  • Since the discovery of graphene by mechanical exfoliation from graphite[1], various fabrication methods are available today such as chemical exfoliation, epitaxial graphene on SiC substrates, etc. In view of industrialization, the mechanical exfoliation method may not be an option. Epitaxial graphene on SiC substrates, in this respect, is by far more practical because the method consists of conventional thermal treatments familiar to semiconductor industry. Still, the use of the SiC substrate itself, and hence the incompatibility with the Si technology, lessens the importance of this technology in its future industrialization. In this context, we have tackled the problem of forming graphene on Si substrates (GOS). Our strategy is to form an ultrathin (~80 nm) SiC layer on top of a Si substrate, and to graphitize the top SiC layers by a vacuum annealing. We have actually succeeded in forming the GOS structure [2,3,4]. Raman-scattering microscopy indicates presence of few-layer graphene (FLG) formed on our annealed SiC/Si heterostructure, with the G ($1580\;cm^{-1}$) and the G'($2700\;cm^{-1}$) bands, both related to ideal graphene, clearly observed. Presence of the D ($1350\;cm^{-1}$) band indicates presence of defects in our GOS films, whose elimination remains as a challenge in the future. To obtain qualified graphene films on Si substrate, formation of qualified SiC films is crucial in the first place, and is achieved by tuning the growth parameters into a process window[5]. With a potential for forming graphene films on large-scale Si wafers, GOS is a powerful candidate as a key technology in bringing graphene into silicon technology.

  • PDF

Reactive Dispersion and Mechanical Property of Dicyanate/Montmorillonite Nanocomposite (반응이 수반된 Dicyanate/Montmorillonite Nanocomposite의 분산과 물성특성 연구)

  • 장원영;이근제;남재도
    • Polymer(Korea)
    • /
    • v.27 no.1
    • /
    • pp.75-83
    • /
    • 2003
  • Dicyanate-clay nanocomposite has been prepared by a melt in-situ polymerization method for different modifiers and cation exchange capacity (CEC) values in order to study dispersion and mechanical property. Various dicyanate nanocomposites were prepared by using different MMT systems containing different intercalants which led to different initial gallery heights and packing density. Depending on compatibility between dicyanate and clays, the degree of dispersion varied. Dispersion of clay plates in dicyanate resin depended mainly on CEC and aliphatic chain length of modifier. The lower CEC and shorter aliphatic chain length of modifier gave the exfoliation structure. It was also found that the reactivity of intercalant with dicyanate resin was one of the key factors facilitating the intercalation/exfoliation process of dicyanate/MMT nanocomposites. Shear modulus of reaction-induced dicyanate nanocomposite was significantly increased.

Preparation of poly(methyl methacrylate)/clay nanocomposites by microwaveassisted in-situ radical polymerization

  • Jeong, Ji-Won;Kim, Dong-Hyun;Jang, Jae-Ho;Lee, Jung-Taek;Yoo, Kyung-Hyeon;Yoon, Seog-Young
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.29 no.1
    • /
    • pp.19-23
    • /
    • 2019
  • The PMMA (polymethyl methacrylate)/clay nanocomposites were synthesized by in situ radical polymerizations with different clay contents (3 and 7 wt%) using microwave heating. The nanostructure, optical, and thermal properties of the synthesized PMMA/clay nanocomposites were measured by XRD, TEM, AFM, UV-vis, and TGA. It was found that the intercalated- or exfoliated structure of PMMA/clay nanocomposites was strongly dependent on the content of clay. Thus, the imposition of microwave-assisted polymerization facilitated a delamination process of layered silicates to achieve exfoliation state of interlayer distance. The PMMA/3 wt% C10A nanocomposite with well-dispersed and exfoliated clay nano-layers showed the good optical transparency similar to pure PMMA in this study. The thermal decomposition rates of the PMMA/clay nanocomposites become to be lower compared to that of the pure PMMA, indicating the intercalated- or exfoliated inorganic silicate has high thermal stability. A possible reason is that the thermally segmental motion of PMMA polymer into inorganic silicate interlayer spacing has increased the thermal stability of the PMMA/clay nanocomposites.

PREMATURE ERUPTION OF PERMANENT SUCCESSORS : A CASE REPORT (영구 계승치의 조기 맹출에 관한 증례 보고)

  • Koo, Hyun-Jung;Lee, Jae-Cheoun;Hahn, Se-Hyun
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.26 no.2
    • /
    • pp.232-239
    • /
    • 1999
  • Exfoliation of the primary teeth and eruption of the permanent teeth is a normal and predictable physiologic process. The accurate prediction of tooth development is of major importance in treatment planning for children. Norms that correspond to the child's age and development have been determined by many investigators. However, there are a variety of factors that may hasten, retard, or otherwise affect the normal developmental process. Among the factors that influence tooth eruption is the premature loss of primary teeth. An abscess of a primary molar, followed by bone resorption and early extraction or exfoliation may lead to premature eruprion of the permanent succesor, and a variety of clinical sequelae. I, hereby present the patients who have prematurely erupted permanent successor in Seoul National University Hospital Pediatric Dentistry, and report the clinical and radiologic characteristics, its sequelae, proper managements, and followed up findings.

  • PDF

Flame Retardant Treatment's Effects and Detection Method on Wooden Buildings' Pigment Layer (Dan-cheong) (국내 목조건축물 단청의 방염제 처리에 따른 영향 및 탐지방법 연구)

  • Kim, Dae Woon;Kim, Chul Woong;Han, Sung Hee;Chung, Yong Jae;Han, Gyu Seong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.42 no.4
    • /
    • pp.393-406
    • /
    • 2014
  • To figure out the problems of flame retardant treatment (FRT) on wooden buildings, field investigation and analysis of statistical data are performed. After FRT on historical wooden building, efflorescence and exfoliation showed most often. These problems appeared especially on column, rafter and Ga-gu (Ingredients for supporting structure of a roof) which are liberally spreaded. To compare before and after FRT, analyzed 20 elements using P-XRF. In this process, found sulfur which informs FRT. This helped set up nondestructive assay. Through this process, confirmed field application by analysis residue component of Songgwang-sa Temple.

The exfoliation of irradiated nuclear graphite by treatment with organic solvent: A proposal for its recycling

  • Capone, Mauro;Cherubini, Nadia;Cozzella, Maria Letizia;Dodaro, Alessandro;Guarcini, Tiziana
    • Nuclear Engineering and Technology
    • /
    • v.51 no.4
    • /
    • pp.1037-1040
    • /
    • 2019
  • For the past 50 years, graphite has been widely used as a moderator, reflector and fuel matrix in different kinds of gas-cooled reactors. Resulting in approximately 250,000 metric tons of irradiated graphite waste. One of the most significant long-lived radioisotope from graphite reactors is carbon-14 ($^{14}C$) with a half-life of 5730 years, this makes it a huge concern for deep geologic disposal of nuclear graphite (NG). Considering the lifecycle of NG a number of waste management options have been developed, mainly focused on the achievement the radiological requirements for disposal. The existing approaches for recycling depend on the cost to be economically viable. In this new study, an affordable process to remove $^{14}C$ has been proposed using samples taken from the Nuclear Power Plant in Latina (Italy) which have been used to investigate the capability of organic and inorganic solvents in removing $^{14}C$ from exfoliated nuclear graphite, with the aim to design a practicable approach to obtain graphite for recycling or/and safety disposed as L& LLW.

A Brief Review on 2-Dimensional Dielectric Nanosheets (이차원 유전체 나노시트의 개발 동향)

  • Yim, Haena;Choi, Ji-Won
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.35 no.1
    • /
    • pp.1-10
    • /
    • 2022
  • Two-dimensional materials have shown a great promise for the next-generation electronic materials due to their unique optical, physical, and chemical properties that are distinct from their bulk counterparts. Their atomic-level thickness, the feature for flexible tenability, and exposed huge surface allow various approaches for high-performance nanoscale devices. Especially, this review highlights the recent progress on two-dimensional dielectric nanosheets, which are obtained by cheap and massproducible solution-based exfoliation process, accompanied by the preparation methods, various deposition methods, and the characteristics of devices using a dielectric nanosheet thin films. We also present a perspective on the advantages offered by this two-dimensional dielectric nanosheets for the upcoming future nanoelectonics.

Rates and Processes of Bare Patch Denudation in the Subalpine Grassland of Mt. Halla (한라산 아고산 초지대 나지의 확대속도와 침식작용)

  • Kim, Tae-Ho
    • Journal of the Korean Geographical Society
    • /
    • v.41 no.6 s.117
    • /
    • pp.657-669
    • /
    • 2006
  • Rates and processes of bare patch denudation were observed at Janggumokoreum(1,710m) and Minoruem(1,600m) in order to clarify some characteristics of turf exfoliation in the subalpine grassland of Mt. Halla. The bare patches have marginal terrace fronts with a maximum height of 85 cm. The terrace risers usually develop an overhanging edge 2 to 38 cm long that eventually hangs down and protects the riser beneath. The patches are largely covered with angular pebbles and cobbles. The mean rate of riser retreat for the period 2002-2004 is 39.2 mm, equivalent to 19.6 mm/yr. However, there is a disparity of the rate of riser retreat at individual sites. The maximum rate is 131 mm measured at Janggumokoreum patch while the minimum rate is 0 mm at Minoreum patch. The rate of riser retreat also varies with seasons. The thawing season of April exhibits a maximum rate of retreat. The freezing season of October and November and the rainy season of June and July show relatively high rates of retreat. Several Processes such as frost action, aeolian deflation, rainwash, rainsplash and fauna activity cause the denudation of bare patches. In particular, the needle ire action which is combined with rainwash or deflation plays a primary role in turf exfoliation due to the diurnal freeze-thaw cycles occurred over 100 days, melted snow and strong wind in the subalpine zone of Mt. Halla. Rainwash is also an important contributing process in the rainy season because Mt. Halla has the highest precipitation in Korea. By contrast, rainsplash erosion has a minor effect on the bare patch denudation due to the overhanging edge of terrace risers. Recent increase in roe deer appears to be responsible for turf destruction.

Acoustic Emission Characteristics of Plasma Sprayed Ceramic Coating Layer after Salt Spray (플라즈마용사 세라믹코팅 피막부식재의 음향방출 특성)

  • 김귀식;박경석;홍용의
    • Journal of Ocean Engineering and Technology
    • /
    • v.15 no.3
    • /
    • pp.69-74
    • /
    • 2001
  • This paper was to investigate of a adhesiveness for the plasma sprayed coating materials did salt spray by acoustic emission method in tensile loadings. The powders used for the coating were nickel aluminum composite powder Ni-4.5wt.%Al and titanium dioxide powder $TiO_2$. These powders were coated on a carbon steel S45C by plasma spray method. The result solution was a 5% NaCl and the slat spray times were 2, 5 and 10 hours respectively. The salt solution penetrated into the surface of the substrate through pore of the coating layer built in the process of plasma spay. Corrosion productions formed on the surface of substrate. The adhesiveness between the substrate and the coating layer is weaken by corrosion and the exfoliation initiated chiefly at the corrosion surface of the substrate. The AE events and energy of the corroded coating specimens decreased as the salt spray times increased.

  • PDF

Acoustic Emission Characteristics of Plasma Sprayed Ceramic Coating Layer after Salt Spray (플라즈마용사 세라믹코팅 피막부식재의 음향방출 특성)

  • 김귀식;박경석;홍용의
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2001.05a
    • /
    • pp.344-349
    • /
    • 2001
  • This paper was to investigate of a adhesiveness for the plasma sprayed coating materials did salt spray by acoustic emission method in tensile loadings. The powders used for the coating were nickel aluminum composite powder Ni-4,5wt.%Al and titanium dioxide powder Ti02. These powders were coated on a carbon steel S45C by plasma spray method. The salt solution was a 5% NaCl and the salt spray times were 2, 5 and 10 hours respectively. The salt solution penetrated into the surface of the substrate through pore of the coating layer built in the process of plasma spay. Corrosion productions formed on the surface of substrate. The adhesiveness between the substrate and the coating layer is weaken by corrosion and the exfoliation initiated chiefly at the corrosion surface of the substrate. The AE events and energy of the corroded coating specimens decreased as the salt spray times increased.

  • PDF