모재의 재질 및 질화층 형성에 따른 Arc PVD 코팅의 접합특성 평가 (Evaluation of Adhesion Properties of Arc PVD Coatings on Non-Nitrided and Nitrided Various Substrates)

  • 이정민;전성진;고대철;김병민
    • 대한기계학회논문집A
    • /
    • 제30권10호
    • /
    • pp.1179-1186
    • /
    • 2006
  • This paper was designed to assess the adhesive properties of hard coatings on non-nitrided and nitrided various tool steels. Estimations of adhesion were done to scratch test which is mainly used in hard coating. The critical load$(L_c)$ between coating and substrate is defined through analysis of frictional load vs. normal load curve, signals of acoustic emission and optical observations. Coatings employed in this study are TiN, CrN and TiAlN, tools as substrates are STD11, STD61 and SKH51. It was classified to substrates with/without intermediate nitrided layer and hard coatings on substrate were deposited by arc PVD. Results showed that harder substrates and coatings give higher values of critical loads.

미세성형용 금형 Arc PVD 코팅의 밀착력 평가 (Evaluation of Adhesion properties of Arc PVD coatings for Micro Forming Die)

  • 이정민;고대철;김병민
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.186-189
    • /
    • 2005
  • This paper was designed to assess the adhesive properties of hard coatings on non-nitrided and nitrided various tool steels. Estimations of adhesion were done to scratch test which is mainly used in hard coating. The critical load(Lc) between coating and substrate is defined through analysis of frictional load vs. normal load curve, signals of acoustic emission and optical observations. Coatings employed in this study are TiN, CrN and TiAlN, tools as substrates are STD11, STD61 and SKH51. It was classified to substrates with/without nitrided layer and hard coatings on substrate were deposited by arc PVD. Results showed that harder substrates and coatings give higher values of critical loads.

  • PDF

표면처리된 Ni-Cr계 합금의 FLiNaK 용융염 하에서의 고온 안정성 (Thermal stability of surface modified Ni-Cr-alloys in molten FLiNaK salt)

  • 조현;방광현;이태석;이병우
    • 한국결정성장학회지
    • /
    • 제22권5호
    • /
    • pp.227-232
    • /
    • 2012
  • 차세대 원자력발전용 고온 열교환기 소재로 이용될 가능성이 높은 Ni-Cr계 고온합금인 Inconel 617과 Hastelloy X의 표면처리에 따른 FLiNaK(LiF-NaF-KF) 용융염 하에서의 고온물성에 대한 연구를 수행하였다. Inconel 617과 Hastelloy X기판 상에 각각 PVD인 arc discharge 및 sputtering법에 의해 TiAlN 및 $Al_2O_3$ 박막을 코팅 하였다. 이러한 표면처리가 이들 합금의 FLiNaK 용융염 하 고온 안정성에 미치는 영향에 대해 연구하였다. 용융염 하 Ni-Cr계 고온합금의 부식 원리를 이해하기 위해, 용융염 수송 loop에 사용 중 파단된 Inconel 파이프에 대한 미세구조 분석을 수행하였다. 표면처리 된 합금들을 $600^{\circ}C$ 용융염 내에서 열처리 하였으며, 열처리 전후 시편들에 대해 상형성, 미세구조 등 고온 물성 변화를 측정하였다. 연구결과 코팅되지 않은 경우 보다 TiAlN 및 $Al_2O_3$ 박막이 코팅된 소재에서 보다 우수한 고온 안정성을 보여주었다.

다양한 박막을 증착한 디젤 엔진용 피스톤링과 실린더 블록의 마찰 마멸 및 스커핑 수명 평가 (Friction, Wear and Scuffing Life of Piston Rings With Several Coating for Low Friction Diesel Enging)

  • 안태식;조대현;정순오;이영제
    • Tribology and Lubricants
    • /
    • 제23권4호
    • /
    • pp.170-174
    • /
    • 2007
  • Wear and scuffing tests were conducted using friction and wear measurement of piston rings and cylinder blocks in low friction diesel engine. The frictional forces, wear amounts and cycles to scuffing in boundary lubricated sliding condition were measured using the reciprocating wear tester. The cylinder blocks were used as reciprocating specimens, and the piston rings with several coatings were used as fixed pin. Several coatings were used such as DLC, TiN, Cr-ceramic and TiAlN in order to improve the tribological characteristics. From the tests wear volume of piston ring surfaces applied various coatings were compared. During the tests coefficients of friction were monitored. Test results showed that DLC coatings showed good tribological properties. TiN and Cr-ceramic coated rings showed good wear resistance properties but produced high friction.

WC-CO 인써트의 절삭 성능에 미치는 TiAIN계 나노 다층막 코팅의 영향 (Effect of TiAIN-based Nanoscale Multilayered Coating on the Cutting Performance of WC-Co Insert)

  • 임희열;박종극;김경배;최두진;백영준
    • 한국진공학회지
    • /
    • 제15권1호
    • /
    • pp.110-116
    • /
    • 2006
  • 본 연구에서는 나노 두께를 갖는 두 층을 반복적으로 증착하여 나노 다층 구조를 갖는 질화 물이 코팅된 절삭공구의 기계적 성능과 절삭성능의 향상에 대해 고찰하였다. 이러한 질화물계 나노 다층막에 대한 재료는 격자상수와 결정구조에 따라 $Ti_{0.54}Al_{0.46}N-CrN$계와 $Ti_{0.84}Al_{0.16}N-NlN$계를 선택하여, UBM sputtering 증착법을 이용하여 초경(WC-Co) 인서트(insert)위에 증착하였다. 공정 변수들인 증착온도, 압력. 기판 바이어스 전압, 기판회전 속도 등을 조절하여 다른 주기 값을 갖는 일정한 두께의 다층막들을 증착 시켰고, 주기에 따른 초격자 형성, 경도 값과 절삭성능을 관찰하였다. 증착된 다층막들은 그 주기 값에 따라 경도 값이 다르게 나타났으며. 경도 값이 상대적으로 높았던 특정 주기의 다층막이 코팅된 절삭 공구의 경우, 기존의 상용화된 제품에 비해 frank wear로 비교한 절삭 성능이 $20\%$이상 향상됨을 관찰하였다

초고장력강판 성형용 냉간 프레스 금형의 Ti/Cr계 PVD코팅에 대한 마모 특성 평가 (Evaluation of Wear Characteristics on Ti/Cr PVD Coatings of Cold Press Die for the Forming of UHSS)

  • 허재영;윤국태;송재선;강익수;윤일채;박춘달
    • 소성∙가공
    • /
    • 제31권4호
    • /
    • pp.186-193
    • /
    • 2022
  • The application of UHSS sheet is being expanded up to 50% to reduce the weight of automobiles and improve safety. However, due to the high strength and low elongation of the ultra-high tensile strength steel sheet, product defects such as spring back and mold defects such as cracks and chippings also occur. In this study, Pin/Ring on Disc and Spiral wear tests were conducted to evaluate the durability of Ti/Cr-coated molds for forming 1.2GPa grade UHSS sheets. Component analysis and thickness were measured for each coating layer, and hardness and adhesion were investigated to determine mechanical properties. Combining the results of various wear tests, it was found that the TiAlN coating had the best wear and sticking resistance.

이온주입 제어에 의한 재료특성 개선에 관한 연구 (A Study on Improvement of Material Characteristics by Control of Ion Implantation)

  • 양영준;이치우;후지타 카즈히사
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제32권8호
    • /
    • pp.1178-1184
    • /
    • 2008
  • In this study, techniques of ion implantation were used in order to improve the characteristics of metal materials such as the oxidation and wear resistant. In particular it is necessary to develope their oxidation and wear resistant that could be used in severe environmental conditions. There are mainly two elementary technologies including ion implantation and/or thin film coating. Ion implantation method was performed for surface modification. As a result, it was found that some ion implantations methods such as Nb, high-temperature Nb ion implantation and Nb+C combined implantation are somewhat effective for improving the oxidation resistance of TiAl alloy. Furthermore, the fluorine PBII treatment is more effective for improving the oxidation resistance of the TiAl alloy with three-dimensional shapes. The implantation of boron ion into thin film of TiN was also effective for improving the properties of materials like high temperature wear resistance. TiCrN film was applied to the actual seal ring for steam turbines, and it was observed that its sliding property showed a successfully good performance.

Ni-Cr합금과 도재간의 결합력에 gold-based bonding agent가 미치는 영향 (The effect of the gold based bonding agents on the bond between Ni-Cr alloys and ceramic restorations)

  • 이정환;주규지
    • 대한치과기공학회지
    • /
    • 제29권2호
    • /
    • pp.213-223
    • /
    • 2007
  • The success of a porcelain fused to metal (PFM) restoration depends upon the quality of the porcelain-metal bond. The adhesion between metal substructure and dental porcelain is related to the diffusion of oxygen to the reaction layer formed on cast-metal surface during firing. The purposed of this investigation was to study the effects of gold based bonding agent on Ni-Cr alloy-ceramic adhesion between porcelain matrix, gold based bonding agent and metal substructure interface. gold based bonding agent have been applied as an intermediate layer between a metal substructure and a ceramic coating. gold based bonding agent(Aurofilm NP, Metalor, Swiss) was applied on Ni-Cr alloy surface by four method. Surfaces only air abraded with 110${\beta}\neq$ Al2O3 particles were used as control. metal ceramic adhesion was evaluated by a biaxial flexure test(N=5) and volume fraction of adherent porcelain was determined by SEM/EDS analysis. Result of this study suggest that the layering sequence of gold based bonding agent is very important and can improve porcelain adherence to PFM.

  • PDF

TiN피막 코팅된 치과주조용 합금의 부식거동 (Corrosion Behaviors of TiN Coated Dental Casting Alloys)

  • 조호형;박근형;김원기;최한철
    • 대한금속재료학회지
    • /
    • 제47권2호
    • /
    • pp.129-137
    • /
    • 2009
  • Corrosion behaviors of TiN coated dental casting alloys have been researched by using various electrochemical methods. Three casting alloys (Alloy 1: 63Co-27Cr-5.5Mo, Alloy 2: 63Ni-16Cr-5Mo, Alloy 3: 63Co-30Cr-5Mo) were prepared for fabricating partial denture frameworks with various casting methods; centrifugal casting(CF), high frequency induction casting(HFI) and vacuum pressure casting(VP). The specimens were coated with TiN film by RF-magnetron sputtering method. The corrosion behaviors were investigated using potentiostat (EG&G Co, 263A. USA) in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The corrosion morphologies were analyzed using FE-SEM and EDX. Alloy 1 and Alloy 2 showed the ${\alpha}-Co$ and ${\varepsilon}-Co$ phase on the matrix, and it was disappeared in case of TiN coated Alloy 1 and 2. In the Alloy 3, $Ni_2Cr$ second phases were appeared at matrix. Corrosion potentials of TiN coated alloy were higher than that of non-coated alloy, but current density at passive region of TiN coated alloy was lower than that of non-coated alloy. Pitting corrosion resistances were increased in the order of centrifugal casting, high frequency induction casting and vacuum pressure casting method from cyclic potentiodynamic polarization test.

Al-Si 용융도금된 11%Cr 페라이트 스테인리스강, STS409L GTA 용접부의 미세조직과 경도 (Microstructures and Hardness of Al-Si Coated 11%Cr Ferritic Stainless Steel, 409L GTA Welds)

  • 박태준;공종판;나혜성;강정윤;엄상호;김정길;우인수;이종섭
    • Journal of Welding and Joining
    • /
    • 제28권3호
    • /
    • pp.92-98
    • /
    • 2010
  • Ferritic stainless steels, which have relatively small thermal expansion coefficient and excellent corrosion resistance, are increasingly being used in vehicle manufacturing, in order to increase the lifetime of exhaust manifold parts. But, there are limits on use because of the problem related to cosmetic resistance, corrosions of condensation and high temperature salt etc. So, Aluminum-coated stainless steel instead of ferritic stainless steel are utilized in these parts due to the improved properties. In this investigation, Al-8wt% Si alloy coated 409L ferritic stainless steel was used as the base metal during Gas Tungsten Arc(GTA) welding. The effects of coated layer on the microstructure and hardness were investigated. Full penetration was obtained, when the welding current was higher than 90A and the welding speed was lower than 0.52m/min. Grain size was the largest in fusion zone and decreased from near HAZ to base metal. As welding speed increased, grain size of fusion zone decreased, and there was no big change in HAZ. Hardness had a peak value in the fusion zone and decreased from the bond line to the base metal. The highest hardness in the fusion zone resulted from the fine re-precipitation of the coarse TiN and Ti(C, N) existed in the base metal during melting and solidification process and the presence of fine $Al_2O_3$ and $SiO_2$ formed by the migration of the elements, Al and Si, from the melted coating layer into the fusion zone.