Simulation of Material Properties of Amorphous Carbon Nitride with Non-uniform Nitrogen Distribution

  • Lu, Y.F.;He, Z.F.
    • Transactions on Electrical and Electronic Materials
    • /
    • 제2권3호
    • /
    • pp.1-6
    • /
    • 2001
  • A simulation method is proposed to study the amorphous structure of carbon nitride. The material properties of a non-uniform nitrogen distribution in an amorphous CN matrix can be studied. The cohesive energy of a group of randomly generated atoms can be minimized to find the relative positions of atoms. From the calculated configuration of atoms, many properties of amorphous carbon nitride can be calculated such as bulk modulus, P-V curve, sp$^3$/sp$^2$ ratio of carbon, and vibrational spectra. The calculation shows that the cohesive energy of non-uniform nitrogen distribution is lower than that of a uniform distribution. This may suggest that the regular structure of carbon nitride can at most be metastable. It is not easy to incorporate nitrogen atoms into a carbon matrix.

  • PDF

Low voltage operated top gated polymer thin film transistors with a high capacitance polymer dielectric

  • Jung, Soon-Won;You, In-Kyu;Noh, Yong-Young
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2009년도 9th International Meeting on Information Display
    • /
    • pp.907-909
    • /
    • 2009
  • Low voltage operated top gated polymer transistors were fabricated with a high permittivity polymer, P(VDF-TrFE) and F8T2 as a gate dielectric and semiconducting layer, respectively. The operating voltage of transistors was effectively reduced under -10 V and typical threshold voltages were as low as -1 ~ -4 V with the reasonable charge carrier mobility of $10^{-3}cm^2$/Vs for the amorphous polymer. The large hysteresis in transfer curve was improved effectively by annealing at low temperature.

  • PDF

The Electron Trap Analysis in Thermoluminescent LiF Crystal

  • Park, Dae-Yoon;Ko, Chung-Duck;Lee, Sang-Soo
    • Nuclear Engineering and Technology
    • /
    • 제4권3호
    • /
    • pp.214-222
    • /
    • 1972
  • 광학급 LiF단결정의 열형광유선은 r선조사선양이 증가함에 따라서 변화한다. 즉 선량이 적을 때는 2개의 glow peak를 가지나, 선양이 정차 증가하여 10$_{5}$ rontgen 정도에 이르면 5개의 glow peak를 나타낸다. 이들 glow peak에 대응하는 energy 준위 Ei(i=1,2,3,4, 및 5)는 전도대 밑으로 부터의 깊이로 표시할 때 다음과 같은 값을 갖는다. 이들 E$_i{$의 값은 가열속도 $\theta_1$=6.6$^{\circ}C$/sec와 $\theta_2$=3.4$^{\circ}C$/sec에 대한 glow peak의 온도를 얻은 다음, Randall-Wilkins의 이론에 따라서 계산되었다. 광학급 LiF단결정에서 E$_1$과 E$_2$이외의 전자 trap은 열적으로 불안정하며 LiF(Mg) 열형광선양계에 불가결한 것으로 되어있는 sensitization의 효과가 거의 없다. LiF(Mg)는 $\theta$=6.6$^{\circ}C$/sec 일때, 17$0^{\circ}C$와 23$0^{\circ}C$에 glow peak를 나타내며 이들에 대응하는 전자 trap E$_4$와 E$_{5}$ 이외에 방사선이 조사됨에 따라서 E$_1$, E$_2$, E$_3$ 및 E$_{6}$의 전자 trap이 형성되며 이들 값은 다음과 같다. LiF(Mg)에서 방사선상해 때문에 형성된 E$_1$, E$_2$, E$_3$및 E$_{6}$는 모두 상당히 열적으로 안정하며, sensitization과정에서 형성된다. 이 안정한 6준위계에서 LiF(Mg)예 의한 방사선 선양측정이 시행되어야 한다. E$_1$,E$_2$,E$_3$ 및 E$_{6}$의 안정성은 LiF결정내의 $Mg^{$ ++/ 불순물의 영향으로 사료된다. 광학급 LiF단결정의 열형광에서 r선양의 대수표시양과 전열형광양의 대수표시 사이에 비선형성을 나타낸다. 그러나 열적으로 안정한 12$0^{\circ}C$ glow peak만을 고려하여 r선양의 대수표시양과 12$0^{\circ}C$ slow peak의 높이의 대수표시량 사이에서 비선형성이 감소되어, LiF(Mg)에 대한 곡선과 매우 유사한 곡선을 얻게 된다.

  • PDF

초크랄스키 방법으로 성장한 CaF2 단결정 분석 (Analysis of calcium fluoride single crystal grown by the czochralski method)

  • 이하린;나준혁;박미선;장연숙;정해균;김두근;이원재
    • 한국결정성장학회지
    • /
    • 제32권6호
    • /
    • pp.219-224
    • /
    • 2022
  • 광학 윈도우, 프리즘, 렌즈 등에 사용되는 CaF2 단결정은 3개의 부격자를 가진 face-centered cubic(FCC) 구조를 가지고 있으며 밴드갭(12 eV)이 크고 넓은 파장영역에서 투과율이 우수하고 굴절률이 낮다는 특징이 있다. CaF2 단결정 성장은 대표적으로 높은 생산효율과 큰 결정을 만들 수 있는 초크랄스키(Czochralski) 방법으로 생산되고 있다. 이 연구에서는 초크랄스키 방법으로 성장한 일본의 Nikon 사와 미국의 M TI 사 (100)면, (111)면의 CaF2 단결정 상용화 웨이퍼의 결정성과 결함밀도를 분석하기 위해 X선 회절(XRD), XRC(X-ray rocking curve) 측정 및 Chemical Etching을 수행하였고 푸리에 변환 적외선 분광법(FT-IR)과 UV-VIS-NIS을 이용하여 CaF2 결정의 광학적 특성을 분석하였다. 다양한 분석 결과를 통해 CaF2 단결정의 다양한 분야에서의 응용가능성을 체계적으로 살펴보았다.

Hot Wall Epitaxy(HWE) 방법에 의한 $CuInTe_2$ 단결정 박막 성장과 특성에 관한 연구 (Growth and Characterization of $CuInTe_2$ Single Crystal thin Films by Hot Wall Epitaxy)

  • 홍광준;이관교;이상열;유상하;정준우;정경아;백형원;방진주;신영진
    • 한국결정학회지
    • /
    • 제11권4호
    • /
    • pp.212-223
    • /
    • 2000
  • A stochiometric mix of CuInTe₂ polycrystal was prepared in a honizonatal furnace. To obtain the single crystal thin films, CuInTe₂ mixed crystal was deposited on throughly etched GaAs(100) by the HWE system. The source and substrate temperatures were 610℃ and 450℃ respectively, and the thickness of the deposited single crystal thin film was 2.4㎛. CuInTe₂ single crystal thin film was proved to be the optimal growth condition when the excition emission spectrum was the strongest at 1085.3 nm(1.1424 eV) of photoluminescence spectrum at 10 K, and also FWHM of Double Crystal X-ray Rocking Curve (DCRC) was the smallest, 129 arcsec. The Hall effect on this sample was measured by the method of Van der Pauw, and the carrier density and mobility dependent on temperature were 9.57x10/sup 22/ electron/㎥, 1.31x10/sup -2/㎡/V·s at 293 K, respectively. The ΔCr(Crystal field splitting) and the ΔSo (spin orbit coupling splitting( measured at f10K from the photocurrent peaks in the short wavelength of the CuInTe₂ single crystal thin film were about 0.1200 eV, 0.2833 eV respectively. From the PL spectra of CuInTe₂ single crystal thin film at 10 K, the free exciton (E/sub x/) was determined to be 1064.5 nm(1.1647 eV) and the donor-bound exciton(D/sup 0/, X) and acceptor-bound exciton (A/sup 0/, X) were determined to be 1085.3 nm(1.1424 eV) and 1096.8 nm(1.1304 eV0 respectively. And also, the donor-acciptor pair (DAP)P/sub 0/, DAP-replica P₁, DAP-replica P₂ and self-activated (SA) were determined to be 1131 nm (1.0962 eV), 1164 nm(1.0651 eV), 1191.1 nm(1.0340 eV) and 1618.1 nm (0.7662 eV), respectively.

  • PDF

Differential Absorption Analysis of Nonmagnetic Material in the Phantom using Dual CT

  • Kim, Ki-Youl;Lee, Hae-Kag;Cho, Jae-Hwan
    • Journal of Magnetics
    • /
    • 제21권2호
    • /
    • pp.286-292
    • /
    • 2016
  • This study evaluates the change of computer tomography (CT) number in the case of the metal artifact reduction (MAR) algorithm, using the phantom. The images were obtained from dual CT using a gammex 467 tissue characterization phantom, which is similar to human tissues. The test method was performed by dividing pre and post MAR algorithm and measured CT values of nonmagnetic materials within the phantom. In addition, the changes of CT values for each material were compared and analyzed after measuring CT values up to 140 keV, using the spectral HU curve followed by CT scan. As a result, in the cases of N rod (trabecular bone) and E rod (trabecular bone), the CT numbers decreased as keV increasing but were constant above 90 keV. In the cases of I rod (dense bone) and K rod (dense bone), the CT numbers also decreased as keV increased but were uniform above 90 keV. The CT numbers from 40 keV to 140 keV were consistent in the cases of J rod (liver), D rod (liver), L rod (muscle), and F rod (muscle). For A rod (adipose), G rod (adipose), B rod (breast) and O rod (breast), the CT numbers increased as keV increased but were constant after 90 keV. The CT numbers from 40 keV to 140 keV were consistent in the cases of C rod (lung (exhale)), P rod (lung (exhale)), M rod (lung (inhale)) and H rod (lung (exhale)). Conclusively, because dual CT exhibits no changes in image quality and is able to analyze nonmagnetic materials by measuring the CT values of various materials, it will be used in the future as a useful tool for the diagnosis of lesions.

유방 부분 절제술 후 방사선 치료 시 TOMO Direct를 이용한 접선 조사의 선량적 유용성에 관한 고찰 (Evaluation of Tangential Fields Technique Using TOMO Direct Radiation Therapy after Breast Partial Mastectomy)

  • 김미정;김주호;김훈겸;조강철;전병철;조정희
    • 대한방사선치료학회지
    • /
    • 제23권1호
    • /
    • pp.59-66
    • /
    • 2011
  • 목 적: 유방 부분 절제술 후 방사선 치료 시 기존의 라이낙을 이용한 치료기법과 비교하여 TOMO Direct를 이용한 접선 치료 기법의 임상적 유용성을 알아보고자 한다. 대상 및 방법: 유방 부분 절제술 후 방사선 치료를 받은 좌측 유방암 환자 3명을 대상으로 라이낙을 이용한 쐐기 접선 조사 기법(Wedged tangential fields technique)과 조사면 내 선량 보강 기법(Field In Field technique, FIF), TOMO Direct, TOMO Direct 세기 변조 방사선 치료(Intensity Modulated Radiation Therapy, IMRT)기법을 이용하여 동일한 처방 조건(CTV 내 $D_{90%}$: 50.4 Gy/28 fx)으로 치료계획을 수립하였다. 선량 분석을 위해 선량 체적 히스토그램(Dose Volume Histogram, DVH)과 등선량 곡선 (Isodose curve)을 이용하여 종양 내 표적체적(Clinical Target Volume, CTV)과 손상위험장기(Organ At Risk, OAR)에 대한 선량을 비교분석 하였다. 표적체적의 선량 인자로는 $D_{99}$, $D_{95}$, 선량 균일 지수(Dose homogeneity index, DHI: $D_{10}/D_{90}$)와 $V_{105}$, $V_{110}$을 손상위험장기의 선량 인자로는 심장의 $V_{10}$, $V_{20}$, $V_{30}$, $V_{40}$과 좌측 폐의 $V_{10}$, $V_{20}$, $V_{30}$을 비교 분석하였다. 결 과: 표적체적의 선량 분석 결과로 $D_{99}$, $D_{95}$의 평균값은 각각 쐐기 접선 조사(W)에서 $47.7{\pm}1.1Gy$, $49.4{\pm}0.1Gy$이었으며, 조사면 내 선량 보강 기법(F)은 각각 $47.1{\pm}0.6Gy$, $49.2{\pm}0.4Gy$, 그리고 TOMO Direct(D)와 TOMO Direct IMRT(I)에서는 각각 $49.2{\pm}0.4$ vs. $48.6{\pm}0.8Gy$, $49.9{\pm}0.4$ vs. $49.5{\pm}0.3Gy$이었다. 선량 균일 지수의 평균값은 W: $1.1{\pm}0.02$, F: $1.07{\pm}0.02$, D: $1.03{\pm}0.001$, I: $1.05{\pm}0.02$이었다. 각각의 치료 기법으로 $V_{105}$, $V_{110}$의 평균값을 비교하였을 때 쐐기 접선 조사 시 각각 $34.6{\pm}9.3%$, $7.5{\pm}7.9%$로 가장 높았고 조사면 내 선량 보강 기법은 $16.5{\pm}14.8%$, $2.1{\pm}3.5%$로, TOMO direct IMRT는 $7.5{\pm}8.3%$, $0.1{\pm}0.1%$로 낮아졌으며 TOMO direct에서는 두 값 모두 0%로 나타났다. 손상 위험 장기에 대한 선량 분석 결과 각각의 치료 기법 사이에 유의한 차이를 보이지 않았다. 결 론: TOMO Direct를 이용한 접선 조사 기법은 기존의 쐐기 접선 치료 기법보다 치료 용적 내에 균일한 선량분포를 얻을 수 있을 뿐만 아니라 IMRT 또는 Tomotherapy와 달리 정상조직의 저 선량 영역의 노출용적을 증가시키지 않았으며 조사면 내선량 보강 기법 보다 용이한 치료계획 절차를 수행하므로 유방 부분 절제술 후 방사선 치료 시 임상적으로 유용하리라 사료된다.

  • PDF

메조스코픽 구조를 가지는 급냉응고 Al-Nd-(Cu,Ag)합금의 기계적 성질 (Mechanical Properties in Rapidly Solidified Al-Nd-(Cu,Ag) Alloys with Mesoscopic Structure)

  • 고근우;김영환;김한군
    • 열처리공학회지
    • /
    • 제12권4호
    • /
    • pp.320-326
    • /
    • 1999
  • In rapidly solidified $Al_{92-x}Nd_8$(Cu,Ag)x ($0{\leq}X{\leq}10at%$) alloys, amorphous single phases were obtained in the ranges of $Oat%{\leq}X{\leq}4at%$ for Al-Nd-Cu system and $Oat%{\leq}X{\leq}6at%$ for Al-Nd-Ag system, respectively. Mesoscopic structures consisted of amorphous and crystalline phases were formed above solute ranges. It was founded that the mesoscopic structures were also formed near 1st exothermic peak on DSC curve by aging in amorphous single phase alloys. For example, amorphous $Al_{92-x}Nd_8$(Cu,Ag)x (X=2.4at%) alloys containing nanoscale Al particles and compounds, i.e., mesoscopic structure, exhibited higher tensile fracture strength(${\sigma}_f$) than those of amorphous single phase alloys with the same composition. The ${\sigma}_f$ showed a maximum value in the $V_f$ ranges of 10~15%. The reason is presumed that the nanoscale precipitates which have higher mechanical strength compared with the amorphous phase with the same composition act as an effective resistance to shear deformation of the amorphous matrix.

  • PDF

Changes in Photosynthetic Characteristics during Grain Filling of a Functional Stay-Green Rice SNUSG1 and its $F_1$ Hybrids

  • Fu, Jin-Dong;Lee, Byun-Woo
    • Journal of Crop Science and Biotechnology
    • /
    • 제11권1호
    • /
    • pp.75-82
    • /
    • 2008
  • Functional stay-green is a beneficial trait that may increase grain yield through the sustained photosynthetic competence during monocarpic senescence in cereal crops. The temporal changes of photosynthesis and related characteristics throughout the grain filling period of a stay-green japonica rice "SNU-SG1" was compared in growth chamber conditions with three high-yielding cultivars(HYVs) and their $F_1$ hybrids with SNU-SG1. SNU-SG1 exhibited a typical characteristic of functional stay-green in terms of chlorophyll degradation and photosynthetic competence during grain filling. According to the photosynthesis-light response curve measured at 10 and 35 d after heading for the flag leaf, SNU-SG1 exhibited higher initial light conversion efficiency and thus higher gross photosynthetic rate at light saturation compared to HYVs. Light saturation point was not different among genotypes, ranging from 1000 to 1500 ${\mu}mol$ photon $m^{-2}s^{-1}$. Net photosynthetic rate at light saturation($P_{max}$) of the upper four leaves in SNU-SG1 was much higher and sustained longer throughout grain-filling than HYVs and $F_1$ hybrids. The sustained high photosynthetic competence of SNU-SG1 during grain filling was ascribed to the longer maintenance of high mesophyll conductance that resulted from not only high chlorophyll content and its delayed degradation but also the slow degeneration of photosystem II(PS II) as judged by chlorophyll fluorescence($F_v/F_m$) of flag leaves. $F_1$ hybrids showed slow degeneration of photosystem II similar to the male parent SNU-SG1 while chlorophyll degradation pattern close to female parents, thus exhibiting a little higher $P_{max}$ than female parents. These results suggest that SNU-SG1 has a typical functional stay-green trait that can be utilized for increasing rice yield potential through the improved dry matter production during grain filling.

  • PDF

고집적 반도체 배선용 Cu(Mg) 박막의 전기적, 기계적 특성 평가 (Electrical and Mechanical Properties of Cu(Mg) Film for ULSI Interconnect)

  • 안재수;안정욱;주영창;이제훈
    • 마이크로전자및패키징학회지
    • /
    • 제10권3호
    • /
    • pp.89-98
    • /
    • 2003
  • 반도체 소자의 배선용 재료로서 사용가능한 합금원소 Mg를 첨가한 Cu(Mg) 박막의 기계 및 전기적 특성 변화를 조사하였다. Cu(2.7at.%Mg) 박막은 열처리를 할 경우 Cu 박막에 비하여 표면거칠기는 약 1/10 정도로 줄고 $SiO_2$와의 접착력도 2배 이상 향상된 결과를 나타내었다. 또한 $300^{\circ}C$이상의 온도에서 10분 이상 열처리를 할 경우 급격한 저항감소를 보여주었는데 이는 Mg 원소의 확산으로 인해 표면 및 계면에서 Mg 산화물이 형성되고 내부에는 순수 Cu와 같이 되었기 때문이다. 경도 및 열응력에 대한 저항력도 Cu박막에 비해 우수한 것으로 나타났으며 열응력으로 인해 Cu 박막에 나타나던 표면 void가 Cu(Mg) 박막에서는 전혀 관찰되지 않았다. EM Test 결과 lifetime은 2.5MA/$cm^2$, $297^[\circ}C$에서 순수 Cu 라인보다 5배 이상 길고 BTS Test 결과 Capacitance-Voltage 그래프의 플랫 밴드 전압(V$_{F}$ )의 shift현상이 Cu에서는 나타났지만 Cu(Mg) 박막에서는 발생하지 않는 우수한 신뢰성을 보여주었다. 누설전류 측정을 통한 $SiO_2$의 파괴시간은 Cu에 비하여 약 3배 이상 길어 합금원소에 의한 확산방지 효과가 있음을 확인하였다.

  • PDF