• Title/Summary/Keyword: Dieletric Properties

Search Result 13, Processing Time 0.187 seconds

Columbite Precursor법에 의해 제조된 PNN-PZN-PZT계 세라믹의 유전 및 전기적 특성 (Dieletric and Electric properties of PNN-PZN-PZT Ceramic Using Columbite Precursor Method)

  • 이수호;손무헌;사공건
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 C
    • /
    • pp.1028-1030
    • /
    • 1995
  • In the fields of the optics, precise machine, semiconducting processing, the micro-positioning actuators are required for the control of position in the submicron range. In this study, $Pb(Ni_{1/3}Nb_{2/3})O_3-Pb({Zn}_{1/3}Nb_{2/3})O_3-Pb({Zr}_{1/2}Ti_{1/2})O_3$ ceramics were fabricated by solid state reaction. The structural, dielectric and electric properties were investigated for sintering condition. The specimen sintered at $1,150(^\circ}C)$ for 1hr, had the highest density and dielectric contant. The resistivity, dielectric and density were increased with increasing PZN contents.

  • PDF

Polyvinylidene Fluoride를 게이트 전극으로 이용한 MgO bicrystal Josephson junction의 전기 특성 및 마이크로파 특성 연구 (Electrical Characteristics and Microwave Properties of MgO Bicrystal Josephson Junction with Polyvinylidene Fluoride Gate Electrode)

  • 윤용주;김형민;박광서;김진태
    • Progress in Superconductivity
    • /
    • 제3권1호
    • /
    • pp.74-77
    • /
    • 2001
  • We have fabricated a high-Tc superconductive transistor with polyvinylidene fluoride (PVDF) gate electrode on MgO bicrystal Josephson junction by spin-coating method. The PVDF ferroelectric film is found to be suitable fur a gate electrode of the superconductive transistor since it has not only small leakage current but also high dieletric constant at low temperature. For the application of superconducting-FET, we investigated millimeter wave properties (60 GHz band) of the Josephson junction with PVDF gate electrode.

  • PDF

용융염합성법과 화학공침법에 의한 $A_2B_2O_{7}$형 압전세라믹스의 저온소성과 유전특성 (Low Temperature Sintering and Dieletric Properties of $Sr_2Nb_2O_{7}$ Ceramics by the Flux and the Chemical Coprecipitation Methods)

  • 김태규;박인호;남효덕
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1995년도 추계학술대회 논문집
    • /
    • pp.213-216
    • /
    • 1995
  • Strontium niobate, $Sr_2Nb_2O_{7}$ was prepared by the molten stilt synthesis (MSS) and the chemical coprecipitation method (CCP). Single phase $Sr_2Nb_2O_{7}$ was obtained by MSS and CCP at $750^{\circ}C$ and $800^{\circ}C$, respectively. An intermediate phase of composition, $Sr_{5}Nb_4O_{15}$, appeared at $700^{\circ}C$ when CCP method was employed. The resulting powder was observed to have finer particles and more uniform distribution of particle sizes, as compared to those obtained through the conventional method. Such powder characteristics allowed the use of a much lower sintering temperature of $1400^{\circ}C$. Grain-orientation along (0k0) direction, which is advantageous for improving dielectric properties, was also observed. The sintering characteristics and the dielectric properties prepared by MSS and CCP, were better than those by the conventional method.

  • PDF

내장형 capacitor를 위한 LCP와 $BaTiO_3-SrTiO_3$ 복합재의 유전특성 (Dielectric Properties of LCP and $BaTiO_3-SrTiO_3$ Composites for Embedded Matching Capacitors)

  • 김진철;윤상준;윤금희;오준록
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.60-60
    • /
    • 2008
  • We manufactured Liquid Crystal Polymer (LCP) and (1-x)$BaTiO_3-xSrTiO_3$(BST) ceramic composites and investigated dielectric properties to use as embedded capacitor in printed circuit boards and replace LTCC substrates. The dielectric properties of these composites are varied with volume fraction of BST and ratios of BT/ST. Dielectric constants are in the range of 3~28. In addition, we could get low TCC and High Q value that could not achieve in other ceramic-polymer composites. Especially, in composite with x=0.4 and 50vol% BST, the dieletric constant and Q-value are 27 and 300, respectively. And more TCC is -116~145ppm/$^{\circ}C$ in the temperature range of -55~$125^{\circ}C$. We think that this composites can be used high-Q substrate material like LTCC and embedded temperature compensation capacitor in printed circuit boards.

  • PDF

내장형 capacitor를 위한 LCP와 $CaTiO_3-LaAlO_3$ 복합재의 유전특성 (Dielectric Properties of Liquid Crystalline Polymers and $CaTiO_3-LaAlO_3$ Composites for Embedded Matching Capacitors)

  • 김진철;오준록
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.232-233
    • /
    • 2007
  • We manufactured Liquid Crystal Polymer (LCP) and (1-x)CaTiO3-xLaAlO3 (CT-LA) ceramic composites and investigated dielectric properties to use as embedded capacitor in printed circuit boards and replace LTCC substrate. The dielectric properties of these composites are varied with volume fraction of CT-LA and ratios of CT/LA. Dielectric constants are in the range of 3~15. In addition, we could get low TCC and High Q value that could not achieve in other ceramic-polymer composites. Especially, in composite with x=0.01 and 30 vol% CT-LA, the dieletric constant and Q-value are 10 and 200, respectively. And more TCC is $-28{\sim}300ppm/^{\circ}C$ in the temperature range of $-55{\sim}125^{\circ}C$. We think that this composites can be used high-Q substrate material like LTCC and embedded temperature compensation capacitor in printed circuit boards.

  • PDF

흡습이 탄성형 에폭시의 기계적 특성에 미치는 영향 (Study on Mechanical and Water absorbing Property of Elastic Epoxy for Electric Use)

  • 이관우;최용성;박대희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.1
    • /
    • pp.460-463
    • /
    • 2003
  • In this paper, we present the properties of water absorption of elastic epoxy for high voltage. The ratio of water absorption shows linearly increase according to ${\sqrt}t$ till 66 hours. And rigid epoxy is 0.053 [%], elastic epoxy at addictives 35 [phr] is 0.309 and it at addictives 70 [phr] is 0.44 [%]. The reason where absorption of elastic epoxy is high is because of micro void. It can be confirmed by SEM analysis. Dieletric constant increased linearly by addictives' concentration and tans is also increased by addictives' concentration.

  • PDF

L $u_2$ $O_3$ 치환에 따른 Pb(Sb,Mn) $O_3$-Pb(Zr,Ti) $O_3$ 세라믹스의 압전특성 (Piezoelectric properties of Pb(Sb,Mn) $O_3$- Pb(Zr,Ti) $O_3$ Ceramics doped L $u_2$ $O_3$)

  • 이동균;윤석진;;김현재;한득영
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 추계학술대회 논문집
    • /
    • pp.60-63
    • /
    • 1997
  • Dieletric ailed piezoelectric properties of Pb[$Zr_{0.45}$/ $Ti_{0.5-x}$/L $u_{x}$ (M $n_{1}$3//S $b_{2}$3)$_{0.05}$] $O_3$(0$\leq$x $\leq$0.03) were investigated. The partial substitution of $Ti^{4+}$ by a L $u^{3+}$ permitted improvement of the piezoelectric constant( $d_{33}$ ), electromechanical coupling factor ( $k_{p}$ ) and dielectric constant($\varepsilon$$_{33}$ /Sup T/). The dielectric loss(tan $\delta$ ) increased and mechanical quality factor(Qm) decreased with an increase of x were observed. A new piezoelectric material for actuator application was developed at x=0.02 with $d_{33}$ =370$\times$10$^{-2}$ /C/N, $k_{p}$ =58.5%, $\varepsilon$$_{33}$ $^{T}$ =1321, $Q_{m}$ =714 and tan $\delta$ =0.98%.%..%.%.

  • PDF

Pb(Fe$_{1/2}Sb_{1/2})$O$_3$+ Pb(Zr$_{0.52}Ti_{0.48})o_3$ 계 세라믹스의 압전 특성 (Piezoeletric properties of Pb(Fe$_{1/2}Sb_{1/2})$O$_3$+ Pb(Zr$_{0.52}Ti_{0.48})o_3$system ceramics)

  • 양병모;박용욱;윤석진;김현재;박창엽
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 추계학술대회 논문집
    • /
    • pp.54-58
    • /
    • 1996
  • In this paper, the structure, dieletric and piezoelectric properties of Pb(Fe$_{\frac{1}{2}}$/Sb$_{\frac{1}{2}}$$O_3$+ Pb(Zr$_{0.52}$ Ti$_{0.48}$ )O$_3$system ceramics were investigated and the effects of donor Nb$^{+5}$ on these properties were characterized for the application of the actuator. In xPb(Fe$_{\frac{1}{2}}$Sb$_{\frac{1}{2}}$)O$_3$+ (1-x) Pb(Zr$_{0.52}$ Ti$_{0.48}$ )O$_3$system ceramics, tetragonality decreased as x and Nb$_2$O$_{5}$ wt% were increased. In 0.05Pb(Fe$_{\frac{1}{2}}$Sb$_{\frac{1}{2}$}$)O$_3$+ 0.95 Pb(Zr$_{0.52}$ Ti$_{0.48}$ )O$_3$system, grain size was smallest but showed best dielectric and piezoelectric properties. The specimen sintered at 120$0^{\circ}C$ in 0.05pb(Fe$_{\frac{1}{2}}$Sb$_{\frac{1}{2}}$ )O$_3$+ 0.95 Pb(Zr$_{0.52}$ Ti$_{0.48}$ )O$_3$+ Nb$_2$O$_{5}$ 0.6wt% exihibited best piezoeletric properties such as $K^{p}$ =64%, d$_{33}$ =490 [$\times$10$^{-12}$ C/N] and strain was 1320[$\times$10$^{-6}$ Δ$\ell$/$\ell$]at AC 6kV/cm

  • PDF

초음파 처리된 sol로 제조된 PZT 박막의 미세구조 및 전기적 특성 (Microstructure and electrical properties of PZT thin films by sonicated sol in an ultrasonic bath)

  • 김종국;박병옥
    • 한국결정성장학회지
    • /
    • 제9권1호
    • /
    • pp.101-106
    • /
    • 1999
  • Pb$(Zr_{0.5},Ti_{0.5})O_3$ 박막을 $Pt/Ti/SiO_2/Si$ 기판 위에 spin-coating법으로 제조하였다. 제조된 sol을 초음파 bath 내에서 초음파 처리하여 균일화를 촉진시킨 다음, 박막을 제조하여 초음파 처리되지 않은 sol로 제조된 박막과의 비교를 통해 초음파의 영향을 고찰하였다. 초음파 처리된 sol로 제조된 박막의 경우, $550^{\circ}C$에서 perovskite 단일상을 얻을 수 있었고, "rosette" 구조가 사라졌음을 관찰할 수 있엇따. 초음파 처리되지 않은 sol로 제조된 박막의 유전상수(10kHz), 잔류분극(Pr) 및 항전계(Ec) 값은 335, 12.3$\mu$C/$\textrm{cm}^2$, 168.4 kV/cm 였고, 초음파 처리된 sol로 제조된 박막은 각각 443, 172$\mu$C/$\textrm{cm}^2$, 153,5kVcm 로 전기적 특성이 개선되어 졌음을 알 수 있었다.