취성재의 손상후 잔류강도 평가 (Evaluation of Residual Strength in Damaged Brittle Materials)

  • 오상엽;신형섭;서창민
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 추계학술대회논문집A
    • /
    • pp.137-142
    • /
    • 2001
  • In structural applications, brittle materials such as soda-lime glasses and ceramics are often subjected to multiaxial stress. Brittle materials with crack or damaged by foreign object impacts are abruptly fractured from cracks, because of their properities of very high strength and low fracture toughness. But in most cases, the residual strength has been derived from tests under uniaxial stress such as a 4-point bend test. The strengths under multiaxial stresses might be different from the strength. In comparable tests, the residual strength under biaxial stress state by the ball-on-ring test was greater than that under the uniaxial one by the 4-point bend test. In the case that crack having 90deg. to loading direction, the ratio of biaxial to uniaxial flexure strength was 1.12. At a different crack angle to loading direction when it was evaluated by the 4-point bend test, the residual strength was different and the ratio of 45deg. to 90deg. was 1.16.

  • PDF

Spot 가진을 이용한 평면결함의 음향방출 위치표정 (AE Source Location in Planar Defects using Spot Excitation)

  • 이장규;박성완;우창기
    • 한국공작기계학회논문집
    • /
    • 제13권5호
    • /
    • pp.87-95
    • /
    • 2004
  • From the results of AE(Acoustic Emission) source location occurred by the spot exciting as suggested in this research, it has been confirmed that AE technique is quite fruitful in figuring out the location of the occurrence, form, size and direction of the defects. As the results of examining the distribution of event for the angle of crack $\alpha$ to Xs and Ys, as the increases from $0^{\circ}$ ~ $90^{\circ}$, gradually changes its width from the axis Xs to the axis Ys. So event appears approximately similar in its size at the angle of crack $\alpha$=$45^{\circ}$, yet opposite when $\alpha$ is lager. It is believed that this is a phenomenon where its crack legnth $\alpha$, assumed as a planar defect, is to be prcjected toward the direction with a larger size. Thus, it is expected that the application of the experimental method suggested in this study would make it possible to identify the location of the defect in the material in the nondestructive way.

오스테나이트 분포에 따른 수퍼 2상 스테인리스강의 기계적 특성과 피로균열 진전거동 (Mechanical Characteristics and Fatigue Crack Propagation of Super Duplex Stainless Steel by Distribution of Austenite)

  • 도재윤;이상기;안석환;남기우;강창룡
    • 열처리공학회지
    • /
    • 제14권4호
    • /
    • pp.205-211
    • /
    • 2001
  • The characteristics of super duplex stainless steel were investigated on its fibrous structure and dispersed structure. These structures consist of various volume fractions and distributions of the austenite phase that were obtained by changing the heat treatment temperature and cycle. The fibrous structure had higher austenite volume fraction than dispersed structure on the same temperature. As the austenite volume fraction increased in both structures, tensile strength and elongation increased, but hardness decreased. Fatigue life of fibrous structure parallel to rolling direction was shorter than that of perpendicular to rolling direction. Fatigue life of dispersed structure was longer than parallel fibrous structure, and shorter than perpendicular fibrous structure. Fatigue crack propagation rate of fibrous structure was faster than that of dispersed structure.

  • PDF

탄소섬유보강 플라스틱시트로 외부보강된 RC 슬래브의 p-Version 비선형 유한요소 해석 (p-Version Nonlinear Finite Element Analysis of RC Slabs Strengthened with Externally Bonded CFRP Sheets)

  • 조진구;박진환
    • 한국농공학회논문집
    • /
    • 제48권1호
    • /
    • pp.61-68
    • /
    • 2006
  • The p-version nonlinear finite element model has been developed to analyze the nonlinear behavior of simply supported RC slabs strengthened with carbon fiber reinforced plastic sheets. The shape function is adopted with integral of Legendre polynomials. The compression model of concrete is based on the Kupfer's yield criterion, hardening rule, and crushing condition. The cracking behavior is modeled by a smeared crack model. In this study, the fixed crack approach is adopted as being geometrically fixed in direction once generated. Each steel layer has a uniaxial behavior resisting only the axial force in the bar direction. Identical behavior is assumed fur tension and compression of steel according to the elastic modulus. The carbon fiber reinforced plastic sheets are considered as reinforced layers of equivalent thickness with uniaxial strength and rigidity properties in the present model. It is shown that the proposed model is able to adequately predicte the displacement and ultimate load of nonlinear simply supported RC slabs by a patch with respect to reinforcement ratio, thickness and angles of CFRP sheets.

High-cycle fatigue characteristics of quasi-isotropic CFRP laminates

  • Hosoi, Atsushi;Arao, Yoshihiko;Karasawa, Hirokazu;Kawada, Hiroyuki
    • Advanced Composite Materials
    • /
    • 제16권2호
    • /
    • pp.151-166
    • /
    • 2007
  • High-cycle fatigue characteristics of quasi-isotropic carbon fiber reinforced plastic (CFRP) laminates [-45/0/45/90]s up to $10^8$ cycles were investigated. To assess the fatigue behavior in the high-cycle region, fatigue tests were conducted at a frequency of 100 Hz, since it is difficult to investigate the fatigue characteristics in high-cycle at 5 Hz. Then, the damage behavior of the specimen was observed with a microscope, soft X-ray photography and a 3D ultrasonic inspection system. In this study, to evaluate quantitative characteristics of both transverse crack propagation and delamination growth in the high-cycle region, the energy release rate associated with damage growth in the width direction was calculated. Transverse crack propagation and delamination growth in the width direction were evaluated based on a modified Paris law approach. The results revealed that transverse crack propagation delayed under the test conditions of less than ${\sigma}_{max}/{\sigma}_b$ = 0.3 of the applied stress level.

Equivalent reinforcement isotropic model for fracture investigation of orthotropic materials

  • Fakoor, Mahdi;Rafiee, Roham;Zare, Shahab
    • Steel and Composite Structures
    • /
    • 제30권1호
    • /
    • pp.1-12
    • /
    • 2019
  • In this research, an efficient mixed mode I/II fracture criterion is developed for fracture investigation of orthotropic materials wherein crack is placed along the fibers. This criterion is developed based on extension of well-known Maximum Tensile Stress (MTS) criterion in conjunction with a novel material model titled as Equivalent Reinforced Isotropic Model (ERIM). In this model, orthotropic material is replaced with an isotropic matrix reinforced with fibers. A comparison between available experimental observations and theoretical estimation implies on capability of developed criterion for predicting both crack propagation direction and fracture instance, wherein the achieved fracture limit curves are also compatible with fracture mechanism of orthotic materials. It is also shown that unlike isotropic materials, fracture toughness of orthotic materials in mode $I(K)_{IC}{\mid})$ cannot be introduced as the maximum load bearing capacity and thus new fracture mechanics property, named here as maximum orthotropic fracture toughness in mode $I(K_{IC}{\mid}^{ortho}_{max})$ is defined. Optimum angle between crack and fiber direction for maximum load bearing in orthotropic materials is also defined.

산성안개하에서 기계·구조용강의 응력부식균열 거동 (Behavior of Stress Corrosion Cracking in Structural Steel under Acid Fog Environment)

  • 임용호;김민건
    • 산업기술연구
    • /
    • 제17권
    • /
    • pp.291-295
    • /
    • 1997
  • The tests of stress corrosion cracking in structural carbon steel were carried out under the conditions of acid fog and general water. As the result of measurement SCC rupture time under acid fog was observed to be much shorter than that of general water at the same stress level. Therefore, acid fog drops the SCC strength in structural carbon steel due to strong corrosion. In the SCC process by acid fog, crack initiation was caused by pit corrosion and local stress concentration, and distinctive feature of crack growth shows branching since crack grows to the corrosion direction. Moreover, corrosion products were observed by clevage corrosion on the crack surfaces.

  • PDF

Y방향을 따라 물성치구배를 갖는 직교이방성 함수구배 재료에서 전파하는 모드 III 균열의 응력장과 변위장 (Stress and Displacement Fields of a Propagating Mode III Crack in Orthotropic Functionally Gradient Materials with Property Gradation Along Y Direction)

  • 이광호
    • 한국산업융합학회 논문집
    • /
    • 제9권1호
    • /
    • pp.37-44
    • /
    • 2006
  • Stress and displacement fields of a Mode III crack propagating along the normal to gradient in an orthotropic functionally gradient materials (OFGM), which has (1) an exponential variation of shear modulus and density, and (2) linear variation of shear modulus with a constant density, are derived. The equations of motion in OFGM are developed and solution to the displacement and stress fields for a propagating crack at constant speed though an asymptotic analysis. The first three terms in expansion of stress and displacement are derived to explicitly bring out the influence of nonhomogeneity. When the FGM constant ${\zeta}$ is zero or $r{\rightarrow}0$, the fields for OFGM are almost same as the those for homogeneous orthotropic material. Using the stress components, the effects of nonhomogeneity on stress components are discussed.

  • PDF

가스터빈 고온부품의 재생 접합을 위한 손상부 파악 (The Consideration of the Damage in Gas Turbine Hot Parts for Repair Bonding Process)

  • 김성욱;최철;김재철;이창희
    • 동력기계공학회지
    • /
    • 제7권2호
    • /
    • pp.73-79
    • /
    • 2003
  • The present study was aimed at analysing the damage of a used gas turbine bucket after 39,500h of total service. Microstructures and cracks of service-induced bucket were observed. The crack might have initiated from the coating in the bucket surface by thermal fatigue and propagated into the GTD111 base metal. Maximum depth of penetration was 2.7 mm(full penetration) at the leading edge. Crack contains a lot of Cr-,Ti-,Al-oxide which will prohibit filling and wetting of insert metal. Depth and propagation direction of crack were accorded with centrifugal force and temperature distribution in turbine bucket. Present result will provide basic data for repair bonding process.

  • PDF

Finite Element Analysis of Multiple Subsurface Cracks in Half-space Due to Sliding Contact

  • Lee, Sang Yun;Kim, Seock Sam
    • KSTLE International Journal
    • /
    • 제2권1호
    • /
    • pp.12-16
    • /
    • 2001
  • A finite element analysis of crack propagation in a half-space due to sliding contact was performed. The sliding contact was simulated by a rigid asperity moving across the surface of an elastic half-surface containing single and multiple cracks. Single, coplanar, and parallel cracks were modeled to investigate the interaction effects on the crack growth in contact fatigue. The analysis was based on linear elastic fracture mechanics and the stress intensity factor concept. The crack propagation direction was predicted based on the maximum range of the shear and tensile stress intensity factors.

  • PDF