• 제목/요약/키워드: Crack-free AlGaN

검색결과 8건 처리시간 0.026초

Stimulated Emission with 349-nm Wavelength in GaN/AlGaN MQWs by Optical Pumping

  • Kim, Sung-Bock;Bae, Sung-Bum;Ko, Young-Ho;Kim, Dong Churl;Nam, Eun-Soo
    • Applied Science and Convergence Technology
    • /
    • 제26권4호
    • /
    • pp.79-85
    • /
    • 2017
  • The crack-free AlGaN template has been successfully grown by using selective area growth with triangular GaN facet. The triangular GaN stripe structure was obtained by vertical growth rate enhanced mode with low growth temperature of $950^{\circ}C$ and high growth pressure of 500 torr. The lateral growth rate enhanced mode of AlGaN for crack-free and flat surface was also investigated. Low pressure of 30 torr and high V/III ratio of 4400 were favorable for lateral growth of AlGaN. It was confirmed that the $4{\mu}m$ -thick $Al_{0.2}Ga_{0.8}N$ was crack-free over entire 2-inch wafer. The dislocation density of $Al_{0.2}Ga_{0.8}N$ was as low as ${\sim}7.6{\times}10^8/cm^2$ measured by cathodoluminescence. Based on the high quality AlGaN with low dislocation density, the ultraviolet laser diode epitaxy with cladding, waveguide and GaN/AlGaN multiple quantum well (MQW) was grown by metalorganic chemical vapor deposition. The stimulated emission at 349 nm with full width at half maximum of 1.8 nm from the MQW was observed through optical pumping experiment with 193 nm KrF laser. We also have fabricated the deep ridge type ultraviolet laser diode (UV-LD) with $5{\mu}m-wide$ and $700{\mu}m-long$ cavity for electrical properties. The turn on voltage was below 5 V and the resistance was ${\sim}55{\Omega}$ at applied voltage of 10 V. The amplified spontaneous emission spectrum of UV-LD was also observed from pulsed current injection.

Pt/AlGaN Schottky-Type UV Photodetector with 310nm Cutoff Wavelength

  • 김보균;김정규;박성종;이헌복;조헌익;이용현;한윤봉;이정희;함성호
    • 센서학회지
    • /
    • 제12권2호
    • /
    • pp.66-71
    • /
    • 2003
  • Pt/AlGaN Schottky-type UV photodetectors were designed and fabricated. A low-temperature AlGaN interlayer buffer was grown between the AlGaN and GaN film in the diode structure epitaxy to obtain crack-free AlGaN active layers. A comparison was then made of the structural, electrical, and optical characteristics of two different diodes: one with an AlGaN($0.5\;{\mu}m$)/n+-GaN(2 nm) structure (type 1) and the other with an AlGaN($0.5\;{\mu}m$)/AlGaN interlayer($150\;{\AA}$)/n+-GaN($3\;{\mu}m$) structure(type 2). A crack-free AlGaN film was obtained by the insertion of a low-temperature AlGaN interlayer with an aluminum mole fraction of 26% into the $Al_xGa_{1-x}N$ layer. The fabricated Pt/$Al_{0.33}Ga_{0.67}N$ photodetector had a leakage current of 1 nA for the type 1 diode and $0.1\;{\mu}A$ for the type 2 diode at a reverse bias of -5 V. For the photoresponse measurement, the type 2 diode exhibited a cut-off wavelength of 300 nm, prominent responsivity of 0.15 A/W at 280 nm, and UV-visible extinction ratio of $1.5{\times}10^4$. Accordingly, the Pt/$Al_{0.33}Ga_{0.67}N$ Schottky-type ultraviolet photodetector with an AlGaN interlayer exhibited superior electrical and optical characteristics and improved UV detecting properties.

Si(111) 기판을 이용한 crack-free GaN 박막 성장과 PL특성 (A Study of Growth and Properties of GaN films on Si(111) by MOCVD)

  • 김덕규;김호걸;송민종;박춘배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.187-188
    • /
    • 2005
  • The characteristics of GaN epitaxial layers grown on silicon (111) substrates by metalorganic vapor phase epitaxy have been investigated. The only control of AlN thickness was found to decrease the stress sufficiently for avoiding crack formation in an overgrown thick ($2.6{\mu}m$) GaN layer. X-ray diffraction and photoluminescence measurements are used to determine the effect of AlN thickness on the strain in the subsequent GaN layers. Strong band edge photoluminescence of GaN on Si(111) was observed with a full width at half maximum of the bound exciton line as low as 17meV at 13K.

  • PDF

HVPE법에 의해 대구경 GaN 기판 성장 (Growth of Large GaN Substrate with Hydride Vapor Phase Epitaxy)

  • 김정돈;고정은;조철수;김영수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.99-99
    • /
    • 2008
  • 대구경, 고품질 GaN 단결정 기판은 HVPE 방법을 이용하여 제조하였다. 이때 성장 방법은 기판인 $Al_2O_3$ 단결정 기판을 질화처리 하였으며, 이종기판 성장 시 야기되는 격자 불일치와 성장 후 냉각동안에 열팽창 계수의 불일치로 야기되는 휨이나 crack 발생을 제거하기 위하여 step-growth 방법을 사용하였다. 사파이어 위에 성장된 GaN의 기판은 두께가 380um이며, 직경은 3"로 crack 발생은 없었으며, $600^{\circ}C$에서 레이저 분리 방법을 이용하여 사파이어와 분리하였다. 그러나 분리된 기판은 이종기판과의 접촉면에서 고밀도 결함발생으로 인하여 휨이 발생하였으며, 표면을 연마한 후 DCXRD의 FWHM은 107 arcsec, PL을 이용한 결함밀도는 $6.2\times10^6/cm^2$으로 나타났다.

  • PDF

Hybrid MBE Growth of Crack-Free GaN Layers on Si (110) Substrates

  • 박철현;오재응;노영균;이상태;김문덕
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제44회 동계 정기학술대회 초록집
    • /
    • pp.183-184
    • /
    • 2013
  • Two main MBE growth techniques have been used: plasma-assisted MBE (PA-MBE), which utilizes a rf plasma to supply active nitrogen, and ammonia MBE, in which nitrogen is supplied by pyrolysis of NH3 on the sample surface during growth. PA-MBE is typically performed under metal-rich growth conditions, which results in the formation of gallium droplets on the sample surface and a narrow range of conditions for optimal growth. In contrast, high-quality GaN films can be grown by ammonia MBE under an excess nitrogen flux, which in principle should result in improved device uniformity due to the elimination of droplets and wider range of stable growth conditions. A drawback of ammonia MBE, on the other hand, is a serious memory effect of NH3 condensed on the cryo-panels and the vicinity of heaters, which ruins the control of critical growth stages, i.e. the native oxide desorption and the surface reconstruction, and the accurate control of V/III ratio, especially in the initial stage of seed layer growth. In this paper, we demonstrate that the reliable and reproducible growth of GaN on Si (110) substrates is successfully achieved by combining two MBE growth technologies using rf plasma and ammonia and setting a proper growth protocol. Samples were grown in a MBE system equipped with both a nitrogen rf plasma source (SVT) and an ammonia source. The ammonia gas purity was >99.9999% and further purified by using a getter filter. The custom-made injector designed to focus the ammonia flux onto the substrate was used for the gas delivery, while aluminum and gallium were provided via conventional effusion cells. The growth sequence to minimize the residual ammonia and subsequent memory effects is the following: (1) Native oxides are desorbed at $750^{\circ}C$ (Fig. (a) for [$1^-10$] and [001] azimuth) (2) 40 nm thick AlN is first grown using nitrogen rf plasma source at $900^{\circ}C$ nder the optimized condition to maintain the layer by layer growth of AlN buffer layer and slightly Al-rich condition. (Fig. (b)) (3) After switching to ammonia source, GaN growth is initiated with different V/III ratio and temperature conditions. A streaky RHEED pattern with an appearance of a weak ($2{\times}2$) reconstruction characteristic of Ga-polarity is observed all along the growth of subsequent GaN layer under optimized conditions. (Fig. (c)) The structural properties as well as dislocation densities as a function of growth conditions have been investigated using symmetrical and asymmetrical x-ray rocking curves. The electrical characteristics as a function of buffer and GaN layer growth conditions as well as the growth sequence will be also discussed. Figure: (a) RHEED pattern after oxide desorption (b) after 40 nm thick AlN growth using nitrogen rf plasma source and (c) after 600 nm thick GaN growth using ammonia source for (upper) [110] and (lower) [001] azimuth.

  • PDF

A Review of Epitaxial Metal-Nitride Films by Polymer-Assisted Deposition

  • Luo, Hongmei;Wang, Haiyan;Zou, Guifu;Bauer, Eve;Mccleskey, Thomas M.;Burrell, Anthony K.;Jia, Quanxi
    • Transactions on Electrical and Electronic Materials
    • /
    • 제11권2호
    • /
    • pp.54-60
    • /
    • 2010
  • Polymer-assisted deposition is a chemical solution route to high quality thin films. In this process, the polymer controls the viscosity and binds metal ions, resulting in a homogeneous distribution of metal precursors in the solution and the formation of crack-free and uniform films after thermal treatment. We review our recent effort to epitaxially grow metal-nitride thin films, such as hexagonal GaN, cubic TiN, AlN, NbN, and VN, mixed-nitride $Ti_{1-x}Al_xN$, ternary nitrides tetragonal $SrTiN_2$, $BaZrN_2$, and $BaHfN_2$, hexagonal $FeMoN_2$, and nanocomposite TiN-$BaZrN_2$.

Properties and SPICE modeling for a Schottky diode fabricated on the cracked GaN epitaxial layers on (111) silicon

  • 이헌복;백경흠;이명복;이정희;함성호
    • 센서학회지
    • /
    • 제14권2호
    • /
    • pp.96-100
    • /
    • 2005
  • The planar Schottky diodes were fabricated and modeled to probe the device applicability of the cracked GaN epitaxial layer on a (111) silicon substrate. On the unintentionally n-doped GaN grown on silicon, we deposited Ti/Al/Ni/Au as the ohmic metal and Pt as the Schottky metal. The ohmic contact achieved a minimum contact resistivity of $5.51{\times}10.5{\Omega}{\cdot}cm^{2}$ after annealing in an $N_{2}$ ambient at $700^{\circ}C$ for 30 sec. The fabricated Schottky diode exhibited the barrier height of 0.7 eV and the ideality factor was 2.4, which are significantly lower than those parameters of crack free one. But in photoresponse measurement, the diode showed the peak responsivity of 0.097 A/W at 300 nm, the cutoff at 360 nm, and UV/visible rejection ratio of about $10^{2}$. The SPICE(Simulation Program with Integrated Circuit Emphasis) simulation with a proposed model, which was composed with one Pt/GaN diode and three parasitic diodes, showed good agreement with the experiment.