Conservation Treatment, Deterioration Assessment and Petrography of the Hongjimun Ogansumun (Five-arched Floodgates) in Seoul (서울 홍지문 오간수문의 암석기재적 분석과 손상도 평가 및 보존처리)

  • Lee, Myeong Seong;Kim, Jiyoung;Lee, Chan Hee;Kim, Yeong Taek;Han, Byoung Il
    • Journal of Conservation Science
    • /
    • v.29 no.1
    • /
    • pp.1-14
    • /
    • 2013
  • The Hongjimun Ogansumun (Five-arched floodgates) is composed mainly of biotite granite, pink feldspar granite and granodiorite that are very similar with granitic rocks around the Seoul. Main damage in the floodgates was gray, yellow and predominantly white discoloration on the surface of stone blocks. All floodgates showed more discoloration in the wall than ceiling, and there were growing stalactite on the ceiling. Scientific analyses determined that the white discoloring substrates were mainly calcite. Therefore, conservation treatment was carried out to remove the substrates by using dry cleaning, high pressure cleaning and chemicals. The floodgates have been restored to good state, but it is still significantly necessary to install drainage on the top of the gates.

Studies on the epoxy resins of stone cultural properties (석조문화재 에폭시수지 개발 시험 연구)

  • Kim, Sa-Dug;Kim, Soon-Kwan;Kim, Chang-Suk;Hong, Jung-Ki;Kang, Dai-Il;Lee, Myong-Hee
    • 보존과학연구
    • /
    • s.20
    • /
    • pp.139-154
    • /
    • 1999
  • We tested to obtain the excellent Epoxy resins on the property of matter. Existing Epoxy resins is tested to regulate the viscosity, color and hardening time etc. Benzen-ring structure of Bisphenol A type (AY 103) is replaced by Hydrogenated B.P.A type. And hardener is replaced by Polyoxyalkylene Amine. So we are developed into the two resins(L-30, L-40).To know if this Epoxy resins was fitted to repairing and restoration of stone cultural properties. Three kinds of Epoxy resins (AY 103, L-30, L-40) are tested on the artificial weathering test, freezing-melting test, exposure test etc. As a result of test, L-30 is less the discoloration than that of other Epoxy resins and was superior to the excellent property of matter.

  • PDF

Quantitative Deterioration Assessment and Microclimatic Analysis of the Gyeongju Seokbinggo (Ice-storing Stone Warehouse), Korea (경주석빙고의 정량적 훼손도 평가와 미기후환경 분석)

  • Kim, Ji-Young;Lee, Chan-Hee;Lee, Myeong-Seong
    • Journal of Conservation Science
    • /
    • v.25 no.1
    • /
    • pp.25-38
    • /
    • 2009
  • The Gyeongju Seokbinggo (Treasure No. 66) is an ice-storing stone warehouse, consisting mainly of alkaligranite which shows milky white color and medium-grained textures with drusy cavities. As results of deterioration assessment, the deterioration rates were determined as crack (12.5%), disjoining (6.7%), breaking-out (25.1%), exfoliation (20.9%), efflorescence (6.5%), brown discoloration (9.8%), darkgray discoloration (2.0%) and biological discoloration (36.5%). Comprehensive physical deterioration rate and discoloration rate were calculated as 43.7% and 68.7%, respectively, that indicates the Seokbinggo has been severely weathered. Indoor relative humidity was above 90% except in winter season. Indoor microclimate was hardly fluctuating although indoor microclimate was dependent on the outdoor climate. The main cause of deterioration was high relative humidity and a long time of wetness due to penetration of rain, underground water and condensation. It was identified that the water brought out biological discoloration, dissolution of minerals, structural movement and efflorescence, and the dust from the ground soil in front of the entrance accelerated brown and dark gray discoloration on the stone surface.

  • PDF

Investigation of Wood Species and Conservation Status of Wooden Seated Amitabha Buddha Triad and Wooden Amitabha Buddha Altarpiece of Yongmunsa Temple, Yecheon, Korea (Treasure)

  • CHOI, Jaewan;PARK, Junghae;KIM, Soochul
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.3
    • /
    • pp.193-217
    • /
    • 2022
  • The Wooden Seated Amitabha Buddha Triad and Altarpiece have not been the subjects of definitive species identification and scientific analysis. In this study, visual investigation, portable X-ray fluorescence (p-XRF), species identification, and lacquer layer observations were carried out to determine the original materials and conservation status. Cracks, exfoliation and discoloration were detected during the visual investigation. The p-XRF data indicated that chrome oxide green, malachite, gold, cadmium red, cinnabar, minium, hematite, lead white, ink stick (Carbon), and copper were used for pigments and the coronet accessory. Tilia spp., Abies spp., and Pinus spp. were identified from both the Buddha Triad and Altarpiece. Finally, lacquer layer analyses of the base layer, lacquer layer, orange pigment layer, and gold leaf layer observed modern synthetic pigments likely used in previous conservation. As the Korean Cultural Heritage Charter and the International Charter for the Conservation and Restoration of Monuments and Sites clearly state that objects of cultural heritage must be conserved using their original materials, future conservation of these objects should utilize the data obtained in this study to employ traditional materials. Furthermore, a deterioration map diagnosis can be applied together with the obtained analysis data to understand the conservation status of and inform an appropriate and authentic conservation treatment for the Buddha Triad and Altarpiece.

Deterioration Mechanism Interpretation and Surface Contaminant Analysis of the Five-Storied Stone Pagoda in Tapriri, Uiseong (의성 탑리리 오층석탑의 표면오염물 분석 및 손상메커니즘 해석)

  • Lee, Mi Hye;Chun, Yu Gun;Lee, Myeong Seong
    • Economic and Environmental Geology
    • /
    • v.46 no.5
    • /
    • pp.445-453
    • /
    • 2013
  • The Uiseong Tapriri Five-Storied Stone Pagoda (National Treasure No. 77) is typical stone cultural heritage in Unified Silla Dynasty, Korea. The pagoda has been occurred black, brown discoloration and microcrack, exfoliation, granularity decomposition with white discoloration because of continuous weathering. As the results of analysis for the contaminants, chemical weatherings are generated that black contaminant by manganese oxide, brown contaminant by iron oxide, white contaminants by gypsum and taranakite. And physical weatherings, such as microcrack, exfoliation, are occurred by salt(gypsum) crystallization. Therefore, these need to remove the contaminants according to the conservation treatment manual, and regular monitoring using P-XRF to preserve long-term the Five-Storied Stone Pagoda at Tapri-ri, Uiseong.

Measurement of Crack Depth and Weathering Degree Using Ultrasonic Velocity and Deterioration Evaluation of the Unhyungung Stone Water Container (운현궁수조의 손상평가와 초음파 속도를 이용한 풍화도 및 균열심도 측정)

  • Chun, Yu-Gun;Lee, Chan-Hee;Jo, Seung-Nam;Jo, Yeong-Hoon;Park, Gi-Jung;Yang, Pil-Seung
    • Journal of Conservation Science
    • /
    • v.24
    • /
    • pp.1-11
    • /
    • 2008
  • The Unhyungung Water Container in the possession of the Seoul Museum of History in Korea is consisted of a calcareous marble developed laminated bedding and numerous argillaceous veinlets. This monument should need to conservation treatment because of black discoloration and seriously numerous cracks. Vertical and horizontal cracks in the monument are developed following stratification and argillaceous veinlets that are relatively low coherence between the rock materials. We have proved that the material inducing discoloration on the surface is carbon which is formed by deposited organic matters. As the result of the ultrasonic measurements, although highly surface weathering degree, the physical properties of the Unhyungung Water Container is confirmed slightly weathered state. The depths of cracks in the monument are calculated at maximum 60mm in some cracks completely penetrating into the wall and at minimum 9mm in the other crack. The cracks, developed following veinlet, are revealed that there penetrate from an outer wall to an inside wall for the monument. And most depths of cracks, developed following stratification, are calculated 20 to 30mm. This result will offer a significant data for conservation of the Unhyungung Water Container.

  • PDF

A Study of Stone Cultural Heritage on Filler Status and Clinical Trials of Conservation Treatment in Cracks - Focusing on the Change in Surface of the Filler by Mixing the Talc - (석조문화재 균열부 보존처리 충전제의 현황과 임상실험 고찰 - 활석을 혼합 한 충전제의 표면변화를 중심으로 -)

  • Lee, Tae Jong;Oh, Hyeon Jung;Kim, Sa Dug;Lee, Jang Jon
    • Journal of Conservation Science
    • /
    • v.30 no.4
    • /
    • pp.383-393
    • /
    • 2014
  • It is used for the epoxy resin, a mixture of various fillers conservation of cracks of the stone cultural heritage. Such as conservation treatment is need to for long-term conservation. However, field research and experiments on the conservation treatment results when included 54 cases of talc filler was confirmed that the damage, such as discoloration and cracks. The field research is talc was used to determine whether the reports and conservator interviews conducted, microscopy, ICP analysis of the samples collected from the field site. Experiments is color difference measurement and Ultrasonic measurement were arried out, and artificial weathering tests to investigate the effect of talc. As a result, lower the property of matter of the samples containing the talc. Therefore, we propose that the selection process is not allowed to use talc as the filler of stone powder filler cracks is conservation treatment.

Inhibitory Activity of Asarum sieboldii against Wood Rot Fungi on Traditional Paper, Hanji (한지에서 셀룰로오스 분해 미생물에 대한 세신 추출물의 저해 활성)

  • Hong, Jin Young;Kim, Young Hee;Jo, Chang Wook;Lee, Jeong Min;Kim, Su Ji;Jeong, So Young
    • Korean Journal of Medicinal Crop Science
    • /
    • v.25 no.5
    • /
    • pp.282-289
    • /
    • 2017
  • Background: To investigate the possibility of using Asarum sieboldii as an environment-friendly fumigant for protecting organic cultural heritages, the inhibitory effect of A. sieboldii extract against wood rot fungi on Hanji was examined. Methods and Results: The physical, optical, and morphological properties of Hanji inoculated with Trametes versicolor and Tyromyces palustris, and exposed to the n-hexane fraction of A. sieboldii extract, were measured. The physical properties were expressed as weight loss, zero-span tensile strength and viscosity and the optical properties were depicted by luminance and chromaticity ($L^*$, $a^*$, and $b^*$). The results showed that, the n-hexane fraction of A. sieboldii extract inhibited the growth of fungi on Hanji, and preserved its condition. At a concentration of 25 mg, the n-hexane fraction of A. sieboldii extract maintained zero-span tensile strength, increased viscosity, and restricted discoloration of Hanji. It also was confirmed that the weight of fungi infested Hanji exposed to the extract did not decrease. Scanning electron microscopic images revealed that the spores and hyphae of T. versicolor and T. palustris were not present on Hanji during treatment with > 25 mg of the n-hexane fraction of A. sieboldii extract. Conclusions: These results indicate that the n-hexane fraction of A. sieboldii extract by virtue of its antifungal effectiveness may help in preserving Korean paper cultural heritages, including Hanji.

Material Characteristics and Quantitative Deterioration Assessment of the Sinwoldong Three-storied Stone Pagoda in Yeongcheon, Korea (영천 신월동삼층석탑의 재질특성과 훼손도 정량평가)

  • Yi, Jeong-Eun;Lee, Chan-Hee;Chae, Seong-Tae;Jung, Young-Dong
    • Journal of Conservation Science
    • /
    • v.26 no.4
    • /
    • pp.349-360
    • /
    • 2010
  • The Yeongsheon Sinwoldong three-storied stone pagoda (Treasure No. 465) composed mainly of drusy alkali-granite. The major rock-forming minerals are biotite, quartz, amphiboles, orthoclase and plagioclase. Yellowish brown and black discoloration are formed at the eight sculpture Buddha of the stylobate. A broken rock fragments in the roof material were repaired using epoxy resin and cement mortar in the past. As a result of the infrared thermography analysis from the pagoda, cracks and exfoliation were not serious. Also, P-XRF analysis showed that concentration of Fe (mean 5,599ppm) and S (mean 3,270ppm) were so high in yellowish discoloration parts. Black discoloration area was detected highly Mn (mean 2,155ppm) concentration around the eight sculpture Buddha of the stylobate. The main reason for these are inorganic contaminants from disengaged rock ingredient and organic contaminants from withered plant body. Degree of physical weathering is relatively high in the southern and northern side. The eastern and western side had similar with weathering condition. The northern and eastern side were serious discoloration and biological weathering relatively. Therefore, we suggest that the pagoda need to do cleaning of biological contaminant and conservation treatment to weakened materials of rock and long term monitoring.