• 제목/요약/키워드: Dental gold alloy

검색결과 105건 처리시간 0.025초

시판치과주조용 고금합금의 물리적 성질 및 상변태 (Physical Property and Phase Transformation in a Commercial Dental Casting High Gold Alloy)

  • 이희경;박명호;이화식
    • 대한치과기공학회지
    • /
    • 제28권1호
    • /
    • pp.27-41
    • /
    • 2006
  • The physical property and phase transformation in a commercial dental casting high gold alloy was investigated as a function of ageing temperature and time using microvickers hardness tester, X-ray diffraction, optical and electron microscopy and EPMA analyser. 1. With increasing ageing time, the hardness of solution-treated gold alloys increased slowly at the initial stage of ageing treatment at an ageing temperature of $300{\sim}400^{\circ}C$, and it reached a maximum value of hardness at the medium stage. Finally, it decreased gradually during further ageing. The maximum value of hardness at was similar with that of the conventional materials and suitable for using as the crown & bridge. 2. During isothermal ageing at a temperature range of $300{\sim}400^{\circ}C$, three phases consisting of the Au-rich ${\alpha}_1$phase with a face-centered cubic structure, the Pt3Zn ${\alpha}_2$phase with an ordered AuCu3(L12) type(f.c.c.) and the Pt-rich ${\alpha}_3$phase with face-centered cubic structure in solution-treated gold alloys were transformed into different three phases consisting of the ${\alpha}_1$phase, the ${\alpha}_3$phase and the PtZn $\beta$phase with an ordered AuCu I(L10) type. 3. The hardening of gold alloys was attributed to the lattice strains of the matrix resulting from the transformation of the ${\alpha}_2$phase to the $\beta$phase. 4. The softening of gold alloys during over-ageing was attributed to the coarsening of the nodules consisting of the $\beta$phase and ${\alpha}_1$matrix.

  • PDF

Pd-Ag 및 Ni-Cr 합금의 금 전착이 전장 레진의 색채에 미치는 영향 (EFFECT OF GOLD ELECTRODEPOSIT OF PD-AG, NI-CR ALLOYS ON THE COLOR OF VENERRED RESIN)

  • 양홍서;박영준
    • 대한치과보철학회지
    • /
    • 제33권4호
    • /
    • pp.645-661
    • /
    • 1995
  • As the mechanical property of composite resin improved, composite resin has been widely used esthetic dentistry. In the field of esthetic dentistry, the color of prosthetic material is very important. The purpose of this study was to evaluate the color difference of specimens, by the types of alloys and gold electrodeposit. Experimental groups were as follows : Group Prec : Au-Pt alloy with no gold coating and no resin veneer. Group Semi : Pd-Ag alloy with no gold coating and no resin veneer. Group BAse : Ni-Cr alloy with no gold coating and no resin veneer. Group Gsem : Pd-Ag alloy with no gold coating and no resin veneer. Group Gbas : Ni-Cr alloy with no gold coating and no resin veneer. Group PreR : Resin veneer on the Pd-Ag alloy without gold coating. Group SemR : Resin veneer on the Pd-Ag alloy without gold coating. Group GbsR : Resin veneer on the Ni-Cr alloy with gold coating Group BasR : Resin veneer on the Ni-Cr alloy without gold coating. In this study, colors of metal surfaces and veneered resins were evaluated by the CIE $L^{*}a^{*}b$ system. The results obtained were as follows : 1. different alloy types and gold coating make the $L^{*}a^{*}b$ system. 2. The ${\Delta}E^*$ab value between groups semi and Base was less than 1.5 and there was no $a^*$ and $b^*$ value difference between groups Gsem and Gbas 3. The values of $L^*$ and $a^*$ ain groups GsemR and GbasR were so similar that the ${\Delta}E^*$ab value was as small as 0.58. 4. In resin specimens with gold coated semiprecious or base alloys showed yellower and redder deviation than the resin specimens with precious alloy. 5. The ${\Delta}E^*$ab values between goups PreR-GsemR and groups PreR-GbasR were as small as 2.68 and 2.22 respectively.

  • PDF

조임 회전력에 따른 치과 임플랜트 지대나사의 응력에 관한 연구 (STRESS OF DENTAL IMPLANT ABUTMENT SCREW BY THE TIGHTENING TORQUE)

  • 이원주;임주환;조인호
    • 대한치과보철학회지
    • /
    • 제36권5호
    • /
    • pp.721-737
    • /
    • 1998
  • Abutment screw loosening of implant restorations is a common problem in the treatment of dental implant. The purpose of this study was to calculate stress and preload from the elongation measurements and to determine maximum tightening torque without plastic deformation of the screw. The length of each gold alloy UCLA screw was measured after tightening to the manufacturer's recommended torque of 32 N-cm. Similarity, titanium UCLA screws were measured after tightening to the manufacturer's recommended torque of 20 N-cm. Loosening torque was also measured after tightening to 32 N-cm torque for gold alloy abutment screws and 20 N-cm for titanium abutment screws. The results were as follows ; 1. There was a regressive relationship between screw elongation and tightening torque (gold alloy : $r^2=0.987$, titanium : $r^2=0.978$), and the mean preload calculated from elongation measurements was $501.11{\pm}26.85\;N$ (gold alloy) and $399.43{\pm}7.61\;N$ (titanium). 2. Stress calculated for the gold alloy and titanium screws at maximum recommended tightening torque was less than 60% of their respective yield strengths and with-in the elastic range. Maximum tightening torque without plastic deformation was 61 N-cm (gold alloy) and 39 N-cm (titanium). 3. For titanium screws, there was a significant difference between loosening after trial 1 and loosening after trials 2 to 5 (p<0.05). No statistically significant difference was seen in mean loosening torques between the first and subsequent trials for gold alloy screws.

  • PDF

Corrosion of Dental Au-Ag-Cu-Pd Alloys in 0.9 % Sodium Chloride Solution

  • Chiba, Atsushi;Kusayanagi, Yukiharu
    • Corrosion Science and Technology
    • /
    • 제4권1호
    • /
    • pp.19-22
    • /
    • 2005
  • Two Au-Ag-Cu-Pd dental casting alloys (Au:12% and 20%) used. The test solutions used 0.9 % NaCl solution (isotonic sodium chloride solution), 0.9 % NaCl solution containing 1 % lactic acid, and 0.9 % NaCl solution containing 1 % lactic acid and 0.1 mol $dm^{-3}$ $Na_2S$. The surface of two samples in three sample solutions was not natural discoloration during one year. The alloy containing 12 % gold was easily alloyed and the composition was uniform comparing with the alloy containing 20 % gold. The rest potentials have not a little effect after three months. The kinds of metals could not definitely from the oxidation and reduction waves of metal on the cyclic voltammograms. The dissolutions of gold and palladium were 12 % Au sample in the 0.9 % NaCl solution containing 1 % lactic acid and 0.1 mol $dm^{-3}$ $Na_{2}S$. The pH of solution had an affect on dissolution of copper, and sulfur ion had an affect on dissolution of silver. The copper dissolved amount from 20 % gold sample was about 26 times comparing with that of 12 % gold sample in the 0.9 % solution containing 1 % lactic acid. Corrosion products were silver chloride and copper chloride in NaCl solution, and silver sulfide and copper sulfide in NaCl solution containing $Na_{2}S$.

Screw joint stability according to abutment screw materials

  • Jeong Yong-Tae;Chung Chae-Heon;Lee Heung-Tae
    • 대한치과보철학회지
    • /
    • 제39권3호
    • /
    • pp.297-305
    • /
    • 2001
  • Statement of problem. There have been previous studies about instability according to screw material by means of calculating preload in tightening screw or recording of the torque necessary to loosen screw after tightening screw. Purpose. The purpose of this study was to evaluate screw joint stability through the analysis of fitness at the mating thread surfaces between implant and screw after tightening screws made of different materials. Material and methods. In this study, screws were respectively used to secure a cemented abutment to a hexlock implant fixture; teflon coated titanium alloy screw and titanium alloy screw(Steri-Oss), gold-plated gold-palladium alloy screw and titanium alloy screw(Implant Innovation), gold screw and titanium screw(AVANA Dental Implant System). Each abutment screw was secured to the implant with recommended torque value using a digital torque controller. Each screw was again tightened after 10minutes. All samples were cross sectioned with sandpaper and polished. Then samples were evaluated with an scanning electron microscope analysis. Results. In titanium alloy screw, irregular contact and relatively large gap was present at mating thread surface. Also in teflon-coated titanium screw, incomplete seating and only partially contact was present at the mating thread surface. In gold-plated gold-palladium alloy screw, relatively close and tight contact without the presence of large gap was present by existing of gold coating at the mating thread surfaces. In gold alloy screw, relatively small gap between the mating components was seen. Conclusions. This result suggested that gold plated gold-palladium alloy screw and gold alloy screw achieved a greater degree of contact at the mating thread surfaces compared to titanium alloy screw and teflon-coated titanium alloy screw.

  • PDF

치과용 주조 합금의 방전가공에 따른 표면 성분 변화 (Elemental alteration of the surface of dental casting alloys induced by electro discharge machining)

  • 장용철;이명곤
    • 대한치과기공학회지
    • /
    • 제31권1호
    • /
    • pp.55-61
    • /
    • 2009
  • Passive fitting of meso-structure and super-structures is a predominant requirement for the longevity and clinical success of osseointegrated dental implants. However, precision and passive fitting has been unpredictable with conventional methods of casting as well as for corrective techniques. Alternative to conventional techniques, electro discharge machining(EDM) is an advanced method introduced to dental technology to improve the passive fitting of implant prosthesis. In this technique material is removed by melting and vaporization in electric sparks. Regarding the efficacy of EDM, the application of this technique induces severe surface morphological and elemental alterations due to the high temperatures developed during machining, which vary between $10,000{\sim}20,000^{\circ}C$. The aim of this study was to investigate the morphological and elemental alterations induced by EDM process of casting dental gold alloy and non-precious alloy used for the production of implant-supported prosthesis. A conventional clinical dental casting alloys were used for experimental specimens patterns, which were divided in three groups, high fineness gold alloy(Au 75%, HG group), low fineness gold alloy(Au 55%, LG group) and nonprecious metal alloy(Ni-Cr, NP group). The UCLA type plastic abutment patterns were invested with conventional investment material and were cast in a centrifugal casting machine. Castings were sandblasted with $50{\mu}m\;Al_2O_3$. One casting specimen of each group was polished by conventional finishing(HGCON, LGCON, NPCON) and one specimen of each group was subjected to EDM in a system using Cu electrodes, kerosene as dielectric fluid in 10 min for gold alloy and 20 min for Ni-Cr alloy(HGEDM. LGEDM, NOEDM). The surface morphology of all specimens was studied under an energy dispersive X-ray spectrometer (EDS). The quantitative results from EDS analysis are presented on the HGEDM and LGEDM specimens a significant increase in C and Cu concentrations was found after EDM finishing. The different result was documented for C on the NPEDM with a significant uptake of O after EDM finishing, whereas Al, Si showed a significant decrease in their concentrations. EDS analysis showed a serious uptake of C and Cu after the EDM procedure in the alloys studied. The C uptake after the EDM process is a common finding and it is attributed to the decomposition of the dielectric fluid in the plasma column, probably due to the development of extremely high temperatures. The Cu uptake is readily explained from the decomposition of Cu electrodes, something which is also a common finding after the EDM procedure. However, all the aforementioned mechanisms require further research. The clinical implication of these findings is related with the biological and corrosion resistance of surfaces prepared by the EDM process.

  • PDF

골유착성 치과 임플랜트 고정체 직경에 따른 지지골의 응력분포에 관한 삼차원 유한요소 분석적 연구 (A 3-dimensional Finite Element Analysis of Stress Distribution in the Supporting Bone by Diameters of Dental Implant Fixture)

  • 이명곤
    • 대한치과기공학회지
    • /
    • 제26권1호
    • /
    • pp.69-76
    • /
    • 2004
  • The objective of this finite element method study was to analyze the stress distribution induced on a supporting bone by 3.75mm, 4.0mm, 5.0mm diameter of dental implant fixture(13mm length). 3-dimensional finite element models of simplified gold alloy crown(7mm height) and dental implant structures(gold cylinder screw, gold cylinder, abutment screw, abutment, fixture and supporting bone(cortical bone, cancellous bone) designs were subjected to a simulated biting force of 100 N which was forced over occlusal plane of gold alloy crown vertically. Maximum von Mises stresses(MPa) under vertical loading were 9.693(3.75mm diameter of fixture), 8.885(4.0mm diameter of fixture), 6.301(5.0mm diameter of fixture) and the highest von Mises stresses of all models were concentrated in the surrounding crestal cortical bone. The wide diameter implant was the good choice for minimizing cortical bone-fixture interface stress.

  • PDF

각종매몰재와 주조 금속에 따른 주조관의 적합도에 관한 실험적 연구 (Comparing Fitness of Casting Crowns with Various Investments and Casting Metals)

  • 이병기;차성수;김원태
    • 대한치과기공학회지
    • /
    • 제5권1호
    • /
    • pp.13-17
    • /
    • 1983
  • The experimental investication wax performed to study fitness of casting crowns with various investment widely used in Korea. 36 wax patterns were invested and casted according to the regular casting method. The result were as follow : 1. Casting with cristobalite investments of Shofu were seen apart, 0.04mm the tightest space in the linguo and bucco-cervical margin. And the largest deviation, 0.1mm was shown in the central groove 0.1mm was shown in the central groove area of occlusal surface(Jensen Metal) 2. Casting with cristobalite investments of kerr were seen apart, 0.04mm the tightest space in the linguo and bucco-cervical margin And the largest deviation, 0.09 was shown in the central groove area of occlusal surface(Jensen Metal) 3. Casting with Quartz investments of G-C were seen apart, 0.04mm the tightest space in the linguo-cervical margin, And the largest deviation, 0.1mm was shown in the central groove area of occlusal surface(Jensen Metal) 4. Casting with cristobalite investments of shofu were seen apart, 0.01mm the tightest space in the linguo-cervical margin, And the largest deviation, 0.03mm was shown in the central groove of occusal surface(Bo-sung A type gold alloy) 5. Casting with cristobalite investments of kerr showed the best fintness in linguo-cervical margin. And the largest deviation, 0.02mm was shown in the central groove area of occlusal surface(Bosung A type gold alloy) 6. Casting with Quartz investments of G-C were Seen apart, 0.02mm the tightest space in the linguo-cervical margin, And the largest deviation, 0.04mm was shown in the central groove area of occlusal surface(Bo-sung A type gold alloy) 7. Casting with cristobalite investments of shofu were seen apart, 0.01mm the tightest space in the linguo-cervical margin. And the largest deviation, 0.08mm was shown in the buccal cusp area of occlusal surface(Bo-sung B type gold alloy) 8. Casting with cristobalite investments of kerr shown the best fitness in linguo-cervical margin. And the largest deviation, 0.04mm was shown in the central groove atea of occlusal surface(Bosung B type gold alloy) 9. Casting with Quartz investments of G-C were seen apart, 0.03mm the tightest space in the linguo-cervical margin. And the largest deviation, 0.04mm was shown in the central groove area of occlusal surface(Bo-sung B type gold alloy) 10. Casting with cristobalite investments of kerr shown the best fitness and Bo-sung A type gold alloy showed the best fitness.

  • PDF

Effects of silanation time on shear bond strength between a gold alloy surface and metal bracket

  • Jung, Min-Ho;Shon, Won-Jun;Park, Young-Seok;Chung, Shin-Hye
    • 대한치과교정학회지
    • /
    • 제43권3호
    • /
    • pp.127-133
    • /
    • 2013
  • Objective: We aimed to investigate the effects of silanation time on the shear bond strength (SBS) of metal brackets on gold alloy in a silicoating procedure and compare the SBS of metal brackets on gold alloy and enamel. Methods: Type III gold alloy plates were sandblasted with 30-${\mu}m$ silicon dioxide. Excess particles were removed with gentle air after silica coating, and silane was applied. Maxillary central-incisor metal brackets were bonded to each conditioned alloy surface with a light curing resin adhesive for 1 s, 30 s, 60 s, or 120 s after applying silane. The brackets were also bonded to 36 upper central incisors with the same adhesive. All samples were cured for 40 s with a light emitting diode curing light. The SBS was tested after 1 h and after 24 h. The adhesive remnant index (ARI) of the samples was also compared. Results: The 60-s and 120-s silanation time groups showed a higher SBS than the other groups (p < 0.05). Samples tested after 24 h showed a significantly higher SBS than did the samples tested after 1 h (p < 0.05). The 1-s group showed higher ARI scores. The one-way analysis of variance and Student-Newman-Keuls test showed that the SBS values of the 60-s and 120-s silanation time groups were not significantly different from the SBS values of enamel. Conclusions: Adequate silanation time is required to produce sufficient bond strength during silicoating.