• 제목/요약/키워드: Dye penetration test

검색결과 64건 처리시간 0.032초

다양한 파장폭의 가시광선에 의해 중합된 복합레진의 미세경도와 변연누출도 (MICROHARDNESS AND MICROLEAKAGE OF COMPOSITE RESIN CURED BY VISIBLE LIGHT WITH VARIOUS BAND OF WAVELENGTH)

  • 박수만;이재용;한승렬;하상윤;신동훈
    • Restorative Dentistry and Endodontics
    • /
    • 제27권4호
    • /
    • pp.403-410
    • /
    • 2002
  • Several ways of curing are being tried to improve material's properties and reduce marginal gap. However, all are considering about the pattern of light intensity. It was noted from the preliminary study the change of light wavelength from filter changing may give an impact on material's property and microleakage. The object of this study was to verify the effect of filters with various wavelength width on the microhardness and microleakage of composite resin ; hybrid type of DenFil and submicron hybrid type of Esthet X. Composite resins were cured using 3 kinds of filter; narrow-banded(465-475 nm), mid-banded(430-470 nm), wide-banded(400-500 nm). After the estimation of microhardness. degree of dye penetration and the maximum gap from SEM evaluation were done between 4 groups that showed no difference in microhardness value of the lower surface . The results were as follows : 1 Adequate microhardness could not be gained with a narrow-banded filter irrespective of curing time. At the upper surface, DenFil should be polymerized with middle or wide-banded filter for 20 seconds at least, while Esthet X be col$.$ed with middle or wide-banded filter for 30 seconds at least to get simitar hardness value to control group. 2. There was little dye penetration in enamel margin, but all dentin margins skewed much more dye penetration irrespective of curing conditions. Although there was no statistical difference, groups cured with mid-banded filter for 40 seconds and with wide-width filter for 20 seconds showed relatively less dye penetration. 3. It was revealed from the SEM examination that group cured with wide-banded filter had the smallest gap without statistical significance. Spearman's rho test showed that the correlation between the results of dye penetration and SEM examination was very low. From these results, it could be concluded that curing with wide-width filter would be better than the other techniques, even though the curing technique using mid-width filter seems to have its own unique advantage.

The effect of thermocycling on the bonding of different restorative materials to access opening through porcelain fused to metal restorations

  • Al-Moaleem, Mohammed M.;Shah, Farhan Khalid;Khan, Nausheen Saied;Porwal, Amit
    • The Journal of Advanced Prosthodontics
    • /
    • 제3권4호
    • /
    • pp.186-189
    • /
    • 2011
  • PURPOSE. Porcelain fused to metal (PFM) crowns provide the best treatment option for teeth that have a large or defective restoration. More than 20% of teeth with PFM crowns or bridges require non-surgical root canal treatment (NSRCT). This may be due to the effect of restorative procedures and the possible leakage of bacteria and or their by-products, which leads to the demise of the tooth pulp. Thus, this study was planned to compare the ability of the restorative materials to seal perforated PFM specimens. MATERIALS AND METHODS. The study evaluates the ability of amalgam, composite or compomer restorative materials to close perforated PFM specimen's in-vitro. Ninety PFM specimens were constructed using Ni-Cr alloys and feldspathic porcelain, and then they were divided into 3 groups: amalgam (A), composite + Exite adhesive bond (B) and compomer + Syntac adhesive bond (C). All the PFM samples were embedded in an acrylic block to provide complete sealing of the hole from the bottom side. After the aging period, each group was further divided into 3 equal subgroups according to the thermocycling period (one week for 70 cycles, one month for 300 cycles and three months for 900 cycles). Each subgroup was put into containers containing dye (Pelikan INK), one maintained at $5^{\circ}C$ and the other at $55^{\circ}C$, each cycle for 30 sec time. The data obtained was analyzed by SPSS, 2006 using one way ANOVA test and student t-test and significant difference level at (P<.01). RESULTS. The depth of dye penetration was measured at the interfaces of PFM and filling materials using Co-ordinate Vernier Microscope. The lowest levels of the dye penetration for the three groups, as well as subgroups were during the first week. The values of dye leakage had significantly increased by time intervals in subgroups A and C. CONCLUSION. It was seen that amalgam showed higher leakage than composite while compomer showed the lowest level of leakage.

근관 밀폐도에 미치는 도말층 및 상아질 접착강화제의 영향 (EFFECTS OF SMEAR LAYER AND DENTIN PRIMERS ON THE SEALING ABILITY OF ROOT CANAL)

  • 양진석;황인남;김원재;오원만
    • Restorative Dentistry and Endodontics
    • /
    • 제25권4호
    • /
    • pp.527-535
    • /
    • 2000
  • The purpose of this study was to evaluate effects of smear layer and dentin primers on the sealing ability of root canals. 126 extracted human teeth with single, straight canals and mature apices were used. The Samples were first classified into six groups as follows: presence of smear layer; absence of smear layer; Scotchbond Bond Multi-Purpose; All Bond 2; Mac Bond 2; Clearfil Liner Bond 2. A Positive control was also established. All teeth except the control group were then obturated with thermoplasticized gutta-percha and AH26. Electrochemical and dye penetration technique were later used to evaluate the degree of micro leakage through the root canal. Seventy teeth were then immersed in a 1% potassium chloride solution and An external power supply(DC 10 V) was then applied to the circuit for the electrochemical microleakage test. The degree of Microleakage was determined over period of 28 days before being evaluated. In total, 48 teeth were submitted to the dye infiltration technique. All specimen were suspended in 2% methylene blue dye for 1 week before being longitudinally split. The degree of dye infiltration was measured under a stereo microscope at ${\times}10$ magnification and evaluated. The results were as follows: 1. Apical microleakage increased throughout the test period in all group and one group having a smear layer showed a dramatic increase under electrochemical test (p<0.05). In the group having smear layer, the degree of apical microleakage was the highest, and the micro leakage was much higher than in the smear layer removed group in electrochemical test (p<0.05). Scotchbond Multi-Purpose, All Bond 2, Mac Bond 2 and Clearfil Liner Bond 2 showed lower micro leakage than one group having smear layer. The All Bond 2 and Clearfil Liner Bond 2 treated groups showed the lowest microleakage in electrochemical test (p<0.05). 2. There was no significant difference between the experimental groups in dye penetration technique. These results suggested that the removal of the smear layer from root canal and concomitantly the application of dentin primer into root canal could improve the sealing ability of root canal obturation.

  • PDF

상아질 표면처리가 글라스 아이오노머 시멘트의 변연누출에 미치는 영향에 관한 연구 (THE EFFECT OF THE DENTINE PRETREATMENT ON THE MARGINAL LEAKAGE OF A GLASS IONOMER CEMENT)

  • 조정희;홍찬의;신동훈
    • Restorative Dentistry and Endodontics
    • /
    • 제17권1호
    • /
    • pp.95-103
    • /
    • 1992
  • The purpose of this study was to evaluate the effect of the dentin pretreatment on the marginal leakage of a glassionomer cement. 1n this study, 60 molars with sound and healthy crown portion were used. The dentin surface of these teeth were exposed and polished with 600 grit silicon carbide paper. Square - shaped cavities were prepared on the flattened dentin surfaces and these were divided into 4 groups according to the dentin pretreatment procedures. Group I : Dentin pretreatment with distilled water as a control group. Group II : Dentin pretreatment with 5% sodium hypochlorite solution. Group III : Dentin pretreatment with Ketac conditioner. Group IV : Dentin pretreatment with 40% polyacrylic acid. The degrees of dye penetration in the cavity walls were assessed using a stereoscope at ${\times}40$ magnification according to the maximum dye penetration. The results were analyzed by using Mann - Whitney U test. The results were as follows : 1. All groups showed varying depth of dye penetration. 2. Distilled water group showed the most severe marginal leakage when compared with the other groups(P<0.05). 3. 40% polyacrylic acid group showed the least amount of marginal leakage compared with the other groups (P<0.05). 4. There were significant differences between Goup I(distilled water) and Group IV (40% polyacrylic acid)(P<0.05), but there were no significant differences among Group I(distilled water), Group II(sodium hypochlorite), Group III(Ketac conditioner) (P>0.05).

  • PDF

다양한 방식으로 적용한 이장재가 2급와동 복합레진 수복의 미세누출에 미치는 영향 (Effect of lining application techniques on microleakage in class II composite restorations)

  • 황병문;김주형;박지만;;박은진
    • 구강회복응용과학지
    • /
    • 제30권2호
    • /
    • pp.145-151
    • /
    • 2014
  • 목적: 본 연구는 두가지 다른 방법에 의한 레진강화형 글래스 아이오노머(RMGI) 이장재의 적용이 2급와동 복합레진수복의 미세누출에 미치는 영향을 조사하고자 하였다. 연구 재료 및 방법: 36개의 발치한 치아에 2급 와동을 형성한 뒤 무작위로 3개의 군으로 나누었다. 1군은 대조군으로 이장재를 적용하지 않았으며, 2군은 치과용 탐침으로 RMGI 이장재 적용, 3군은 특별히 고안된 버로 RMGI 이장재를 적용한 뒤 복합레진은 똑같이 통상적인 방법으로 적층수복하였다. 2% 메틸렌 블루 염색한 뒤 치아장축과 평행하게 순설 방향으로 절단하여 미세누출을 현미경과 컴퓨터 프로그램을 사용하여 분석을 하였다. 데이터는 Kruskal-Wallis test와 Mann-Whitney U-test (P < 0.05)로 분석하였다. 결과: RMGI 이장재가 적용된 군은 그렇지 않은 군보다 월등히 적은 미세누출을 보였으며, 특히 특수 고안된 버를 사용한 군의 50%에서는 전혀 미세누출을 보이지 않았다. 그러나, 2군과 3군의 결과에서 통계적으로 유의한 차이는 관찰되지 않았다. 결론: 2급와동의 복합레진 수복에서 RMGI 이장재는 그 적용 방법에 관계없이 미세누출을 감소시키는데 효과적인 재료이다.

Resilon을 이용한 근관충전 시 수종의 치면처리제에 따른 미세누출 평가 (MICROLEAKAGE OF RESILON: EFFECTS OF SEVERAL SELF-ETCHING PRIMER)

  • 오종현;박세희;신혜진;조경모;김진우
    • Restorative Dentistry and Endodontics
    • /
    • 제33권2호
    • /
    • pp.133-140
    • /
    • 2008
  • 이 실험의 목적은 Resilon으로 근관충전된 치아에서 자가산부식전처리제에 따른 치근단 미세누출을 평가하고자 함이다. 70개의 단근치를 사용하였고 .04 Taper ProFile을 사용하여 ISO #40까지 근관성형 하였다. 치아는 근관충전 재료와 자가산부식 전처리제에 따라서 15개씩 4개의 실험군과 5개씩 2개의 대조군으로 나누었다. 실험 치아는 치아 장축에 평행하게 잘라내어 염색액의 최대 침투 길이를 측정하였다. 통계분석은 One-way ANOVA test로 분석하였으며 Scheffe test로 사후검정 하였다. 실험결과 자가산부식전처리제를 사용한 2, 3, 4군 사이에서는 통계적으로 유의한 차이를 나타내지 않았다. 그러나 1군과 4군 사이에서는 통계적으로 유의한 차이가 나타났으며 (p < 0.05), 1군에서 가장 적은 치근단 미세누출을 나타냈다. 이 실험 결과에 따르면 Resilon으로 근관충전을 한 치아는 gutta percha와 $AH26^{(R)}$으로 근관충전한 치아와 비교했을 때 더 좋은 치근단 밀폐를 나타내지 않는다는 결론을 얻었으며, Resilon을 사용하여 근관충전을 한 경우에 자가산부식 전처리제의 차이에 따른 치근단 밀폐효과의 차이를 보이지 않는다는 결론을 얻었다.

Ball-on-3 ball test에 의한 알루미나 세라믹스의 열충격 거동 (Thermal shock behavior of alumina ceramics by ball-on-3 ball test)

  • 이중현;박성은;한봉석;이홍림
    • 한국세라믹학회지
    • /
    • 제36권10호
    • /
    • pp.1062-1068
    • /
    • 1999
  • 상온 25$^{\circ}C$의 증류수에 단일 열충격을 시행한 후 ball-on-3 ball test로 강도를 측정하고 강도의 변화를 관찰하였다. 시편은 상용 알루미나 시편을 사용하였고, disc 형태의 시편에 대하여 열충격 후의 균열의 모양과 강도 시험 후의 균열의 모양을 잉크 침투법에 의해 관찰하였다. 통계적인 파괴 확률방법을 제시하였으며, thermal shock Weibull plot을 이용하여 3점 꺾임 강도와 비교하였다. ball-on-3 ball test 강도에 미치는 인자에 대해 통계학적인 접근을 통해 관찰한 결과, 시편중심에서 균열까지의 거리가 균열 밀도보다 더 큰 영향을 미치고 있음을 알 수 있었다.

  • PDF

Thermal Fatigue Test of an Annular Structure

  • Hwang Jeong-Ki;Suh Chang-Min;Kim Chae-Ho
    • Journal of Mechanical Science and Technology
    • /
    • 제20권1호
    • /
    • pp.59-65
    • /
    • 2006
  • A half-scaled large test model for the main components of the real annular structure was built and the thermal behaviors were experimented and obtained by thermal cyclic loads. The model design and the test conditions for the thermal loads were determined to take into consideration the thermal and mechanical loads acting on the real annular structure by finite element analyses. Temperature profiles and strains of the main components of the model were measured at an early stage of the test and periodically throughout the test in the given test conditions. After completion of the thermal cyclic tests, no evidence of crack initiation and propagation were identified by a dye penetration test. The measured strains at the critical parts were slightly increased proportionally with the increase in the number of the thermal cycles.

Vivadent의 변연누출에 관한 실험적 연구 (Marginal Leakage Test on 'Vivadent' Composite Resin)

  • 권혁춘
    • 대한치과의사협회지
    • /
    • 제23권12호통권199호
    • /
    • pp.1031-1037
    • /
    • 1985
  • The purpose of this study was to evaluate the marginal sealing ability of 'vivadent.' Using freshly extracted human teeth and 2% aqueous methylene blue, the marginal leakage of dye in restorative materials such as vivadent with acid etching technique, Durafill with acid etching technique, silar with acid etching technique, Adaptic, and Amalgam were investigated at 37℃ and under temperature cycling in range of 4℃-60℃. The results were as follows; 1. All filling materials showed some degree of marginal penetration by 2% methylene blue dye. 2. Vivadent with acid etching technique revealed effective marginal sealing ability, but under temperature cycling it showed increased marginal leakage. 3. All resins showed greater marginal leakage than amalgam restoration. 4. Vivadent had the most effective marginal sealing ability in experimented resins.

  • PDF

Silar(Composite Resin계)의 변연누출(變緣漏出)에 관(關)한 실험적(實驗的) 연구(硏究) (MARGINAL LEAKAGE TEST ON "SILAR" COMPOSITE RESIN)

  • 권혁춘
    • Restorative Dentistry and Endodontics
    • /
    • 제8권1호
    • /
    • pp.167-172
    • /
    • 1982
  • The purpose of this study was to evaluate the marginal sealing ability of "Silar". Using freshly extracted human teeth and 2% acquous methylene blue, the marginal leakage of dye in restorative materials such as Silar, Silar with acid etching technique, Hi-Pol, Hi-Pol Enamel Bond system, Adaptic and Amalgam were investigated at $37^{\circ}C$ and under temperature cycling in range of $4^{\circ}C-60^{\circ}C$. The results as follows; 1. All filling materials showed some degree of marginal penetration by 2% methylene blue dye. 2. Silar with acid etching technique revealed effective marginal sealing ability, but under temperature cycling it showed increased marginal leakage. 3. All composite resins showed greater marginal leakage than amalgam restoration. 4. Silar had the most effective marginal sealing ability in experimented composite resins.

  • PDF