Variation of Microstructure and Hardness of Contact Tips during GMA Welding (GMA용접 중 콘택트팁의 미세조직과 경도변화)

  • 김남훈;김가희;김희진;유회수;고진현
    • Journal of Welding and Joining
    • /
    • v.22 no.1
    • /
    • pp.43-49
    • /
    • 2004
  • Contact tip is located so near to welding arc that it is heated to high temperature during long time welding. In such a situation, tip changes in its microstructure and in turn its mechanical properties. This study was intended to investigate those changes by using simulated heat treatment. As a result of this study, it was confirmed that tip of Cu-P alloy hardened with severe cold deformation lose its initial hardness to a large extent within 60 min due to the occurrence of rapid recrystallization while that of Cu-Cr composition hardened by proper aging treatment can preserve its intial hardness for about 1,000 min or longer. Based on these results, suggested was a guideline that can classify contact tips into two different grades: deformation-hardened type and precipitation-hardened type. Following a guideline, a tip with Cu-Cr composition can be classified into the deformation-hardened type if it is in the over-aged condition. Such a guideline is well described.

A STUDY ON THE CHANCES OF TOOTH CONTACTS FOLLOWING ORTHODONTIC TREATMENT BY USE OF THE T-SCAN SYSTEM (T-SCAN을 이용한 교정치료후의 교합접촉 변화에 관한 연구)

  • Jeong, Ki-Hoon;Kim, Jae-Duck;Kim, Kwang-Won
    • The korean journal of orthodontics
    • /
    • v.25 no.3 s.50
    • /
    • pp.323-331
    • /
    • 1995
  • This study was undertaken to investigate the changes of tooth contacts following orthodontic treatment , using T-Scan system. Occlusal contacts in maximum intercuspation were examined in 26 patients at the end of the active phase of orthodontic treatment and again 3 months into the retention phase to abbess the initial posttreatment occlusal changes. The obtained results of this study were as follows : 1. The mean total number of contacts increased from 11.27 at the end of orthodontic treatment to 13.15 at the fellow up visit, which was found to be statistically significant (P<0.05). 2. The change of number of contacts on anterior teeth was unchanged. 3. The change of number of contacts on posterior teeth was found to be statistically significnat (P<0.01). 4. The change of fetal number of teeth in contact was significant (P<0.05). 5. The number of ant. teeth in contact was slightly increased. but Which was not found to be statistically significant (P>0.05). 6. The number of post. teeth in contact significantly increased, which was statistically significant (P<0.05). 7. A statistically significant relationship was found between the total number of contacts at the end of treatment and the change in the contacts over time. The fewer the number of tooth contact was at the end of orthodontic treatment, the greater number of tooth contact increased over time(r=-0.38, P<0.05).

  • PDF

Interface and Surface Properties by Surface Treatment of Zirconia for All Ceramic Crown (전부도재관용 지르코니아의 표면처리에 따른 표면특성 및 계면특성 관찰)

  • Kim, Chi-Young;Chung, In-Sung;Choi, Sung-Min
    • Journal of Technologic Dentistry
    • /
    • v.35 no.2
    • /
    • pp.137-142
    • /
    • 2013
  • Purpose: This study was to observe the surface and interfacial characteristic of Zirconia by surface treatment. And it was observed the roughness and contact angle according to processing, and the interfacial properties by surface treatment on zirconia. Methods: The oxide formation and ion diffusion between core and veneer ceramic were determined by the X-ray Dot Mapping of EPMA(Electron probe micro analyzer). The roughness was measured by 3D Digital microscope and the contact angle according to processing of zirconia was observed using distilled water on the surface. Results: The surface roughness of the specimens Z04, Z12, Z15 was measured $0.67({\pm}0.03){\mu}m$, $0.50({\pm}0.12){\mu}m$, $0.35({\pm}0.09){\mu}m$, respectively. As results of contact angle test, Z04, Z12, Z15 of specimen group without binder treatment was measured $46.79({\pm}3.17)^{\circ}$, $57.47({\pm}4.83)^{\circ}$, $56.19({\pm}2.66)^{\circ}$, respectively. but, L04, L12, L15 of specimen group without binder treatment was measured $63.84({\pm}2.20)^{\circ}$, $66.08({\pm}0.16)^{\circ}$, $65.10({\pm}1.01)^{\circ}$, respectively. Average contact angle of L15 was measured $65.10({\pm}1.01)^{\circ}$. In X-ray Dot Mapping results, thickness of binder including Al element was measured that each of L04, L12, L15 were $20{\mu}m$, $15{\mu}m$, $10{\mu}m$. Conclusion: The more rough surface increases the wettability, but the sintered exclusive binder decreases the wettability.

Adhesion Enhancement of Polyurethane Foam Using Atmospheric Plasma (II) (대기압 플라즈마를 이용한 폴리우레탄 소재의 접착력 향상 (II))

  • Sim, Dong Hyun;Seul, Soo Duk;Oh, Sang Taek
    • Journal of Adhesion and Interface
    • /
    • v.8 no.3
    • /
    • pp.1-8
    • /
    • 2007
  • An atmospheric plasma pre-treatment method was applied to polyurethane foam to improve its contact angle and adhesion. In order to investigate the optimum reaction condition of plasma treatment, type of reaction gas (nitrogen, argon, oxygen, air), rate of gas flow (30~150 mL/min), and reaction time (0~30 sec) were examined in a plate plasma reactor. Also, the effects were compared to those of a conventional vacuum plasma pre-treatment system. The result of the surface modification with respect to the treatment procedure was characterized by using SEM and ATR-FTIR. Due to a decrease of the contact angle of polyurethane foam, the greatest adhesion strength was achieved at a flow rate of 100 mL/min and at a reaction time of 10s for N2 gas. Consequently, the atmospheric plasma treatment reduced the contact angle of the polyurethane foam and also resulted in the improvement of the peel strength.

  • PDF

Surface Modification of PET Irradiated by Ultra-Violet (Part I) -Transformation of Chemical Structure and Surface Properties- (UV조사를 통한 PET의 표면개질 (제1보) -화학구조 변화 및 표면특성 변화-)

  • Choi Hae Young;Lee Jung Soon
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.29 no.3_4 s.141
    • /
    • pp.561-568
    • /
    • 2005
  • The irradiation of Ultra-Violet (UV) is an efficient treatment for polymer to improve hydrophilic properties. 4-Channel PET knit fabrics were treated with UVA and UVC to develop functional and environment-friendly fabric. The fabric was treated with various treatment times and distances from UV lamps having different wavelength. FT-IR and XPS investigated the chemical changes. To confirm the change of surface properties, contact angle, surface energy and SEM were examined. The study of UV as a treatment for PET knit fabric shows significant changes in chemical and surface properties, which is proved by analyses. FT-IR and XPS analyses prove the augmentation of carboxylic, Hydrophilic groups on the surfaces treated by UV. The increase of water contact angle and surface energy means more water wettable and surface energy of PET film was substantially increased by UV irradiation time. The ageing after surface treatment had little influence on the surface energy of the irradiated PET film. SEM proves the surface modification of PET such as etching, bubble and crack. The negative effects are increased in accordance with increasing treatment time.

Hydrophilic Effect of the Polyimide by Atmospheric Low-temperature Plasma Treatment (대기압 저온 플라즈마 처리에 의한 폴리이미드의 친수화 효과)

  • Cho, J.H.;Kang, B.K.;Kim, K.S.;Choi, B.K.;Kim, S.H.;Choi, W.Y.
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.18 no.2
    • /
    • pp.148-152
    • /
    • 2005
  • Atmospheric low-temperature plasma was produced using dielectric barrier discharge (DBD) plate-type plasma reactor and high frequency of 13.56 Hz. The surfaces of polyimide films for insulating and packaging materials were treated by the atmospheric low-temperature plasma. The contact angle of 67$^{\circ}$ was observed before the plasma treatment. The contact angle was decreased with deceasing the velocity of plasma treatment. In case of oxygen content of 0.2 %, electrode gap of 2 mm, the velocity of plasma treatment of 20 mm/sec, and input power of 400 W, the minimum contact angle of 13$^{\circ}$ was observed. The chemical characteristics of polyimide film after the plama treatment were investigated using X-ray photoelectron spectroscopy (XPS), and new carboxyl group bond was observed. The surfaces of polyimide films were changed into hydrophilic by the atmospheric low-temperature plasma. The polyimide films having hydrophilic surface will be very useful as a packaging and insulating materials in electronic devices.

The literature study on Contact dermatitis (接觸性 皮膚炎에 關한 文獻的 考察)

  • Jeon, Jae-Hong;Kim, Hyun-A;Kang, Yun-Ho
    • The Journal of Korean Medicine Ophthalmology and Otolaryngology and Dermatology
    • /
    • v.10 no.1
    • /
    • pp.263-283
    • /
    • 1997
  • The study has been carried out to investigate of the Contact dermatitis by referring to 37 literature. The results were as follows; 1. In oriental medical science, Contact dermatitis is belong to the cartegory of the 'Chilchang(漆瘡)', 'Honyoja(狐尿刺)', 'Bunhwachang(粉花瘡)', 'Goyakpoong(膏藥風)', 'Matongsun(馬桶癬)'. 2. The cause of a disease is combination of internal factor-the weak of skin or the constitutional factor and external factor-the toxic substance. When the toxic substance contacts skin, pathologial change-stagnation of vital energy and blood(氣血鬱滯)-appears, and after the stagnation of vital energy and blood change heat(化火熱). 3. The symptom of a disease is topical itching, burning pain, erythematous papule, vesicle etc in skin in the acute state and itching, pachyderma, lichenification etc in skin in the chronic state. The symptom is differentiated to wind-heat(風熱) syndrom, damp-heat(濕熱) syndrom, toxic heat(熱毒) syndrom in the acute state and blood dryness(血燥) sydrom in the chronic state. 4. The treatment-methodes is as follow ; Until chung dynasty(淸代) the greater part of treatment is externl treatment The present age in china use together internal treatment and external treatment, in the acute state use method of remove heat(淸熱), remove wind(祛風), remove damp(利濕), detoxicating(解毒), remove heat from blood(凉血), in the chronic state use method of remove wind(祛風) and nourishing the blood(養血).

  • PDF

The analysis of surface degradation on polymer material by contact angle properties (접촉각 특성을 이용한 고분자복합재료의 표면열화 해석)

  • Park, Jong-Kwan
    • Journal of the Institute of Electronics Engineers of Korea TE
    • /
    • v.39 no.3
    • /
    • pp.8-14
    • /
    • 2002
  • UV, heat, and discharge treatments are arbitrary simulated for finding out the initiations and processes of surface degradation on the polymer surface. Especially, this study is focused on the inter-relation between chemical changes and electrical properties. In contact angle to measure the change of activated degree, that of polymers surface shows a slight hydrophobicity of 73$^{\circ}$~91$^{\circ}$. But, discharge treatment and UV treatment of 300 nm wavelength changed it to the hydrophilic one with the decrease of contact angle, 13.8$^{\circ}$ and 20$^{\circ}$ respectively. Thermal-treatment and UV treatment of 430~500 nm wavelength changed the surface to the hydrophobic one with the increase of contact angle, 90$^{\circ}$ and 80.1$^{\circ}$ respectively.  

Effects of Mixing Condition and Filtration Velocity on Turbidity Removal in a Contact Roughing Filter (접촉여과방식 거친여과지에서 혼화조건과 여과속도가 고탁도 제거에 미치는 영향)

  • Park, Noh-Back;Park, Sang-Min;Hong, Jin-Ah;Jun, Hang-Bae
    • Journal of Korean Society of Water and Wastewater
    • /
    • v.21 no.3
    • /
    • pp.359-366
    • /
    • 2007
  • Slow sand filtrations have been widely used for water treatment in small communities, however their capacity is often limited by high turbidity in the raw water. For this reason, several pre-treatment facilities were required for a slow sand filter. Turbidity removal from the highly turbid raw water was investigated in roughing filters as a pre-treatment process. The roughing filters followed by rapid mixing tank were operated in the form of a contact filtration. In several jar tests, the predetermined optimum aluminium sulfate (alum) doses for turbid water of 30 and 120NTU were 30 and 50mg/L, respectively. At the optimum alum dose, physically optimum parameters including G value of $220sec^{-1}$ and rapid mixing time of 3 minutes were applied to the contact filtration system. Without addition of alum, the filtrate turbidity from the roughing filters, packed respectively with different media such as sand, porous diatomite ball and gravel, was in the range of 5~30NTU at filtration velocities of 30 and 50m/day. However, the application of a contact filtration to roughing filters showed stably lower filtrate turbidity below 1.0NTU at filtration velocity of 30 m/day. Although the filtration velocity increased to 50m/day, filtrate turbidity was still below 1.0NTU in both single and double layer roughing filters. At influent turbidity of 120NTU, the filtrate turbidity was over 5 NTU in the triple layer roughing filter, which shortened the filter run time. The flocs larger than $10{\mu}m$, formed in the rapid mixing tank, were almost captured through the roughing filter bed, while the almost flocs smaller than $10{\mu}m$ remained in filtrate.