• Title/Summary/Keyword: Composite spheroid

Search Result 2, Processing Time 0.015 seconds

Agglomeration of human dermal fibroblasts with ECM mimicking nano-fragments and their effects on proliferation and cell/ECM interactions

  • Ahmad, Taufiq;Shin, Young Min;Lee, Jinkyu;Shin, Hyeok Jun;Perikamana, Sajeesh Kumar Madhurakart;Shin, Heungsoo
    • Journal of Industrial and Engineering Chemistry
    • /
    • v.67
    • /
    • pp.80-91
    • /
    • 2018
  • Here, we engineered spheroids by using ECM mimicking nano-fragments (NFs) with fibroblasts and investigated their effect on proliferation and cell/ECM interactions. NF incorporation resulted in formation of a stable spheroid, which improved proliferation and viability of cells by assisting oxygen transport confirmed by LOX-1 staining. In addition, hypoxic and apoptotic genes were significantly downregulated in spheroids with PD-NFs. Furthermore, ECM and cell junction proteins were highly expressed. Overall, our findings suggest that incorporation of NFs within spheroids for assembly with various cell types can be an alternative approach for 3D cell culture in many applications.

Manufacture of SiC-TiC System Composite by the Reaction-Bonded Sintering (반응결합 소결에 의한 SiC-TiC계 복합재료 제조)

  • 한인섭;김홍수;우상국;양준환;정윤중
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.8
    • /
    • pp.849-860
    • /
    • 1994
  • The microstructural evolution and crystalline phases of this infiltration of Ti+Al liquids in TiC, SiC, TiC+C, and SiC+C preforms have been investigated. As the Ti and Al mixing ratio in Ti+Al infiltrated liquid changes, the newly formed reaction products, which were reacted from the Ti+Al liquid with preforms, consisted of three major phases as Ti3AlC, Al2Ti4C2 or Al4C3. The TiC grain shape was changed to spheroid, when Ti3AlC was formed. In case of Al2Ti4C2 formation, the platelet grain was formed from the original TiC grain. When Al4C3 was formed, nodular or intergranular fine-grained Al4C3 was formed around the TiC grain, while the original TiC grain shape was not changed.