• Title/Summary/Keyword: Complex Sol-Gel Process

Search Result 18, Processing Time 0.022 seconds

Preparation and Characterization of BaTiO3 Powders and Thin films (티탄산바륨 분말과 박막의 제조 및 특성 연구)

  • Jung, Miewon;Son, Hyunjin;Lee, Jiyun;Kim, Hyunjung
    • Analytical Science and Technology
    • /
    • v.17 no.2
    • /
    • pp.173-179
    • /
    • 2004
  • The $BaTiO_3$ powders and thin films were prepared by an alkoxide modified sol-gel process (polymerization-complex route) using ethylene glycol. The stable starting (Ba-Ti)-mixed metal organic sol was made by addition of acetylacetone. The $BaTiO_3$ powders, which had a particle size of 40~77 nm, were crystallized from an amorphous to a tetragonal phase on annealing at 700 and $1100^{\circ}C$ for 1 h. From FT-IR, solid-state $^{13}C$ CP/MAS NMR spectroscopy and X-ray diffractometry, the trace of the Ba-Ti-oxycarbonate phase first appeared at $400^{\circ}C$. Hydrolyzed sol was spin coated on a quartz wafer at 3500 rpm for 60 s and pyrolyzed at $1100^{\circ}C$ for 1 h. After heat treatment, the coated layer became dense and smooth.

Sol-gel deposited TiInO thin-films transistor with Ti effect

  • Kim, Jung-Hye;Son, Dae-Ho;Kim, Dae-Hwan;Kang, Jin-Kyu;Ha, Ki-Ryong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.200-200
    • /
    • 2010
  • In recent times, metal oxide semiconductors thin films transistor (TFT), such as zinc and indium based oxide TFTs, have attracted considerable attention because of their several advantageous electrical and optical properties. There are many deposition methods for fabrication of ZnO-based materials such as chemical vapor deposition, RF/DC sputtering and pulsed laser deposition. However, these vacuum process require expensive equipment and result in high manufacturing costs. Also, the methods is difficult to fabricate various multicomponent oxide semiconductor. Recently, several groups report solution processed metal oxide TFTs for low cost and non vacuum process. In this study, we have newly developed solution-processed TFTs based on Ti-related multi-component transparent oxide, i. e., InTiO as the active layer. We propose new multicomponent oxide, Titanium indium oxide(TiInO), to fabricate the high performance TFT through the sol-gel method. We investigated the influence of relative compositions of Ti on the electrical properties. Indium nitrate hydrate [$In(NO^3).xH_2O$] and Titanium isobutoxide [$C_{16}H_{36}O_4Ti$] were dissolved in acetylacetone. Then monoethanolamine (MEA) and acetic acid ($CH_3COOH$) were added to the solution. The molar concentration of indium was kept as 0.1 mol concentration and the amount of Ti was varied according to weighting percent (0, 5, 10%). The complex solutions become clear and homogeneous after stirring for 24 hours. Heavily boron (p+) doped Si wafer with 100nm thermally grown $SiO_2$ serve as the gate and gate dielectric of the TFT, respectively. TiInO thin films were deposited using the sol-gel solution by the spin-coating method. After coating, the films annealed in a tube furnace at $500^{\circ}C$ for 1hour under oxygen ambient. The 5% Ti-doped InO TFT had a field-effect mobility $1.15cm^2/V{\cdot}S$, a threshold voltage of 4.73 V, an on/off current ratio grater than $10^7$, and a subthreshold slop of 0.49 V/dec. The 10% Ti-doped InO TFT had a field-effect mobility $1.03\;cm^2/V{\cdot}S$, a threshold voltage of 1.87 V, an on/off current ration grater than $10^7$, and a subthreshold slop of 0.67 V/dec.

  • PDF

Monitoring of pH and dissolved oxygen in microorganism fermentation processes using a 24-well microplate (24-웰 마이크로 플레이트를 이용한 미생물 발효공정에서 pH 및 용존산소의 모니터링)

  • Kim, Sun-Yong;Kim, Chun-Kwang;Sohn, Ok-Jae;Rhee, Jong-Il
    • KSBB Journal
    • /
    • v.24 no.2
    • /
    • pp.207-211
    • /
    • 2009
  • In this study, the sensing membranes for detection of pH and dissolved oxygen(DO) were prepared by immobilizing 6-aminofluorescein or ruthenium complex onto the sol-gel matrixes of GPTMS, MTMS, and TEOS and then recoated with the mixture of hydrophobic sol-gel and graphite for light insulation. The pH and DO sensing membranes recoated with the light insulation layer showed a higher sensitivity than those without light insulation layer. The sensing membranes were immobilized on the wells of 24-well microplate and used to monitor the fluorescence intensity for pH and DO in E.coli JM109 and P.pastoris X-33 fermentation processes. The change of the fluorescence intensity in the DO sensing membrane agreed with the growth patterns of microorganisms, that the membranes are valuable to monitor the DO in fermentation processes. In the case of pH monitoring, the fluorescence intensity has showed good correlation to the off-line pH data, that the pH membranes are valuable to monitor pH values in fermentations.

Development of Optical Fiber Glucose and Lactate Biosensors for Bioprocess Monitoring (생물공정 모니터링을 위한 광섬유 포도당 및 젖산 센서의 개발)

  • Jung, Chang Hwan;Sohn, Ok-Jae;Rhee, Jong Il
    • KSBB Journal
    • /
    • v.32 no.1
    • /
    • pp.35-45
    • /
    • 2017
  • In this work the optical fiber glucose and lactate biosensors were developed by using fluorescent dye and enzyme immobilized on the end tip of an optical fiber. 3-Glycidyloxypropyl)methyldiethoxysilane (GPTMS), (3-Aminopropyl) trimethoxysilane (APTMS) and Methyltrimethoxysilane (MTMS) were used to immobilize glucose oxidase (GOD), lactate oxidase (LOD) and ruthenium(II) complex (tris(4,7-diphenyl-1,10-phenanthroline) ruthenium(II), $Ru(dpp)_3^{2+}$) as oxygen sensitive fluorescent dye. MTMS sol-gel was an excellent supporting material for the immobilization of $Ru(dpp)_3^{2+}$, GOD, and LOD on the optical fiber. Storage stability of the optical fiber glucose sensor was kept constant over 20 days, while the optical fiber lactate sensor had constant storage stability over 17 days. The optical fiber glucose and lactate biosensors also maintained good operational stability for 20 hours and 14 hours, respectively. The activities of the immobilized enzymes were most excellent at pH 7 and at $25^{\circ}C$. On-line monitoring of glucose and lactate in a simulated process was performed with the optical fiber glucose and lactate biosensors. On-line monitoring results were agreed with those of off-line data measured with high performance liquid chromatography (HPLC).

Synthesis of highly crystalline nanoporous titanium dioxide at room temperature (상온에서 고결정성 나노기공 이산화티탄 제조기술)

  • Chung, Pyung Jin;Kwon, Yong Seok
    • Journal of Energy Engineering
    • /
    • v.25 no.2
    • /
    • pp.65-78
    • /
    • 2016
  • Initial studies of the photocatalyst has been developed from the field relating to the conversion and storage of solar energy. Recently, the study of the various organic decomposition compound and the water purification and waste water treatment by ultraviolet irradiation in the presence of light or a photocatalyst are being actively investigated. In addition, the oxidized material-carbon nanotubes, graphene-nanocomposites have been studied. Such a complex is suitable as a material constituting the solar cells and photolysis nanoelectronics, including the flexible element due to thermal and chemical stability.

Printability of Thermally and Chemically Stable Silica-Titanium Dioxide Composite Coating Layer (실리카-이산화티탄 복합 코팅층의 열적, 화학적 안정성 및 인쇄적성 평가)

  • Kim, Hye Jin;Han, Kyu Sung;Hwang, Kwang Taek;Nahm, Sahn;Kim, Jin Ho
    • Korean Journal of Materials Research
    • /
    • v.29 no.10
    • /
    • pp.631-638
    • /
    • 2019
  • As automation systems become more common, there is growing interest in functional labeling systems using organic and inorganic hybrid materials. Especially, the demand for thermally and chemically stable labeling paper that can be used in a high temperature environment above $300^{\circ}C$ and a strong acid and base atmosphere is increasing. In this study, a composite coating solution for the development of labeling paper with excellent thermal and chemical stability is prepared by mixing a silica inorganic binder and titanium dioxide. The silica inorganic binder is synthesized using a sol-gel process and mixed with titanium dioxide to improve whiteness at high-temperature. Adhesion between the polyimide substrate and the coating layer is secured and the surface properties of the coating layer, including the thermal and chemical stability, are investigated in detail. The effects of the coating solution dispersion on the surface properties of the coating layer are also analyzed. Finally, it is confirmed that the developed functional labeling paper showed excellent printability.

Nano-safety Management and Exposure Assessment of Nanomaterials Producing Facilities (나노물질 생산시설의 환경노출 평가와 안전관리)

  • Umh, Ha Nee;Roh, Jinkyu;Park, Junsu;Kwak, Byoung Kyu;Lee, Byung Cheon;Choi, Kyunghee;Yi, Jongheop;Kim, Younghun
    • Korean Chemical Engineering Research
    • /
    • v.50 no.1
    • /
    • pp.112-117
    • /
    • 2012
  • With the development of nanotechnology, nano-consumer products have been popularized. For the past 10 years, potential risk of nanomaterials to human and environment have been raised carefully. Especially, workers, who directly handle nanomaterials in laboratories and manfacturers, will lead to direct exposure of nanomaterials. Therefore, direct exposure assessment and field monitoring of nanomaterials are required to assess and manage the nanomaterial exposure to human and environment. In this work, two nano-manufacturing companies, which had plasma and sol-gel processes, were selected to analyze the main exposure source and process with in-situ SMPS (scanning mobility particle sizer) and ex-situ TEM (transmission electron microscopy). The results showed that the colloidal nanoparticle in liquid phase was easily evaporated and monitored by SMPS. Most serious thing is that the workers does not know about the potential risk of nanomaterials, and thus they are not taking proper protection activities, such as PPE (personal protective equipment). Therefore, exposure assessment for nanomaterial handling facilities should be additionally carried out, and nano-safety management protocols are also provided.

Solution-Processed Nontoxic and Abundant $Cu_2ZnSnS_4$ for Thin-Film Solar Cells

  • Mun, Ju-Ho
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2012.05a
    • /
    • pp.65-65
    • /
    • 2012
  • Copper zinc tin sulfide ($Cu_2ZnSnS_4$, CZTS) is a very promising material as a low cost absorber alternative to other chalcopyrite-type semiconductors based on Ga or In because of the abundant and economical elements. In addition, CZTS has a band-gap energy of 1.4~1.5eV and large absorption coefficient over ${\sim}10^4cm^{-1}$, which is similar to those of $Cu(In,Ga)Se_2$(CIGS) regarded as one of the most successful absorber materials for high efficient solar cell. Most previous works on the fabrication of CZTS thin films were based on the vacuum deposition such as thermal evaporation and RF magnetron sputtering. Although the vacuum deposition has been widely adopted, it is quite expensive and complicated. In this regard, the solution processes such as sol-gel method, nanocrystal dispersion and hybrid slurry method have been developed for easy and cost-effective fabrication of CZTS film. Among these methods, the hybrid slurry method is favorable to make high crystalline and dense absorber layer. However, this method has the demerit using the toxic and explosive hydrazine solvent, which has severe limitation for common use. With these considerations, it is highly desirable to develop a robust, easily scalable and relatively safe solution-based process for the fabrication of a high quality CZTS absorber layer. Here, we demonstrate the fabrication of a high quality CZTS absorber layer with a thickness of 1.5~2.0 ${\mu}m$ and micrometer-scaled grains using two different non-vacuum approaches. The first solution-processing approach includes air-stable non-toxic solvent-based inks in which the commercially available precursor nanoparticles are dispersed in ethanol. Our readily achievable air-stable precursor ink, without the involvement of complex particle synthesis, high toxic solvents, or organic additives, facilitates a convenient method to fabricate a high quality CZTS absorber layer with uniform surface composition and across the film depth when annealed at $530^{\circ}C$. The conversion efficiency and fill factor for the non-toxic ink based solar cells are 5.14% and 52.8%, respectively. The other method is based on the nanocrystal dispersions that are a key ingredient in the deposition of thermally annealed absorber layers. We report a facile synthetic method to produce phase-pure CZTS nanocrystals capped with less toxic and more easily removable ligands. The resulting CZTS nanoparticle dispersion enables us to fabricate uniform, crack-free absorber layer onto Mo-coated soda-lime glass at $500^{\circ}C$, which exhibits a robust and reproducible photovoltaic response. Our simple and less-toxic approach for the fabrication of CZTS layer, reported here, will be the first step in realizing the low-cost solution-processed CZTS solar cell with high efficiency.

  • PDF