Carbon nanotube / silane hybride film for highly efficient field emitter

  • Jeong, Hae-Deuk;Kim, Ho-Young;Jeong, Hee-Jin;Han, Joong-Tark;Lee, Geon-Woong
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2010.06a
    • /
    • pp.181-181
    • /
    • 2010
  • Few-walled carbon nanotubes (FWNTs)-based field emitters with long term stability are fabricated by using a spray method. Tetraethylorthosilicate (TEOS) sol as a binder was mixed with dispersed solution of FWNTs to enhance the adhesion of FWNTs on the cathode substrate. Due to the strong intermolecular interaction of TEOS to the functional groups attached on CNTs and substrate, CNTs are tightly adhered to the cathode electrode when heat treatment is performed at $150^{\circ}C$ for 1 hour, resulting in a stable electron emission of CNT emitters for long time. Excellent field emission characteristics were exhibited, with a large field enhancement factor and low turn-on voltage, comparable to those of CNT emitters fabricated by a screen printing of CNT paste. Therefore, FWNTs / TEOS hybrid films could be utilized as an alternative for the efficient and reliable field emitters.

  • PDF

Electrochemical Degradation of Phenol Using Dimensionally Stable Anode (촉매성 산화물 전극을 이용한 페놀의 전기화학적 분해)

  • Kim, Dong-Seog;Park, Young-Seek
    • Journal of Environmental Science International
    • /
    • v.22 no.8
    • /
    • pp.999-1007
    • /
    • 2013
  • Electrochemical degradation of phenol was evaluated at DSA (dimensionally stable anode), JP202 (Ru, 25%; Ir, 25%; other, 50%) electrode for being a treatment method in non-biodegradable organic compounds such as phenol. Experiments were conducted to examine the effects of applied current (1.0~4.0 A), electrolyte type (NaCl, KCl, $Na_2SO_4$, $H_2SO_4$) and concentration (0.5~3.0 g/L), initial phenol concentration (12.5~100.0 mg/L) on phenol degradation and $UV_{254}$ absorbance as indirect indicator of by-product degraded phenol. It was found that phenol concentration decreased from around 50 mg/L to zero after 10 min of electrolysis with 2.5 g/L NaCl as supporting electrolyte at the current of 3.5 A. Although phenol could be completely electrochemical degraded by JP202 anode, the degradation of phenol COD was required oxidation time over 60 min due to the generation of by-products. $UV_{254}$ absorbance can see the impact of as an indirect indicator of the creation and destruction of by-product. The initial removal rate of phenol is 5.63 times faster than the initial COD removal rate.

Thermal and Mechanical Properties of Electro-Slag Cast Steel for Hot Working Tools

  • Moon Young Hoon;Kang Boo Hyun;Van Tyne Chester J.
    • Journal of Mechanical Science and Technology
    • /
    • v.19 no.2
    • /
    • pp.496-504
    • /
    • 2005
  • The thermal and mechanical properties of an electro-slag cast steel of a similar chemical composition with an AISI-6F2 steel are investigated and compared with a forged AISI-6F2 steel. AISI-6F2 is a hot-working tool steel. Electro-slag casting (ESC) is a method of producing ingots in a water-cooled metal mold by the heat generated in an electrically conductive slag when current passes through a consumable electrode. The ESC method provides the possibility of producing material for the high quality hot-working tools and ingots directly into a desirable shape. In the present study, the thermal and mechanical properties of yield strength, tensile strength, hardness, impact toughness, wear resistance, thermal fatigue resistance, and thermal shock resistance for electro-slag cast and forged steel are experimentally measured for both annealed and quenched and tempered heat treatment conditions. It has been found that the electro-slag cast steel has comparable thermal and mechanical properties to the forged steel.

Expression and Characterization of G Protein-activated Inward Rectifier $K^+$ Channels in Xenopus Oocytes

  • Kim, Han-Seop;Lee, Chang-Ho;Min, Churl K.
    • Animal cells and systems
    • /
    • v.2 no.4
    • /
    • pp.471-476
    • /
    • 1998
  • The G protein-activated inwardly rectifying $K^+$ channel (GIRK1) was coex-pressed in Xenopus oocytes along with the $5-HT_{1A}$ receptor, a 7-helix receptor known to be coupled to $K^+$ channels in many neural tissues. Thus, the activation of the $5-HT_{1A}$ receptor by its agonist leads to the opening of GIRK1. The GIRK1 current was measured using the two electrode voltage clamp technique with bath application of 5-HT in the presence of various external potassium concentrations $[K^+]_0$. GIRK1 showed a strong inward rectification since only hyperpolarizing voltages evoked inward currents. $K^{+}$ was the major ion carrier as evidenced by about 44㎷ voltage shift corresponding to a 10-fold external 〔$K^+$〕 change. 5-HT induced a concentration-dependent inward $K^+$ current ($EC_{50}{\equation omitted}10.7nM$) which was blocked by $Ba^{2+}$. Pertussis toxin (PTX) pre-treatment reduced the $K^+$ current by as much as about 70%, suggesting that PTX-sensitive G protein ($G_i or G_o$ type) are involved in the $5-HT_{1A}$ receptor-GIRK1 coupling in Xenopus oocytes.

  • PDF

고온 염기성 수용액에서 $TiO_2$가 Alloy 600과 Alloy 690의 응력부식파괴에 미치는 영향

  • 김경모;김홍표;이창규;국일현;김우철
    • Proceedings of the Korean Nuclear Society Conference
    • /
    • 1998.05b
    • /
    • pp.78-83
    • /
    • 1998
  • Alloy 600과 Alloy 690의 응력부식파괴(Stress corrosion cracking, SCC)에 미치는 TiO$_2$의 영향을 315$^{\circ}C$의 10%NaOH 수용액에서 RUB(reverse U-bend) 시편, C-Ring 시편과 CT(compact tension)시편을 사용하여 평가하였다. 시편은 alloy 600 MA(mill anneal), alloy 600 TT(thermal treatment) 그리고 alloy 690 TT로 제작하였다. SCC 시험은 탈산된 10%NaOH 수용액에 2 g/1 TiO$_2$를 첨가한 용액과 첨가하지 않은 용액에서 수행하였으며, 이 조건에서 분극곡선도 얻었다. SCC 시험시 시편을 부식전위로부터 +150 ㎷ 양극분극을 가하였다. 기준전극으로 external Ag/AgCl electrode를 사용하였다. Alloy 600 MA로 제작한 RUB 시편은 TiO$_2$가 없는 용액에서 5일 안에 벽 관통 균열을 보였으나 TiO$_2$가 첨가된 용액에서는 균열을 관찰할 수 없었다. TiO$_2$가 첨가됨에 따라 alloy 600과 alloy 690의 임계전류밀도는 크게 감소하였고 또한 부동태 전류밀도도 감소하였다. 부동테 영역에서 TiO$_2$가 있는 용액의 경우 여러 peak가 있는 반면에 TiO$_2$가 없는 용액은 peak가 뚜렷하지 않았다. 이런 결과는 TiO$_2$가 첨가점에 따라 active region에서도 안정한 부동태 피막이 존재한다는 것을 시사한다. 또한 TiO$_2$가 없는 경우 SCC가 잘 일어나는 영역에 존재하는 부동태 피막이 TiO$_2$ 첨가에 따라 repassivation kinetics 등의 성질이 변화한 것으로 판단된다.

  • PDF

Electrochemical Properties of Manganese Oxide coated onto Carbon Nanotubes for Energy Storage Applications (보조에너지원으로서의 수퍼커패시터용 나노전극소재로서의 탄소/망간산화물의 전기화학적 특성)

  • Ahn, Kyun-Young;Ma, Sang-Bok;Kim, Kwang-Bum
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2007.11a
    • /
    • pp.143-146
    • /
    • 2007
  • Birnessite-type manganese dioxide($MnO_2$) was coated uniformly onto carbon nanotubes (CNTs) through a spontaneous direct redox reaction between CNTs and permanganate ions($MnO_4\;^-$). The initial specific capacitance of the $MnO_2/CNT$ nanocomposite in an organic electrolyte at a large current density of 1 A/g was 250 F/g, which is equivalent to 139 mAh/g based on the total weight of the electrode material including the electroactive material, conducting agent and binder. The specific capacitance of the $MnO_2$ in the $MnO_2/CNT$ nanocomposite was as high as 580 F/g (320 mAh/g), indicating excellent electrochemical utilization of the $MnO_2$. The addition of CNTs as a conducting agent can improve the high rate capability of $MnO_2/CNT$ nanocomposite considerably. An analysis of the in-situ X-ray absorption near-edge structure (XANES) showed an improvement in the structural and electrochemical reversibility of the $MnO_2/CNT$ nanocomposite by heat-treatment.

  • PDF

Electrodes for contact electric welding of aluminium alloys

  • Bondar, M.P.;Moon, J.G.
    • Proceedings of the KWS Conference
    • /
    • 1997.10a
    • /
    • pp.184-193
    • /
    • 1997
  • Aluminium and aluminium alloys have the high electrical and heat conductivity. It gives rise to difficulties for a choice of electrodes material for their contact electric welding. This paper describes the investigations performed to solve the above problem. The purpose of this investigation was to obtain dispersion-hardening alloys by the internal oxidation method, to optimize their contents and treatment modes, to produce electrodes of these alloys and to test them. The strengthing effect of alloys with oxide particles depends on their size stability at high temperatures. Despite of the fact, that oxides are the most stable of all the non-metallic phases their coagulation takes place. Based on the early results, we chose two types of alloys, first No. 1 Cu - 0,4%Al and second No. 2 Cu - 0,2%Be for production of electrodes. These alloys had not additional alloying elements. These alloys were prepared as 1 mm plates and flake-formed 200 m thick, and also No. 1 as a powder of size 100 mkm (received from Korea). The large samples for electrodes were produced by three methods : explosive welding method, dynamic one including the explosion compression of electrode blank and the quasi-dynamic method including the high-speed compression of dense briquest and the further hot extrusion of a rod.

  • PDF

Current Research Trends in Microbial Fuel Cell Based on Polymer Electrolyte Membranes (고분자 전해질 분리막 기반 미생물 연료전지의 최근 연구동향)

  • Choi, Tae-Hwan;Kim, Hyo-Won;Park, Ho-Bum
    • Membrane Journal
    • /
    • v.20 no.3
    • /
    • pp.173-184
    • /
    • 2010
  • Microbial fuel cell (MFC) is a promising renewable energy source that can generate electrical energy from organic wastes using microbe. This technology has been regarded as a future green alternative energy in that MFC makes use of organic-rich wastewater and also reduces waste sludges as well as produces electricity. To be practically realized, however, achieving higher power density than now is demanded, which may be possible by eliminating various negative factors to act as resistances in MFC operations. For instance, highly activated microbes, highly conductive electrode materials, and fast electron transfer between microbes and electrodes can lead to MFC with high power density. In particular, polymer electrolyte membranes are also a key component for improved MFC performance.

Electrochemical Properties of Spinel $LiMn_2O_4$ Synthesized at Various Heat Treatment for Lithium lon Battery (리튬 이온 전지용 스피넬 $LiMn_2O_4$의 열처리 온도에 따른 전기 화학적 특성)

  • Han, Tae-Hee;Min, Hyung-Sik;Han, Byoung-Sung
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.48 no.3
    • /
    • pp.179-184
    • /
    • 1999
  • In the past ten years, $LiMn_2O_4$-based spinels have been extensively studied as positive electrode materials for lithium-ion batteries. To improve the cycle performance of spinel $LiMn_2O_4$ as the cathode of 4V class lithium secondary batteries, spinel phases $LiMn_2O_4$ were prepared at various temperatures ranging form 600-900$^{\cire}C$ in air. The results showed that charge.dischare capacity of $LiMn_2O_4$ varied at 1st temperature from $200^{\circ}C to 600^{\circ}C$ increase with increasing temperature. $LiMn_2O_4$ synthesized at 2nd temperature $750^{\circ}C$excellent charge.discharge capacity, efficiency and cyclability compared to the samplesynthesized different temperatures. The value of lst charge.discharge capacity was 121mAh/g, 118mAh/g, Also, the efficiency value was about 97%.

  • PDF

The Influence ${Sb_2}{O_3)$ Addition on Humidity Sensing Properties of $SnO_2$Thick Film Devices (${Sb_2}{O_3)$ 의 첨가가 $SnO_2$후막의 감습 특성에 미치는 영향)

  • 김종택;이덕출;김철수
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.4
    • /
    • pp.294-299
    • /
    • 2000
  • For practical application as a humidity sensor SnO$_2$thick films devices were fabricated on the refresh type electrode by screen printing method and their material and humidity sensing properties were investigated. As a function of Sb$_{2}$/O$_{3}$ addition rate grain size was increased while porosity and initial resistance were rapidly decreased. And the area of resistance variation according to relative humidity was decreased with increasing heat treatment temperature. SnO$_2$thick film device heat treated at 95$0^{\circ}C$ and contained 0.05mole% Sb$_{2}$/O$_{3}$ had a best humidity sensing properties. From this result it is conformed that humidity sensing properties of SnO$_2$thick film devices could be approved by very small amount of Sb$_{2}$/O$_{3}$ addition.

  • PDF