Influence of Dislocation Substructure on Ultrasonic Velocity under Tensile Deformation

  • Kim, C.S.;Lissenden, Cliff J.;Kang, Kae-Myhung;Park, Ik-Keun
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.28 no.6
    • /
    • pp.477-482
    • /
    • 2008
  • The influence of dislocation substructure of metallic materials on ultrasonic velocity has been experimentally investigated. The test materials of pure Cu, brass (Cu-35Zn), 2.25Cr-1Mo steel, and AISI 316 with different stacking fault energy (SFE) are plastically deformed in order to generate dislocation substructures. The longitudinal wave velocit $(C_L)$ decreases as a function of tensile strain in each material. The $C_L$ of Cu-35Zn and AISI 316 decreases monotonously with tensile strain, but $C_L$ of Cu and 2.25Cr-1Mo steel shows plateau phenomena due to the stable dislocation substructure. The variation of ultrasonic velocity with the extent of dislocation damping and dislocation substructures is discussed.

Effect of Thermo-Mechanical Treatment on the Damping Capacity of Alloy with Deformation Induced Martensite Transformation (가공유기 마르텐사이트 변태를 갖는 합금의 감쇠능에 미치는 가공열처리의 영향)

  • Han, Hyun-Sung;Kang, Chang-Yong
    • Korean Journal of Materials Research
    • /
    • v.29 no.3
    • /
    • pp.160-166
    • /
    • 2019
  • This study investigates the effect of thermo-mechanical treatment on the damping capacity of the Fe-20Mn-12Cr-3Ni-3Si alloy with deformation induced martensite transformation. Dislocation, ${\alpha}^{\prime}$ and ${\varepsilon}-martensite$ are formed, and the grain size is refined by deformation and thermo-mechanical treatment. With an increasing number cycles in the thermo-mechanical treatment, the volume fraction of ${\varepsilon}-martensite$ increases and then decreases, whereas dislocation and ${\alpha}^{\prime}-martensite$ increases, and the grain size is refined. In thermo-mechanical treated specimens with five cycles, more than 10 % of the volume fraction of ${\varepsilon}-martensite$ and less than 3 % of the volume fraction of ${\alpha}^{\prime}-martensite$ are attained. Damping capacity decreases by thermo-mechanical treatment and with an increasing number of cycles of thermo-mechanical treatment, and this result shows an opposite tendency for general metal with deformation induced martensite transformation. The damping capacity of the thermo-mechanical treated damping alloy with deformation induced martensite transformation greatly affect the formation of dislocation, grain refining and ${\alpha}^{\prime}-martensite$ and then ${\varepsilon}-martensite$ formation by thermo-mechanical treatment.

Transient analysis of two dissimilar FGM layers with multiple interface cracks

  • Fallahnejad, Mehrdad;Bagheri, Rasul;Noroozi, Masoud
    • Structural Engineering and Mechanics
    • /
    • v.67 no.3
    • /
    • pp.277-281
    • /
    • 2018
  • The analytical solution of two functionally graded layers with Volterra type screw dislocation is investigated under anti-plane shear impact loading. The energy dissipation of FGM layers is modeled by viscous damping and the properties of the materials are assumed to change exponentially along the thickness of the layers. In this study, the rate of gradual change ofshear moduli, mass density and damping constant are assumed to be same. At first, the stress fields in the interface of the FGM layers are derived by using a single dislocation. Then, by determining a distributed dislocation density on the crack surface and by using the Fourier and Laplace integral transforms, the problem are reduce to a system ofsingular integral equations with simple Cauchy kernel. The dynamic stress intensity factors are determined by numerical Laplace inversion and the distributed dislocation technique. Finally, various examples are provided to investigate the effects of the geometrical parameters, material properties, viscous damping and cracks configuration on the dynamic fracture behavior of the interacting cracks.

Comparison of Damping Capacities in Mg-Al and Mg-Zn Solid Solutions (Mg-Al 및 Mg-Zn 고용체의 진동감쇠능 비교)

  • Joong-Hwan Jun
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.36 no.6
    • /
    • pp.389-395
    • /
    • 2023
  • Damping capacities of Mg-2.5%Al and Mg-2.5%Zn (in atomic) solid solutions were comparatively investigated in order to clarify the influence of solutionized Al and Zn elements on the damping characteristics of Mg. In this study, solid solutions with similar grain size were obtained by solution treatment at 678 K for different times (24 h for Mg-2.5%Al and 36 h for Mg-2.5%Zn), followed by water quenching at RT. The Mg-2.5%Al and Mg-2.5%Zn solid solutions showed similar damping capacities in the strain-amplitude independent region of 1 × 10-6 ~ 1 × 10-5 and in the strain-amplitude dependent region below 6 × 10-4, over which the Mg-2.5%Zn solid solution possessed better damping capacity than the Mg-2.5%Al solid solution. The damping tendencies depending on strain-amplitude for the two solid solutions were analyzed and discussed in terms of similar length between weak pinning points (solutes) and different solute/dislocation interaction forces in Granato-Lücke model.

Ultrasonic linear and nonlinear properties of fatigued aluminium 6061-T6 with voids (기공을 포함한 피로손상 알루미늄 6061-T6의 초음파 특성평가)

  • Kang, To;Song, Sung-Jin;Na, Jeong K.;Park, Jin-Ho
    • Journal of the Korean Institute of Gas
    • /
    • v.19 no.5
    • /
    • pp.41-46
    • /
    • 2015
  • It is known that in aluminum 6061-T6, which is composed of $Mg_2Si$ and ${\beta}-Al_5FeSi$, void nucleation grows around ${\beta}-Al_5FeSi$ of Al606-T6. In this work, growth of voids was checked by scanning a 6061-T6 specimen with SEM observation. The effects of dislocation damping, coherency strain and voids on ultrasonic attenuation and nonlinearity parameters were experimentally measured. It was observed that a nonlinearity parameter increases until 75 percent of fatigue life and decreases after that. From the results, the authors inferred that dislocation damping and coherency damping increase nonlinearity parameters and void nucleation decreases them as ultrasonic scattering increases with void. The application of nonlinearity parameters in estimating degradation of materials with complex microstructures through fatigue process, therefore, should be carefully considered.

Effect of Thermo-mechanical Treatment on the Tensile Properties of Fe-20Mn-12Cr-3Ni-3Si Damping Alloy (Fe-20Mn-12Cr-3Ni-3Si 합금의 인장성질에 미치는 가공열처리의 영향)

  • Han, H.S.;Kang, C.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.32 no.2
    • /
    • pp.61-67
    • /
    • 2019
  • This study was carried out to investigate the effect of thermo-mechanical treatment on the tensile properties of Fe-20Mn-12Cr-3Ni-3Si alloy with deformation induced martensite transformation. ${\alpha}^{\prime}$ and ${\varepsilon}$-martensite, dislocation, stacking fault were formed, and grain size was refined by thermo-mechanical treatment. With the increasing cycle number of thermo-mechanical treatment, volume fraction of ${\varepsilon}$ and ${\alpha}^{\prime}$-martensite, dislocation, stacking fault were increased, and grain size decreased. In 5-cycle number thermo-mechanical treated specimens, more than 10% of the volume fraction of ${\varepsilon}$-martensite and less than 3% of the volume fraction of ${\alpha}^{\prime}$-martensite were attained. Tensile strength was increased and elongation was decreased with the increasing cycle number of thermo-mechanical treatment. Tensile properties of thermo-mechanical treated alloy with deformation induced martensite transformation was affected to formation of martensite by thermo-mechanical treatment, but was large affected to increasing of dislocation and grain refining.

Dependence of Damping Capacity on ${\beta}$ Phase Precipitation in Mg Alloy (Mg 합금에서 진동감쇠능의 ${\beta}$상 석출 의존성)

  • Jun, Joong-Hwan
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.20 no.6
    • /
    • pp.306-310
    • /
    • 2007
  • Changes in microstructure and damping capacity with aging time for solutionized Mg-Al alloy have been investigated. Discontinuous ${\beta}\;(Mg_{17}Al_{12})$ precipitates form along the primary grain boundaries, the amount of which increases as the aging time increases. The hardness of the matrix with respect to aging time shows a typical "S" shape, indicating a generation of fine continuous precipitates in the matrix during the aging. The peak level of damping capacity is obtained after 1 hour of aging, over which the damping capacity becomes deteriorated continuously. The formation of optimum density of continuous ${\beta}$ precipitates with fine morphology which would act as pinning points for dislocation lines, might be responsible for the improvement of damping capacity.

Effect of Cooling Rate on Damping Capacity of Magnesium (마그네슘의 진동감쇠능에 미치는 냉각 속도의 영향)

  • Jun, Joong-Hwan
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.30 no.6
    • /
    • pp.258-263
    • /
    • 2017
  • The effect of cooling rate on the damping capacity of pure Mg was studied. Two Mg samples with different cooling rates were prepared by heat treatment at 873 K for 24 h, followed by water quenching and by furnace cooling to room temperature, respectively. The average grain sizes of the Mg samples were almost identical regardless of the cooling rate, but more twins were observed in the sample with faster cooling rate. The calculated vacancy fraction was higher in the fast cooling sample than the slow cooling one. It is noted that the fast cooling sample exhibited lower damping capacity both in the strain-amplitude independent and strain-amplitude dependent regions. Higher values of vacancy concentration and number density of twins in the fast cooling sample are considered to be responsible for the deteriorated damping capacity in the strain-amplitude independent and strain-amplitude dependent regions, respectively.

Effect of Martensite Morphology on Damping Capacity and Mechanical Property of Fe-Ni-C Alloys (Fe-Ni-C 마르텐사이트 합금에서 마르텐사이트의 형상이 진동감쇠능과 기계적 성질에 미치는 영향)

  • Lee, Young-Kook;Shin, Han-Chul;Choi, Chong-Sool
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.10 no.3
    • /
    • pp.188-197
    • /
    • 1997
  • Effect of martensite morphology on damping capacity and hardness of Fe-Ni-C martensitic alloys were studied. The morphologies of martensite such as lath, butterfly, lenticular and thin plate were prepared by adjusting nickel content and austenite grain size. The hardness increased in order of lath, lenticular, thin plate, butterfly. The damping capacities of the lath and butterfly martensites were higher than those of the other two morphologies, indicating that the dislocation substructure is more effective in the damping capacity than the twin substructure. Especially, the butterfly martensite showed the highest damping capacity among these morphologies because of presence of not tangled but free dislocations in there.

  • PDF

Microscopic damping mechanism of micro-porous metal films

  • Du, Guangyu;Tan, Zhen;Li, Zhuolong;Liu, Kun;Lin, Zeng;Ba, Yaoshuai;Ba, Dechun
    • Current Applied Physics
    • /
    • v.18 no.11
    • /
    • pp.1388-1392
    • /
    • 2018
  • Metal thin films are used widely to solve the vibration problem. However, damping mechanism is still not clear, which limits the further improvement of the damping properties for film and the development of multi-functional damping coating. In this paper, Damping microscopic mechanism of porous metal films was investigated at both macroscopically and microscopically mixed levels. Molecular dynamics simulation method was used to model and simulate the loading-unloading numerical experiment on the micro-pore and vacancy model to get the stress-strain curve and the microstructure diagram of different defects. And damping factor was calculated by the stress-strain curve. The results show that dislocations and new vacancies appear in the micro-pores when metal film is stretched. The energetic consumption from the motion of dislocation is the main reason for the damping properties of materials. Micro-mechanism of damping properties is discussed with the results of in-situ experiment.