• Title/Summary/Keyword: Dry Shrinkage

Search Result 220, Processing Time 0.022 seconds

Change of Physical Properties of Lining Fabrics by Washing (세탁에 따른 안감의 물성변화에 관한 연구)

  • 최은희
    • Journal of the Korean Home Economics Association
    • /
    • v.17 no.4
    • /
    • pp.15-22
    • /
    • 1979
  • This paper was studied changes of physical properties of Lining fabrics by washing and difference between dry method. I experimented four kinds of Lining fabrics for the sample . The analysis was performed by correlation coefficient analysis and significance tested between correlation coefficients. The results are summarized as follows : 1) Increasing rate of shrinkage tends to call high density and weight. 2) Rayon fabrics is shown the most high rate of shrinkage and decreasing strength by increasing washing times. 3) Drip dry makes little change of physical properties. 4) Polyester fabrics is little by washing times and dry method.

  • PDF

A Study on Hydration Heat and Dry Shrinkage of High Durability / Strength Concrete for the Bridge Slab of Express Railway (고속철도 교량상판 슬래브용 고내구/고강도 콘크리트의 수화열 및 건조수축 특성 개선연구)

  • 박정준;백상현;정재헌;박경재;윤원기;엄태선
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.10a
    • /
    • pp.725-728
    • /
    • 1999
  • The bridge slab of express railway was designed for high strength concrete (design strength 400kgf/$\textrm{cm}^2$). In case the slab is made with the concrete using type I cement, used much amount of cement can cause cracks through concrete by hydration heat or dry shrinkage. In this study we targeted to solve above problems using type III cement. We could decrease the cement ratio in concrete using type III cement than type I cement. The concrete using type III cement showed good workability and compressive strength, and showed better properties in hydration heat and dry shrinkage than that using type I cement

  • PDF

Characteristics of Desiccation on the Stabilized Layer in Waste Landfill (쓰레기 매립지에서 표층고화처리층의 건조수축특성)

  • 천병식;임종윤;최창현;차용혁
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 1999.10a
    • /
    • pp.301-308
    • /
    • 1999
  • With the shortage of the land and NIMBY syndrome, it is issued recently that the capacity of waste-landfill site is needed though the decreasing tendency of waste landfill. From this point, the stability is the most essential problem in the landfill that will be constructed. Advanced design and construction are most important for that. In this paper, for the study of desiccation, dry-shrinkage crack from drying and chemical reaction in cement hydration, which is occurred when the surface layer stabilization method is applied in wast landfill, laboratory test of the ground and specimen according to the mixture ratio of stabilizer is performed. From the result, it is notified that the uni-axial strength increases with the stabilizer, but dry-shrinkage increases too, therefore, it is important and the goal of this study to find the optimal mixture ratio of each stabilizer. Analysis of variance for regression with acting variables is performed to find optimal mixture ratio of each stabilizer.

  • PDF

A Numerical Model for Plastic Shrinkage Cracking of Concrete Slab (콘크리트 슬래브의 소성수축균열 해석모델)

  • Kwak Hyo-Gyoung;Ha Soo-Jun
    • Proceedings of the Computational Structural Engineering Institute Conference
    • /
    • 2005.04a
    • /
    • pp.448-455
    • /
    • 2005
  • In this paper, an analytical model for estimation of the time at which the concrete surface begins to dry is introduced to predict whether or not plastic shrinkage cracks occur. First of all, the validity of a consolidation model for bleeding of cement paste proposed by Tan et al. is verified by comparing the analytical results with the experimental results, and used to evaluate the rate and amount of bleed water of concrete. Also an analytical model for evaporation of bleed water which considers the effect of the temperature variation of concrete surface due to hydration heat on the evaporation rate is proposed, and the experimental and analytical results are then compared to verify the validity of the introduced model. In advance, the time at which the concrete surface begins to dry is estimated using above two analytical models, and compared with the experimental results about the time at which plastic shrinkage cracks occur. From the comparison, it is verified that the proposed model can predict the occurrence of plastic shrinkage cracking with comparative precision.

  • PDF

Investigating the long-term behavior of creep and drying shrinkage of ambient-cured geopolymer concrete

  • Asad Ullah Qazi;Ali Murtaza Rasool;Iftikhar Ahmad;Muhammad Ali;Fawad S. Niazi
    • Structural Engineering and Mechanics
    • /
    • v.89 no.4
    • /
    • pp.335-347
    • /
    • 2024
  • This study pioneers the exploration of creep and shrinkage behavior in ambient-cured geopolymer concrete (GPC), a vital yet under-researched area in concrete technology. Focusing on the influence of sodium hydroxide (NaOH) solution concentration, the research utilizes low calcium fly ash (Class-F) and alkaline solutions to prepare two sets of GPC. The results show distinct patterns in compressive strength development and dry shrinkage reduction, with a 14 M NaOH solution demonstrating a 26.5% lower dry shrinkage than the 16 M solution. The creep behavior indicated a high initial strain within the first 7 days, significantly influenced by curing conditions and NaOH concentration. This study contributes to the existing knowledge by providing a deeper understanding of the time-dependent properties of GPC, which is crucial for optimizing its performance in structural applications.

Adhesive Strength and Setting Shrinkage of UP Polymer Mortar Intermixed with Waste Rubber Powder (폐고무분말을 혼입한 UP 폴리머모르타르의 경화수축 및 부착강도)

  • Yeon, Kyu-Seok;Jin, Nan-Ji;Choi, Jong-Yun;Beck, Jong-Man
    • Proceedings of the Korean Society of Agricultural Engineers Conference
    • /
    • 2003.10a
    • /
    • pp.383-386
    • /
    • 2003
  • In this study, the MMA-modified paste mixed waste rubber powder, which has a small elastic modulus and a large modification, was produced by using the soft unsaturated polyester resin(UP) as a binder. Then the adhesive properties according to the matrices in both underwater and air-dry conditions and the hardening shrinkage according to the contents of shrinkage reducing agent(SRA) and of MMA were surveyed. The experimental results show that, regardless of humidity of matrices the adhesive strength of polymer concrete was larger than cement concrete. the adhesive strength of MMA content of 20% was larger than MMA content of 30%. regardless of matrix materials the adhesive strength in water condition were $20{\sim}30%$ comparing with the air-dry condition. The case of MMA content of 20% showed the largest adhesive strength. In the hardening shrinkage experiment, the hardening shrinkage reduced as MMA and SRA contents increased, and the decrease of the hardening shrinkage by SRA was larger.

  • PDF

Characteristics of Compressive Strength and Drying-shrinkage Equation of Alkali-activated Mortar (알칼리 활성화 결합재 모르타르의 압축강도 특성 및 건조수축 추정식에 관한 연구)

  • Park, Kwang-Min;Kim, Hyung-Suk;Cho, Young-Keun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.21 no.2
    • /
    • pp.114-121
    • /
    • 2017
  • The purpose of this study is to understand a compressive strength and propose a dry shrinkage strain equation being able to predict dry shrinkage of alkali-activated materials(AAM) mortar samples manufactured using fly-ash(FA) and ground granulated blast furnace slag(GGBFS). The main parameters investigated were the GGBFS replace ratios(30, 50, 70 and 100%) and sodium silicate modules(Ms[$SiO_2/Na_2O$] 1.0, 1.5 and 2.0). The compressive strength of AAM increased with increases GGBFS replace ratios or Ms contents. The dry shrinkage strain of AAM decreased with increases Ms contents. But, the dry shrinkage strain of AAM increased as the GGBFS replace ratio increases. Therefore, the GGBFS replace ratio seems to have very significant and important consequences for the mix design of the AAM mortar. The results indicated the R-square of single regression analysis based on each mix properties was the highest value; 0.7539~0.9786(average 0.9359). And the presumption equation of dry shrinkage strain with all variables(GGBFS, Ms and material age) has higher accuracy and its R-square was 0.8020 at initial curing temperature 23 degrees Celsius and 0.8018 at initial curuing temperature 70 degrees Celsius.

An Experimental Study on The Differential Dry Shrinkage of Concrete Using Artificial Lightweight Aggregate (인공 경량골재를 사용한 콘크리트의 부등 건조수축에 관한 실험적 연구)

  • Lee, Chang-soo;Kim, Young-ook;Lin, Yan
    • Journal of the Society of Disaster Information
    • /
    • v.6 no.1
    • /
    • pp.78-90
    • /
    • 2010
  • Exposure to the outside, the concrete is differential moisture distribution depending on the depth. Such a differential moisture distribution causes the differential drying shrinkage in concrete structures. This thesis is researched to compare the shrinkage of lightweight concrete depending on depth to normal concrete. It is used artificial lightweight aggregate which has 20% of pre-absorb value by lightweight concrete. When water-binder ratio is 30%, average shrinkage of lightweight concrete section decreased than normal concrete, but differential shrinkage of lightweight concrete section increased. However water-binder ratio is 40% and 50% average shrinkage and differential shrinkage of lightweight concrete section decreased than normal concrete.

Study on Properties of Dry Shrinkage according to Amount of Shrinkage Reduction Agent (수축저감제 혼입량에 따른 건조수축 특성 검토)

  • Seo, Tae Seok;Lee, Hyun Seung;Kim, Kang Min;Yoon, Seob
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.05a
    • /
    • pp.209-210
    • /
    • 2021
  • This study aims to develop ultra-low-shrinkage high-quality concrete. Therefore, the concrete drying shrinkage characteristics according to the type and amount of the shrinkage reducing agent were reviewed. As a result, the performance of Hexylene Glycol(HG) and Polyol was superior to that of PolyEthylene Glycol(PEG), which is most widely used in Korea. In addition, the shrinkage reduction effect was improved as the amount of PEG was increased, but the disadvantage of the strength reduction when excessive use was confirmed.

  • PDF

Mechanical and Drying Shrinkage of Concrete Replaced with Recycled Coarse Aggregate with Less than 13mm in Size (13mm이하 순환 굵은골재 치환에 따른 콘크리트의 역학적 특성 및 건조수축)

  • Lee, Sun-Jae;Kim, Sang-Sup;Park, Young-Jun;Han, Dong-Yeop;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2015.05a
    • /
    • pp.63-64
    • /
    • 2015
  • This study has analyzed mechanical and dry shrinkage properties according to the recycled coarse aggregate by nominal strength actually being widely used at the Remicon companies for the purpose of qualitative improvement of concrete, practical use and examination at various strengths. As a result, although the modulus of elasticity showed a tendency of getting decreased as the replacement ratio of recycled coarse aggregate has increased, the difference was insignificant while the compressive strength showed a tendency of about 3MPa increase in the recycled coarse aggregate replacement ratio of 30% compared to the ratio of 0%. In case of the dry shrinkage length variation ratio, the recycled coarse aggregate replacement ratio of 30% showed a tendency of about 20% shrinkage reduction compared to the ratio of 0%.

  • PDF