• Title/Summary/Keyword: Equiaxed microstructure

Search Result 130, Processing Time 0.022 seconds

Formation of ultrafine Grains in the Al 5083 Alloy by Cryogenic Rolling Process (극저온 압연에 의한 초세립 Al 5083 Alloy 제조)

  • 이영범;심혜정;남원종
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2003.10a
    • /
    • pp.163-167
    • /
    • 2003
  • The large deformation at cryogenic temperature would be one of the effective methods to produce large bulk UFG materials. The effects of annealing temperature 150∼300$^{\circ}C$, on microstructure and mechanical properties of the sheets received 85% reduction at cryogenic temperature were investigated. In comparison with those at room temperature. Annealing of 5083 Al alloy deformed 85%, at 200$^{\circ}C$ for an hour, results in the considerable increase of tensile elongation without the great loss of strength and the occurrence of equiaxed grains less than 300nm in diameter.

  • PDF

Effect of Initial Orientation and Austenitic Phase on Texture Evolution in Ferritic Stainless Steels (페라이트계 스테인레스강의 집합조직 형성에 미치는 초기 방위 및 오스테나이트사의 영향)

  • 이용득
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1999.03a
    • /
    • pp.149-152
    • /
    • 1999
  • The effect of initial orientation on the microstructure and texture evolution of two ferritic stainless steels was investigated. the columnar and equiaxed crystal specimens which were prepared from continuous casting slab were hot rolled annealed cold rolled and annealed respectively. The rolling and recrystallization textures at each process stage were examined by orientation distribution function (ODF) and electron back-scattered diffraction (EBSD); The observation showed that the orientation density of the $\alpha$-fibre of hot rolled band of columnar crystal specimen was more pronounced than that of the equaxed one at the center layer. Nevertheless the cold rolled textures of Type 430 steel have demonstrated a rather similar development . Compared to Type 430 steel the development of the $\alpha$-fibre in the center layer of Type 409L steel was much more pronounced. The relation between texture evolution and ridging behaviour has been discussed.

  • PDF

Effect of Microstructures on the Deformation Behavior of Ti-6Al-4V Alloy at Ultra High Strain rate (Ti-6Al-4V합금의 미세조직에 따른 초고속 변형특성)

  • 이유환;이동근;이성학;최준홍;허선무;이종수
    • Journal of the Korea Institute of Military Science and Technology
    • /
    • v.5 no.3
    • /
    • pp.89-97
    • /
    • 2002
  • In this study, the effect of $\alpha$-phase morphology on the dynamic deformation behavior at ultra high strain rate was investigated by EBW(Explosive Bridge Wire) test. All of tests and analyses were conducted on three typical microstructures of Ti-6Al-4V alloy, i.e. equiaxed, widmanstatten and bimodal microstructures. The spall strength and HEL(Hugoniot Elastic Limit) of the specimens that have the thickness of 2mm and 4mm were highest with the bimodal microstructure. These results were similar with previous study which was performed by dynamic torsion test(Kolsky torsion test).

Effect of SiC mean particle size on mechanical properties and microstructure of $Si_{3}N_{4}/SiC$ nanocomposites (SiC 입자크기가 $Si_{3}N_{4}/SiC$ 초미립복합재료의 기계적 특성과 미세구조에 미치는 영향)

  • 황광택;김창삼;정덕수;오근호
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.6 no.3
    • /
    • pp.392-398
    • /
    • 1996
  • $Si_{3}N_{4}/SiC$ nanocomposites reinforced with tow different mean particle size were fabricated by hot press. Grain growth of matrix gran was inhibited by adding of SiC particles, and then number of equiaxed and fine grains were increased. The effect of grain growth inhibition was higher in the nanocomposites dispersed small size SiC. herefore fracture strength and hardness were increased, but fracture toughness was decreased in small size SiC dispersed samples.

  • PDF

Post-heat Treatment Properties of Thixoformed of A357 Al Alloy Product (반응고 성형된 A357 Al 합금 성형품의 후열처리 특성)

  • Choi, W.H.;Shin, P.W.;Lee, S.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.16 no.1
    • /
    • pp.16-25
    • /
    • 2003
  • Recently, semi-solid forming (SSF) Process has been applied in many automobile parts for improved weight reduction, better environmental protection and energy savings. SSF process was well developed for high volume production of light weight aluminum components. In this paper, knuckle has been manufactured by SSF and then the microstructures and mechanical properties were investigated followed by various heat-treatment conditions. It was found that the examined microstructure was equiaxed at the whole cross-section area.

Effect of Initial Microstructures on Hot Formability of Ti-10V-2Fe-3Al Alloy (Ti-10V-2Fe-3Al 합금의 열간성형성에 미치는 초기미세조직의 영향)

  • 신동혁
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1999.03b
    • /
    • pp.153.2-158
    • /
    • 1999
  • A study has been made to investigate how the fomability of Ti-10V-2Fe-3Al alloy is related to the initial microstructure and process variables such as temperature and strain rate. It has been found that the deformation resistance at high temperature is increased with the increase in the thickness of grain boundary a (GB)a and/or acicular a phase and however the effect of a morphology on the hot formability is considered insignificant due to the breakage of GB a and/or acicular a into several equiaxed a particles

  • PDF

PREFERRED ORIENTATION AND MICROSTRUCTURE OF MOD DERIVED SrBi$_{2x}$Ta$_2$O$_9$ THIN FILMS WITH Bi CONTENT x

  • Yeon, Dae-Joong;Park, Joo-Dong;Oh, Tae-Sung
    • Journal of the Korean institute of surface engineering
    • /
    • v.29 no.6
    • /
    • pp.621-627
    • /
    • 1996
  • $SrBi_{2x}TaO_9$ ferroelectric thin films were prepared on platinized silicon substrates using MOD proces, and crystallization behavior of the films was investigated with variation of the annealing temperature and Bi content x. Crystalline phase of bismuth layered perovskite structure was formed even by baking the films at $800^{\circ}C$ for 5 minutes in air, and was not changed by annealing at temperatures raning from $700^{\circ}C$ to $900^{\circ}C$ for 1 hour in oxygen ambient. When $SrBi_{2x}TaO_9$ thin films ($0.8\lex\ie1.6$) were annealed at $800^{\circ}C$, Preferred orientation of the films along c-axis was observed with $x\ge1.2$. With increasing Bi content x, surface morphology of the films was changed from equiaxed grains to elongated grains.

  • PDF

Effect of AIN on properties of materials for spectacle lens cutting (AIN첨가가 안경렌즈 절삭용 재료특성에 미치는 영향)

  • Lee, Young ll
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.7 no.1
    • /
    • pp.25-27
    • /
    • 2002
  • To improve the properties of materials for spectacle lens cutting. AIN was included as a sintering additive. The amount of AIN was 0, 1, 3, 5 wt% and materials for spectacle lens cutting were fabricated by hot-pressing at $1830^{\circ}C$ for 2h. Microstructure was consisted of equiaxed SiC and elongated TIC. Typical fracture toughness and hardness of materials for spectacle lens cutting with AIN $4.8MPa{\cdot}m^{1/2}$ and 15.3 GPa, respectively.

  • PDF

Microstructural Evolution during the Equal Channel Angular Pressing of Ti-6Al-4V Alloy (Ti-6Al-4V 합금의 ECAP 가공시 미세 조직의 변화 연구)

  • 고영건;정원식;신동혁;이종수
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2002.05a
    • /
    • pp.177-180
    • /
    • 2002
  • The effects of pressing temperatures on the formability and the microstructural evolution during equal channel angular pressing (ECAP) of lamellar Ti-6Al-4V alloy were investigated in this study. ECAP above isothermally 600$^{\circ}C$ was successful without producing any noticeable segments at the specimen surfaces after a single pass of pressing. After 4 passes of ECA pressing, lamellar microstructures were significantly refined revealing equiaxed grains of 0.3$\mu\textrm{m}$ in diameter consisting of high angle grain boundaries. Also these ultrafine grains were relatively stable with little grain growth when annealed up to 600$^{\circ}C$ for 1hour.

  • PDF

Mechanical and electrical responses of submicrocrystalline Cu-3%Ag alloy (초미세 결정립 Cu-3%Ag 합금의 기계적 물성과 전기 전도도)

  • Ko, Y.G.;Lee, C.W.;NamGung, S.;Shin, D.H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2009.05a
    • /
    • pp.413-416
    • /
    • 2009
  • The paper deals with the mechanical and electrical responses of submicrocrystalline Cu-3%Ag alloy as a function of strain imposed by equal-channel angular pressing. When inducing the effective strain of 12, the initial grain site of ${\sim}50{\mu}m$ is evidently reduced within the range of $0.2-0.3{\mu}m$ in size, having a reasonably equiaxed shape. The results of tension tests at room temperature exhibit that the tensile strength of the present alloy increases with increasing the amount of strain whereas losing electrical conductivity slightly. This phenomenon can be explained based on fine grained structure together with the non-equilibrium state of grain boundaries.

  • PDF