Current Status and Investigation of International Co-operative Research Program-PINC(Program for the Inspection of Nickel Alloy Components) (국제공동연구 PINC(Program for the Inspection of Nickel Alloy Components) 현황 및 고찰)

  • Kim, Kyung-Cho;Kang, Sung-Sik;Song, Kyung-Ho;Chung, Koo-Kap;Chung, Hae-Dong
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.29 no.2
    • /
    • pp.153-161
    • /
    • 2009
  • After several PWSCCs were found in Bugey(France), Ringhals(Sweden), Tihange(Belgium), Oconee, Arkansas, Crystal Fever, Davis-Basse, VC Summer(U.S.A.), Thuruga(Japan), USNRC and PNNL started the research on PWSCC, that is, PINC project. The aim of this project is to fabricate and obtain representative NDE mock-ups with flaws to simulate tight PWSCC cracks, to identify and quantitatively assess NDE methods for accurately detecting, sizing and characterizing tight cracks such as PWSCC, to document the range of locations and crack morphologies associated with PWSCC and observed responses and to incorporate findings from other ongoing PWSCC research programs, as appropriate. By participating in PINC project, Korean morphology technique about PWSCC and NDE technique have improved and become similar lever with other advanced country. Therefore, the evaluation technique of integrity for nickel alloy component has been improved by cooperation with university, research institute and industries.

Characteristics of defect on segmental lining of TBM tunnel in operational subway (운용중인 국내 지하철 TBM터널의 세그먼트라이닝 결함특성 분석)

  • Choo, Jinho;Lee, DongHun;Noh, EunChul
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.24 no.1
    • /
    • pp.109-128
    • /
    • 2022
  • The precise inspection for safety and diagnosis (PISD) of tunnel has been conducted by the special act on safety control of public structures. However, the present assessment for the segmental lining of TBM tunnel has limitation such as: NDTs for integrity, segmental configuration for field inspection, and consideration for jacking system. Even if the number of TBM tunnel is less than 1% of enrolled facility in FMS, more attention to maintenance should be necessary due to its usage such as multi-use facility and national important facility. Compared to NATM tunnel, excavated by drilling and blasting and then installed lining by cast-in-place within 6~12 m, TBM tunnel is cut out ground by disk and cutter-bit and then assembled 7 pieces of precast segment, 1.2~1.4 m wide. Different features of design, construction, and maintenance should be considered to be more exact evaluation of TBM tunnel. The characteristics of defect is categorized and analyzed with 11 operational TBM tunnels in domestic subway. To be more comprehend various particular defects, foreign studies have been also adapted. Crack and leakage are categorized in 7 patterns. Breakage/spalling and corrosion are also grouped into 3 patterns. Patterned defects or damages are fed back in design, construction, and are useful guidelines for maintenance stage in future.

Study of Quantitative Assessment Standard for Type 1 and Type 2 Gas Cylinders Using Acoustic Emission Testing (음향방출법을 이용한 Type 1 및 Type 2 가스실린더의 정량적 평가기준에 대한 연구)

  • Kim, Dong-Hyun;Lee, Sang-Bum;Kim, Kyung-Hoon;Yoon, Dong-Jin;Bae, Dong-Myung
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.34 no.2
    • /
    • pp.176-183
    • /
    • 2014
  • Acoustic emission testing (AET) of cylinders is advantageous in that it can be directly conducted on cylinders installed in a car, without needing to dissemble them on a real-time basis. Therefore, users prefer AET over other nondestructive testing methods. Owing to these advantages of AET, it has been approved by the Department of Transportation of the U.S. as a safety evaluation method for pressure containers or as an alternative to the hydroproof testing method. This paper presents a study of the quantitative evaluation criteria for a container having ultrasonic testing defects and also for Type 1 and Type 2 gas cylinders, which are defective seamless pressure containers provided by NK, a manufacturer of pressure containers. For the Type 1 cylinder, the process from crack growth to leak was observed in a repetitive fatigue test using a 113 L container according to ASTM E 1419-02. Further, for the Type 2 cylinder, integrity was evaluated using a 119 L sound container and a container damaged by hydraulic pressure, by the slow-fill method according to ASTM E 2191-02. Based on the AET results of the Type 1 and Type 2 cylinders, quantitative evaluation criteria were established for a defective and non-defective container.

Applicability of Composite Polyurea Method Considering the Required Performance in Underground Parking Lot Upper Slab (공동주택 지하주차장 상부슬래브의 요구성능을 고려한 복합형 폴리우레아 공법의 적용성 검토)

  • Lee, Jung-Hun;Choi, Eun-Kyu;Song, Je-Young;Kim, Soo-Yeon;Oh, Sang-Keun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.3
    • /
    • pp.243-254
    • /
    • 2019
  • In this study, problems of the waterproofing methods in which water leakage occurs in the upper slab of the underground parking lot of apartment houses and the requirements considering the characteristics of the upper slab, and selected the appropriate performance(proposal) for the composite polyurea process are reviewed. As a result of the study, it is necessary to review performance such as responsiveness to upper slab of the multi-unit underground parking lot that is comprised of (1) crack and behavior responsiveness, (2) surface integrity, (3) vertical watertight stability, (4) pressure layer construction, (5) impact and pressure response and (6) vehicle moving load. As a result of evaluating 5 items corresponding to the requirements for the soft and hard complex polyurea, all of them were found to meet the conditions, and each materials were improved by compounding the materials that had problems when applying a single-ply method, thereby clarifying the advantages and disadvantages of the material property. However, in order to apply to the actual site, additional evaluation on site applicability such as mock-up evaluation should be conducted, and subsequent studies on the applicability of the market through review of economic feasibility and maintenance is required.

A STUDY ON FRACTURAL BEHAVIOR OF DENTIN-RESIN INTERFACE (상아질-복합레진 접착계면의 파괴거동에 대한 연구)

  • Ryu, Gil-Joo;Choi, Gi-Woon;Park, Sang-Jin;Choi, Kyung-Kyu
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.3
    • /
    • pp.208-221
    • /
    • 2007
  • The fracture toughness test is believed as a clinically relevant method for assessing the fracture resistance of the dentinal restoratives. The objectives of this study were to measure the fracture toughness $(K_{1C})$ and microtensile bond strength of dentin-resin composite interface and compare their relationship for their use in evaluation of the integrity of the dentin-resin bond. A minimum of six short-rod specimens for fracture toughness test and fifteen specimens for microtensile bond strength test was fabricated for each group of materials used. After all specimens storing for 24 hours in distilled water at $37^{\circ}C$, they were tensile-loaded with an EZ tester universal testing machin. Statistical analysis was performed using ANOVA and Tukey's test at the 95% confidence level, Pearson's coefficient was used to verify the correlation between the mean of fracture toughness and microtensile bond strength. FE-SEM was employed on fractured surface to describe the crack propagation. Fracture toughness value of Clearfil SE Bond (SE) was the highest, followed by Adper Single Bond 2 (SB), OptiBond Solo (OB), ONE-STEP PLUS (0S), ScotchBond Multi-purpose (SM) and there was significant difference between SE and other 4 groups (p < 0.05). There were, however, no significant difference among SB, OB, OS, SM (p > 0.05). Microtensile bond strength of SE was the highest, followed by SB, OB, SM, OS and OS only showed significant lower value (p < 0.05). There was no correlation between fracture toughness and microtensile bond strength values. FE-SEM examination revealed that dentin bonding agent showed different film thickness and different failure pattern according to the film thickness. From the limited results of this study, it was noted that there was statistically no correlation between K1C and ${\mu}TBS$. We can conclude that for obtaining the reliability of bond strength test of dentin bonding agent, we must pay more attention to the test procedure and its profound scrutiny.