PMWN-PZT계 압전세라믹의 압전 및 유전특성 (Characteristics of Piezoelectric and dielectric of PMWN-PZT Ceramics)

  • 홍종국;이종섭;채홍인;윤만순;정수현
    • 한국전기전자재료학회논문지
    • /
    • 제14권6호
    • /
    • pp.455-459
    • /
    • 2001
  • In this paper, the dielectric and pizoelectric properties of 0.05Pb(M $n_{04}$ $W_{0.2}$N $b_{0.4}$) $O_3$-0.95(PbZ $r_{x}$ $Ti_{1-x}$ ) $O_3$+yN $b_2$ $O_{5}$ , are investigated as a function of the mole ratio of Zr and the amount of N $b_2$ $O_{5}$ . Also, the phase is analyzed by XRD. When the mole ratio of Zr is 0.51, the electromechanical coupling coefficient( $k_{p}$ ), relative dielectric constant ($\varepsilon$$^{T}$ $_{33}$ /$\varepsilon$$_{0}$ ), piezoelectric stain constrain ( $d_{33}$ and dielectric loss tangent show maximum, while the mechanical quality factor shows minimum value ; $k_{p}$ =56.5%, $d_{33}$ =258pC/N, $\varepsilon$$^{T}$ $_{33}$ /$\varepsilon$$_{0}$ =1170, $Q_{m}$ =1150, tan$\delta$=0.51%. At that composition, MPB which rhombohedral and tetragonal phase coexist in this ternary system is shown by the results of XRD analysis. Also, when the amount of N $b_2$ $O_{5}$ is 0.3wt%, the mechanical quality factor is increased to about 2000. The phase transition temperature of the ternary piezoelectric ceramic system showed about 35$0^{\circ}C$.TEX>.>.>.

  • PDF

PZT-PMN 압전 세라믹의 압전 및 유전 특성 (The Piezoelectric and Dielectric Properties of PZT-PMN Piezoelectric Ceramics)

  • 이종섭;이용희;채홍인;정수현;임기조
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 하계학술대회 논문집 C
    • /
    • pp.1439-1441
    • /
    • 2001
  • In this paper, the piezoelectric and dielectric properties as a function of x and r in $yPbZr_xTi_{1-x}O_3-(1-y)Pb(Mn_{1/3}Nb_{2/3})O_3$ piezoelectric ceramics is investigated. As a results, when y is 0.95 and x is 0.505, electromechanical coupling factor($k_p$), permittivity(${{\varepsilon}_{33}}^T/{\varepsilon}_0$), piezoelectric strain constant($d_{33}$) and mechanical quality factor($Q_m$) are 58[%], 1520, 272 [pC/N] and 1550, respectively. From XRD analysis, when x is 0.505, it is MPB which present rhombohedral and tetragonal phase in same quantity. Also, From SEM observation. when sintering temperature is 1150[$^{\circ}C$], grain size is about 2 [${\mu}m$]. As y decreases, piezoelectric and dielectric properties and curie temperature decreases, but mechanical quality factor and sintering temperature increases.

  • PDF

$Fe_2O_3$ 첨가에 따른 $Pb(Y_{1/2}Ta_{1/2})O_3-PbZrO_3-PbTiO_3$ 세라믹스의 전기적 특성 (Electrical Properties of $Pb(Y_{1/2}Ta_{1/2})O_3-PbZrO_3-PbTiO_3$ Ceramic s as a function of $Fe_2O_3$content)

  • 강도원;김태열;김범진;박태곤;김명호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 추계학술대회 논문집
    • /
    • pp.297-299
    • /
    • 1999
  • Effects of additives on the ceramic and electrical properties of Pb(Y$_{1}$2/Ta$_{1}$2/)O$_3$-PbZrO$_3$-PbTiO$_3$ceramics in a perovskite type structure were investigated. The dielectric and piezoelectric properties of the base composition were improved markedly through selection of Fe$_2$O$_3$ additives in proper amounts. The composition Pb(Y$_{1}$2/Ta$_{1}$2/)O$_3$-PbZrO$_3$-PbTiO$_3$ obtained the dielectric constant ($\varepsilon$$_{r}$=1,425). Also, electromechanical couping factors for planar(k$_{p}$) and piezoelectric constant(d$_{33}$) were obtained 0.50 and 294[pC/N] at the additives 0wt% Fe$_2$O$_3$ respectively. The mechanical quality facor(Q$_{m}$) of Pb(Y$_{1}$2/Ta$_{1}$2/)O$_3$-PbZrO$_3$-PbTiO$_3$+Fe$_2$O$_3$(0.3 wt%) is about 510.510.510.

  • PDF

비납계 $(1-x)(Bi_{0.5}K_{0.5})TiO_3-xBiFeO_3$ 세라믹의 유전 및 압전 특성

  • 김정민;성연수;송태권;김명호
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 춘계학술발표대회
    • /
    • pp.33.2-33.2
    • /
    • 2009
  • Dielectric and piezoelectric properties of Lead-free $(1-x)(Bi_{0.5}K_{0.5})TiO_3-xBiFeO_3$ceramics prepared by a conventional solid state reaction method were investigated in the range of x = 0~10 mol%. Piezoelectric coefficient was increased from 31 pC/N at x = 0 mol% to 64 pC/N at x = 6 mol% then decreased with increasing x. Electromechanical coupling factor ($K_p$) was increased up to 0.18 at x = 10 mol%. On the other hand, mechanical quality factor ($Q_m$) was decreased. Grain size was not much changed with various x and a single perovskite with tetragonal symmetry was maintained at all compositions forming a solid solution between $(Bi_{0.5}K_{0.5})TiO_3$ and $BiFeO_3$. Depolarization temperature ($T_d$) was gradually decreased with increasing x from $302^{\circ}C$ at x = 0 to $245^{\circ}C$ at x = 10 mol%.

  • PDF

K5.4Cu1.3Ta10O29 첨가에 따른 0.97[(K0.5Na0.5)(Nb0.97Sb0.03)O3]-0.03[(Bi0.5K0.5)TiO3] 세라믹스의 압전 및 유전 특성 (Piezoelectric and Dielectric Properties of 0.97[(K0.5Na0.5)(Nb0.97Sb0.03)O3]-0.03[(Bi0.5K0.5)TiO3] Ceramics Modified with K5.4Cu1.3Ta10O29)

  • 이갑수;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제24권9호
    • /
    • pp.728-732
    • /
    • 2011
  • In this study, piezoelectric and dielectric properties of Lead-free $0.97[(K_{0.5}Na_{0.5})(Nb_{0.97}Sb_{0.03})O_3]+0.03[(Bi_{0.5}K_{0.5})TiO_3]$ (abbreviated as 0.97NKNS-0.03BKT)ceramics synthesized by conventional solid-state reaction process were investigated as a function of $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition. The results indicated that the $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition significantly improved the sinterability, grain growth and piezoelctric properties of 0.97NKNS-0.03BKT ceramics. The optimum values as planar piezoelectric coupling coefficient ($k_p$= 0.355), piezoelectric constant ($d_{33}$= 207 pC/N) and mechanical quality factor ($Q_m$= 128) were obtained when 0.009KCT was added. The electromechanical coupling factor($k_p$) was slightly decreased according to the increasing temperature.

Effect of CuO on the Low Temperature Sintering Properties of PSN-PNN-PZT Ceramics

  • Jeong, Yeong-Ho;Yoo, Ju-Hyun;Nam, Seung-Hyon;Lee, Su-Ho;Chung, Kwang-Hyun;Lee, Duck-Chool
    • Transactions on Electrical and Electronic Materials
    • /
    • 제5권3호
    • /
    • pp.109-112
    • /
    • 2004
  • In this study, in order to develop the low temperature sintering ceramics for ultrasonic vibrator, Pb(Sb$\_$$\frac{1}{2}$/Nb$\_$$\frac{1}{2}$/) O$_3$-Pb(Ni$\_$1/3/Nb$\_$2/3/)O$_3$-Pb(Zr$\_$0.48/Ti$\_$0.52/)O$_3$ ceramics were manufactured as a function of the amount of CuO addition, and their dielectric and piezoelectric characteristics were investigated. With increasing CuO addition, the grain size and density increased up to 0.3 wt% CuO addition. Taking into consideration electromechanical coupling factor(k$\_$p/) of 0.53, mechanical quality factor(Q$\_$m/) of 423, dielectric constant($\varepsilon$$\_$r/) of 1,759 and piezoelectric constant(d$\_$33/) of 362pC/N, it could be concluded that 0.5 wt% CuO added composition ceramic sintered at 920$^{\circ}C$ was suitable for ultrasonic vibrator application.

CuO첨가에 따른 $(K_{0.5}Na_{0.5})_{0.97}(Nb_{0.96}Sb_{0.04})O_3$세라믹스의 유전 및 압전 특성 (Dielectric and piezoelectric properties of CuO added $(K_{0.5}Na_{0.5})_{0.97}(Nb_{0.96}Sb_{0.04})O_3$ ceramics)

  • 이유형;박민호;노정래;류주현;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.160-161
    • /
    • 2009
  • In this study, in order to develop the lead free piezoelectric ceramics with excellent piezoelectric properties, (Na,K)$NbO_3$ ceramics according to the amount CuO addition were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated. At the 0.8mol% CuO added composition, density, electromechanical coupling factor(kp), echanical quality factor(Qm), dielectric constant$(\varepsilon_r$) and piezoelectric constant($d_{33}$) showed the optimum value of $4.459g/cm^3$, 0.469, 540, 410, 69.57pC/N, respectively.

  • PDF

고에너지 밀링에 따른 PMN-PNN-PZT 세라믹의 유전 및 압전 특성 (Piezoelectric and Dielectric Properties of PMN-PNN-PZT Ceramic according to the High Energy Ball Milling)

  • 이유형;류주현;백동수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.203-204
    • /
    • 2008
  • In this study, in order to develop the multilayer piezoelectric actuator and ultrasonic resonator, PMN-PNN-PZT ceramics were fabricated by the variations of ball size at sintering temperature of $900^{\circ}C$ and their piezoelectric and dielectric characteristics were investigated as a function of the variations of ball size. When the ball size was 3mm$\phi$, density, dielectric constant$({\varepsilon}r)$, electromechanical coupling factor(kp) and piezoelectric d constant$(d_{33})$ were increased. At the ball size of 3mm$\phi$, the specimen showed the optimum values of density=7.909g/$cm^3$, kp=0.592, Qm=1292, $d_{33}$=368pC/N, $\varepsioln_r$=1502, respectively.

  • PDF

불순물 첨가에 따른 저온소결 PMN-PNN-PZT 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT Ceramics according to the addition of dopant)

  • 이상호;이창배;정광현;류주현;홍재일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.33-34
    • /
    • 2005
  • In this study, in odor to develop low temperature sintering multilayer piezoelectric actuator and ultrasonic vibrator, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3$ and $Na_2CO_3$ as sintering aids and their piezoelectric and dielectric characteristics were investigated according to the addition of dopant CuO and $Fe_2O_3$, respectively. The CuO added PMN-PNN-PZT ceramics improved mechanical quality factor Qm due to the acceptor doping effect. And also, $Fe_2O_3$ reacted as softner in this composition system in addition to the increase of grain size and sinterability. Taking into consideration electromechanical coupling factor kp of 0.62, dielectric constant $\varepsilon_r$, of 1275, Piezoelectric $d_{33}$ constant of 377[pC/N] and mechanical quality factor Qm of 975, it was concluded that the ceramics with the $Fe_2O_3$, added composition sintered at 900[$^{\circ}C$] were best for the multilayer piezoelectric actuator and ultrasonic vibrator application.

  • PDF

$MnO_2$ 첨가방법에 따른 PMN-PNN-PZT 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Characteristics of PMN-PNN-PZT Ceramics with the methods of $MnO_2$ additon)

  • 김도형;김국진;류주현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.255-256
    • /
    • 2007
  • In the study, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator, PMN-PNN-PZT ceramics were fabricated using $Na_2CO_3,\;Li_2CO_3$ as sintering aids and their dielectric and piezoelectric properties were investigated according to the variations of $MnO_2$ as additives and sintering aids. At the sintering temperature of $900^{\circ}C$ and 0.1wt% $MnO_2$ as sintering aids, density, electromechanical coupling factor$(k_p)$, mechanical quality factor$(Q_m)$, piezoelectric constant$(d_{33})$, and dielectric constant $({\varepsilon}_r)$ showed the optimum value of $7.87[g/cm^3]$, 0.61, 1131, 1127 and 376, respectively, for multilayer piezoelectric actuator application.

  • PDF