  • During May of 2003, smoke from fires in the Yucatan Peninsula was transported across the Gulf of Mexico and into Texas where it caused significant enhancement in measured aerosol concentrations and reduced visibility. During this event, the formation and growth of aerosol particles has been observed by a differential mobility analyzer (DMA) / tandem differential mobility analyzer (TDMA) system to characterize the size distribution and size-resolved hygroscopicity of the aerosol. The most number concentration is by the particles smaller than 100 nm, but the integrated number concentrations for over 100 nm increased due to the aerosol growth. Hygroscopic growth factor increase from 1.2 to 1.4 for 25, 50, and 100 nm particles during the nucleating period. This distribution and the aerosol properties derived from the TDMA data were used to calculate the growth rate. Particle growth rates were in the range 1-12 nm/hr.

Differential Mobility Analyzer(DMA)와 Condensation Nuclei Counter(CNC)를 이용한 입자크기 분포 측정에서 샘플링 튜브와 CNC에서의 혼합 효과가 입자 크기 분포 측정에 미치는 영향에 관한 연구 (Study on the Contribution of Mixing Effects in Sampling Tube and Condensation Nuclei Counter(CNC) to the measurement of size distribution obtained using Differential Mobility Analyzer and CNC)

  • 이윤수;안강호
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집D
    • /
    • pp.104-109
    • /
    • 2001
  • The time to measure the size distribution using Condensation Nuclei Counter(CNC) and Differential Mobility Analyzer(DMA) can be shortened by classifying particles ramping the DMA voltage exponentially and continuously. In measurement, particles sampled at different time are mixed together going through sampling tube and CNC. Because the size distribution is inversed by using detector responses to sampling time intervals in this accelerated method, the mixing effects give inversion errors to the size distribution. The mixing effects can be considered by appling the transfer function with mixing effects to the data inversion. The inversion considering this effects gives birth to the size distribution shifted to the opposite direction of the size scanning.

  • PDF

폐기물 소각시 생성되는 유해 중금속물질과 연소실내 비산재와의 응축, 응집 현상에 대한 연구 (Condensation and coagulation of metallic species with fly ash particles in a waste incinerator)

  • 유주현;황정호
    • 대한기계학회논문집B
    • /
    • 제21권2호
    • /
    • pp.264-274
    • /
    • 1997
  • A numerical analysis on condensation and coagulation of the metallic species with fly ash particles pre-existing in an incinerator was performed. Waste was simplified as a mixture of methane, chlorine, and small amounts of Pb and Sn. Vapor-phase amounts of Pb- and Sn -compounds were first calculated assuming a thermodynamic equilibrium state. Then theories on vapor-to-particle conversion, vapor condensation onto the fly ash particles, and particle-particle interaction were examined and incorporated into equations of aerosol dynamics and vapor continuity. It was assumed that the particles followed a log-normal size distribution and thus a moment model was developed in order to predict the particle concentration and the particle size distribution simultaneously. Distributions of metallic vapor concentration (or vapor pressure) were also obtained. Temperature drop rate of combustion gas, fly ash concentration and its size were selected as parameters influencing the discharged amount of metallic species. In general, the coagulation between the newly formed metal particles and the fly ash particles was much greater than that between the metal particles themselves or between the fly ash particles themselves. It was also found that the amount of metallic species discharged into the atmosphere was increased due to coagulation. While most of PbO vapors produced from the combustion were eliminated due to combined effect of condensation and coagulation, the highly volatile species, PbCl$_{2}$ and SnCl$_{4}$ vapors tended to discharge into the atmosphere without experiencing either the condensation or the coagulation. For Sn vapors the tendency was between that of PbO vapors and that of PbCl$_{2}$ or SnCl$_{4}$. To restrain the discharged amount of hazardous metallic species, the coagulation should be restrained, the number concentration and the size of pre-existing fly ash particles should be increased, and the temperature drop rate of combustion gas should be kept low.

중유 연소 시 발생하는 미세입자 및 니켈과 바나듐의 대기 중 배출특성 (Emission Characteristics of Fine Particles, Vanadium and Nickel from Heavy Oil Combustion)

  • 장하나;김성현;이주형;황규원;유종익;석정희;서용칠
    • 한국대기환경학회지
    • /
    • 제22권3호
    • /
    • pp.353-360
    • /
    • 2006
  • This study identified a particle size distribution (PSD) of fine particulate matter and emission characteristics of V and Ni by the comparison between anthropogenic sources of oil combustion (industrial boiler, oil power plant, etc.) and lab-scale combustion using a drop-tube furnace. In oil combustion source, the mass fraction of fine particles (less than 2.5 micrometers in diameter) was higher than that of coarse particles (larger than 2.5 micrometers in diameter) in $PM_{10}$ (less than 10 micrometers in diameter) as like in lab-scale oil combustion. In addition to this, it was identified that ultra-fine particles (less than 0.1 micrometers in diameter) had a large distribution in fine particles. Toxic metals like V and Ni had large mass fractions in fine particles, and most of all was distributed in ultra-fine particles. Most of ultra-fine particles containing toxic metals have been emitted into ambient by combustion source because it is hard to control by the existing air pollution control device. Hence, we must be careful on these pollutants because it is obvious that these are associated with adverse health and environmental effect.

액상수은 제어를 위한 다공성 탄소입자 제조에 관한 연구 (Synthesis of Porous Carbon Particles for the Absorption of Mercury)

  • 이정민;강신재;박수진
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2009년도 추계학술대회 논문집
    • /
    • pp.305-305
    • /
    • 2009
  • The carbon nano-structured materials could be applied to the fields of advanced fillers, templates, electrode materials, sensor, storage, and absorption materials. The polyacrylonitrile (PAN) based carbon nano-particles provide the remarkable properties of high specific surface area, large pore volume, chemical inertness, and good mechanical stability. In this study, well-defined carbon nano-particles were obtained through pyrolysis of polyacrylonitrile based particles. The precursor nano-particles were prepared by modified aqueous dispersion polymerization using hydrophilic poly(vinyl alcohol) in a water/ N,N-dimethylformamide mixture media. Synthesized precursor nanoparticles have relatively monodisperse particles ranging 80 ~ 250nm. Stable spherical particles are obtained without coagulum or secondary particles in our system. The characteristic of the carbon nanoparticles were investigated in terms of surface area, morphology, and size distribution.

  • PDF

[Retraction]Size measurement and characterization of ceria nanoparticles using asymmetrical flow field-flow fractionation (AsFlFFF)

  • Kim, Kihyun;Choi, Seong-Ho;Lee, Seungho;Kim, Woonjung
    • 분석과학
    • /
    • 제32권5호
    • /
    • pp.173-184
    • /
    • 2019
  • As the size of semiconductors becomes smaller, it is necessary to perform high precision polishing of nanoscale. Ceria, which is generally used as an abrasive, is widely used because of its uniform quality, but its stability is not high because it has a high molecular weight and causes agglomeration and rapid precipitation. Such agglomeration and precipitation causes scratches in the polishing process. Therefore, it is important to accurately analyze the size distribution of ceria particles. In this study, a study was conducted to select dispersants useful for preventing coagulation and sedimentation of ceria. First, a dispersant was synthesized and a ceria slurry was prepared. The defoamer selection experiment was performed in order to remove the air bubbles which may occur in the production of ceria slurry. Dynamic light scattering (DLS) and asymmetrical flow field-flow fractionation (AsFlFFF) were used to determine the size distribution of ceria particles in the slurry. AsFlFFF is a technique for separating nanoparticles based on sequential elution of samples as in chromatography, and is a useful technique for determining the particle size distribution of nanoparticle samples. AsFlFFF was able to confirm the presence of a little quantities of large particles in the vicinity of 300 nm, which DLS can not detect, besides the main distribution in the range of 60-80 nm. AsFlFFF showed better accuracy and precision than DLS for particle size analysis of a little quantities of large particles such as ceria slurry treated in this study.

Synthesis of scheelite-type nanocolloidal particles by pulsed laser ablation in liquid and their size distribution analysis

  • Lee, Jung-Il;Shim, Kwang Bo;Ryu, Jeong Ho
    • 한국결정성장학회지
    • /
    • 제24권3호
    • /
    • pp.111-119
    • /
    • 2014
  • A novel pulsed laser ablation process in liquid was investigated to prepare scheelite-type ceramic [calcium tungstate ($CaWO_4$) and calcium molybdate ($CaMoO_4$)] nanocolloidal particles. The crystalline phase, particle morphology, particle size distribution, absorbance and optical band-gap were investigated. Stable colloidal suspensions consisting of well-dispersed $CaWO_4$ and $CaMoO_4$ nanoparticles with narrow size distribution could be obtained without any surfactant. Particle tracking analysis using optical microscope combined with image analysis was applied for a fast determination of particle size distribution in the prepared nanocolloidal suspensions. The mean nanoparticle size of $CaWO_4$ and $CaMoO_4$ colloidal nanoparticles were 16 nm and 30 nm, with the standard deviations of 2.1 and 5.2 nm, respectively. The optical absorption edges showed blue-shifted values about 60~70 nm than those of reported in bulk crystals. And also, the estimated optical energy band-gaps of $CaWO_4$ and $CaMoO_4$ colloidal particles were 5.2 and 4.7 eV. The observed band-gap widening and blue-shift of the optical absorbance could be ascribed to the quantum confinement effect due to the very small size of the $CaWO_4$ and $CaMoO_4$ nanocolloidal particles prepared by pulsed laser ablation in liquid.

[Retraction]Characterization of carbon black nanoparticles using asymmetrical flow field-flow fractionation (AsFlFFF)

  • Kim, Kihyun;Lee, Seungho;Kim, Woonjung
    • 분석과학
    • /
    • 제32권3호
    • /
    • pp.77-87
    • /
    • 2019
  • High viscosity carbon black dispersions are used in various industrial fields such as color cosmetics, rubber, tire, plastic and color filter ink. However, carbon black particles are unstable to heat due to inherent characteristics, and it is very difficult to keep the quality of the product constant due to agglomeration of particles. In general, particle size analysis is performed by dynamic light scattering (DLS) during the dispersion process in order to select the optimum dispersant in the carbon black dispersion process. However, the existing low viscosity analysis provides reproducible particle distribution analysis results, but it is difficult to select the optimum dispersant because it is difficult to analyze the reproducible particle distribution at high viscosity. In this study, dynamic light scattering (DLS) and asymmetrical flow field-flow fractionation (AsFlFFF) analysis methods were compared for reproducible particle size analysis of high viscosity carbon black. First, the stability of carbon black dispersion was investigated by particle size analysis by DLS and AsFlFFF according to milling time, and the validity of analytical method for the selection of the optimum dispersant useful for carbon black dispersion was confirmed. The correlation between color and particle size of particles in high viscosity carbon black dispersion was investigated by using colorimeter. The particle size distribution from AsFlFFF was consistent with the colorimetric results. As a result, the correlation between AsFlFFF and colorimetric results confirmed the possibility of a strong analytical method for determining the appropriate dispersant and milling time in high viscosity carbon black dispersions. In addition, for nanoparticles with relatively broad particle size distributions such as carbon black, AsFlFFF has been found to provide a more accurate particle size distribution than DLS. This is because AsFlFFF, unlike DLS, can analyze each fraction by separating particles by size.

침강 장-흐름 분획법을 이용한 CdS 양자점 입자의 특성 분석 (Characterization of CdS-quantum dot particles using sedimentation field-flow fractionation (SdFFF))

  • 최재영;김도균;정의창;권해두;이승호
    • 분석과학
    • /
    • 제28권1호
    • /
    • pp.33-39
    • /
    • 2015
  • CdS 양자점 입자는 특정 파장의 빛을 방출하는 반도체 나노 결정으로 이러한 광학적 특성 때문에 질병 진단 시약, 광학기술, 미디어 산업 및 태양전지와 같은 다양한 분야에서 응용되는 물질이다. 방출하는 빛의 색은 입자의 크기에 의존하기 때문에 CdS 양자점 입자의 크기 및 크기분포를 정확하게 분석하는 것이 필요하다. 본 연구에서는 CdS 양자점 입자를 감마-선 조사법(${\gamma}$-ray irradiation method)을 이용하여 합성하고, 크기 및 크기 분포도를 결정하기 위하여 침강 장-흐름 분획법 (SdFFF)를 이용하였다. 침강 장-흐름 분획법을 이용한 CdS 양자점 입자의 정확한 분석을 위하여 분석조건의 최적화(유속, 외부장 세기, field-programming)에 대하여 조사되었다. 투과 전자 현미경(transmission electron microscopy, TEM)으로 확인된 단일 입자의 크기는 ~4 nm 였으며, 단일 입자의 응집으로 생성된 2차 입자 크기의 평균은 159 nm로 확인되었다. 첨가된 입자 안정제의 농도가 증가할수록 CdS 양자점 입자의 크기가 감소하는 경향성을 확인하였다. 침강 장-흐름 분획법, 투과 전자 현미경, 그리고 동적 광 산란법(dynamic light scattering, DLS)으로 결정된 CdS 양자점 크기는 각각 126, 159, 그리고 152 nm 였다. 본 연구의 결과로 침강 장-흐름 분획법은 비교적 넓은 크기분포를 갖는 다양한 종류의 무기입자의 크기 및 크기 분포도를 결정하는데 유용한 방법임을 확인하였다.

Hydrazine Hydrate 환원(還元)에 의한 질산은(窒酸銀) 수용액(水溶液)으로부터 은(銀) 나노분말(粉末)의 제조(製造) 연구(硏究) (Preparation of Ag Nano-Powder from Aqueous Silver Nitrate Solution through Reduction with Hydrazine Hydrate)

  • 이화영
    • 자원리싸이클링
    • /
    • 제15권4호
    • /
    • pp.19-26
    • /
    • 2006
  • 함은 폐재의 리싸이클링을 위한 연구의 일환으로써 Hydrazine Hydrate을 환원제로 사용하여 질산은 수용액으로부터 Ag 나노분말을 제조하기 위한 실험을 수행하였다. 이를 위해 질산은을 소정 농도로 증류수에 용해시킨 수용액에 Ag 미립자의 응집방지를 위한 분산제로써 Tamol NN8906 혹은 Tween 20을 미리 혼합한 다음 환원제인 Hydrazine Hydrate 용액을 첨가하는 방법으로 환원반응을 실시하였다. 환원반응을 통하여 제조한 Ag 미립자는 입도분석기 및 TEM 측정을 통하여 형상과 평균입도를 측정하였다. Hydrazine Hydrate에 의한 은의 환원을 위해서는 이론치의 약 2배를 첨가해 주어야 하는 것으로 나타났으며, Tamol NN8906을 분산제로 사용하여 제조한 Ag 나노분발은 매우 좁은 입도범위의 분포특성을 보여 주었다. Tween 20을 분산제로 사용한 경우의 입도 분포는 bimodal 혹은 multimodal distribution을 보였으며, 입자 모양에 있어서는 Tamol NN8906과 Tween 20이 모두 비슷하게 표면이 매끄러운 불규칙한 모양의 입자들로 구성되어 있었다.