Application of Automated Microscopy Equipment for Rock Analog Material Experiments: Static Grain Growth and Simple Shear Deformation Experiments Using Norcamphor (유사물질 실험을 위한 자동화 현미경 실험 기기의 적용과 노캠퍼를 이용한 입자 성장 및 단순 전단 변형 실험의 예)

  • Ha, Changsu;Kim, Sungshil
    • Economic and Environmental Geology
    • /
    • v.54 no.2
    • /
    • pp.233-245
    • /
    • 2021
  • Many studies on the microstructures in rocks have been conducted using experimental methods with various equipment as well as natural rock studies to see the development of microstructures and understand their mechanisms. Grain boundary migration of mineral aggregates in rocks could cause grain growth or grain size changes during metamorphism or deformation as one of the main recrystallization mechanisms. This study suggests improved ways regarding the analog material experiments with reformed equipment to see sequential observations of these grain boundary migration. It can be more efficient than the existing techniques and carry out an appropriate microstructure analysis. This reformed equipment was implemented to enable optical manipulation by mounting polarizing plates capable of rotating operation on a stereoscopic microscope and a deformation rig capable of experimenting with analog materials. The equipment can automatically control the temperature and strain rate of the deformation rig by microcontrollers and programming and can take digital photomicrographs with constant time intervals during the experiment to observe any microstructure changes. The composite images synthesized using images by rotated polarizing plates enable us to see more accurate grain boundaries. As a rock analog material, norcamphor(C7H10O) was used, which has similar birefringence to quartz. Static grain growth and simple shear deformation experiments were performed using the norcamphor to verify the effectiveness of the equipment. The static grain growth experiments showed the characteristics of typical grain growth behavior. The number of grains decreases and the average grain size increases over time. These case experiments also showed a clear difference between the growth curves with three temperature conditions. The result of the simple shear deformation experiment under the medium temperature-low strain rate showed no significant change in the average grain size but presented the increased elongation of grain shapes in the direction of about 53° regarding the direction perpendicular to the shearing direction as the shear strain increases over time. These microstructures are interpreted as both the plastic deformation and the internal recovery process in grains are balanced by the deformation under the given experimental conditions. These experiments using the reformed equipment represent the ability to sequentially observe changing the microstructure during experiments as desired in the tests with the analog material during the entire process.

Effects of Temperature and Mechanical Deformation on the Microhardness of Lead free and Composite Solders (무연 복합 솔더의 미소경도에 미치는 기계적 변형과 온도의 영향)

  • Lee Joo Won;Kang Sung K.;Lee Hyuck Mo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.12 no.2 s.35
    • /
    • pp.121-128
    • /
    • 2005
  • Solder joints in microelectronic devices are frequently operated at an elevated temperature in service. They also experience plastic deformation caused by temperature excursion and difference in thermal expansion coefficients. Deformed solders can go through a recovery and recrystallization process at an elevated temperature, which would alter their microstructure and mechanical properties. In this study, to predict the changes in mechanical properties of Pb-free solder joints at high temperatures, the high temperature microhardness of several Pb-free and composite solders was measured as a function of temperature, deformation, and annealing condition. Solder alleys investigated include pure Sn, Sn-0.7Cu, Sn-3.5Ag, Sn-3.8Ag-0.7Cu, Sn-2.8Ag-7.0Cu (composite), and Sn-2.7Ag-4.9Cu-2.9Ni (composite). Numbers are all in wt.$\%$ unless specified otherwise. Solder pellets were cast at two cooling rates (0.4 and $7^{\circ}C$/s). The pellets were compressively deformed by $30\%$ and $50\%$ and annealed at $150^{\circ}C$ for 2 days. The microhardness was measured as a function of indentation temperature from 25 to $130^{\circ}C$. Their microstructure was also evaluated to correlate with the changes in microhardness.

  • PDF

Beach Deformation Caused by Typhoon Chaba in 2016 Along the Manseongri Coast Related Coastal Improvement Project (연안정비사업이 수행된 만성리 해수욕장에서 2016년 태풍 차바에 의한 해빈변화)

  • Park, Il Heum;Park, Wan-Gyu;Jeong, Seung Myong;Kang, Tae-Soon
    • Journal of the Korean Society of Marine Environment & Safety
    • /
    • v.23 no.6
    • /
    • pp.710-718
    • /
    • 2017
  • After Typhoon Chaba (No.18, 2016) collided with Manseongri Beach, a coastal improvement project was carried out since strong external forces such as waves, storm surges and wave-induced currents were observed to cause beach deformation. The shoreline, beach area and beach volume were periodically surveyed. On the basis of this field data, the beach deformation that occurred at Manseongri Beach has been formally described. Over three months after beach nourishment work began, the beaches were gradually stabilized in terms of natural external forces. However, this stabilization was interrupted by Typhoon Chaba. After two months of typhoon weather, the beach returned to a stable state and no changes were observed until one year after the beach recovery work. Just after the typhoon hit, the shoreline receded from the northern side, where no reduction of external forces occurred, while the rear beach area submerged by breakwater advanced. Also, the beach volume decreased by $3,395m^3$ after the typhoon, due to erosion that occurred on the northern beach, with deposition taking place on the southern backshore area. Therefore, it has been concluded that the coastal improvement project undertaken at Manseongri Beach has significantly contributed to conservation in areas of wave-dominant sediment transport.

Cross-sectional Optimization of a Human-Powered Aircraft Main Spar using SQP and Geometrically Exact Beam Model (기하학적 정밀 보 이론 및 SQP 기법에 의한 인간동력항공기 Main Spar 단면 설계 최적화 연구)

  • Kang, Seung-Hoon;Im, Byeong-Uk;Cho, Hae-Seong;Shin, Sang-Joon
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.31 no.4
    • /
    • pp.183-190
    • /
    • 2018
  • This paper presents optimization of the main spar of Human-Powered Aircraft (HPA) wing. Mass minimization was attempted, while considering large torsional deformation of the beam. Sequential Quadratic Programming (SQP) method was adopted as a relevant tool to conduct structural optimization algorithm. An inner diameter and ply thicknesses of the main spar were selected as the design variables. The objective function includes factors such as mass minimization, constant tip bending displacement, and constant tip twist of the beam. For estimation of bending and torsional deformation, the geometrically exact beam model, which is appropriate for large deflection, was adopted. Properties of the cross sectional area which the geometrically exact beam model requires were obtained by Variational Asymptotic Beam Sectional Analysis (VABS), which is a cross sectional analysis program. As a result, maintaining tip bending displacement and tip twist within 1.45%, optimal design that accomplished 7.88% of the mass reduction was acquired. By the stress and strain recovery, structural integrity of the optimal design and validity of the present optimization procedure were authenticated.

Characteristic Evaluation of Impact Absorption Materials for the Development of Fall Impact Protective Pants (낙상 보호 팬츠개발을 위한 충격흡수 소재특성 평가)

  • Park, Jung Hyun;Lee, Jin Suk;Lee, Jeong Ran
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.40 no.3
    • /
    • pp.495-505
    • /
    • 2016
  • This study explores and selects an appropriate material that considers light and soft physical properties as well as activity for impact absorption pads that can be used to develop practical impact protective clothes worn during daily life by the elderly to reduce the impact of falls. Physical properties, impact absorption performance, and compression characteristics were evaluated on 5 types of foam, 2 types of 3D spacer fabric, and 3 types of polymer gel to select a material appropriate for the pad to be inserted into impact protective clothes. The evaluation of the physical properties showed that 3D spacer fabrics had lower density compared to other materials and polymer gels had the highest density. The elongation percentage was higher in foams than 3D spacer fabrics and EPDM foam had the highest elongation percentage. The impact absorption performance of honeycomb polymer gel was better than foams and 3D spacer fabrics. As a result of looking into compression energy and compression characteristics of materials, 'CR foam A' was found to absorb the largest amount of compression energy, 24.1%, among foams and polymer gels. A high energy absorption rate of 50.0% (or above) was indicated by 3D spacer fabrics; however, foams and polymer gels showed a progressive deformation of energy compression / recovery curve with 3D spacer fabrics that showed drastic deformation. Based on characteristics of materials, 'CR foam C' and EPDM with relatively high absorption performance can be used as protective pad materials among foams. Among polymer gels, 2 open-type polymer gels that have relatively low impact protective performance but a relatively lighter weight on human body (compared to closed-type) are considered appropriate protective pad materials.

Cardiovascular beriberi: rare cause of reversible pulmonary hypertension

  • Song, Joon Hyuk;Cheon, Sang Soo;Bae, Myung Hwan;Lee, Jang Hoon;Yang, Dong Heon;Park, Hun Sik;Cho, Yongkeun;Chae, Shung Chull
    • Journal of Yeungnam Medical Science
    • /
    • v.31 no.1
    • /
    • pp.38-42
    • /
    • 2014
  • Cardiovascular beriberi is caused by thiamine deficiency and usually presents as high cardiac output failure associated with predominantly right-sided heart failure and rapid recovery after treatment with thiamine. Because of its rarity in developed countries, the diagnosis can often be delayed and missed. We recently experienced a case of cardiovascular beriberi with pulmonary hypertension which successfully treated with thiamine infusion. A 50-year-old man with chronic heavy alcoholics was refered to our department for dyspnea with mental change. Echocardiography showed marked right ventricular (RV) dilatation and flattening of the interventricular septum with a D-shaped deformation of the left ventricle. Moderate tricuspid valve regurgitation was found and estimated RV systolic pressure was 52 mm Hg. Because of his confused mentality and history of chronic alcohol intake, neurological disorder due to thiamine deficiency was suspected and intravenous thiamine was administered and he continuously received a daily dose of 100 mg of thiamine. Follow up echocardiography showed marked reduction of RV dilatation and improvement of a D-shaped deformation of the left ventricle. He finally diagnosed as cardiovascular beriberi on the basis of dramatic response to intravenous thiamine. Thiamine deficiency can cause reversible pulmonary hypertension, and can still be encountered in the clinical setting. Thus high index of suspicion is critically needed for diagnosis.

Strength Change due to Plastic Deformation in Al 2024 Ultrafine Grained ECAP Metal (ECAP 성형가공한 Al 2024 초미세결정립 재료의 소성변형량에 따른 강도 변화)

  • Choi, Jeong-Woo;Ma, Young-Wha;Yoon, Kee-Bong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.29 no.10 s.241
    • /
    • pp.1407-1415
    • /
    • 2005
  • Strength change of an over-aged A12024 material was studied after being subjected to stages of severe plastic deformation by ECAP (Equal Channel Angular Pressing). Various kinds of strength value were measured using the conventional tensile test, Rockwell and Vickers hardness and the SP (small punch) test Due to limitation of the specimen size, tension test in transverse direction could not be conducted. Hence, SP test was employed for assessing the strength in transverse direction. Based on TEM observation the measured strength characteristics were explained based on the relation between microstructure, dislocation and strength. As the number of ECAP pass increases, the strength of A12024 was also increased. However, considerable change of strength, which is generally predicted, was not observed in this study. For the strength in transverse direction even decrease of the strength was observed after 6 passes of ECAP. It was argued that this decrease was due to dynamic recovery of dislocation density during or after ECAP processes at $150^{\circ}C$. The strength assessment equation proposed by the authors in the previous paper was shown to be very accurate. This argument was supported by comparing the results of conventional tensile test with those of SP test. It was also pointed that the Rockwell har(3ness value seemed to be able to represent the strength in the transverse direction.

A Semi-Implicit Integration for Rate-Dependent Plasticity with Nonlinear Kinematic Hardening (비선형 이동경화를 고려한 점소성 모델의 내연적 적분)

  • Yoon, Sam-Son;Lee, Soon-Bok
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.27 no.9
    • /
    • pp.1562-1570
    • /
    • 2003
  • The prediction of the inelastic behavior of the structure is an essential part of reliability assessment procedure, because most of the failures are induced by the inelastic deformation, such as creep and plastic deformation. During decades, there has been much progress in understanding of the inelastic behavior of the materials and a lot of inelastic constitutive equations have been developed. The complexity of these constitutive equations generally requires a stable and accurate numerical method. The radial return mapping is one of the most robust integration scheme currently used. Nonlinear kinematic hardening model of Armstrong-Fredrick type has recovery term and the direction of kinematic hardening increment is not parallel to that of plastic strain increment. In this case, The conventional radial return mapping method cannot be applied directly. In this investigation, we expanded the radial return mapping method to consider the nonlinear kinematic hardening model and implemented this integration scheme into ABAQUS by means of UMAT subroutine. The solution of the non-linear system of algebraic equations arising from time discretization with the generalized midpoint rule is determined using Newton method and bisection method. Using dynamic yield condition derived from linearization of flow rule, the integration scheme for elastoplastic and viscoplastic constitutive model was unified. Several numerical examples are considered to demonstrate the efficiency and applicability of the present method.

Estimation of Rutting Property of Artificially-Aged Asphalt Mixtures Based on LMS(%) and $S_D$ (LMS(%)와 $S_D$에 의한 노화 아스팔트 혼합물의 소성번형 추정)

  • Jung, Jae-Hun;Park, Tae-Won;Doh, Young-Soo;Kim, Kwang-Woo
    • International Journal of Highway Engineering
    • /
    • v.9 no.3
    • /
    • pp.123-134
    • /
    • 2007
  • This study was carried out for evaluating correlation of aging level and deformation resistance of asphalt mixtures conditioned by artificial aging treatment. The specimens were made of the short-term aged loose asphalt mixture which was kept in a convection oven at $154^{\circ}C$ for 2 hours, and then were artificially aged at $110^{\circ}C$ for 24, 48, 72 and 96 hours for long-term aging. Deformation strength ($S_D$) and large molecular size ratio (LMS(%)) were measured after short-term and each long-term aging treatment to evaluate aging extents of each mixture with aging time using GPC(Gel-permeation chromatograph) test. It is shown that the $S_D$ and LMS(%) were increased with aging time increment, and that LMS(%) quantity and $S_D$ have relatively good correlation each other. This study found that the aged asphalt mixture had better resistance against rutting and it was possible to estimate rutting characteristics of asphalt mixtures by using LMS(%) without a binder recovery.

  • PDF

Analytical Approaches of Surface-Local Deformations for the Measurement of Indentation Hardness (압입경도 측정을 위한 표면변형 분석기법 비교)

  • Lee, Yun-Hee;Kim, Kuk-Hwan;Nahm, Seung-Hoon;Kwon, Dongil
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.7
    • /
    • pp.416-422
    • /
    • 2009
  • Approaches for analyzing indentation hardness are still controversial, although the instrumented indentation technique has been generalized as one powerful method that can record surface deformation behaviors. Material pile-ups around the indenter/surface contact region make the conventional Oliver and Pharr's analysis on the instrumented indentation curve inaccurate. Thus, in order to prove the validity of the hardness analyses, five approaches were applied to the experimental data obtained from fused quartz and (100) monocrystalline tungsten specimens; an elastic recovery analysis on instrumented indentation curves, three indentation work analyses on the unit plastic volume, and a differentiation analysis on remnant indentation morphologies were tried. Five kinds of indentation hardness overlapped on one result plot showed the validity of each analysis. The modified indentation work approach based on a new definition of plastic volume showed consistent results with those from the Oliver-Pharr's and image differentiation methods. In the case of pile-up accompanying deformation, the Oliver-Pharr's and image differentiation methods showed the upper and lower limits of indentation hardness, respectively.