• Title/Summary/Keyword: Elongation and Hardness

검색결과 364건 처리시간 0.101초

Study of different flexible aeration tube diffusers: Characterization and oxygen transfer performance

  • Hongprasith, Narapong;Dolkittikul, Natchanok;Apiboonsuwan, Kamolnapach;Pungrasmi, Wiboonluk;Painmanakul, Pisut
    • Environmental Engineering Research
    • /
    • 제21권3호
    • /
    • pp.233-240
    • /
    • 2016
  • The research aims to study the different flexible rubber tube diffusers used in urban wastewater treatment processes and aquaculture systems. The experiment was conducted in small-scale aeration tank with different physical properties of the tubes that were used as aerators. The volumetric mass transfer coefficient ($k_La$), oxygen transfer efficiency (OTE) and aeration efficiency (AE) were measured and determined to compare the diffusers. Moreover, the bubble hydrodynamic parameters were analyzed in terms of bubble diameter ($d_B$) and rising velocity ($U_B$) by a high speed camera (2,000 frames/s). Then the interfacial area (a) and liquid-side mass transfer coefficient ($k_L$) can be calculated. The physical properties (tube wall thickness, tensile strength, orifice size, hardness and elongation) have been proven to be the key factor that controls the performance (kLa and OTE). The effects of hardness and elongation on bubble formation, orifice size and a-area were clearly proved. It is not necessary to generate too much fine bubbles to increase the a-area: this relates to high power consumption and the decrease of the kL. Finally, the wall thickness, elongation and hardness associated of the flexible tube diffuser (tube No. 12) were concluded, to be the suitable properties for practically producing, in this research.

600MPa급 TRIP강의 $CO_2$ 및 Nd:YAG 레이저 용접부의 특성 (Characteristics of $CO_2$ or Nd:YAG Laser Welded 600MPa Grade TRIP Steel)

  • 한태교;김성준;이봉근;김대업;강정윤
    • Journal of Welding and Joining
    • /
    • 제24권1호
    • /
    • pp.56-63
    • /
    • 2006
  • The characteristics of $CO_2$ or Nd:YAG laser welded 600MPa ade TRIP steel was investigated. He or Ar gas was used as a shield gas in case of $CO_2$ laser welding, but the shield gas was not used in case of Nd:YAG laser welding. Bead on plate welding was performed with various welding conditions. Defects in the joints of both welding type occurred at 1.8m/min but were not observed over the welding speed of 2.1m/min in case of Nd:YAG laser welding. However, porosity occurred in $CO_2$ laser welding and the tendency of decreasing with the increase of welding speed. The hardness was the highest at heat affected zone near fusion zone as well as at the fusion zone and decreased on approaching the base metal. In a perpendicular tensile test to the weld line, all specimens that have been welded at optimum conditions were fractured at the base metal, and the tensile properties showed the rather higher than those of raw material. In a parallel tensile test, the strength of the joints was higher than that of the base metal. Elongation was found to be lower than that of the raw material. Forming height by Erichsen test and elongation were deeply related with the ratio of base metal/weld metal and the maximum hardness of the weld metal. Also porosity induced to decrease the strength and the elongation. The maximum formability was recorded at approximately 80% as compared with that of the raw material with the optimum condition.

고 Mn 오스테나이트계 스테인리스강의 기계적 성질에 미치는 가공온도의 영향 (Effect of Deformation Temperature on Mechanical Properties of High Manganese Austenitic Stainless Steel)

  • 강창룡;허태영;김영화;구차진;한현성;이상희
    • 한국해양공학회지
    • /
    • 제26권3호
    • /
    • pp.55-60
    • /
    • 2012
  • This study was carried out to investigate the effect of the deformation temperature in high manganese austenitic stainless steel. ${\alpha}$'-martensite was formed with a specific direction by deformation. The volume fraction of the deformation induced martensite was increased by increasing the degree of deformation and decreasing the deformation temperature. With the increase in the deformation, the hardness and tensile strength were increased, while the elongation was rapidly decreased at the initial stage of the deformation, and then gradually decreased. The hardness and tensile strength were increased and the elongation was decreased with adecrease in the deformation temperature. The hardness and tensile strength were strongly controlled by the volume fraction of martensite, but the elongation was controlled by the transformation behavior of the deformation induced martensite.

PVC 컴파운드의 기계적 물성에 대한 가소제의 영향 (Effect of Plasticizers on Mechanical Properties of PVC Compounds)

  • 오대희;김대진;서관호
    • Elastomers and Composites
    • /
    • 제34권5호
    • /
    • pp.391-398
    • /
    • 1999
  • 폴리염화비닐(PVC)에 프탈산계 가소제인 di-2-ethyl hexyl phthalate (DOP)와 아디프산계 가소제인 di-2-ethyl hexyl adiphate (DOA)를 혼련하였다. 혼련한 컴파운드의 비중, 인장강도, 신율, 경도, 내마모성, 내한굴곡성을 측정하였다. 먼저 PVC의 중합도에 따른 물성을 알아보면, 중합도 2500인 PVC를 사용한 컴파운드(이하 P2500계)가 중합도 1300인 PVC를 사용한 컴파운드(이하 P1300계)보다 인장강도, 경도에서 상대적으로 우수하게 나타났고, 신율, 내마모성, 내한굴곡성에서는 P1300계가 P2500계 보다 우수하게 나타났다. 그리고, 비중은 PVC의 중합도에 상관없이 비슷하게 나타났다. 또 가소제의 종류에 따른 PVC 컴파운드의 기계적 물성을 알아보면, 가소제로 DOP를 첨가한 PVC 컴파운드(이하 DOP계)가 DOA를 첨가한 PVC 컴파운드(이하 DOA계)보다 인장강도, 신율에서 우수하게 나타났고, 내마모성, 내한굴곡성에서는 DOA계가 상대적으로 DOP계보다 우수하게 나타났다. 그리고 경도는 DOP계가 높게, 비중은 DOA계가 더 낮게 나타났다.

  • PDF

H-NBR/NBR 블렌드의 열노화거동 (Thermal Aging Behavior of H-NBR/NBR Blend)

  • 최원석;김건완;도제성;유명우;류승훈
    • Elastomers and Composites
    • /
    • 제46권2호
    • /
    • pp.132-137
    • /
    • 2011
  • 본 연구는 H-NBR 함량 변화에 따른 H-NBR/NBR 블렌드의 열노화 거동에 대하여 살펴보았다. 이 때 가교제로는 dicumyl peroxide와 황 혼합물을 사용하였으며, 열노화에 따른 H-NBR/NBR 블렌드의 인장강도, 파괴신율, 경도 그리고 내마모성의 변화를 살펴보았다. H-NBR을 첨가함에 따라 인장강도는 증가하였으나 내마모성은 감소하는 현상을 나타내었다. 파괴신율과 경도는 H-NBR의 영향을 받지 않았다. 노화가 진행된 모든 시편은 초기 시편보다 낮은 인장강도, 파괴신율, 경도를 나타내었다. 그러나 H-NBR의 함량이 증가함에 따라 이러한 물성저하 속도가 감소함을 알 수 있었다. 즉 H-NBR 첨가에의해 열노화 특성이 향상됨을 알 수 있었다. 모든 NBR/H-NBR 블렌드는 노화시간이 증가함에 따라 내마모성이 감소하였으며, H-NBR을 첨가한 경우 내마모성의 저하가 상대적으로 낮음을 알 수 있었다.

베이나이트계 후판강의 모재 및 열영향부의 미세조직과 기계적 특성에 미치는 화학 조성의 영향 (Effect of Chemical Compositions on Microstructure and Mechanical Properties of Base Metal and HAZ of Bainitic Steel Plates)

  • 조성규;주형건;신상용
    • 한국재료학회지
    • /
    • 제29권4호
    • /
    • pp.211-220
    • /
    • 2019
  • In this study, three kinds of bainitic steel plates are manufactured by varying the chemical compositions and their microstructures are analyzed. Tensile and Charpy impact tests are performed at room and low temperature to investigate the correlation between microstructure and mechanical properties. In addition, heat affected zone (HAZ) specimens are fabricated by a simulation of welding processes, and the HAZ microstructure is analyzed. The base steel that has the lowest carbon equivalent has the highest volume fraction of acicular ferrite and the lowest volume fraction of secondary phases, so the strength is the lowest and the elongation is the highest. The Mo steel has a higher volume fraction of granular bainite and more secondary phases than the base steel, so the strength is high and the elongation is low. The CrNi steel has the highest volume fraction of the secondary phases, so the strength is the highest and elongation is the lowest. The tensile properties of the steels, namely, strength and elongation, have a linear correlation with the volume fraction of secondary phases. The Mo steel has the lowest Charpy impact energy at $-80^{\circ}C$ because of coarse granular bainite. In the Base-HAZ and Mo-HAZ specimens, the hardness increases as the volume fraction of martensite-austenite constituents increases. In the CrNi-HAZ specimen, however, hardness increases as the volume fraction of martensite and bainitic ferrite increases.

Ni-Co 합금강의 기계적 특성에 대한 탄소함량의 영향 (Influence of Carbon Content on the Mechanical Properties of the Ni-Co Alloy)

  • 장경천;국중민;정장만;권택용;최병기
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2004년도 춘계학술대회 논문집
    • /
    • pp.129-135
    • /
    • 2004
  • This study was to evaluate the effect of carbon content on metallic change and fatigue characteristics with Fe-29% Ni-17% Co, low heat expansion alloy, widely using electronic components, precision machines, and sealing with glass and metal etc. The steels were fabricated with variation of carbon content, 0, 0.03, 0.06, 0.1, and 0.20% with VIM and tensile test and fatigue test were performed to achieve the above purpose. The more carbon content, the higher hardness value and yield strength. But elongation of 0.03%C, 0.06%C, and 0.10%C specimen decreased about 2.2%, 1.5% and 0.8% respectively mote than that of the base metal. Especially the strength and elongation of 0.20%C specimen increased simultaneously about 14.4% and 7.5%. Fatigue life of 0.03%C specimen decreased but the more carbon content, the higher fatigue life over 0.06% carbon content more than that of base metal.

  • PDF

200 Grade 마르에이징강의 기계적성질 향상을 위한 연구 (A Study on the Promotion. of Mechanical Properties for 200 Grade Maraging Steel)

  • 장경천;국중민;이동길;최병기
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2004년도 추계학술대회 논문집
    • /
    • pp.60-66
    • /
    • 2004
  • Hardness value decreased about 3% for annealed specimens and increased about 60% for one hour aged specimens. But the values of the other specimens aged two hours or more showed almost the same. The yield strength was the highest about 1,800㎫ in 0.06%Nb specimen having twice as much as the base meta1 specimen. Also, the elongation was the highest in 0.03%Nb specimen showing the same as base metal specimen. The higher aging temperature and the longer aging time, the higher fatigue life. On the other hand, the 0.03%Nb specimen showed the highest fatigue life which increased about 12% more than base metal specime. 0.06%Nb specimen aged at 482$^{\circ}C$ for 8 hours simultaneously satisfied the 250 grade strength and 200 grade elongation having the most superior mechanical properties.

  • PDF

ECAP 가공에 의해 제조된 초미세립 OFHC Cu 봉재의 미세조직 및 기계적 특성의 균질성 (Homogeneity of Microstructure and Mechanical Properties of Ultrafine Grained OFHC Cu Bars Processed by ECAP)

  • 지정훈;박이주;김형원;황시우;이종수;박경태
    • 대한금속재료학회지
    • /
    • 제49권6호
    • /
    • pp.474-487
    • /
    • 2011
  • Bars of OFHC Cu with the diameter of 45 mm were processed by equal channel angular pressing up to 16 passes via route $B_c$, and homogeneity of their microstructures and mechanical properties was examined at every four passes which develop the equiaxed ultrafine grains. In general, overall hardness, yield strength and tensile strength increased by 3, 7, and 2 times respectively compared with those of unECAPed sample. Cross-sectional hardness exhibited a concentric distribution. Hardness was the highest at the center of bar and it decreased gradually from center to surface. After 16 passes, overall hardness decreased due to recovery and partial recrystallization. Regardless of the number of passage, yield strength and tensile strength were quite uniform at all positions, but elongation showed some degree of scattering. At 4 passes, coarse and ultrafine grains coexisted at all positions. After 4 passes, uniform equiaxed ultrafine grains were obtained at the center, while uniform elongated ultrafine grains were manifested at the upper half position. At the lower half position, grains were equiaxed but its size were inhomogeneous. It was found that inhomogeneity of grain morphology and grain size distribution at different positions are to be attributed to scattering in elongation but they did not affect strength. The present results reveal the high potential of practical application of equal channel angular pressing on fabrication of large-sized ultrafine grained bars with quite homogeneous mechanical properties.

오스템퍼링한 低合金 球狀黑鉛鑄鐵의 機械的 性質에 관한 硏究 (A study on the mechanical properties of austempered low-alloy ductile cast iron)

  • 강명순;박흥식
    • 대한기계학회논문집
    • /
    • 제12권6호
    • /
    • pp.1296-1302
    • /
    • 1988
  • The study has been carried out under various experimental conditions to investigate mechanical properties by the transformation conditions of austempered low-alloy ductile cast iron. The amount of retained austenite and bainite after quenching was determined by the X-ray diffractometer and the point counting method and which the microstructure was investigated by the S.E.M. The mechanical properties of austempered low-alloy ductile cast iron can be varried over a comparatively wide range by changing the transformation conditions. During isothermal transformation of austenite in the bainite region, low-alloy ductile cast iron austempered at holding time of 40 minute has the maximum volume fraction(24%) of retained austenite in the cast iron matrix and which optimum values of mechanical properties correspond to the maximum amount of retained austenite, which falls with decreasing transformation temperature. The low values of both tensile strength and elongation in the initial stage of bainite transformation can be explained by premature fracture of tensile specimens and the tensile strength, hardness and elongation do not change considerably after a certain period. With a decreasing transformation temperature the tensile strength increase while the elongation decrease, especially the elongation has the maximum value at temperature $370^{\circ}C$.