• 제목/요약/키워드: Dissolved hydrogen

검색결과 210건 처리시간 0.023초

핵연료 피복관 부식생성물 부착에 대한 용존수소의 영향 (Effect of Dissolved Hydrogen on Fuel Crud Deposition)

  • 백승헌;김우철;심희상;임경수;원창환;허도행
    • Corrosion Science and Technology
    • /
    • 제13권2호
    • /
    • pp.56-61
    • /
    • 2014
  • The purpose of this work is to investigate the effect of dissolved hydrogen concentration on crud deposition onto the fuel cladding surface in the simulated primary environments of a pressurized water reactor. Crud deposition tests were conducted in the dissolved hydrogen concentration range of 5~70 cc/kg at $325^{\circ}C$ for 14 days. Needle-shaped NiO deposits were formed in the hydrogen range of 5~25 cc/kg, while polygonal nickel ferrite deposits were observed at a hydrogen concentration above 35 cc/kg. However, the dissolved hydrogen content seems to have little effect on the amount of crud deposits.

Electrochemical behavior of dissolved hydrogen at Pt electrode surface in a high temperature LiOH-H3BO3 solution: Effect of chloride ion on the transient current of the dissolved hydrogen

  • Myung-Hee Yun;Jei-Won Yeon
    • Nuclear Engineering and Technology
    • /
    • 제55권10호
    • /
    • pp.3659-3664
    • /
    • 2023
  • The electrochemical behavior of dissolved hydrogen (H2) was investigated at a Pt electrode in a high temperature LiOH-H3BO3 solution. The diffusion current of the H2 oxidation was proportional to the concentration of the dissolved H2 as well as the reciprocal of the temperature. In the polarization curve, a potential region in which the oxidation current decreases despite an increase in the applied potential between the H2 oxidation and the water oxidation regions was observed. This potential region was interpreted as being caused by the formation of a Pt oxide layer. Using the properties of the Cl- ion that reduces the growth rate of the Pt oxide layer, it was confirmed that there is a correlation between the Cl- ion concentration and the transient current of the H2 oxidation.

팔라듐이 코팅된 광섬유 격자를 이용한 절연유속의 용존 수소가스 검출 (Detection of Hydrogen Gas Dissolved in Insulation Oil Based on Palladium-coated Fiber Bragg Grating)

  • 김광택;최누리;백세종
    • 센서학회지
    • /
    • 제27권6호
    • /
    • pp.403-406
    • /
    • 2018
  • We have investigated a fiber-optic sensor for detecting the hydrogen gas dissolved in insulation oil based on a palladium (Pd)-coated fiber Bragg grating (FBG). As the palladium absorbs the hydrogen gas dissolved in the insulation oil, its volume expands and the Bragg wavelength shifts to a longer wavelength. The experimental results showed that the Bragg wavelength of FBG increased to 70 nm when the concentration of hydrogen dissolved in the insulation oil was 409 ppm.

붕산수용액 매질에서 용존수소와 과산화수소의 고온 전기화학 거동연구 (Electrochemical Behavior of Dissolved Hydrogen and Hydrogen Peroxide in Boric Acid Solution at the Elevated Temperature)

  • 연제원;우승균;최영구;정용주;김원호
    • 전기화학회지
    • /
    • 제7권1호
    • /
    • pp.21-25
    • /
    • 2004
  • 용존수소와 과산화수소의 전기화학 거동을 백금 디스크 전극을 사용하여 정전위 분극법으로 $25^{\circ}C$$200^{\circ}C$붕산수용액에서 측정하였다. $25^{\circ}C$에서 용존수소의 산화반응은 전극표면에서의 전자전달속도에 의존하는 반응속도론적 지배반응이었다. 그러나 온도가 올라감에 따라 용존수소의 전기화학 거동은 반응속도론적 지배반응에서 확산지배반응으로 변하였다. 고온 용존수소 조건에서 한 가지 주목할 만한 사실은 물의 산화가 시작되는 직전 전위에서 용존수소의 산화반응이 급격히 줄어드는 특이한 전위영역이 관찰되었다는 점이다. 이 현상은 백금 전극표면에 수산화이온의 흡착에 기인한 것으로 생각된다. 반면에 과산화수소의 경우. 온도가 증가함에 따라 증가하는 확산계수로 인한 전류밀도의 증가를 제외하고는 온도에 따른 전극반응의 명백한 변화는 보이지 않았다.

가스센서를 이용한 부분방전특성에 따른 유중수소가스 측정연구 (Measurement Technology of the Dissolved Hydrogen Gas Due to Partial Discharge in Oil using Gas Sensor)

  • 허종철;선종호;강동식;정주영;추영배;박정후
    • 전기학회논문지
    • /
    • 제58권9호
    • /
    • pp.1784-1789
    • /
    • 2009
  • This paper describes the measurement technology of the dissolved hydrogen gas due to partial discharge in oil using gas sensor. For higher resolution and less error in measurement of the dissolved hydrogen gas in oil, the sensor outputs with ambient temperature which affect the sensor output characteristics should be considered. The sensor output trends with ambient temperature and the properties of the dissolved hydrogen gas in oil with partial discharge characteristic were analyzed through the test results. It was indicated that the sensor peak and the base voltage with measuring time were affected by ambient temperature and the measurement errors of the sensor output by temperature were reduced by using the difference between the peak and the base voltage rather than just the peak voltage. In addition, the hydrogen gas sensor outputs were increased with the increase of partial discharge energy.

수소 첨가 열처리에 따른 Ti-6Al-4V 합금 분말의 격자 변형 및 내산화성 향상 (Lattice Deformation and Improvement Oxidation Resistance of Ti-6Al-4V Alloy Powders Prepared by Hydrogen Added Argon Heat Treatment)

  • 조계훈;오정민;임재원
    • 한국분말재료학회지
    • /
    • 제26권2호
    • /
    • pp.126-131
    • /
    • 2019
  • In the present work, a new hydrogen added argon heat treatment process that prevents the formation of hydrides and eliminates the dehydrogenation step, is developed. Dissolved hydrogen has a good effect on sintering properties such as oxidation resistance and density of greens. This process can also reduce costs and processing time. In the experiment, commercially available Ti-6Al-4V powders are used. The powders are annealed using tube furnace in an argon atmosphere at $700^{\circ}C$ and $900^{\circ}C$ for 120 min. Hydrogen was injected temporarily during argon annealing to dissolve hydrogen, and a dehydrogenation process was performed simultaneously under an argon-only atmosphere. Without hydride formation, hydrogen was dissolved in the Ti-6Al-4V powder by X-ray diffraction and gas analysis. Hydrogen is first solubilized on the beta phase and expanded the beta phases' cell volume. TGA analysis was carried out to evaluate the oxidation resistance, and it is confirmed that hydrogen-dissolved Ti-6Al-4V powders improves oxidation resistance more than raw materials.

가스수집시간을 이용한 유중수소가스 측정감도 향상 연구 (Sensitivity Enhancement in Measurement of Hydrogen Gas Dissolved in Oil using Gas Collection Time)

  • 허종철;선종호;강동식;정주영;박정후
    • 전기학회논문지
    • /
    • 제58권3호
    • /
    • pp.539-543
    • /
    • 2009
  • This paper describes the sensitivity enhancement in measurement of the hydrogen gas dissolved in oil using gas collection time. On-line gas measurement is a useful for continuous monitoring of power transformer. Recently many studies on hydrogen gas measurement, due to their simplicity and low price, have been done for transformer monitoring. In measurement of the hydrogen gas in oil, the suitable sensitivity and resolution in the desired ranges of the gas concentrations are needed for the reliable monitoring of power transformers. In this study, the sensor output trends were analyzed with the hydrogen gas collection time which means the time to collect the hydrogen gas before reaction of hydrogen gas sensor. It is indicated that the sensor outputs were increased with the increase of hydrogen gas collection times at the same hydrogen gas concentrations.

온도의 영향에 따른 니켈페라이트의 입자 크기 분포 연구 (A Study on Effect of Temperature on Particle Size Distribution of Nickel Ferrite)

  • 안현경;이인형;정현준;박병기
    • 한국산학기술학회논문지
    • /
    • 제9권6호
    • /
    • pp.1768-1774
    • /
    • 2008
  • PWR 정지화학 조건에서 모사실험하여 니켈페라이트 입자의 거동을 조사하였다. 농도가 Li 0.1 ppm, B 2000 ppm인 모사실험 용액의 온도는 $300^{\circ}C$에서 $0.625^{\circ}C/min$의 비율로 $150^{\circ}C$까지 감소시킨 후 일정 시간 동안 $150^{\circ}C$를 유지하였고 이때의 압력은 2500psi 이하로 유지하였다. 수소 농도 5, 15, 25 cc/kg $H_2O$ 일 때 온라인으로 입자 분포를 측정하였고 용해된 니켈 농도도 분석하였다. 실험결과 온도 감소 시 세 가지 수소 농도일 때 모두 총입자 수는 큰 변화가 없었다. 그러나 온도가 감소하고 일정하게 유지될 때 입자는 작아졌다. 입자 크기 분포 변화의 정도는 $H_2$ 15cc/kg $H_2O$ 일 때가 가장 크게 나타났다. 니켈 이온의 농도는 온도가 감소하고 수소 15 cc/kg $H_2O$ 일 때 증가하였다. 이 결과 니켈 페라이트는 온도 변화 시, 수소 15 cc/kg $H_2O$ 일 때 불안정 한 것으로 보여 진다.

Novel oxygenation for lipopeptide production from Bacillus sp. GB16

  • Lee, Baek-Seok;Lee, Jae-Woo;Shin, Haw-Shook;Choi, Sung-Won;Choi, Ki-Hyun;Lee, Jae-Ho;Kim, Eun-Ki
    • 한국생물공학회:학술대회논문집
    • /
    • 한국생물공학회 2003년도 생물공학의 동향(XII)
    • /
    • pp.240-244
    • /
    • 2003
  • A novel integrated method for increasing dissolved oxygen concentration in culture media has been developed. It involves adding hydrogen peroxide to the medium, which is then decomposed to oxygen and water by catalase and adding vegetable oil to the medium as antifoam agent and oxygen vector. A new apparatus for automated addition of hydrogen peroxide to the bioreactor to keep the dissolved oxygen concentration constant over the range $10-100%\;{\pm}\;5%$ was tested. A significant increase (over threefold) of cultivation time was obtained while the dissolved oxygen concentration remained stable ($30%\;{\pm}\;5%$). Therefore, use of corn oil mixed with Ca-stearate as oxygen vector and antifoam and hydrogen peroxide as oxygen source to control excessive foam that was generated by microorganism biosurfactant, GB16-BS produced at Bacillus sp. GB16 cultivation was appropriate for stable cultivation.

  • PDF

Gas Detector for Hydrogen Dissolved in Transformer Oil

  • Seo Ho-Joon;Hwang Kyu-Hyun;Rhie Dong-Hee
    • KIEE International Transactions on Electrophysics and Applications
    • /
    • 제5C권2호
    • /
    • pp.72-75
    • /
    • 2005
  • In oil-filled equipment such as transformers, partial discharge or local overheating will precede a final shutdown. Accompanied with such problems is a decomposition of insulating material into gases, which are dissolved into the transformer oil. The gases dissolved in oil can be separated with some membranes based on the differences in permeability of membranes to different gases. This paper discuss the permeability characteristics of several membranes for separation hydrogen gas in oil. With result of this paper, it may become possible to detect fault-related gases from transformer oil and predict incipient failures in the