• 제목/요약/키워드: Dissimilar aluminum alloy

검색결과 50건 처리시간 0.029초

마찰교반접합의 공정변수가 AA2219-AA2195 이종 알루미늄 접합에 미치는 영향 (Effect of Process Parameters on Friction Stir Welds on AA2219-AA2195 Dissimilar Aluminum Alloys)

  • 노국일;유준태;윤종훈;이호성
    • 한국재료학회지
    • /
    • 제27권6호
    • /
    • pp.331-338
    • /
    • 2017
  • This study was carried out to investigate the optimum condition of a friction stir welding process for a joint of AA2219-T87 and AA2195-T8 dissimilar aluminum alloys. These alloys are known to have good cryogenic properties, and as such to be suitable for use in fuel tanks of space vehicles. The welding parameters include the travelling speed, rotation speed and rotation direction of the tool. The experiment was conducted under conditions in which the travelling speed of the tool was 120-300 mm/min and the rotation speed of the tool was 400-800 rpm. To investigate the effect of the rotation direction of the tool, the joining was performed by switching the positions of the two dissimilar alloys. After welding, the microstructure was observed and the micro-hardness were measured; non-destructive evaluation was carried out to perform tensile tests on defect-free specimens. The result was that the microstructure of the weld joint underwent dynamic recrystallization due to sufficient deformation and frictional heat. The travelling speed of the tool had little effect on the properties of the joint, but the properties of the joint varied with the rotation speed of the tool. The conditions for the best joining properties were 600 rpm and 180-240 mm/min when the AA2219-T8 alloy was on the retreating side(RS).

Effect of Resistance Spot Welding Parameters on AA1100 Aluminum Alloy and SGACD Zinc coated Lap Joint Properties

  • Chantasri, Sakchai;Poonnayom, Pramote;Kaewwichit, Jesada;Roybang, Waraporn;Kimapong, Kittipong
    • International Journal of Advanced Culture Technology
    • /
    • 제3권1호
    • /
    • pp.153-160
    • /
    • 2015
  • This article is aimed to study the effects of resistance spot welding (RSW) on the lap joint properties between AA1100 aluminum alloy and SGACD zinc coated steel and its properties. The summarized experimental results are as follows. The summarized experimental results are as follows. The optimum welding parameters that produced maximum tensile shear strength of 2200 N was a welding current of 95 kA, a holding time of 10 cycles, and a welding pressure of 0.10 MPa. Increasing of welding current, increased the tensile shear strength of the joint and also increased the amount of aluminum dispersion at the joint interface. The lap joint of steel over the aluminum (Type I) showed the higher joint tensile shear strength than a lap joint of aluminum over the steel (Type II). The indentation depth and the ratio of the indentation depth to the plate thickness decreased when the welding current was increased in the type I lap joint and also decreased when the welding current was decreased in the type II lap joint. The interface structure showed the formation of the brittle $FeAl_3$ intermetallic compound that deteriorated the joint strength.

알루미늄 합금과 고장력 강판 접합을 위한 헬리컬 SPR의 설계 (Design of Helical Self-Piercing Rivet for Joining Aluminum Alloy and High-Strength Steel Sheets)

  • 김원영;김동범;박진근;김도훈;김기호;이인환;조해용
    • 대한기계학회논문집A
    • /
    • 제38권7호
    • /
    • pp.735-742
    • /
    • 2014
  • Self-piercing rivet(SPR)은 이종재료 접합을 위해 사용되는 결합용 기계요소로써, 대표적으로는 알루미늄 합금과 강판 등 용융점이 서로 다른 재료의 접합에 사용된다. SPR 접합은 일반 리벳접합과 달리 스스로 홀을 가공하며 삽입되기 때문에 사전의 홀 가공이 필요 없다.(1) 상부판재를 천공하고 하부판재와 함께 소성 변형되어 결합된다. 자동차의 차체 경량화를 위해서는 알루미늄 합금과 같은 경량소재가 사용되며, 부분적으로 스틸과 알루미늄 합금의 이종재료 접합이 요구된다. 그러나 알루미늄 합금과 강판은 용융점이 다르므로 기존의 차체 결합방법으로 이용되고 있는 저항 용접이 불가능하다. 이에 따라, 기계적 결합방법의 하나인 SPR 접합이 요구된다.(2) 따라서 본 연구에서는 강소성 유한요소해석 프로그램을 이용하여 리벳과 판재의 접합 성형성을 검토하고, 고장력 강판을 접합할 수 있는 새로운 형상의 SPR을 설계하였다. 또한 해석결과와 실험의 비교를 통하여 해석의 신뢰성을 검증하였다.

타이타늄 소재 마찰교반용접 기술 동향 (Recent Trends of Friction Stir Welding of Titanium)

  • 천창근;김성욱;김흥주;장웅성;노중석
    • Journal of Welding and Joining
    • /
    • 제31권2호
    • /
    • pp.16-20
    • /
    • 2013
  • Titanium and its alloys have been widely using in the various field of industry application due to high corrosion resistant properties and mechanical properties. Titanium is highly reactive in the high temperature state and the formation of titanium oxide and porosities in the nuggets of fusion welding will results in the degradation of the mechanical properties. For this reason the studies of friction stir welding for titanium have been investigated recently. The FSW zones of titanium were classified by the weld nugget (WN), the linear transition boundary (TB) and the heat affected zone (HAZ). The WN along with titanium parent was characterized by the presence of twins and dislocations. The average grain size and hardness of WN has been changed according to heat input. The grain refinement resulted from the FSW increased the hardness in the stir zone. Sound dissimilar joints between SUS 304 and CP-Ti were achieved using an advancing speed of 50 mm/min and rotation speeds in the range of 700-1100 rpm. Aluminum 1060 and titanium alloy Ti-6Al-4V plates were lap joined by friction stir welding, hence the ultimate tensile shear strength of joint reached 100% of Al 1060. Mg alloy and Ti were successfully butt joined by inserting a probe into the Mg alloy plate with slightly offsetting. But Ti-Al intermetallic compound layers formed at the interface of these joints.

소실모형주조법에 의한 내마모 복합조직층 형성에 미치는 공정인자의 영향 (Effects of Parameters on Abrasion-Resistant Layer of Composite Structure Formed by Evaporation Pattern Casting)

  • 최창영;모남규;김건호;윤종천;정유현;김동혁;최용진;이인규;조용재
    • 한국기계가공학회지
    • /
    • 제17권2호
    • /
    • pp.89-94
    • /
    • 2018
  • Due to industrial advancement and environmental concerns, there is a demand for light-weight material parts with high-performance characteristics. In order to meet this demand, various studies have been conducted on developing high-performance castings to achieve composite features by coating only specific parts that require high performance, with dissimilar joining, rather than coating the entire material part. This study analyzed the possibility of forming a local composite layer on an aluminum alloy through evaporation pattern casting, and the effects of parameters on the aluminum alloy.

이종알루미늄합금 FSW 접합부의 피로균열진전 특성 (Fatigue Crack Growth Properties of Friction Stir Welded Dissimilar Aluminum Alloys)

  • 이원준;이효재;김형진;박원조
    • 한국해양공학회지
    • /
    • 제27권1호
    • /
    • pp.37-42
    • /
    • 2013
  • The presence of a crack can increase the local stress or strain, which can cause inelastic deformation and significantly reduce the life of a component or structure. Therefore, in this study, the fatigue crack growth (FCG) behaviors of friction stir welded Al 2024-T3 and Al 7075-T6 specimens were examined, with fatigue cracks growing parallel to the dynamically recrystallized zone at variable ${\Delta}K$ values and an R ratio of 0.3. In addition, the FCG values of the base metal Al 2024-T3 and Al 7075-T6 were tested under the same conditions and parameters as comparative groups. The results showed that compared with the base metal Al 2024 specimen, which had the best fatigue property, the welded specimen had only 88% of the fatigue cycles.

Galvanic Corrosion Between Component Parts of Aluminum Alloys for Heat Exchanger of Automobile

  • Y. R. Yoo;D. H. Kim;G. B. Kim;S. Y. Won;S. H. Choi;Y. S. Kim
    • Corrosion Science and Technology
    • /
    • 제22권5호
    • /
    • pp.322-329
    • /
    • 2023
  • There are a variety of heat exchangers used in automobiles, such as shell and tube heat exchangers, double tube heat exchangers, and plate heat exchangers. Most of them are water-cooled to prevent engine overheating. There have been reports of corrosion damage to these heat exchangers due to continuous wetting caused by external temperature differences, road pollutants, and snow removal. In addition, galvanic corrosion, which occurs when two dissimilar materials come into contact, has been identified as a major cause. In this study, corrosion characteristics and galvanic corrosion behavior of Al alloy (AA3003, AA4045 and AA7072) used in automobile heat exchangers were analyzed. Effective clad materials for heat exchanger tubes and fins were also evaluated. It was found that AA7072 should be applied as the cladding material for fin AA3003 and that AA4045 was suitable as a cladding material for tube AA3003 because this clad materials application was the most effective clad design to delay the occurrence of pinhole in the tube. Main factors influencing galvanic corrosion dissolution were found to be galvanic corrosion potential difference and galvanic corrosion current density.

도금 강판 CMT 용접부위의 재료특성평가 (Characterization of Cold Metal Transfer Welding Coated Steel)

  • 송현수;최보성;윤존도;박승태
    • 한국정밀공학회지
    • /
    • 제32권10호
    • /
    • pp.891-896
    • /
    • 2015
  • In order to protect the environment, using light material is becoming more and more attractive within the automobile industry. Aluminum alloys are the best and lightest metallic materials used in the automotive, electron, and aerospace industries. Al alloy and SGARC were joined by cold metal transfer (CMT) welding, using AlSiMn4 as a filler. Results showed that dissimilar metals from the Al 6000 series/SGARC could be successfully joined by CMT under proper processing parameters. The micro-hardness value of 125Hv was obtained at an interface.

레이저를 이용한 알루미늄 합금과 스테인리스강의 용접 (A Study on the Welding of Aluminum Alloy and Stainless Steel by Laser)

  • 이철구;채병대
    • 한국공작기계학회논문집
    • /
    • 제14권2호
    • /
    • pp.91-95
    • /
    • 2005
  • A feasibility study was performed to see the welding possibility of dissimilar thin-plat materials. These materials were welded for finding the optimum welding condition and evaluating the soundness of welding zone. The welding was attempted under the condition of laser power 500~600w, Pulse width 1.0~2.5ms and frequency 11~18Hz. In this study, the highest tensile-shear strength was observed at laser the low frequency. The suitable welding condition can be obtain at the large pulse width and the low frequency.

EFFECT OF INTERMETALLIC COMPOUND ON MECHANICAL PROPERTIES OF Al-Cu DISSIMILAR BRAZING JOINT

  • Koyama, Ken;Shinozaki, Kenji;Ikeda, Kenji;Kuroki, Hidenori
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.555-560
    • /
    • 2002
  • Brazing of Al to Cu using AI-Si-Mg-Bi brazing alloy has been carried out in the vacuum furnace. In the bonded interlayer, there were two kinds of intermetallic compounds. One of these intermetallic compounds was e phase and the other was b phase. The growth of b phase was controlled by diffusion Al into Cu. Deformation behavior of Al-Cu brazing joint was brittle without deformation of the base metal. Shear strength of the joint was only about 20MPa. The shear specimen broken in the intermetallic compound, which was mainly e phase. Shear strength did not depend on the bonding temperature.