Browse > Article
http://dx.doi.org/10.4047/jap.2022.14.6.335

Analysis of surface characteristics of (Y, Nb)-TZP after finishing and polishing  

Seong-keun, Yoo (Department of Prosthodontics, School of Dentistry and Dental Research Institute, Seoul National University)
Ye-Hyeon, Jo (Dental Research Institute, Seoul National University School of Dentistry)
In-Sung Luke, Yeo (Department of Prosthodontics, School of Dentistry and Dental Research Institute, Seoul National University)
Hyung-In, Yoon (Department of Prosthodontics, School of Dentistry and Dental Research Institute, Seoul National University)
Jae-Hyun, Lee (Department of Prosthodontics, School of Dentistry and Dental Research Institute, Seoul National University)
Jin-Soo, Ahn (Department of Dental Biomaterials Science and Dental Research Institute, School of Dentistry, Seoul National University)
Jung-Suk, Han (Department of Prosthodontics, School of Dentistry and Dental Research Institute, Seoul National University)
Publication Information
The Journal of Advanced Prosthodontics / v.14, no.6, 2022 , pp. 335-345 More about this Journal
Abstract
PURPOSE. This in vitro study aimed to evaluate the surface characteristics of a full veneer crown fabricated chairside (CS) from a (Y, Nb)-TZP zirconia block in response to conventional zirconia grinding and polishing. MATERIALS AND METHODS. Zirconia crowns (n = 40) were first prepared and divided into two groups of materials: Labside (LS) and CS, after which each specimen went through a five-step grinding and polishing procedure. Following each surface treatment, surface characteristics were analyzed using confocal laser microscopy (CLSM), average surface roughness (Ra) values were processed from the profile data through Gaussian filtering, and X-ray diffraction pattern analysis was performed to evaluate the monoclinic (M) phase content. Then, a representative specimen was selected for field-emission scanning electron microscopy (FE-SEM), followed by a final analysis of the roughness and X-ray diffraction of the specimens using the independent t-test and repeated measures analysis of variance (RM-ANOVA). RESULTS. In every group, polishing significantly reduced the Ra values (P < .001). There was no significant difference in Ra between the polished state CS and LS. Furthermore, CLSM and FE-SEM investigations revealed that even though grain exposure was visible in CS specimens throughout the as-delivered and ground states, the exposure was reduced after polishing. Moreover, while no phase transformation was visible in the LS, phase transformation was visible in CS after every surface treatment, with the M phase content of the CS group showing a significant reduction after polishing (P < .001). CONCLUSION. Within the limits of this study, clinically acceptable level of surface finishing of (Y, Nb)-TZP can be achieved after conventional zirconia polishing sequence.
Keywords
Fully sintered zirconia; Partially sintered zirconia; CAD-CAM restoration; Surface roughness; Phase transformation;
Citations & Related Records
Times Cited By KSCI : 1  (Citation Analysis)
연도 인용수 순위
1 Al-Haj Husain N, Camilleri J, Ozcan M. Effect of polishing instruments and polishing regimens on surface topography and phase transformation of monolithic zirconia: An evaluation with XPS and XRD analysis. J Mech Behav Biomed Mater 2016;64:104-12.   DOI
2 Zucuni CP, Guilardi LF, Rippe MP, Pereira GKR, Valandro LF. Fatigue strength of yttria-stabilized zirconia polycrystals: Effects of grinding, polishing, glazing, and heat treatment. J Mech Behav Biomed Mater 2017;75:512-20.   DOI
3 Ramos GF, Pereira GK, Amaral M, Valandro LF, Bottino MA. Effect of grinding and heat treatment on the mechanical behavior of zirconia ceramic. Braz Oral Res 2016;30:e12.
4 Pereira GK, Amaral M, Simoneti R, Rocha GC, Cesar PF, Valandro LF. Effect of grinding with diamond-disc and -bur on the mechanical behavior of a Y-TZP ceramic. J Mech Behav Biomed Mater 2014;37:133-40.   DOI
5 Pereira GKR, Fraga S, Montagner AF, Soares FZM, Kleverlaan CJ, Valandro LF. The effect of grinding on the mechanical behavior of Y-TZP ceramics: A systematic review and meta-analyses. J Mech Behav Biomed Mater 2016;63:417-42.   DOI
6 Go H, Park H, Lee J, Seo H, Lee S. Effect of various polishing burs on surface roughness and bacterial adhesion in pediatric zirconia crowns. Dent Mater J 2019;38:311-6.   DOI
7 Walia T, Brigi C, KhirAllah ARMM. Comparative evaluation of surface roughness of posterior primary zirconia crowns. Eur Arch Paediatr Dent 2019;20:33-40.   DOI
8 Kozmacs C, Hollmann B, Arnold WH, Naumova E, Piwowarczyk A. Polishing of monolithic zirconia crowns-results of different dental practitioner groups. Dent J (Basel) 2017;5:30.   DOI
9 Mohammadi-Bassir M, Babasafari M, Rezvani MB, Jamshidian M. Effect of coarse grinding, overglazing, and 2 polishing systems on the flexural strength, surface roughness, and phase transformation of yttrium-stabilized tetragonal zirconia. J Prosthet Dent 2017;118:658-65.   DOI
10 Martins FV, Mattos CT, Cordeiro WJB, Fonseca EM. Evaluation of zirconia surface roughness after aluminum oxide airborne-particle abrasion and the erbium-YAG, neodymium-doped YAG, or CO2 lasers: A systematic review and meta-analysis. J Prosthet Dent 2019;121:895-903.e2.   DOI
11 Zahoui A, Bergamo ET, Marun MM, Silva KP, Coelho PG, Bonfante EA. Cementation protocol for bonding zirconia crowns to titanium base CAD-CAM abutments. Int J Prosthodont 2020;33:527-35.    DOI
12 Collares K, Correa MB, Laske M, Kramer E, Reiss B, Moraes RR, Huysmans MC, Opdam NJ. A practice-based research network on the survival of ceramic inlay/onlay restorations. Dent Mater 2016;32:687-94.   DOI
13 Sannino G, Germano F, Arcuri L, Bigelli E, Arcuri C, Barlattani A. Cerec CAD-CAM chairside system. Oral Implantol (Rome) 2015;7:57-70.
14 Cokic SM, Vleugels J, Van Meerbeek B, Camargo B, Willems E, Li M, Zhang F. Mechanical properties, aging stability and translucency of speed-sintered zirconia for chairside restorations. Dent Mater 2020;36:959-72.   DOI
15 Luthardt RG, Holzhuter MS, Rudolph H, Herold V, Walter MH. CAD-CAM-machining effects on Y-TZP zirconia. Dent Mater 2004;20:655-62.   DOI
16 Pieger S, Salman A, Bidra AS. Clinical outcomes of lithium disilicate single crowns and partial fixed dental prostheses: a systematic review. J Prosthet Dent 2014;112:22-30.   DOI
17 Zarone F, Di Mauro MI, Ausiello P, Ruggiero G, Sorrentino R. Current status on lithium disilicate and zirconia: a narrative review. BMC Oral Health 2019;19:134.   DOI
18 Lim CH, Jang YS, Lee MH, Bae TS. Evaluation of fracture strength for single crowns made of the different types of lithium disilicate glass-ceramics. Odontology 2020;108:231-9.   DOI
19 Kern M, Sasse M, Wolfart S. Ten-year outcome of three-unit fixed dental prostheses made from monolithic lithium disilicate ceramic. J Am Dent Assoc 2012;143:234-40.   DOI
20 Alao AR, Stoll R, Song XF, Abbott JR, Zhang Y, Abduo J, Yin L. Fracture, roughness and phase transformation in CAD-CAM milling and subsequent surface treatments of lithium metasilicate/disilicate glass-ceramics. J Mech Behav Biomed Mater 2017;74:251-60.   DOI
21 Ahmed WM, Troczynski T, McCullagh AP, Wyatt CCL, Carvalho RM. The influence of altering sintering protocols on the optical and mechanical properties of zirconia: A review. J Esthet Restor Dent 2019;31:423-30.   DOI
22 Valenti M, Valenti A. Retrospective survival analysis of 261 lithium disilicate crowns in a private general practice. Quintessence Int 2009;40:573-9.
23 Kaizer MR, Gierthmuehlen PC, Dos Santos MB, Cava SS, Zhang Y. Speed sintering translucent zirconia for chairside one-visit dental restorations: Optical, mechanical, and wear characteristics. Ceram Int 2017;43:10999-1005.   DOI
24 Denry I, Kelly JR. State of the art of zirconia for dental applications. Dent Mater 2008;24:299-307.   DOI
25 Khaledi AAR, Vojdani M, Farzin M, Pirouzi S, Orandi S. The effect of sintering time on the marginal fit of zirconia copings. J Prosthodont 2019;28:e285-9.   DOI
26 Jeong KW, Yoon HI, Lee JH, Yeo IL, Kim DJ, Han JS. Clinical feasibility of fully sintered (Y, Nb)-TZP for CAD-CAM single-unit restoration: a pilot study. Materials (Basel) 2021;14:2762.
27 Cho JH, Yoon HI, Han JS, Kim DJ. Trueness of the inner surface of monolithic crowns fabricated by milling of a fully sintered (Y, Nb)-TZP block in chairside CADCAM system for single-visit dentistry. Materials (Basel) 2019;12:3253.   DOI
28 Aljomard YRM, Altunok EC, Kara HB. Enamel wear against monolithic zirconia restorations: A meta-analysis and systematic review of in vitro studies. J Esthet Restor Dent 2022;34:473-89.   DOI
29 Burgess JO, Janyavula S, Lawson NC, Lucas TJ, Cakir D. Enamel wear opposing polished and aged zirconia. Oper Dent 2014;39:189-94.   DOI
30 Janyavula S, Lawson N, Cakir D, Beck P, Ramp LC, Burgess JO. The wear of polished and glazed zirconia against enamel. J Prosthet Dent 2013;109:22-9.   DOI
31 Caglar I, Ates SM, Yesil Duymus Z. The effect of various polishing systems on surface roughness and phase transformation of monolithic zirconia. J Adv Prosthodont 2018;10:132-7.   DOI
32 Mathew MG, Samuel SR, Soni AJ, Roopa KB. Evaluation of adhesion of Streptococcus mutans, plaque accumulation on zirconia and stainless steel crowns, and surrounding gingival inflammation in primary molars: randomized controlled trial. Clin Oral Investig 2020;24:3275-80.
33 Khayat W, Chebib N, Finkelman M, Khayat S, Ali A. Effect of grinding and polishing on roughness and strength of zirconia. J Prosthet Dent 2018;119:626-31.   DOI
34 Park C, Vang MS, Park SW, Lim HP. Effect of various polishing systems on the surface roughness and phase transformation of zirconia and the durability of the polishing systems. J Prosthet Dent 2017;117:430-7.   DOI
35 Huh YH, Park CJ, Cho LR. Evaluation of various polishing systems and the phase transformation of monolithic zirconia. J Prosthet Dent 2016;116:440-9.   DOI
36 Preis V, Grumser K, Schneider-Feyrer S, Behr M, Rosentritt M. The effectiveness of polishing kits: influence on surface roughness of zirconia. Int J Prosthodont 2015;28:149-51.   DOI
37 De Souza RH, Kaizer MR, Borges CEP, Fernandes ABF, Correr GM, DiOgenes AN, Zhang Y, Gonzaga CC. Flexural strength and crystalline stability of a monolithic translucent zirconia subjected to grinding, polishing and thermal challenges. Ceram Int 2020;46:26168-75.   DOI
38 Sieper K, Wille S, Kern M. Fracture strength of lithium disilicate crowns compared to polymer-infiltrated ceramic-network and zirconia reinforced lithium silicate crowns. J Mech Behav Biomed Mater 2017;74:342-8.   DOI
39 Kosmac T, Oblak C, Marion L. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics. J Eur Ceram Soc 2008;28:1085-90.   DOI
40 Carrabba M, Vichi A, Vultaggio G, Pallari S, Paravina R, Ferrari M. Effect of finishing and polishing on the surface roughness and gloss of feldspathic ceramic for chairside CAD-CAM systems. Oper Dent 2017;42:175-84.   DOI
41 Toraya H, Yoshimura M, Somiya S. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by X-ray diffraction. J Am Ceram Soc 1984;67:C-119-C-121.
42 Lee DY, Kim DJ, Jang JW, Choi DW, Lee SJ. Phase stability of (Y, Nb)-TZP/Al2O3 composites under low temperature hydrothermal conditions. Mater Lett 1999;39:221-6.   DOI
43 Kim DJ, Jung HJ, Jang JW, Lee HL. Fracture toughness, ionic conductivity, and low-temperature phase stability of tetragonal zirconia codoped with yttria and niobium oxide. J Am Ceram Soc 1998;81:2309-14.   DOI
44 Kowalski K, Bernasik A, Camra J, Radecka M, Jedlinski J. Diffusion of niobium in yttria-stabilized zirconia and in titania-doped yttria-stabilized zirconia polycrystalline materials. J Eur Ceram Soc 2006;26:3139-43.   DOI
45 Kim DJ, Jung HJ, Cho DH. Phase transformations of Y2O3 and Nb2O5 doped tetragonal zirconia during low temperature aging in air. Solid State Ion 1995;80: 67-73.   DOI
46 Yin L, Nakanishi Y, Alao A-R, Song X-F, Abduo J, Zhang Y. A review of engineered zirconia surfaces in biomedical applications. Procedia CIRP 2017;65:284-90.   DOI
47 Shin HS, Lee JS. Comparison of surface topography and roughness in different yttrium oxide compositions of dental zirconia after grinding and polishing. J Adv Prosthodont 2021;13:258-67.