Microwave Dielectric Properties of $0.6TiTe_3O_8-0.4CaWO_4$ Ceramics with Sintering Temperature (소결온도에 따른 $0.6TiTe_3O_8-0.4CaWO_4$ 세라믹스의 마이크로파 유전특성)

  • Kim, Jae-Sik;Lee, Moon-Kee;Ryu, Ki-Won;Lee, Sung-Gap;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.342-343
    • /
    • 2005
  • In this study,. the microwave dielectric properties of the $0.6TiTe_3O_8-0.4CaWO_4$ ceramics with sintering temperature were investigated for LTCC application. According to the X-ray diffraction patterns, the $0.6TiTe_3O_8-0.4CaWO_4$ ceramics had columbite structure of the $TiTe_3O_8$ phase and scheelite structure of the $CaWO_4$ phase. Increasing the sintering temperature, the bulk density, the dielectric constant and the quality factor of the $0.6TiTe_3O_8-0.4CaWO_4$ ceramics were increased. In the case of the $0.6TiTe_3O_8-0.4CaWO_4$ ceramics sintered at $810^{\circ}C$, the bulk density, the dielectric constant and the quality factor were 5.72$g/cm^2$, 33.6, 22,013GHz respectively.

  • PDF

Dielectric and Piezoelectric Properties of PNN-PZN-PZT Ceramics for Microdisplacement Element Application (미소 변위 소자용 PNN-PZN-PZT 세라믹스와 유전 및 압전특성)

  • 이수호;조현철;박정학;최헌일;사공건
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1996.05a
    • /
    • pp.142-145
    • /
    • 1996
  • In this study, dielectric and piezoelectric properties of 0.5PNN-(0.5-x)PZN-xPZT system ceramics with PZT mole ratio were investigated. As the amount of PZT increases, curie temperature was increased. The maximum of dielectric and piezoelectric constant was shoun at 0.3 mole of PZT amount. As a results, we have found that the structure of ceramics with PZT 0.3 mole was morphotropic phase boundary.

  • PDF

Dielectric and Electrical Properties of Ce,Mn:SBN

  • Kang, Bong-Hoon;Paek, Young-Sop;Rhee, Bum-Ku;Lim, Ki-Soo;Joo, Gi-Tae
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.7
    • /
    • pp.615-619
    • /
    • 2003
  • Temperature and frequency dependence of dielectric and electrical properties was investigated in cerium and manganese doped Sr$\_$0.6/Ba$\_$0.4/Nb$_2$O$\_$6/(60SBN) ceramic system. Structural deformation of 60SBN by dopants did not appeared. 1350$^{\circ}C$-10 h sintered specimen had higher densification than 1250$^{\circ}C$-10 h sintered one, to which dielectric properties are related. That the feature of dielectric maxima peaks was typical Diffusive Phase Transition (DPT), it was explained by "random-field Ising model". Even though 60SBN has large dielectric loss at high frequency above 100 ㎑, it is desirable for optical applications because of low dielectric loss at low frequency. From Arrhenius plot of temperature, the activation energy was calculated to 0.45-0.49 eV.

Dielectric properties with variation of a Composition and Sintering temperature of BSCT ceramics (조성비와 소결온도에 따른 BSCT 세라믹스의 유전특성)

  • Cho, Hyun-Moo;Lee, Sung-Gap;Lim, Sung-Soo;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05c
    • /
    • pp.114-117
    • /
    • 2001
  • $(Ba_{0.6-x}Sr_{0.4}Ca_x)TiO_3$(x=0.10, 0.15, 0.20) ceramics were fabricated by the mixed-oxide method and their structural and dielectric properties were investigated with variation of composition ratio and sintering temperature. As a result of the differential thermal analysis(DTA), exothermic peak was observed at around $1020^{\circ}C$ due to the formation of the polycrystalline perovskite phase. BSCT(50/40/10) specimen sintered at $1500^{\circ}C$ showed the highest average grain size(18.25$[{\mu}m]$). Curie temperature and dielectric constant at room temperature decreased with increasing amount of Ca. BSCT(50/40/10) specimen sintered at $1450^{\circ}C$ showed a good dielectric constant, K, (=4324) and dielectric loss, $tan{\delta}$, (=0.972%) properties at 1[KHz].

  • PDF

Microwave Dielectric Properties of $BaO-TiO_2$ Ceramics ($BaO-TiO_2$계 세라믹스의 마이크로파 유전 특성)

  • Park, In-Gil;Lee, Young-Hie;Kim, Hyun-Jae;Yoon, Seok-Jin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1993.05a
    • /
    • pp.11-14
    • /
    • 1993
  • $BaO-TiO_2$ ceramics ($BaO:TiO_2$=18.2:81.8[mol.%]) were fabricated by mixed-oxide method. Microwave dielectric properties were investigated with sintering temperature and annealing time. Increasing the sintering temperature, the sintered density was decreased. At the sintering temperature of 1400$[^{\circ}C]$, dielectric constant, quality factor and temperature coefficient of resonant frequency had a good values of 35.03, 5690, -4.433$[ppm/^{\circ}C]$, respectively. Increasing the annealing time, dielectric constant and quality factor were increased and temperature coefficient of resonant frequency was decreased.

  • PDF

Dielectric and piezoelectric properties of $Pb(Zr,Ti)O_3$ for Acoustic Emission sensor ceramics (AE센서용 $Pb(Zr,Ti)O_3$ 세라믹의 유전 및 압전 특성)

  • 정영호;김성진;윤현상;홍재일;박창엽
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.625-629
    • /
    • 1999
  • In this study, in order to develop high sensitivity and low noise acoustic emission sensor, we manufactured the Pb(Zr, Ti)O$_3$ ceramics with the addition of WO$_3$ wt% to search for its required characteristics. Dielectric constant was increased as a function of the increase of WO$_3$ wt%. The Pb(Zr, Ti)O$_3$ (EC-65) ceramics added with 0.1lwt% WO$_3$ showed excellent dielectric constant and piezoelectric constants of 1931 and 199.55$\times$10$^{-12}$ (C/N), respectively. Accordingly It was shown as the composition ceramics suitable for AE sensor.

  • PDF

Microwave Dielectric Properties of $Ba(Mg_{1/3}Ta_{2/3})O_3$[BMT] Ceramics with Ca1cining Condition (하소조건에 따른 $Ba(Mg_{1/3}Ta_{2/3})O_3$[BMT] 세라믹스의 마이크로파 유전특성)

  • Hwang, Tae-Kwang;Lim, Sung-Soo;Chung, Jang-Ho;Bae, Seon-Gi;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.04b
    • /
    • pp.84-87
    • /
    • 2000
  • The microwave dielectric properties of complex perovskite-structured $Ba(Mg_{1/3}Ta_{2/3})O_3$ ceramics were investigated with calcining condition. The BMT ceramics were prepared by conventional mixed oxide method. Calcining conditions were $1200^{\circ}C$ for 10hr., $1300^{\circ}C$ for 2hr., and 5hr., respectively. And the specimens were sintered at $1650{\mu}m$. The structural and microwave properties of BMT ceramics were investigated by XRD, SEM and network analyzer. In the case of BMT ceramics calcined at $1300^{\circ}C$ for 5 hr., dielectric constant, quality factor and temperature coefficient of resonant frequency were 20.26, 31,144(at 1GHz), 6.11[ppm/$^{\circ}C$], respectively.

  • PDF

The stuctural and dielectric properties of the $BaTiO_{3}+xNb_{2}O_{5}$ ceramics ($BaTiO_{3}+xNb_{2}O_{5}$ 세라믹스의 구조 및 유전특성)

  • Lee, Sang-Chul;Ryu, Ki-Won;Lee, Sung-Gap;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.426-429
    • /
    • 2001
  • The $BaTiO_{3}+xNb_{2}O_{5}$[x=6, 8, 10wt%] ceramics were prepared by conventional mixed oxide method. The structural properties of the $BaTiO_{3}+xNb_{2}O_{5}$ ceramics with the sintering temperature and addition of $Nb_{2}O_{5}$ were investigated by XRD and SEM. Increasing the sintering temperature, the $2{\Theta}$ value of BT (110) peak was shifted to the lower degree and intensity of the BN (310) peak was increased. Increasing the addition of $Nb_{2}O_{5}$, the intensity of BN (100) peak was decreased and BN (310), (110) peaks were increased. The grain size of the $BaTiO_{3}+xNb_{2}O_{5}$ ceramics sintered at $1350^{\circ}C$ were almost uniform. In the $BaTiO_{3}+xNb_{2}O_{5}$ ceramics sintered at $1350^{\circ}C$, the dielectric constant and dielectric loss were 5424, 0.02 respectively.

  • PDF

Structural and Microwave Dielectric Properties of BMT-BCN Ceramics (BMT-BCN 세라믹스의 구조 및 마이크로파 유전특성)

  • Lee, Mun-Gi;Ryu, Gi-Won;Jeong, Jang-Ho;Lee, Yeong-Hui
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.48 no.4
    • /
    • pp.232-240
    • /
    • 1999
  • In this study, the $(1-\chi)Ba(Mg_{\fraction one-third}Ta_{\fraction two-thirds}O_3-\chiBa(Co_{\fraction one-third}\Nb_{\fraction two-thirds})O_3$ ceramics($\chi$=0.3,0.4,0.5,0.6) were prepared by the conventional mixed oxide method. The ceramics were sintered at the temperature of $1500~1575^{\circ}C$ for5 hours in air. The BMT-BCN ceramics have a complex perovskite structure, and have peaks of (101), (102), (201), (202) and (212). Increasing the sintering temperature, dielectric constant was increased. Temperature coefficients of resonant frequency of the specimens were decreasing with increasing BCN content. In the case of the 0.7BMT-0.3BCN ceramics sintered at $1575^{\circ}C$ for 5 hours, dielectric constant, quality factor and temperature coefficient of resonant frequency for microwave dielectrics application were a good value of 28, 235500 at ㎓ and -$1.2 ppm/^{\circ}C$, respectively.

  • PDF

Sr/Ba Ratio Dependence of Dielectric Characteristics in Strontium Barium NiobateCeramics (Sr/Ba 비에 따른 Strontium Barium Niobate 세라믹스의 유전특성)

  • 김명섭;이준형;김정주;이희영;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.12
    • /
    • pp.1167-1173
    • /
    • 2001
  • The tetragonal tungsten bronze type of Sr$_{x}Ba_{1-x}Nb_{2}O_{6}$(SBN) (0.3$\le$x$\ge$0.7) ceramics was synthesized by the solid state reaction method, and the dielectric properties of SBN ceramics as a function of Sr/Ba ratio were examined. With increasing Sr/Ba ratio in SBN ceramics, the Curie temperature decreased and the maximum dielectric constant at the Curie temperature increased. The relaxor behavior of the SBN ceramics as a function of Sr/Ba ratio was quantitatively evaluated. More relaxor behavior of dielectric characteristics was observed as the ratio of Sr/Ba increased. The experimental results are explained with a viewpoint of crystallography of tungsten bronze structured SBN ceramics.

  • PDF