a dew point of $-40^{\circ}C$, the surface scale formed on 590 MPa TRIP steel exhibited a microstructure similar to that of the scale formed on the Mn/Si bilayer-coated IF steel, consisting of $Mn_{2}SiO_{4}$ particles embedded in an amorphous $SiO_{2}$ film. The present study results indicated that, during the intercritical annealing process of 590 MPa TRIP steel, surface segregation of Si occurs first to form an amorphous $SiO_{2}$ film, which in turn accelerates the out-diffusion of Mn to form more stable Mn-Si oxide particles on the steel surface. During hot-dip galvanizing, particulate $Fe_{3}O_{4}$, MnO, and Si-Mn oxides were reduced more readily by Al in a Zn bath than the amorphous $SiO_{2}$ film. Therefore, in order to improve the galvanizability of 590 TRIP steel, it is most desirable to minimize the surface segregation of Si during the intercritical annealing process.

표면에너지를 이용한 고규소철 합금의 자기적 특성에 미치는 열처리의 영향 (Heat treating effect on the magnetic properties of high Silicon Iron by control of surface energy)

  • 구자명;이갑호
    • 열처리공학회지
    • /
    • 제9권1호
    • /
    • pp.45-52
    • /
    • 1996
  • Different crystallographic planes, at a gas-metal interface, have different surface energy. To grow the (100) grains of 6.5wt%Si-Fe alloy preferentially, it was heat-treated in the atmosphere of sulfur by using the surface energy. When the specimen is heat-treated for 1 hour at $1175^{\circ}C$ by using the atmosphere of sulfur produced by heating at $75^{\circ}C$, (100) grains were grown to 3.5mm. Owing to the growth of (100) grains, the coercive force was decreased to 2.1 A/mm, and the magnetic induction at 800(A/mm) was increased to 1.61T.

  • PDF

ATO 처리후, 플라즈마 전해 산화 처리된 Ti-6Al-4V 합금의 표면 형태 (Surface Morphology of PEO-treated Ti-6Al-4V Alloy after Anodic Titanium Oxide Treatment)

  • Kim, Seung-Pyo;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2018년도 춘계학술대회 논문집
    • /
    • pp.75-75
    • /
    • 2018
  • Commercially pure titanium (CP-Ti) and Ti-6Al-4V alloys have been widely used in implant materials such as dental and orthopedic implants due to their corrosion resistance, biocompatibility, and good mechanical properties. However, surface modification of titanium and titanium alloys is necessary to improve osseointegration between implant surface and bone. Especially, when titanium oxide nanotubes are formed on the surface of titanium alloy, cell adhesion is greatly improved. In addition, plasma electrolytic oxide (PEO) coatings have a good safety for osseointegration and can easily and quickly form coatings of uniform thickness with various pore sizes. Recently, the effects of bone element such as magnesium, zinc, strontium, silicon, and manganese for bone regeneration are researching in dental implant field. The purpose of this study was researched on the surface morphology of PEO-treated Ti-6Al-4V alloy after anodic titanium oxide treatmentusing various instruments. Ti-6Al-4V ELI disks were used as specimens for nanotube formation and PEO-treatment. The solution for the nanotube formation experiment was 1 M $H_3PO_4$ + 0.8 wt. % NaF electrolyte was used. The applied potential was 30V for 1 hours. The PEO treatment was performed after removing the nanotubes by ultrasonics for 10 minutes. The PEO treatment after removal of the nanotubes was carried out in the $Ca(CH_3)_2{\cdot}H_2O+(CH_3COO)_2Mg{\cdot}4H_2O+Mn(CH_3COO)_2{\cdot}4H_2O+Zn(CH_3CO_2)_2Zn{\cdot}2H_2O+Sr(CH_2COO)_2{\cdot}0.5H_2O+C_3H_7CaO_6P$ and $Na_2SiO_3{\cdot}9H_2O$ electrolytes. And the PEO-treatment time and potential were 3 minutes at 280V. The morphology changes of the coatings on Ti-6Al-4V alloy surface were observed using FE-SEM, EDS, XRD, AFM, and scratch tester. The morphology of PEO-treated surface in 5 ion coating solution after nanotube removal showed formation or nano-sized mesh and micro-sized pores.