Proceedings of the Korea Concrete Institute Conference
/
2003.11a
/
pp.261-264
/
2003
Cold weather can lead to many problems in mixing, placing, setting time, and curing of concrete that can have harmful effects on its properties and service life. Korean Concrete Institute (KCI) defines cold weather as a period when the average daily air temperature is less $4^{\circ}C$ and recommends to cast concrete with special care such as shielding, heating and so on. The use of high early strength cements may improve the rate of hardening characteristics of concrete in cold weather by making it possible to achieve faster setting time and evolving more hydration heat than ordinary Portland cement. Higher early strength can be achieved using Type III cement especially during the first 7 days. The strength increase property of Type III cement at low temperature was studied. As a conclusion the heat or heat insulation curing period can be reduced to 50~75%. So, it can be used for cold weather concreting to reduce construction cost and extend the construction season.
Ha, Ju-Hyung;Cho, Yun-Gu;Hyun, Tae-Yang;Lim, Chang-Keun;Seo, Tae-Seok
Journal of the Korea Concrete Institute
/
v.25
no.2
/
pp.195-200
/
2013
New thermal crack control system for mass concrete was developed to increase quality and to save construction period and cost. The principle of this system is that the curing water having proper temperature is supplied automatically to the surface of mass concrete member to keep the temperature difference between center and surface of concrete less than generally recommended temperature difference ($20^{\circ}C$). Mock-up test was conducted to investigate the validity of newly developed curing system. As a result, no crack was founded in the specimen using automated curing system developed in this study, while many cracks occurred in another specimen without automated curing system. It was also confirmed that the strength and the durability of the concrete cured by automated curing system were improved.
The aim of this study was to investigate the physical properties of visible light curing Glass Ionomer cement for restorative esthetic filling. The control group was the autopolymerizing GC Fuji II Glass Ionomer cement (2.2: 1 P/L ratio) and the experimental groups were made by following procedure. To induce the polymerization by visible light, the powder of GC Fuji II GI cement and the liquid of Vitrabond for base & liner were mixed in an amalgam capsule with 2.5:1, 3.0:1, 3.5:1 P/L ratio (% wt/wt). After fabrication of specimens, compressive strength, fracture toughness ($K_{IC}$) Scanning Electron Microscope and X-ray Diffraction, water-leachable content, marginal leakage and surface roughness were studied. The results were as follows: 1. Only experimental No. 1 group (visible light curing) showed less compressive strength than control group 1 hour after curing. Strength was increased with aging in all groups, so the compressive strength of light curing groups was no less than that of autopolymerizing group after 3 weeks. 2. Experimental No.3 group (visible light curing) was inferior to No.2 group (visible light curing) in fracture resistance but light curing groups were more resistant to fracture than autopolymerizing group and showed ductile fracture pattern as compared with the brittle fracture pattern of autopolymerizing group. 3. From scanning electron microscopic image, various sized unreacted powder particles, surrounded by silica gel, were embedded in polysalt matrix. Light curing groups showed little crack and more dense unreacted particles than autopolymerizing group. 4. From X-ray diffraction analysis, GC Fuji II Glass Ionomer cement powder and all groups showed glassy appearance but light curing groups seemed to be more intensive in crystaline than autopolymerizing group. S. The most significant dissolution was shown in early setting period in all group. Light curing groups were dissolved less than autopolymerizing group. 6. Marginal leakage was not different significantly in case of cavity margin composed of same tooth structure (ex. only enamel margin, only dentin margin) but much more leakage was shown in dentin/cementum margin than enamel margin. In only case of only enamel margin, light curing groups were superior to autopolymerizing group. 7. All groups showed relatively smooth surface, which irregularity was less than $1{\mu}m$. Light curing groups were smoother than autopolymerizing group.
This study is to estimate the uniaxal compressive strength (UCS) for the weak rocks using needle penetrometer test. The appropriate ratio of the artificial rocks for this test was cement (C):bentonite (B):water (W) = 1.3:0.7:2.3 or 1.5:0.5:2.0. From the relationship between needle penetration resistance (NPR) measured by needle penetrometer test and an estimated UCS, NPR and UCS tended to increase with increasing the curing period. Also from the relationship between the measured NPR and the measured UCS, NPR-UCS was linearly increased with the curing periods of 3-day to 14-day regardless of the ratio, then in the curing periods of 14-day to 28-day it was nearly constant. In conclusion, the overall relationship between NPR and UCS shows a linear relation for the most part, it means that UCS is possible to be estimated from NPR by needle penetrometer test in the case of weak rocks.
Al-Bared, Mohammed A.M.;Harahap, Indra S.H.;Marto, Aminaton;Abad, Seyed Vahid Alavi Nezhad Khalil;Ali, Montasir O.A.
Geomechanics and Engineering
/
v.18
no.4
/
pp.427-437
/
2019
Waste materials are being produced in huge quantities globally, and the usual practice is to dump them into legal or illegal landfills. Recycled tiles (RT) are being used in soil stabilisation which is considered as sustainable solution to reduce the amount of waste and solve the geotechnical problems. Although the stabilisation of soil using RT improved the soil properties, it could not achieve the standard values required for construction. Thus, this study uses 20% RT together with low cement content (2%) to stabilise soft soil. Series of consolidated undrained triaxial compression tests were conducted on untreated and RT-cement treated samples. Each test was performed at 7, 14, and 28 days curing period and 50, 100, and 200 kPa confining pressures. The results revealed an improvement in the undrained shear strength parameters (cohesion and internal frication angle) of treated specimens compared to the untreated ones. The cohesion and friction angle of the treated samples were increased with the increase in curing time and confining pressure. The peak deviator stress of treated samples increases with the increment of either the effective confining pressures or the curing period. Microstructural and chemical tests were performed on both untreated and RT-cement treated samples, which included field emission scanning electron microscopic (FESEM), Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), and energy dispersive X-ray spectrometer (EDX). The results indicated the formation of cementation compounds such as calcium aluminium hydrate (C-A-H) within the treated samples. Consequently, the newly formed compounds were responsible for the improvement observed in the results of the triaxial tests. This research promotes the utilisation of RT to reduce the amount of cement used in soil stabilisation for cleaner planet and sustainable environment.
Raw perlite is a volcanic alumino-silicate and is used as aggregate in the construction industry. The high silica and alumina contained in the raw perlite allows the production of geopolymer mortar with the help of alkaline solutions. In this study, different geopolymer mortars are obtained by mixing ground perlite (GP), sodium hydroxide (NaOH), water and CEN standard sand and the strength and microstructure of these mortars are investigated. Mortar specimens are placed in the oven 24 hours after casting and kept at different temperatures and times, then the specimens are cured under laboratory conditions until the day of strength tests. After curing, unit weight, ultrasound pulse velocity, flexural and compressive strengths are determined. Experimental results indicate that the mechanical properties of the mortars enhance with increasing oven-curing period and temperatures as well as increasing NaOH molarity. In addition, SEM/EDS and XRD analyses are performed on the mortar specimens and the results are interpreted.
Proceedings of the Korea Concrete Institute Conference
/
1996.04a
/
pp.95-100
/
1996
This paper presents the experimental study on hardening process of high-strength and high-flowable concrete. The experiments were performed to investigate any unfavorable construction situations since the actual concrete placement has been scheduled in cold weather period, so that the high quality concrete construction is convinced to be successfully carried out. The tests were conducted using 600nm and 1000nm height of steel tube to simulate the practical concrete filled steel tube columns according to the following variables as: the categories of chemical admixtures, curing temperatures and curing schemes. The test results were analyzed in terms of hardening speed, internal heat of hydration and history of strength gain. This paper emphasizes the importance of curing schemes on durability and the use of hardening accelerators on strength gain.
Proceedings of the Korea Concrete Institute Conference
/
2000.10b
/
pp.1073-1078
/
2000
This study is to investigate the effect of construction element such as the number of CFS ply, curing temperature, splice length and curing periods on the mechanical properties of Carbon Fiber Sheet (CFS). Through the tensile tests of CFS specimens, it can be said that the reduction factor stemmed from the number of CFS ply must be considered in the calculation of the design tensile strength of CFS. Also, the minimum splice length of CFS and curing period in $20^{\circ}C$ to satisfy the standard tension strength of CFS are over 5cm and after 3days, respectively. The measuring error of epoxy resin have no effect to tension strength of CFS until $\pm$20% error.
Park, Sung-Sik;Kim, Ki-Young;Kim, Chang-Woo;Choi, Hyun-Seok
Proceedings of the Korean Geotechical Society Conference
/
2009.09a
/
pp.511-518
/
2009
In this study, by the consideration of in situ curing conditions, cemented sand with cement ratio less than 20% is prepared by air dry condition and then wetted. A series of unconfined compression tests are carried out to evaluate the effect of wetting on the strength of cemented soils. Strength of air dry cured specimen drops to maximum 30% after wetting at the end of curing period when cement ratio is low. However, regardless of cement ratio, strength of repetitively wetted specimens during curing increases as the number of wetting increases. The results of this study can predict the strength variation of cemented sand depending on wetting conditions in the field, which can guarantee the safety of geotechnical structures such as dam.
Kim, Jong;Kim, Jong-Back;Jeon, Chung-Keun;Shin, Dong-An;Oh, Seon-Gyo;Han, Cheon-Goo
Proceedings of the Korean Institute of Building Construction Conference
/
2006.11a
/
pp.29-32
/
2006
Experimental test results of field construction, Cheongju University Educational Liberal Art Building, applying the insulating curing method on slab concrete showed that the quality of concrete in fresh and hardened state satisfied all target values. Temperature history of slab concrete in A and B area secured more than $7.8{\sim}9.2^{\circ}C$ higher than outside atmosphere. After completing certain curing period of time on the surface of the structure, crack occurrence was not found. It is concluded that the preventing vaporization of moisture by the insulating curing method reduces plastic and drying shrinkage as welt as improves durability.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.