Optimum Design of Co-cured Steel-Composite Tubular Single Lap Joints (동시경화 강철-복합재료 원형 단일 겹치기 조인트의 최적설계)

  • Jo, Deok-Hyeon;Lee, Dae-Gil
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.5 s.176
    • /
    • pp.1203-1214
    • /
    • 2000
  • In this paper, a failure model for co-cured steel-composite tubular single lap joints has been proposed incorporating the nonlinear mechanical behavior of steel adherends and different failure mode s such as steel adherend failure and composite adherend failure. The characteristics of the co-cured steel-composite tubular single lap joint were investigated with respect to the test temperature, the stacking sequence of composite adherend, the thickness ratio of steel adherend to composite adherend, and the scarf ratio of steel adherend. Thus, the optimum design method for the co-cured steel-composite tubular single lap joint was suggested.

Prediction of the Torque Capacity for Tubular Adhesive Joints with Composite Adherends (복합재료 접착체를 가지는 튜브형 접합부의 토크전달능력 예측)

  • Oh, Je-Hoon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.30 no.12 s.255
    • /
    • pp.1543-1550
    • /
    • 2006
  • Since the performance of joints usually determines the structural efficiency of composite structures, an extensive knowledge of the behavior of adhesive joints and the related effect on joint strength is essential for design purposes. In this study, the torque capacity of adhesive joints was predicted using the combined thermal and mechanical analyses when the adherend was a composite tube. A finite element analysis was performed to evaluate residual thermal stresses developed in the joint, and mechanical s stresses in the adhesive were calculated including both the nonlinear adhesive behavior and the behavior of composite tubes. Three different joint failure modes were considered to predict joint failure: interfacial failure, adhesive bulk failure, and adherend failure. The influence of the composite adherend stacking angle on the residual thermal stresses was investigated, and how the residual thermal stresses affect the joint strength was also discussed. Finally, the predicted results were compared with experimental results available in literature.

Design parameters on the tensile load bearing capacity of a co-cured lap joint with steel and carbon fiber/epoxy composite adherends (강철재료와 탄소섬유/에폭시 복합재료를 이용한 동시경화 조인트의 인장하중 전달용량에 미치는 설계변수에 관한 연구)

  • 신금철;이정주
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2001.05a
    • /
    • pp.172-175
    • /
    • 2001
  • The co-cured Joining method, which is regarded as an adhesively bonded Joining method, is an efficient joining technique because both curing and bonding processes for the composite structures can be achieved simultaneously. It requires neither surface treatment onto the composite adherend nor an additional adhesive joining process because the excess resin, which is extracted from composite materials during consolidation, accomplishes the co-cured Joining process. Since the adhesive of the co-cured joint is the same material as the resin of the composite adherend, the analysis and design of the co-cured joint for composite structures are simpler than those of an adhesively bonded joint, which uses an additional adhesive. In this paper, effects of the manufacturing parameters, namely surface roughness, stacking sequence of the composite adherend, and manufacturing pressure in the autoclave during curing process, on the tensile load bearing capacity of the co-cured single lap joint will be experimentally investigated.

  • PDF

Design parameters on the fatigue characteristics of a co-cured double lap joint (양면겹치기 동시경화조인트의 피로특성에 영향을 미치는 설계변수에 관한 연구)

  • 신금철;이정주
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2002.05a
    • /
    • pp.5-8
    • /
    • 2002
  • The use of the co-cured joining method for composite structures is attractive due to several benefits. However, since the design stress level in cyclic loads is often smaller than the joint strength obtained from the static tensile load test, it is important to establish proper fatigue design criteria. Although some researchers have reported on co-cured joints, there are only a few papers published on the fatigue characteristics of co-cured joints. In this paper, the effect of bond parameters on the fatigue characteristics of a steel-composite co-cured double lap joint under cyclic tensile loads was experimentally investigated. We considered the surface roughness of the steel adherend and the stacking sequence of the composite adherend as bond parameters. A fatigue failure mechanism of the co-cured double lap joint was explained systematically by investigating the surfaces of failed specimens.

  • PDF

A Parametric Study on the Strength of Single-Lap Bonded Joints of Carbon Composite and Aluminum (탄소 복합재-알루미늄 단일겹침 접착 체결부의 강도에 관한 인자연구)

  • Kim, Tae-Hwan;Seong, Myeong-Su;Choi, Jin-Ho;Kweon, Jin-Hwe
    • Composites Research
    • /
    • v.20 no.5
    • /
    • pp.34-42
    • /
    • 2007
  • Strength and failure of adhesively bonded carbon composite-to-aluminum single-lap joints were studied by experiment. The main objective of this study is to investigate the effect of various parameters such as curing pressure for bonding, overlap lengths, and adherend thickness on the failure loads and modes of the bonded Joints with dissimilar materials. Experimental results show that the bonding pressure for composite-to-aluminum dissimilar materials should be 4 atm at the lowest. Failure load of the joints increases as the overlap length increases, but the strength (failure load divided by bonded area) decreases rapidly after the overlap width-to-length ratio is greater than 1. When the adherend thickness increase to double, bonding strength increase $12{\sim}55%$. Major failure mode of the joints is the delamination in the composite laminate and the location of delamination goes deeper into the laminates as the bonding pressure and overlap length increase.

Shear Strength of an Aluminum Alloy Bonded with a DP-460 Adhesive: Single Lap-shear Joints

  • Kim, Hyun-Bum;Nishida, Tomohisa;Oguma, Hiroyuki;Naito, Kimiyoshi
    • Journal of Adhesion and Interface
    • /
    • v.21 no.1
    • /
    • pp.20-26
    • /
    • 2020
  • Single lap-shear joints (SLJ) specimens with and without partial round fillets were fabricated to measure the average shear strength of adhesives. The effects of the length of the adherend on the SLJ specimens were also investigated. An epoxy adhesive was used to bond aluminum alloy. Tensile tests were performed on the adhesive bulk specimens to measure the mechanical properties. The finite element analysis (FEA) method was used to measure the adhesive stress distributions, i.e., the peel and shear stresses, on the bonded part. The experimental results revealed that the specimen consisting short length of adherend and without the partial round fillets exhibited the smallest average shear strength of adhesive among the investigated specimens. FEA revealed that the low average shear strength for the specimen with a short adherend length was caused by high stress concentrations on the adhesive at the edge of the bonded part.

End-Shape Effect for Stress Concentration Reduction of Composite Single-Lap Bonded Joint (끝단형상에 따른 복합소재 단일겹치기 체결부의 응력집중 저감에 관한 연구)

  • Kim, Jung-Seok;Hwang, Jae-Yeon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.35 no.3
    • /
    • pp.333-340
    • /
    • 2011
  • We evaluated the stress-reduction effect for different shapes of a composite adherend with or without a spew fillet. Six different single-lap joint specimens were modeled and assessed using nonlinear finite element analysis. Moreover, we investigated the effect of the stiffness ratio of the adherend and adhesive. The single-lap joint with normal tapering had the highest stress values, and the single-lap joint with reverse tapering and a spew fillet had the lowest stress values. The composite adherends with higher stiffness had lower stress values, and the adhesives with lower stiffness had lower stress values.

Effect of the Cross Sectional Shapes on the Static and Fatigue Torque Transmission Capabilities of Adhesive Single Lap Joints (단면형상에 따른 단일겹치기 이음의 피로 및 정적 토크 전달특성에 관한 실험적 연구)

  • 최진경;이대길
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.18 no.4
    • /
    • pp.835-845
    • /
    • 1994
  • In this paper, the effects of the adhesive thickness and adherend roughness on the static and fatigue strengths of the adhesively bonded circular single lap joints has been investigated by an experimental method. The stacking sequence effect of the composite adherend on the static and fatigue strength and the fracture patterns of the adhesive failure were also observed. Since the circular single lap joint fails catastrophically beyond the static strength of fatigue limit, the tubular polygonal adhesively bonded joints such as triangular, tetragonal, pentagonal, hexagonal as well as elliptical joints were manufactured in order to give partial mechanical characteristics to the adhesively bonded tubular joints. These joints were tested both in static and fatigue modes. From the experimental investigations, it was found that the fatigue strength of the circular adhesively bonded joints was much dependent on the arithmetical average surface roughness of the adherends and the polygonal adhesively bonded joints had better fatigue strength characteristics than the circular adhesively bonded joints.

Strength of Composite Single-Lap Bonded Joints with Various Manufacturing Processes for Aircraft Application (항공용 복합재 단일겹침 접착 체결부의 제작공정에 따른 강도 연구)

  • Song, Min-Gyu;Kweon, Jin-Hwe;Choi, Jin-Ho;Kim, Hyo-Jin;Song, Min-Hwan;Shin, Sang-Joon
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.37 no.8
    • /
    • pp.751-758
    • /
    • 2009
  • Failure strengths of composite single-lap adhesive joints were investigated with various parameters such as manufacturing method, overlap length and adherend thickness. A total of 335 single-lap joint specimens were tested under tension. Specimens were fabricated with 4 different manufacturing processes; cocuring without and with adhesive, secondary bonding and co-bonding. Each manufacturing process has 5 different overlap lengths and 4 different thicknesses, respectively. As expected, failure strength is higher in thicker adherend joints and lower in larger overlap length specimens. Interesting result is that the secondary bonded joints show the higher strength than the cobonded and cocured joints with adhesive, and give close or even higher strength compared with non-adhesive cocured case.

Stress Analysis Of Wavy Lap Joint (WAVY LAP JOINT 응력 해석)

  • 김위대;양승희
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2000.11a
    • /
    • pp.216-219
    • /
    • 2000
  • The adhesive bonded single-lap joint is due to its intrinsic load eccentricity problem, severe peel stresses concentration occur at both end of the joint. In this paper, new lap-joint is designed to avoid the singular peel stress, and to compare the stresses of the middle adhesive layer between the single-lap joint and the wavy-lap joint. Two adherend lay-up, i.e., [90/0/90/0]$_{2s}$ and [0/90/0/90]$_{2s}$ were consider in the study.