Evaluation Method of Healing Performance of Self-Healing Materials Based on Equivalent Crack Width (등가균열폭에 기반한 자기치유 재료의 치유성능 평가 방법)

  • Lee, Woong-Jong;Kim, Hyung-Suk;Choi, Sung;Park, Byung-Sun;Lee, Kwang-Myong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.3
    • /
    • pp.383-388
    • /
    • 2021
  • In this study, constant head water permeability test was adopted to evaluate self-healing performance of mortars containing inorganic healing materials which consist of blast furnace slag, sodium sulfate and anhydrite. Clinker powder and sand replaced for a part of cement and fine aggregates. On constant head water permeability test for self-healing mortars, unit water flow rate of mortar specimens were measured according to crack width and healing period. As a result of evaluating the healing performance of self-healing mortar, it was confirmed that with the initial crack width of 0.3mm, the healing rate at healing period of 28 days increased by more than 30%p compared to plain mortar, greatly improving the healing performance. Furthermore, the coefficient(α) which was estimated from the relationship between crack width and unit water flow rate was used for calculating equivalent crack width. By analyzing the correlation of healing rate and equivalent crack width, the time and initial crack width attaining healing target crack width were predicted.

The Crack Healing Properties of Cement Mortar Materials Using Crystal Growth Type Self-Healing Solid Capsules According to the Crack Induction Age (균열 유도 재령에 따른 결정성장형 자기치유 고상캡슐 활용 시멘트 모르타르의 균열 치유 특성)

  • Choi, Yun-Wang;Nam, Eun-Joon;Kim, Cheol-Gyu;Oh, Sung-Rok
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.4
    • /
    • pp.475-482
    • /
    • 2020
  • In this study, three levels of solid capsules were prepared according to the composition ratio of core materials for the crystal growth type self-healing solid capsule, and a cement mortar was prepared with the crystal growth type self-healing solid capsule. The prepared solid capsule was mixed with 3% of the cement mass to evaluate the healing properties according to the crack induction age of the cement mortar. As a result of test, the crack healing properties according to the crack induction age of cement mortar mixed of solid capsules, it was confirmed that the self-healing performance of the cement mortar with the solid capsules was increased self-healing performance of 7 days than 28 days. This is because the unhydrated binder remains.

Self-Healing Properties in Cracking of Blast Furnace Slag Cement Paste (고로 슬래그 시멘트 페이스트 균열에서의 자기치유 특성)

  • Lee, Seung-Heun;Kang, Kook-Hee;Lim, Young-Jin;Lee, Se-Jin;Park, Byeong-Seon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.1
    • /
    • pp.29-36
    • /
    • 2019
  • This study investigated the self-healing properties of blast furnace slag cement paste sample with $Na_2SO_4$ as a blast furnace slag activator after conducting the permeability test. Self-healing properties were examined by crack filling ratio and quantification of self-healing products. The degree of self-healing was evaluated by the crack filling ratio, and the crack filling ratio was analyzed by panoramic analysis using BSE-DIP for objectivity. The average crack filling ratio showed a tendency of decreasing from the upper part of the specimen to the lower part as the average of the top part was 18%, the middle part was 7% and the bottom part was 5% on average. The maximum crack filling ratio was 44% and the minimum crack filling ratio was 3%. The residual self-healing product after the permeability test contained a large amount of Ca element and Al element derived from the blast furnace slag, and the Si element was mainly present near the crack surface. The most abundant minerals in self-healing products were about 68% C-A-H. $CaCO_3$ was about 13% and C-A-S-H was about 8%. Three minerals accounted for 90% of self-healing products. C-A-H was mainly present at a part slightly distant from the crack surface and showed an angular or acicular shape. The C-A-S-H was generated on the surface naturally connected to the existing specimen, and the $CaCO_3$ was generally observed on the surface of the specimen or the inside of the crack.

Compressive Strength and Healing Performance of Mortar Using Self-healing Inorganic Materials (자기치유형 무기계 혼합재를 사용한 모르타르의 압축강도 및 치유성능)

  • Hyung-Suk, Kim;Woong-Jong, Lee;Sung, Choi;Kwang-Myong, Lee
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.10 no.4
    • /
    • pp.577-583
    • /
    • 2022
  • In this study, the characteristics of self-healing mortars produced using an inorganic self-healing material consisting of ground granulated blast furnace slag, expansion agent, and anhydrite, were investigated. For three types of self-healing mortars with different amounts of the inorganic healing material, compressive strength was measured and the self-healing performance was evaluated through the constant water head permeability test. The healing rate and equivalent crack width according to crack-induced aging were used as indicies of healing performance evaluation. Considering the development of compressive strength of the self-healing mortars, the change in the healing rate with healing periods, and the economic feasibility, the optimal amount of inorganic self-healing materials was suggested as 20 % of the mass of cement.

Correlation between Crack Width and Water Flow of Cracked Mortar Specimens Measured by Constant Water Head Permeability Test (정수위 투수시험에 의해 측정된 균열 모르타르 시편의 유출수량과 균열폭의 상관관계)

  • Choi, Seul-Woo;Bae, Won-Ho;Lee, Kwang-Myong;Shin, Kyung-Joon
    • Journal of the Korea Concrete Institute
    • /
    • v.29 no.3
    • /
    • pp.267-273
    • /
    • 2017
  • Recently, the researches of self-healing concrete technology are being carried out actively due to the advent of importance for the maintenance of concrete structures. A water permeability test has been widely used for the evaluation of self-healing performance. However, it is difficult to compare tests results since there is no standard test method related to the self-healing. A standard method for measuring the crack width does not exist neither though the self-healing performance is significantly influenced by the initial crack width. In this study, the effect of water head and crack width on water flow was investigated using a constant water head permeability test equipment. The correlation equation between the initial crack width and water flow was suggested through the regression analysis of test data, and the predicted crack widths agree well with the real crack widths measured using microscopy.

Experimental study for self-healing performance of concrete using admixture (자가치유형 구체방수 콘크리트의 자가치유성능에 대한 실험적 연구)

  • Hong, Seok-Beom;Kim, Jin-Keun;Lee, Jong-Yoon;Jeon, Hong-Min
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.441-442
    • /
    • 2009
  • Concrete has some self-healing ability if the crack is occurred. Concrete with a inorganic-organic chemical compound, self-healing ability is increased at the surface of the crack. In this study, we investigate self-healing performance of concrete using admixutre by performing permeability test.

  • PDF

A Study on Crack Self-Healing of Concrete Overlay for Bridge Decks (콘크리트 교면포장의 자기균열치유 특성에 대한 검토 연구)

  • Jeon, Sung IL;Yun, Kyung Ku;An, Ji Hwan;Choi, Pan Gil
    • International Journal of Highway Engineering
    • /
    • v.19 no.1
    • /
    • pp.11-19
    • /
    • 2017
  • PURPOSES : The purpose of this study is to verify the property of self-healing, and to propose an appropriate duration for wet curing of bridge deck concrete overlays. METHODS : In this study, reinforced bars were inserted into concrete molds in order to prevent brittle fracture and induced cracks in the concrete resulting from indirect tension mode. The induced time of concrete cracking was 3 to 7 days, following which the concrete specimens were cured in water. The resulting concrete crack width was measured using image analysis equipment. Additionally, the self-healing tests were performed using the following three mixtures: OPC, SFC, and LMC. RESULTS : Concrete mixtures with crack widths of $150{\mu}m$ or lower were completely healed by Day 28. Hydrates of crack fills were found to be the calcium carbonate. CONCLUSIONS : The cement-based mixtures exhibit properties of self-healing. Considering these properties, it is necessary to increase the curing duration of concrete overlays for bridge decks.

Self-Healing Performance of Concrete Using Admixture (구체방수 콘크리트의 균열 자가치유 성능)

  • Lee, Jong-Yun;Lee, Han-Joo;Lee, Yong-Jin
    • Journal of the Korean Society of Safety
    • /
    • v.27 no.6
    • /
    • pp.109-114
    • /
    • 2012
  • This study is the things to experiment and evaluate the performance of self-healing water-proofing on the concrete to be using the crystal growth composite waterproofing admixture. The cylinder to be making on the concrete by ${\varnothing}150{\times}300$ mm for evaluating the performance of self-healing water-proofing was aging 90 days and cut on a 50 mm. So, it prompted the crack and applied. After it measured the quantity of water to be flow the water throughout the crack part of the cylinder, it applied the basic formular of Darcy's law and calculated the coefficient of water permeability. So, it verified the performance of self-healing water-proofing on the basis of the changing shape of the water permeability. This experiment is the thing to be applied the general evaluation of the structure to demand the real watertightness on doing for the evaluating of performance of the quantity of water leak and self-healing water-proofing about the various penetration crack.

Development of Crack Monitoring System for Self-healing Repair Mortar Surface Using Image Processing Technique (이미지 처리 기법을 이용한 자기치유 보수 모르타르 시공표면의 균열 모니터링 시스템 개발)

  • Oh, Sang-Hyuk;Moon, Dae-Jung;Lee, Kwang-Myong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.3
    • /
    • pp.359-366
    • /
    • 2021
  • In this study, It was developed an monitoring cracks system based on image processing techniques in order to measure cracks, which are major damages in concrete, and to convert them into a database. The crack monitoring system consists of crack image captured equipment and a crack detection and analysis software. This system provides objective and quantitative data by replacing the conventional visual inspection. The crack detection algorithm w as verified through an indoor test using virtual cracks, and the amount of crack detection and crack width change was monitored by applying it to the self-healing repair mortar construction site. In the case of the crack width detected through image analysis, the maximum difference from the actual crack width was 0.0334mm. It was possible to detect microcracks of 0.1mm or less, and the effect of crack healing over time of the self-healing repair mortar was confirmed trough the field test.

Development of Oxygen Diffusion Test Method for Crack Width Evaluation of Self-Healing Concrete (자기치유 콘크리트의 균열치유 성능평가를 위한 개선된 산소확산 시험방법 제안)

  • Lee, Do-Keun;Shin, Kyung-Joon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.3
    • /
    • pp.375-382
    • /
    • 2021
  • Self-healing concrete is in the spotlight in that it can effectively extend the lifespan of concrete structures by healing cracks in the structure by themselves without additional repairing or retrofiting actions. Currently, self-healing concrete is a field that is being actively studied around the world, but since most studies focus on the improvement of healing performance, there is a lack of methods to rationally evaluate the self-healing performance of concrete. Although the gas diffusion test method has been developed for the use in the performance evaluation of self-healing concrete, it has revealed that for gas diffusion through the matrix affect the crack diffusion coefficients depending on the environmental conditions such as the saturation of the specimen, the temperature, and humidity during the experiment. Therefore, in this study, the method has been proposed to eliminate the influence of the matrix diffusion when calculating the crack diffusion coefficient. In addition, a pre-conditioning process was introduced to shorten the experimental time. As a result, the crack width could be estimated with an error level of less than 3% in the test time of about 20 minutes.