• Title/Summary/Keyword: Electron diffraction data

Search Result 158, Processing Time 0.021 seconds

Analysis of surface characteristics of (Y, Nb)-TZP after finishing and polishing

  • Seong-keun, Yoo;Ye-Hyeon, Jo;In-Sung Luke, Yeo;Hyung-In, Yoon;Jae-Hyun, Lee;Jin-Soo, Ahn;Jung-Suk, Han
    • The Journal of Advanced Prosthodontics
    • /
    • v.14 no.6
    • /
    • pp.335-345
    • /
    • 2022
  • PURPOSE. This in vitro study aimed to evaluate the surface characteristics of a full veneer crown fabricated chairside (CS) from a (Y, Nb)-TZP zirconia block in response to conventional zirconia grinding and polishing. MATERIALS AND METHODS. Zirconia crowns (n = 40) were first prepared and divided into two groups of materials: Labside (LS) and CS, after which each specimen went through a five-step grinding and polishing procedure. Following each surface treatment, surface characteristics were analyzed using confocal laser microscopy (CLSM), average surface roughness (Ra) values were processed from the profile data through Gaussian filtering, and X-ray diffraction pattern analysis was performed to evaluate the monoclinic (M) phase content. Then, a representative specimen was selected for field-emission scanning electron microscopy (FE-SEM), followed by a final analysis of the roughness and X-ray diffraction of the specimens using the independent t-test and repeated measures analysis of variance (RM-ANOVA). RESULTS. In every group, polishing significantly reduced the Ra values (P < .001). There was no significant difference in Ra between the polished state CS and LS. Furthermore, CLSM and FE-SEM investigations revealed that even though grain exposure was visible in CS specimens throughout the as-delivered and ground states, the exposure was reduced after polishing. Moreover, while no phase transformation was visible in the LS, phase transformation was visible in CS after every surface treatment, with the M phase content of the CS group showing a significant reduction after polishing (P < .001). CONCLUSION. Within the limits of this study, clinically acceptable level of surface finishing of (Y, Nb)-TZP can be achieved after conventional zirconia polishing sequence.

Influence of Co incorporation on morphological, structural, and optical properties of ZnO nanorods synthesized by chemical bath deposition

  • Iwan Sugihartono;Novan Purwanto;Desy Mekarsari;Isnaeni;Markus Diantoro;Riser Fahdiran;Yoga Divayana;Anggara Budi Susila
    • Advances in materials Research
    • /
    • v.12 no.3
    • /
    • pp.179-192
    • /
    • 2023
  • We have studied the structural and optical properties of the non-doped and Co 0.08 at.%, Co 0.02 at.%, and Co 0.11 at.% doped ZnO nanorods (NRs) synthesized using the simple low-temperature chemical bath deposition (CBD) method at 95℃ for 2 hours. The scanning electron microscope (SEM) images confirmed the morphology of the ZnO NRs are affected by Co incorporation. As observed, the Co 0.08 at.% doped ZnO NRs have a larger dimension with an average diameter of 153.4 nm. According to the International Centre for Diffraction Data (ICDD) number #00-036-1451, the x-ray diffraction (XRD) pattern of non-doped and Co-doped ZnO NRs with the preferred orientation of ZnO NRs in the (002) plane possess polycrystalline hexagonal wurtzite structure with the space group P63mc. Optical absorbance indicates the Co 0.08 at.% doped ZnO NRs have stronger and blueshift bandgap energy (3.104 ev). The room temperature photoluminescence (PL) spectra of ZnO NRs exhibited excitonicrelates ultraviolet (UV) and defect-related green band (GB) emissions. By calculating the UV/GB intensity, the Co 0.08 at.% is the proper atomic percentage to have fewer intrinsic defects. We predict that Co-doped ZnO NRs induce a blueshift of near band edge (NBE) emission due to the Burstein-Moss effect. Meanwhile, the redshift of NBE emission is attributed to the modification of the lattice dimensions and exchange energy.

Properties of Ferroelectric Materials Applicable to Nano-storage Media (탐침형 정보 저장장치에 응용 가능한 강유전체 물질의 특성 연구)

  • Choi J.S.;Kim J.S.;Hwang I.R.;Byun I.S.;Kim S.H.;Jeon S.H.;Lee J.H.;Hong S.H.;Park B.H.
    • Journal of the Korean Vacuum Society
    • /
    • v.15 no.2
    • /
    • pp.173-179
    • /
    • 2006
  • We have investigated structural and electrical properties of $PbZr_{0.3}Ti_{0.7}O_{3}$ (PZT) thin films deposited by pulsed laser deposition methods. PZT thin films have been deposited on $LaMnO_3$ (LMO) bottom electrodes with $LaAlO_3$ (LAO) substrates during different deposition times. High-resolution x-ray diffraction data have shown that all the PZT films and bottom electrodes are highly oriented. The thickness of each film is determined by field-emission scanning electron microscope. We have also observed root mean square roughness by using atomic force microscopy mode, and local polarization distribution and retention behavior of a ferroelectric domain by using piezoelectric force microscopy mode. A PZT/LMO structure has shown good ferroelectric and retention properties as the media for nano-storage devices.

Fabrication and Characterization of Lead Oxide (PbO) Film for High Efficiency X-ray Detector (고효율 X선 검출기 적용을 위한 PbO 필름 제작 및 특성 연구)

  • Cho, Sung-Ho;Kang, Sang-Sik;Choi, Chi-Won;Kwun, Chul;Nam, Sang-Hee
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.06a
    • /
    • pp.329-329
    • /
    • 2007
  • Photoconductive poly crystalline lead oxide coated on amorphous thin film transistor (TFT) arrays is the best candidate for direct digital x-ray detector for medical imaging. Thicker films with lessening density often show lower x-ray induced charge generation and collection becomes less efficient. In this work, we present a new methodology used for the high density deposition of PbO. We investigate the structural properties of the films using X-ray diffraction and electron microscopy experiments. The film coatings of approximately $200\;{\mu}m$ thickness were deposited on $2"{\times}2"$ conductive-coated glass substrates for measurements of dark current and x-ray sensitivity. The lead oxide (PbO) films of $200\;{\mu}m$ thickness were deposited on glass substrates using a wet coating process in room temperature. The influence of post-deposition annealing on the characteristics of the lead oxide films was investigated in detail. X-ray diffraction and scanning electron microscopy, and atomic force microscopy have been employed to obtain information on the morphology and crystallization of the films. Also we measured dark current, x-ray sensitivity and linearity for investigation of the electrical characteristics of films. It was found that the annealing conditions strongly affect the electrical properties of the films. The x-ray induced output charges of films annealed in oxygen gas increases dramatically with increasing annealing temperatures up to $500^{\circ}C$ but then drops for higher temperature anneals. Consequently, the more we increase the annealing temperatures, the better density and film quality of the lead oxide. Analysis of this data suggests that incorporation and decomposition reactions of oxygen can be controlled to change the detection properties of the lead oxide film significantly. Post-deposition thermal annealing is also used for densely film. The PbO films that are grown by new methodology exhibit good morphology of high density structure and provide less than $10\;pA/mm^2$ dark currents as they show saturation in gain (at approximate fields of $4\;V/{\mu}m$). The ability to operate at low voltage gives adequate dark currents for most applications and allows voltage electronics designs.

  • PDF

Characterization and Adsorption Properties of Red Mud/Fly Ash Based Geopolymers Adsorbent with Calcination Temperature (Red mud/fly ash 기반 geopolymer 흡착제의 소성온도에 따른 특성 및 흡착거동)

  • Jin-Yeong Shin;Han-Seong Kim;Hwa-Yeong Kang;Soon-Do Yoon
    • Applied Chemistry for Engineering
    • /
    • v.34 no.4
    • /
    • pp.412-420
    • /
    • 2023
  • In this study, red mud/fly ash based geopolymer adsorbents (RFGPA) were prepared with calcination temperatures of 200, 400, and 600 ℃, and the effects of these calcination temperatures on the adsorption of methylene blue (MB) were investigated. In addition, the prepared RFGPA was characterized using X-ray fluorescence (XRF), scanning electron microscopy (SEM), X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FT-IR) spectroscopy, and Brunauer-EmmettTeller (BET) analysis. The results of the adsorption kinetics of MB at RFGPA prepared calcination temperatures indicated that the adsorption equilibrium of MB was reached after about 72 h. From the results of the adsorption isotherm, we verified that the degree of adsorption increased with increasing MB concentrations. In addition, the adsorption amount (Q) of MB decreased with an increase in calcination temperature. The experimental adsorption isotherm data were well fitted to the Freundlich and Sips equations compared to the Langmuir equation. In order to verify the effects of photocatalytic decomposition (C/C0) of MB on Fe2O3 present in prepared RFGPA, the degree of decomposition of MB was examined under dark and visible conditions. Results indicated that the decomposition of MB in visible conditions was about 3.0 times faster than that in dark conditions.

Facile Synthesis of ZnO Nanoparticles and Their Photocatalytic Activity

  • Lee, Soo-Keun;Kim, A Young;Lee, Jun Young;Ko, Sung Hyun;Kim, Sang Wook
    • Bulletin of the Korean Chemical Society
    • /
    • v.35 no.7
    • /
    • pp.2004-2008
    • /
    • 2014
  • This paper reports the facile synthesis methods of zinc oxide (ZnO) nanoparticles, Z1-Z10, using diethylene glycol (DEG) and polyethylene glycol (PEG400). The particle size and morphology were correlated with the PEG concentration and reaction time. With 0.75 mL of PEG400 in 150 mL of DEG and a 20 h reaction time, the ZnO nanoparticles began to disperse from a collective spherical grain shape. The ZnO nanoparticles were characterized by X-ray diffraction, scanning electron microscopy, transmission electron microscopy and a $N_2$ adsorption-desorption studies. The Brunauer-Emmett-Teller (BET) surface areas of Z4, Z5 and Z10 were 157.083, 141.559 and 233.249 $m^2/g$, respectively. The observed pore diameters of Z4, Z5 and Z10 were 63.4, 42.0 and 134.0 ${\AA}$, respectively. The pore volumes of Z4, Z5 and Z10 were 0.249, 0.148 and 0.781 $cm^3/g$, respectively. The photocatalytic activity of the synthesized ZnO nanoparticles was evaluated by methylene blue (MB) degradation, and the activity showed a good correlation with the $N_2$ adsorption-desorption data.

Structural and thermal analysis of electrochemically Li intercalated synthetic graphite (전기 화학적으로 리튬이 층간 삽입된 인조흑연의 구조와 열적 특성 분석)

  • Oh, Won-Chun
    • Analytical Science and Technology
    • /
    • v.14 no.3
    • /
    • pp.197-202
    • /
    • 2001
  • The characteristics of the electrochemically Li intercalated synthetic graphite were determined from the studies with XRD method, DSC and solid $^7Li-NMR$ spectrophotometric analysis. From the results of X-ray diffraction method, it was found that the compounds in the stage 1 structure were predominantly formed. The enthalpy and entropy changes of the compounds can be obtained from the differential scanning calorimetric analysis results. From these results, it was found that exothermic and endothermic reactions of lithium intercalated into synthetic graphite are related to thermal stability of lithium ion between carbon graphene layers. From the $^7Li-NMR$ data, scientific observation found that bands are shift toward higher frequencies with increasing lithium concentration because non-occupied electron shells of Li increased in charge carrier density. Line widths of the Li intercalated synthetic graphite compounds decreased slowly because of non-homogeneous local magnetic order and the random electron spin direction for substituted Li.

  • PDF

A Novel Method to Calculate the Carbides Fraction from Dilatometric Measurements During Cooling in Hot-Work Tool Steel

  • Zhao, Xiaoli;Li, Chuanwei;Han, Lizhan;Gu, Jianfeng
    • Metals and materials international
    • /
    • v.24 no.6
    • /
    • pp.1193-1201
    • /
    • 2018
  • Dilatometry is a useful technique to obtain experimental data concerning transformation. In this paper, a dilation conversional model was established to calculate carbides fraction in AISI H13 hot-work tool steel based on the measured length changes. After carbides precipitation, the alloy contents in the matrix changed. In the usual models, the content of carbon atoms after precipitation is considered as the only element that affects the lattice constant and the content of the alloy elements such as Cr, Mo, Mn, V are often ignored. In the model introduced in this paper, the alloying elements (Cr, Mo, Mn, V) changes caused by carbides precipitation are incorporated. The carbides were identified using scanning electron microscope and transmission electron microscope. The relationship between lattice constant of carbides and temperature are measured by high-temperature X-ray diffraction. The results indicate that the carbides observed in all specimens cooled at different rates are V-rich MC and Cr-rich $M_{23}C_6$, and most of them are V-rich MC, only very few are Cr-rich $M_{23}C_6$. The model including the effects of substitutional alloying elements shows a good improvement on carbides fraction predictions. In addition, lower cooling rate advances the carbides precipitation for AISI H13 specimens. The results between experiments and mathematical model agree well.

Synthesis, Crystal Structure, Spectra Characterization and DFT Studies on a Di-Cycle Pyrazoline Derivative

  • Song, Jie;Zhao, Pu Su;Zhang, Wei Guang
    • Bulletin of the Korean Chemical Society
    • /
    • v.31 no.7
    • /
    • pp.1875-1880
    • /
    • 2010
  • A dicycle pyrazoline derivative, 1-phenyl-5-(p-fluorophenyl)-3,4-($\alpha$-p-fluoro-tolylenecyclohexano) pyrazoline, was synthesized and characterized by elemental analysis, IR, UV-vis, fluorescence spectra and X-ray single crystal diffraction. Density function theory (DFT) calculations were performed by using B3LYP method with 6-$311G^{**}$ basis set. The optimized geometry can well simulate the molecular structure. Vibrational frequencies were predicted, assigned and compared with the experimental values, which suggest that B3LYP/6-$311G^{**}$ method can well predict the IR spectra. Both the experimental electronic absorption spectra and the predicted ones by B3LYP/6-$311G^{**}$ method reveal three electron-transition bands, with the theoretical ones having some red shifts compared with the experimental data. Natural bond orbital analyses indicate that the absorption bands are mainly derived from the contribution of n $\rightarrow\pi^*$ and $\pi\rightarrow\pi^*$ transitions. Fluorescence spectra determination shows that the title compound can emit blue-light at about 478 nm. On the basis of vibrational analysis, the thermodynamic properties of title compound at different temperature have been calculated, revealing the correlations between $C^0_{p,m}$, $S^0_m$, $H^0_m$ and temperature.

High-Temperature Corrosion Characteristics of T22 and T92 Steel in SO2-Containing Gas at 650 ℃ (650 ℃의 SO2 가스 환경 하에서 T22와 T92 강의 고온 부식특성)

  • Jung, Kwang-Hu;Kim, Seong-Jong
    • Corrosion Science and Technology
    • /
    • v.18 no.6
    • /
    • pp.285-291
    • /
    • 2019
  • In this study, the corrosion characteristics of T22 and T92 steel were investigated in 6O2 + 16CO2 + 2SO2 gas environment at 650 ℃. Corrosion characteristics were characterized by weight gain, oxide layer thickness, scanning electron microscope, optical microscope, energy dispersive X-ray spectroscopy, and X-ray diffraction. T22 and T92 steel tended to stagnate oxide layer growth over time. Oxidation kinetics were analyzed using the data of oxide layer thickness, and a regression model was presented. The regression model was significantly acceptable. The corrosion rate between the two steels through the regression model showed significant difference. The T92 steel was approximately twice as large as the time exponent and showed very good corrosion resistance compared to the T22 steel. In both steels, the oxide layer mainly formed a Fe-rich oxide layer composed of hematite (Fe2O3), magnetite (Fe3O4), and spinel (FeCr2O4). Sulfide segregation occurred in the oxide layer due to SO2 gas. However, the locations of segregation for the T22 and T92 steel were different.