• Title/Summary/Keyword: Cu alloys

Search Result 663, Processing Time 0.023 seconds

Pitting Characteristics and Electrochemical Polarization Behaviors in Al-Cu-Si-Mg-Ag-Zr Alloys with Ageing (Al-Cu-Li-Mg-Ag-Zr합금의 시효에 따른 전기화학적 분극 거동과 공식특성)

  • Min, B.C.;Chung, D.S.;Shon, T.W.;Cho, H.K.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.9 no.2
    • /
    • pp.103-111
    • /
    • 1996
  • In this paper, we studied on both electrochemical polarization behaviors and pitting characteristics of ultra high strength Al-Cu-Li-Mg-Ag-Zr alloys(named C1 and C2) and 2090 alloy according to their treatments in the deaerated 3.5% NaCl, using by the potentiodynamic and the potentiostatic method, SEM micrograph and surface roughness including depth of pitting attack. With the cyclic polarization curves, the hysteresis of the C1 and C2 alloys appeared more remarkably than that of the 2090 alloy, because of precipitation microstructural difference between C1, C2 alloys and 2090 alloy. In the pitting experiments, the correlations between pitting growth and aging conditions were analyzed with the SEM micrograph and measurement of the pit depth.

  • PDF

A Study on the Microstructures and Mechanical Properties of Squeeze Cast High Strength Yellow Brass, Al Bronze and Sn Bronze Alloys (고강도 황동, 알루미늄 청동 및 인청동합금의 용탕단조 조직과 기계적 성질에 관한 연구)

  • Han, Yo-Sub;Lee, Ho-In
    • Journal of Korea Foundry Society
    • /
    • v.19 no.6
    • /
    • pp.484-492
    • /
    • 1999
  • The microstructures and mechanical properties of high strength yellow brass, Al bronze and Sn bronze alloys fabricated by gravity die casting and squeeze casting were investigated. A rapid cooling of casting was enhanced by pressure applied during solidification of Cu alloys, the cooling rate of casting was more great for high strength yellow brass alloy than other Cu alloys. Grain size and phases of the squeeze cast products become refined to 1/2 level compared to gravity die castings. Squeeze cast Al bronze and high strength yellow brass has about 10-20% higher yield and tensile strength and slighter decreased or nearly same elongation, compared to gravity die cast ones. Sn bronze has nearly same strength and hardness, but shows increased in elongation, compared to gravity die cast ones.

  • PDF

Microstructural Evolution and Tensile Properties of Cu-Sn Based Alloys Manufactured by Spray Casting Route (분무주조에 의해 제조된 Cu-Sn계 합금의 미세조직 및 인장성질)

  • Shim, Sang-Hyun;Kang, Hee-Soo;Baik, Kyeong-Ho
    • Journal of Powder Materials
    • /
    • v.17 no.6
    • /
    • pp.477-481
    • /
    • 2010
  • Cu-Sn based alloys were manufactured by gas atomization spray casting route in order to achieve a fine scale microstructure and a high tensile strength. The spray cast Cu-10Sn-2Ni-0.2Si alloy had an equiaxed grain microstructure, with no formation of brittle ${\delta}-Cu_{41}Sn_{11}$ phase. Aging treatment promoted the precipitation of finely distributed particles corresponding to ${\delta}-Ni_2Si$ intermetallic phase throughout the $\alpha$-(CuSn) matrix. The cold-rolled Cu-Sn-Ni-Si alloy had a very high tensile strength of 1200 MPa and an elongation of 5%. Subsequent aging treatment at $450^{\circ}C$ for 1h slightly reduced the tensile strength to 700 MPa and remarkably increased the elongation up to 30%. This result has been explained by coarsening the precipitates due to over aging and reducing the dislocation density due to annealing effects.

Oxidation Behavior of Ti Added Alumina Dispersion Strengthening Copper Alloy (티타늄이 첨가된 알루미나 분산강화 동합금의 산화물 형성 거동)

  • Joh, Hongrae;Han, Seung Zeon;Ahn, Jee Hyuk;Lee, Jehyun;Son, Young Guk;Kim, Kwang Ho
    • Korean Journal of Materials Research
    • /
    • v.25 no.4
    • /
    • pp.202-208
    • /
    • 2015
  • Alumina dispersion strengthening copper(ADSC) alloy has great potential for use in many industrial applications such as contact supports, frictional break parts, electrode materials for lead wires, and spot welding with relatively high strength and good conductivity. In this study, we investigated the oxidation behavior of ADSC alloys. These alloys were fabricated in forms of plate and round type samples by surface oxidation reaction using Cu-0.8Al, Cu-0.4Al-0.4Ti, and Cu-0.6Al-0.4Ti(wt%) alloys. The alloys were oxidized at $980^{\circ}C$ for 1 h, 2 h, and 4 h in ambient atmosphere. The microstructure was observed with an optical microscope(OM) and a scanning electron microscope(SEM) equipped with energy-dispersive X-ray spectroscopy(EDS). Characterization of alumina was carried out using a 200 kV field-emission transmission electron microscope(TEM). As a result, various oxides including Ti were formed in the oxidation layer, in addition to ${\gamma}$-alumina. The thickness of the oxidation layer increased with Ti addition to the Cu-Al alloy and with the oxidation time. The corrected diffusion equation for the plate and round type samples showed different oxidation layer thickness under the same conditions. Diffusion length of the round type specimen had a value higher than that of its plate counterpart because the oxygen concentration per unit area of the round type specimen was higher than that of the plate type specimen at the same diffusion depth.

The B2-B19-B19' Transformation in Ti-(45-x)Ni-5Cu-xMn (at%) (x = 0.5-2.0) Alloys

  • Jeon, Yeong-Min;Kim, Min-Gyun;Kim, Min-Su;Lee, Yong-Hee;Im, Yeon-Min;Nam, Tae-Hyun
    • Transactions on Electrical and Electronic Materials
    • /
    • v.12 no.1
    • /
    • pp.24-27
    • /
    • 2011
  • Effect of substitution of Mn for Ni on transformation behavior, shape memory characteristics and superelasticity of Ti45Ni-5Cu alloy has been investigated by means of electrical resistivity measurements, X-ray diffraction, thermal cycling tests under constant load and tensile tests. The one-stage B2-B19' transformation occurred when Mn content was 0.5 at%, above which the two-stage B2-B19-B19' transformation occurred. A temperature range where the B19 martensite exists was expanded with increasing Mn content because decreasing rate of Ms (60 K / % Mn) was larger than that of Ms' (40 K / % Mn). Ti-(45-x)Ni-5Cu-xMn alloys were deformed in plastic manner with a fracture strain of 60 % ~ 32 % depending on Mn content. Clear superelasticity was found in fully annealed Ti-(45-x)Ni-5Cu-xMn alloys with Mn content more than 1.0 at%, which was ascribe to a solid solution hardening by substitution of Mn for Ni.

The Influence of (Pd+Ag) Additions on the Glass Forming Ability of Zr-Al-Cu-Ni based Alloys (Zr-Al-Cu-Ni계 합금의 비정질형성능에 미치는 Pd과 Ag 복합첨가의 영향)

  • Kim, Mi-Hye;Lee, Byung-Woo;Kim, Sung-Gyu;Bae, Cha-Hurn;Jeong, Hae-Yong
    • Journal of Korea Foundry Society
    • /
    • v.24 no.1
    • /
    • pp.40-44
    • /
    • 2004
  • The influence of Pd and Ag additions on the thermal stability, the glass forming ability (GFA) and mechanical property of $Zr_{55}Al_{10}Cu_{20}Ni_{10}Pb_{(5-x)}Ag_x$ (x = $0{\sim}5at%$) alloys obtained by melt spun and injection casting method have been investigated by using of X-ray diffraction, thermal analysis (DTA, DSC) and micro-Vickers hardness(Hv) testing. The thermal properties of melt-spun $Zr_{55}Al_{10}Cu_{20}Ni_{10}Pb_{(5-x)}Ag_x$ (x = $0{\sim}5at%$) alloys exhibit a supercooled liquid region(${\Delta}T_x$) exceeding 91 K before crystallization. The largest ${\Delta}T_x$ reaches as large as 126 K for the $Zr_{55}Al_{10}Cu_{20}Ni_{10}Pb_5$ alloy. The reduced glass transition temperature, $T_{rg}$ increased with increasing Ag content. The largest $T_{rg}$ is obtained for the $Zr_{55}Al_{10}Cu_{10}Ni_{10}Ag_5$ alloy. The $Zr_{55}Al_{10}Cu_{10}Ni_{10}Ag_5$ bulk amorphous alloy rod with 3 mm in diameter was fabricated by injection casting. Hv increased with increasing Ag content and the largest value was obtained for the $Zr_{55}Al_{10}Cu_{10}Ni_{10}Ag_5$ bulk amorphous alloy.

A STUDY ON THE MICROSTRUCTURES OF THE AMALGAM ALLOYS AND AMALGAMS (치과용 아말감합금 및 아말감의 마세구조에 관한 연구)

  • Yeon, Sang-Heum;Lee, Chung-Sik;Lee, Myung-Jong;Um, Chung-Moon
    • Restorative Dentistry and Endodontics
    • /
    • v.21 no.1
    • /
    • pp.87-105
    • /
    • 1996
  • The purpose of this study is to investigate the characteristics of the compositions and phases of amalgam alloys and amalgams by using EMPA and X-ray diffractometer. Each specimen was made from Caulk Fine Cut Clow copper lathe cut amalgam), Caulk Spherical (low copper spherical amalgam), Tytin (high copper unicorn position amalgam), Dispersally (high copper admixed amalgam) and Valiant (Palladium enriched amalgam). For preparing amalgam alloys, Tytin and Valiant were used as powder forms and the others were used as tablet forms after being polished with polishing machine. For preparing amalgams, each amalgam alloy and Hg were measured, and triturated by mechanical amalgamater according to user's instructions. After triturating, the triturated mass was inserted to cylindrical metal mold and simultaneously adapted by cylindrical condenser with same diameter and condensed by Instron universal testing machine with 80kg pressure & 1mm/min speed. Each specimen was removed from the metal mold and stored at room temperature for a week. The specimen was polished with the same polishing machine for amalgam alloy. For observation of microstructure and analysis of composition of amalgam alloys and amalgams, EMPA was used to get secondary electron images, backscattered images and characteristic X-ray images of Ag, Sn, Cu, Zn, Hg. To analyze compositions of amalgam alloys and amalgams, X-ray diffractometer was used. Amalgam alloys were scanned at the range of 2${\theta}$ of 30-$85^{\circ}$ and the speed of $4^{\circ}$/min with Cuka line and amalgams were scanned at the range of 2${\theta}$ of 28-$44^{\circ}$ and the speed of $4^{\circ}$/min with Cuka line. By comparing obtained d(distance between surfaces) and d of expected phases and atoms in amalgam alloys and amalgams in ASTM card, phases and atoms were identified. The results were as follows, 1. In Caulk Fine Cut amalgam alloy typical ${\gamma}$ phase was shown, and in amalgam, ${\gamma}$, ${\gamma}_1$ and ${\gamma}_2$ phases were observed. 2. In Caulk Spherical amalgam alloy ${\gamma}$, Ag, Cu and $\varepsilon$ phases were shown, and in amalgam ${\gamma}$, ${\gamma}_1$, ${\gamma}_2$ and $\eta$ phases were observed. 3. In Tytin amalgam alloy ${\gamma}$, Cu and $\varepsilon$ phases were shown, and in amalgam ${\gamma}$, ${\gamma}_1$, $\eta$ and $\varepsilon$ phases were observed. 4. In Dispersalloy ${\gamma}$, Ag, Cu and $\varepsilon$ phases were shown, and in amalgam ${\gamma}$, ${\gamma}_1$, $\eta$ and $\varepsilon$ phases were observed. 5. In Valiant alloy ${\gamma}$, Cu and e phases were shown, and in amalgam ${\gamma}$, ${\gamma}_1$, $\eta$ and $\varepsilon$ phases were observed.

  • PDF

The Effect of Au Addition on the Hardening Mechanism in Ag-30wt%Pd-10wt%Cu Alloy (Ag-30wt% Pd-10wt% Cu 3원합금(元合金) 및 Au 첨가합금(添加合金)의 시효경화특성(時效硬化特性))

  • Lee, K.D.;Nam, S.Y.
    • Journal of Technologic Dentistry
    • /
    • v.21 no.1
    • /
    • pp.27-41
    • /
    • 1999
  • The Ag-Pd-Cu alloys containing a small amount of Au is commonly used for dental purposes, because this alloy cheaper than Au-base alloys for clinical use. However, the most important characteristic of this alloy is age-hardenability, which is not exhibited by other Ag-base dental alloys. The specimens used were Ag-30Pd-10Cu ternary alloy and Au addition alloy. These alloys were melted and casted by induction electric furnace and centrifugal casting machine in Ar atmosphere. These specimens were solution treated for 2hr at $800^{\circ}C$ and were then quenched into iced water, and aged at 350-$550^{\circ}C$ Age-hardening characteristic of the small Au-containing Ag-Pd-Cu dental alloys were investigated by means of hardness testing, X-ray diffraction and electron microscope observations, electrical resistance, differential scanning calorimetric, energy dispersed spectra and electron probe microanalysis. Principal results are as follows ; Maximum hardening occured in two co-phases of ${\alpha}_2$ + PdCu In stage II, decomposition of the $\alpha$ solid solution to a PdCu ordered phase($L1_o$ type) and an Ag-rich ${\alpha}_2$ phase occurred and a discontinuous precipitation occurred at the grain boundary. From the electron microscope study, it was concluded that the cause of age-hardening in this alloy is the precipitation of the PdCu redered phase, which has AuCu I type face-centered tetragonal structure. Precipitation procedure was ${\alpha}{\to}{\alpha}_1+PdCu{\to}{\alpha}_2+PdCu$ at Pd/Cu = 3 Pd element of Ag-Pd-Cu alloy is more effective dental alloy on anti-corrosion and is suitable to isothermal ageing at $450^{\circ}C$.

  • PDF

On the Manufacturing Technology of some Koryo Bronze Artifacts (고려 청동기 유물의 제작기법에 관한 연구)

  • Choi, K.J.;Park, J.S.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.17 no.1
    • /
    • pp.2-9
    • /
    • 2004
  • This study has examined the metallurgical microstructures and alloy compositions of 3 bronze artifacts, a vessel, a spoon and a chopstick, manufactured in the Koryo Dynasty. The results show that they were made from Cu-Sn alloys whose Sn content ranges from 22 to 24% by weight. It is of significant importance to find that they were all given special thermo-mechanical treatments during their manufacturing. It has been found that the Koryo bronze workers were well aware of the mechanical properties of ${\alpha}$, ${\beta}$, ${\gamma}$ and ${\delta}$ phases that appear in the Cu-Sn alloys. Knowing how to promote or suppress the formation of each phase, they were able to find proper alloy compositions and temperatures for the high Sn alloys to be successfully forged. The present study will detail the Koryo bronze technology as estimated from the microstructures of the 3 bronze artifacts. The results of the reproduction experiments with Cu-24%Sn will also be presented to explain how the microstructures develop and to estimate the mechanical properties of each phase.