The flow properties of binder latices for paper coating were investigated, together with dynamic viscoelastic properties of latex films and electron micrographs of latices, under various conditions. The amphoteric latex, binder pigment latex and anionic latex were used in this work. The amphoteric latex has both anionic and cationic functional group on its surface. The binder-pigment with a core-shell structure has dual functions : plastic pigment and binder. The low shear viscosity of binder latices and clay slurry were measured with Brookfield vis cometer. At low-shear rates. the viscosity decreased with increasing particle size of latex. On the amphoteric latex surface, the carboxyl groups are assumed to be fully dissociated over the region of pH 9~12, but the density of negative groups seems to be increased because of the gradual decrease in the degree of dissociation of amino groups. Since the apparent particle size of latex increases with surface charge, the electroviscous effect can be observed. On the anionic latex surface, the charge density is assumed to be nearly constant above pH 8. However, below pH 8 the coagulation of particles could be observed probably because of the decrease in the charge density.
Experimental work was carried out in order to produce a novel grade of ink-jet paper that has both high print-out quality and price competitiveness. Usually, silica and PVOH has been used for ink-jet paper to design the coating layer that has a hydrophilic and micro-porous structure. However, poor rheological characteristics and low productivity of the silica-PVOH system make the price of the ink-jet paper high. The main focus of this study was replacing the conventional silica (coating pigment) PVOH (binder) coating system with the new PCC (coating pigment) cationic starch (binder) coating system, and optimizing thecoating technology associated with PPC-cationic starch system. In this study, ink-jet print quality of PCC-coated papers was compared with that of silica-coated paper. Two types of PCC were used: conventional type and colloid type. It turned out that PCC C, a conventional coating pigment, has not given a desirable result: it showed high dot reproduction, but it gave low optical density. In spite of low dot reproduction, the qualities of PCC A were comparable or superior to those of silica in optical density, color reproduction, and the uniformity of printing surface. It was also shown that the problems that are happened when the dosage level of cationic starch was too low were varied with ink-type used in each printer. However, in the case of low binder level, the produced image was widely spread resulting fromtoo low optical density of images, or from the lack of bonding ability to set ink into coating surface.
This paper was performed to investigate the effect of pore structure on ink residual behavior. To prepare different coating structures as substrates against inks, fine, medium and coarse calcium carbonate were used in the coating color. It is well known ink properties can affect to print qualities. After printing on the coated paper, ink layer can consider as third structure addition to paper and coating layer. To compare effect of ink properties on the surface structure and print qualities, several properties of ink were also adopted as raw material. Particle size of pigment effect on gloss evaluation of coated paper increased with calendering. It was shown that ink transfer rate increased as surface of the sample was smooth. The ink contained low viscosity resin evaluated more print gloss. Finer pigment particle size, smaller pore size and higher porosity. Pore volume of coated paper was slightly decreased with printing as the coating was prepared with the finest particle size. However, it founded that ink resin could not affect on pore volume and distribution of printed paper
본 연구는 색조화장품에 사용되는 진주광택안료의 특성을 주사전자현미경과 에너지분산분광분석기 및 열분석기를 사용하여 규명하였다. 본 연구에 사용된 인공합성 진주광택안료를 여성의 볼과 눈두덩 부위에 화장을 한 후 육안으로 관찰하였을 때 진주 광택안료는 보는 각도에 따라 흰색에서 보라색까지 다양한 색조로 빛을 반사하였다. 진주광택안료의 주사전자현미경 관찰 결과 안료는 얇은 판상의 다각형의 형태를 하고 있었으며 크기는 규격화된 모양이 아니고 다양하게 관찰되었다. 이런 조각의 크기는 약 $30{\mu}m$에서 $300{\mu}m$까지 측정되었고 안료 조각은 끝이 뾰족하거나 각진 상태로 존재하였다. 고배율의 주사전자현미경상에서 안료조각의 모서리 부위와 측면은 날카롭지 않은 타원형의 형태로 나타났으며 두께는 약 $9{\mu}m$로 측정되었다. 안료조각 표면은 직경이 약 60 nm의 이산화티탄 입자들에 의해서 피복되어 있었다. 진주광택안료의 에너지분산분석기를 사용하여 구성 원소 성분을 분석한 결과 안료의 표면은 O, Si, C, Na, Ca, Ti, Zn 등이 검출되었고 안료의 측면 부위도 동일한 성분들이 검출되었다. 이들 안료는 운모 티타니아(mica titania)로 확인되었다. 진주광택안료의 열분석 결과 초기 $100^{\circ}C$부터 $800^{\circ}C$까지 중량 감소는 큰 차이를 보이지 않았다. 열분석 결과 $115^{\circ}C$에서 1.1% 중량 감소를 하였고 $416^{\circ}C$에서 1.7% 감소하였으며 $797^{\circ}C$ 에서 1.9%의 중량이 감소된 것을 확인하였다.
한국정보디스플레이학회 2002년도 International Meeting on Information Display
/
pp.828-830
/
2002
In this study, we have investigated a simple process of preparation of white pigment particles by physical coating with functionalized wax for the electrophoretic display. We will discuss, especially, the implementation of bistable pigment providing high mobility by using unique charge control agent and also optical properties of wax coated $TiO_2$ particles.
여러 종류의 용제와 수지용액에 있어서의 $CaCO_3$ 안료의 분산 안정성을 Dynometer를 이용하여 조사하였다. Dynometer를 이용하여 비교적 단시간에 분산계의 분산 안정성을 평가할 수 있었으며, Dynometer를 이용한 분산 안정성 평가로부터 구한 $CaCO_3$ 안료의 용해성 파라미터, ${\delta}$는 11.62(${\delta}_d=8.04$, ${\delta}_p=5.05$, ${\delta}_h=6.70$)이었다. 안료와 친화력이 약한 용제가 첨가되는 경우 수지 용액내에서의 안료표면에의 수지 흡착층을 증가시켜 수지 용액내에서의 분산 안정성을 증가시켰다. 수지 용액 제조시 소량 첨가된 용제도 안료를 포함한 전체 분산계의 유동성과 분산 안정성에 큰 영향을 미친다는 것을 알 수 있었다.
The aim of this research was to evaluate the influences of coating components and structures on ink absorbency. The ink absorbency was measured as porosity, K&N ink absorption, gloss and ink set-off. In order to obtain the relationship between the coating structure and the ink absorbency, the binder level was adjusted and two types of pigments were examined. One of the pigments was known to make the porous coating structure and the other one had strong ink affinity. The effects of coating components were studied by applying six different types of latex and various additives . In this research, CLC(cylindrical laboratory coater) and Prufbau printability tester were used. It was found that the decreasing latex dosage and introducing porous pigment were effective solutions to increase ink absorbency. However, the ink absorbency could not be improved by applying the fine pigment even though it had strong ink affinity. Among the characters of the latex, particle size and surface tension were found to have the strong effect on ink absorbency. The ink absorbency increased with large particle size and low surface tension latex. The additives were varied and it was found that applying to the top coating was effective.
Anti-corrosive coatings for steel structures with an alternative anti-corrosive pigment, polyaniline was prepared and anti-corrosive characteristics of the prepared coatings were investigated. The structure of the polyaniline was identified by using FT-IR, UV/Vis. and TGA analysis, and the anti-corrosive properties were analyzed from the results of the salt spray experiment. We found that the anti-corrosion properties of the prepared coatings varied in accordance with the types of primer coating resins as well as with the existence and nonexistence of the top coating. In this condition, the properties of adhesion, chemical resistance, and water resistance were found to be very satisfactory when using the single-packaged urethane resin as the primer coating resin and the urethane resin as the top coating resin.
According to a previous study, talc as a coating pigment can improve the viscosity and the water retention of coating color, the compressibility of coating layer, and hence gravure printability. Talc is also well known for its larger particle size than other pigments, which implies that less binder may be need due to its smaller specific surface area. This study investigated the possibility of reducing binder content for matte grade paper. Coating color was prepared with the Cotalc-2000, which showed the best properties in the previous study. The binder content was varied and the effect of binder content on the physical properties of coated paper and the gravure printability was investigated. It was shown that binder content could be reduced when talc was used as a coating pigment. The reduction in binder content did not influence gloss, roughness and the print density of coated paper but showed improvement in paper porosity, compressibility and missing dot.
For a fundamental study for high concentration pigment coating, the effects of alkali swellable emulsion (ASE) type rheology modifier and surface adsorption emulsion (SAE) type rheology modifier on both the stability and the viscoelastic behavior of a coating color were elucidated. The coating color prepared with SAE type rheology modifier showed superior thermal and mechanical stability than that with ASE type. In the high concentration and high speed coating process, the mechanical stability of a coating color was a key parameter since both impact force and shear force were increased with the increase of coating color concentration and coating speed, respectively.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.