B2형 NiAl에 석출한 $L2_1$형 석출상의 석출거동에 관한 연구 (A Study on the Precipitation Behavior of $L2_1$-type Precipitates in B2-NiAl)

  • 한창석;한승오;이주희
    • 열처리공학회지
    • /
    • 제22권6호
    • /
    • pp.345-353
    • /
    • 2009
  • The precipitates of $L2_1$-type $Ni_2AlHf$ phase in B2-ordered NiAl system has been observed by using transmission electron microscope (TEM). The hardness of as-quenched NiAl-Hf alloys is high due to the larger strengthening. However, age hardening of this alloy is not main effect to increase hardness compared to the large microstructural variations during aging. At the beginning of aging, the $L2_1$-type $Ni_2AlHf$ precipitates keep a lattice coherency with the NiAl matrix. The orientation relationship between the $Ni_2 AlHf$ precipitate and the NiAl matrix is <100>$_{Ni2AlHf}$//<100>$_{NiAl}$, {001}$_{Ni2AlHf}$//{001}$_{NiAl}$. By aging treatment for long time $Ni_2AlHf$ precipitates lost their coherency and change their morphology to the spherical ones surrounded by misfit dislocations. The orientation relationship between the NiAl matrix and the $Ni_2AlHf$ precipitates, however, has been kept even after longer aging time. The lattice misfit between the $Ni_2AlHf$ precipitate and the NiAl matrix has been calculated by the selected electron diffraction patterns, and the spacings of misfit dislocations is about 4.5% at 1173 K.

High Temperature Creep Properties of Al-Al4C3-Al2O3 Alloy by Mechanical Alloying

  • Han, Chang-Suk;Seo, Han-Byeol
    • 한국재료학회지
    • /
    • 제26권7호
    • /
    • pp.370-375
    • /
    • 2016
  • Tensile tests and creep tests were carried out at high temperatures on an Al-$Al_4C_3$ alloy prepared by mechanical alloying technique. The material contains about 2.0% carbon and 0.9% oxygen in mass percent, and the volume fractions of $Al_4C_3$ and $Al_2O_3$ particles are estimated at 7.4 and 1.4%, respectively, from the chemical composition. Minimum creep rate decreased steeply near two critical stresses, ${\sigma}_{cl}$ (the lower critical stress) and ${\sigma}_{cu}$ (the upper critical stress), with decreasing applied stress at temperatures below 723 K. Instantaneous plastic strain was observed in creep tests above a critical stress, ${\sigma}_{ci}$, at each test temperature. ${\sigma}_{cu}$ and ${\sigma}_{ci}$ were fairly close to the 0.2% proof stress obtained by tensile tests at each test temperature. It is thought that ${\sigma}_{cl}$ and ${\sigma}_{cu}$ correspond to the microscopic yield stress and the macroscopic yield stress, respectively. The lower critical stress corresponds to the local yield stress needed for dislocations to move in the soft region within subgrains. The creep strain in the low stress range below 723 K arises mainly from the local deformation of the soft region. The upper critical stress is equivalent to the macroscopic yield stress necessary for dislocations within subgrains or in subboundaries; this stress can extensively move beyond subboundaries under a stress above the critical point to yield a macroscopic deformation. At higher temperatures above 773 K, the influence of the diffusional creep increases and the stress exponent of the creep rate decreases.

유구골 체부 관상면 골절의 치료 (Treatment of Hamate Body Coronal Fracture)

  • 이상현;김누리;장재훈;안태영
    • Journal of Trauma and Injury
    • /
    • 제27권3호
    • /
    • pp.57-62
    • /
    • 2014
  • Purpose: A hamate body coronal fracture is well known as a very rare fracture in the carpal bones and is also hard to diagnose in initial stage due to the bone's architecture. We report our experience in treatment of such a fracture, and we present a review of the relevant literatures. Methods: Four patients who experienced hamate body coronal fractures from October 2006 to October 2013 were enrolled in this study. One patient also had an associated Capitate fracture, and two patients had associated dislocations of the $4^{th}$ metacarpal joint. We performed open reduction and mini-screw fixation on the four patients. In addition, a K-wire was fixed for the two patients with dislocations. Results: The average follow-up period was 24.5 months after surgery, and bone union was observed at the $8^{th}$ week after surgery. We confirmed that bone union had been completed for all the patients, and functional tests showed that joint motion was in the normal range without complications. Conclusion: When a patient has consistent pain on the ulnar side of the wrist, a hamate fracture should be suspected. Computer tomography is better than a simple X-ray scan for confirming the diagnosis of a hamate body coronal fracture. An open reduction and mini-screw fixation led to a good result.

Fabrication and Characterization of InGaN/GaN LED structures grown on selectively wet-etched porous GaN template layer

  • Beck, Seol;Cho, Yong-Hoon
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2009년도 제38회 동계학술대회 초록집
    • /
    • pp.124-124
    • /
    • 2010
  • Much interest has been focused on InGaN-based materials and their quantum structures due to their optoelectronics applications such as light emitting diode (LED) and photovoltaic devices, because of its high thermal conductivity, high optical efficiency, and direct wide band gap, in spite of their high density of threading dislocations. Build-in internal field-induced quantum-confined Stark effect in InGaN/GaN quantum well LED structures results in a spatial separation of electrons and holes, which leads to a reduction of radiative recombination rate. Therefore, many growth techniques have been developed by utilizing lateral over-growth mode or by inserting additional layers such as patterned layer and superlattices for reducing threading dislocations and internal fields. In this work, we investigated various characteristics of InGaN multiple quantum wells (MQWs) LED structures grown on selectively wet-etched porous (SWEP) GaN template layer and compared with those grown on non-porous GaN template layer over c-plane sapphire substrates. From the surface morphology measured by atomic force microscope, high resolution X-ray diffraction analysis, low temperature photoluminescence (PL) and PL excitation measurements, good structural and optical properties were observed on both LED structures. However, InGaN MQWs LED structures grown on SWEP GaN template layer show relatively low In composition, thin well width, and blue shift of PL spectra on MQW emission. These results were explained by rough surface of template layer, reduction of residual compressive stress, and less piezoelectric field on MQWs by utilizing SWEP GaN template layer. Better electrical properties were also observed for InGaN MQWs on SWEP GaN template layer, specially at reverse operating condition for I-V measurements.

  • PDF

Precise EPD Measurement of Single Crystal Sapphire Wafer

  • Lee, Yumin;Kim, Youngheon;Kim, Chang Soo
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제45회 하계 정기학술대회 초록집
    • /
    • pp.223.1-223.1
    • /
    • 2013
  • Since sapphire single crystal is one of the materials that have excellent mechanical and optical properties, the single crystal is widely used in various fields, and the demand for the use of substrate of LED devices is increasing rapidly. However, crystal defects such as dislocations and stacking faults worsen the properties of the single crystal intensely. When sapphire wafer of single crystal is used as LED substrate, especially, crystal defects have a strong influence on the characteristics of a film deposited on the wafer. In such a case quantitative assessment of the defects is essential, and the evaluation technique is now becoming one of the most important factors in commercialization of sapphire wafer. Wet etching is comparatively easy and accurate method to estimate dislocation density of single crystal because etching reaction primarily takes place where dislocations reached crystal surface which are chemically weak points, and produces etch pit. In the present study, the formation behavior of etch pits and etching time dependence were studied systematically. Etch pit density(EPD) analysis using optical microscope was also conducted and measurement uncertainty of EPD was studied to confirm the reliability of the results. EPDs and measurement uncertainties for 4 inch sapphire wafers were analyzed in terms of 5 and 21 points EPD readings. EPDs and measurement uncertainties in terms of 5 points readings for 4 inch wafers were compared by 2 organizations. We found that the average EPD value in terms of 5 points readings for a 4 inch sapphire wafer may represent the EPD value of the wafer.

  • PDF

Dynamic response and waterproof property of tunnel segmental lining subjected to earthquake action

  • Yan, Qixiang;Bao, Rui;Chen, Hang;Li, Binjia;Chen, Wenyu;Dai, Yongwen;Zhou, Hongyuan
    • Earthquakes and Structures
    • /
    • 제17권4호
    • /
    • pp.411-424
    • /
    • 2019
  • In this study, a numerical model of a shield tunnel with an assembled segmental lining was built. The seismic response of the segmental lining of the section of the shield tunnel in Line 1 of the Chengdu Metro is analyzed as it passes through the interface of sand-cobble and mudstone layers. To do so, the node-stress seismic-motion input method was used to input the seismic motion measured during the 2008 Wenchuan earthquake, and the joint openings and dislocations associated with the earthquake action were obtained. With reference to the Ethylene-Propylene-Diene Monomer (EPDM) sealing gaskets used in the shield tunnels in the Chengdu Metro, numerical simulation was applied to analyze the contact pressure along the seepage paths and the waterproof property under different joint openings and dislocations. A laboratory test on the elastic sealing gasket was also conducted to study its waterproof property. The test results accord well with the numerical results and the occurrence of water seepage in the section of the shield tunnel in Line 1 of the Chengdu Metro during the 2008 Wenchuan earthquake was verified. These research results demonstrate the deformation of segmental joint under earthquake, also demonstrate the relationship between segmental joint deformation and waterproof property.

β-type Ti-14Mo-3Nb-3Al-0.2Si 합금의 열처리 조건에 따른 기계적 특성 (Effect of Heat Treatment on the Mechanical Properties of a Ti-15Mo-3Nb-3Al-0.2Si Alloy)

  • 김태호;이준희;홍순익
    • 대한금속재료학회지
    • /
    • 제49권2호
    • /
    • pp.121-127
    • /
    • 2011
  • The mechanical properties of the various heat treatment conditions on Ti-15Mo-3Nb-3Al-0.2Si alloy plates were examined. XRD patterns from the surface of Ti-15Mo-3Nb-3Al-0.2Si were analyzed as a solution-treated Ti alloy has the single-phase ${\beta}$ structure whereas the aged Ti alloys have the ${\beta}$ matrix embedded with ${\alpha}$ needles. High strength (~1500 MPa) with decent ductility (7%) was obtained by the Ti alloy double aged at $300^{\circ}C$ and $520^{\circ}C$ for 8 hours each. The double-aged alloy exhibits the finer structure than the single-aged alloy at $300^{\circ}C$ for 8 hours because of the higher nucleation rate of ${\alpha}$ needles at an initial low aging temperature ($320^{\circ}C$). TEM observation revealed that the fine nanostructure with ${\alpha}$ needles in the ${\beta}$ matrix ensured the excellent mechanical properties in the double aged Ti-15Mo-3Nb-3Al-0.2Si alloy. In the solution treated alloy, the yield drop, stress-serrations and the ductility minimum typically associated with dynamic strain aging can be attributed to the dynamic interaction between dislocations and oxygen atoms. The yield drop and the stress serration were not observed in aged samples because the geometrically introduced dislocations due to phase precipitates suppressed the dynamic strain aging.

직각 쐐기와 응착접촉 하는 반무한 평판 내 전위: 제1부 - 보정 함수 유도 (Dislocation in Semi-infinite Half Plane Subject to Adhesive Complete Contact with Square Wedge: Part I - Derivation of Corrective Functions)

  • 김형규
    • Tribology and Lubricants
    • /
    • 제38권3호
    • /
    • pp.73-83
    • /
    • 2022
  • This paper is concerned with an analysis of a surface edge crack emanated from a sharp contact edge. For a geometrical model, a square wedge is in contact with a half plane whose materials are identical, and a surface perpendicular crack initiated from the contact edge exists in the half plane. To analyze this crack problem, it is necessary to evaluate the stress field on the crack line which are induced by the contact tractions and pseudo-dislocations that simulate the crack, using the Bueckner principle. In this Part I, the stress filed in the half plane due to the contact is re-summarized using an asymptotic analysis method, which has been published before by the author. Further focus is given to the stress field in the half plane due to a pseudo-edge dislocation, which will provide a stress solution due to a crack (i.e. a continuous distribution of edge dislocations) later, using the Burgers vector. Essential result of the present work is the corrective functions which modify the stress field of an infinite domain to apply for the present one which has free surfaces, and thus the infiniteness is no longer preserved. Numerical methods and coordinate normalization are used, which was developed for an edge crack problem, using the Gauss-Jacobi integration formula. The convergence of the corrective functions are investigated here. Features of the corrective functions and their application to a crack problem will be given in Part II.

압력용기용 SA372강의 수소취성 저항성에 미치는 시편 형태의 영향 (Influence of Specimen Geometry and Notch on Hydrogen Embrittlement Resistance of SA372 Steel for Pressure Vessel)

  • 신희창;김상규;김재윤;황병철
    • 한국재료학회지
    • /
    • 제33권7호
    • /
    • pp.302-308
    • /
    • 2023
  • The influence of specimen geometry and notch on the hydrogen embrittlement of an SA372 steel for pressure vessels was investigated in this study. A slow strain-rate tensile (SSRT) test after the electrochemical hydrogen charging method was conducted on four types of tensile specimens with different directions, shapes (plate, round), and notches. The plate-type specimen showed a significant decrease in hydrogen embrittlement resistance owing to its large surface-to-volume ratio, compared to the round-type specimen. It is well established that most of the hydrogen distributes over the specimen surface when it is electrochemically charged. For the round-type specimens, the notched specimen showed increased hydrogen susceptibility compared with the unnotched one. A notch causes stress concentration and thus generates lots of dislocations in the locally deformed regions during the SSRT test. The solute hydrogen weakens the interactions between these dislocations by promoting the shielding effect of stress fields, which is called hydrogen-enhanced localized plasticity mechanisms. These results provide crucial insights into the relationship between specimen geometry and hydrogen embrittlement resistance.

Dislocation after Revision Total Hip Arthroplasty: A Comparison between Dual Mobility and Conventional Total Hip Arthroplasty

  • Hyun Sik Shin;Dong-Hong, Kim;Hyung Seok Kim;Hyung Seob Ahn;Yeesuk Kim
    • Hip & pelvis
    • /
    • 제35권4호
    • /
    • pp.233-237
    • /
    • 2023
  • Purpose: The objective of this study was to analyze the results from a cohort of patients who underwent a revision total hip arthroplasty (THA) using a dual mobility cup (DMC) implant. Materials and Methods: A retrospective review of revised THAs was conducted using the database from a single tertiary referral hospital. A total of 91 revision THAs from 91 patients were included in the study. There were 46 male hips and 45 female hips. The mean age was 56.3±14.6 years, and the mean follow-up period was 6.4±5.9 years. In performance of revision THAs, the DMC implants were used in 18 hips (19.8%), and the conventional implants were used in 73 hips (80.2%). Results: During the follow-up period, three dislocations were identified, and the overall dislocation rate was 3.3%. Early dislocation (at one month postoperatively) occurred in one patient, while late dislocation (at a mean of 7.5 years) occurred in two patients. There was no occurrence of dislocation in the DMC group (0%), and three dislocations were detected in the conventional group (4.1%). However, no significant difference in the rate of dislocation was observed between the two groups (P=0.891). Conclusion: Although the rate of dislocation was higher in the conventional group, there were no statistically significant differences between the two groups due to the small number of patients. Nevertheless, we believe that the dual mobility design is advantageous in terms of reducing dislocation rate and can be recommended as an option for a revision THA.