Al2O3 Coating on Transparent Polycarbonate Substrates for the Hard-coating Application (투명 폴리카보네이트 보호코팅을 위한 산화알루미늄 박막)

  • Kim, Hun;Nam, Kyoung-Hee;Jang, Dong-Su;Lee, Jung-Joong
    • Journal of the Korean institute of surface engineering
    • /
    • v.40 no.4
    • /
    • pp.159-164
    • /
    • 2007
  • Transparent aluminum oxide films were deposited on polycarbonate (PC) substrates by inductively coupled plasma (ICP) assisted reactive sputtering. the oxygen flow rate was regulated by controlling the target voltage with a proportional integrate derivative controller. The PC substrate was treated with plasma prior to the deposition in order to the enhance the adhesive strength of the $Al_2O_3$ film. The characteristics of hardness, structure, density, transmittance, deposition rate, surface roughness and residual stress were investigated to estimate the possibility for the hard coating.

Precise ultrasonic coating and controlled release of sirolimus with biodegradable polymers for drug-eluting stent

  • Joung, Yoon Ki;Jang, Bu Nam;Kang, Jong Hee;Han, Dong Keun
    • Biomaterials and Biomechanics in Bioengineering
    • /
    • v.1 no.1
    • /
    • pp.13-25
    • /
    • 2014
  • In the current study, a drug-eluting stent coated with biodegradable polymers and sirolimus was developed by using an ultrasonic nanocoater and characterized in aspects of surface smoothness and coating thickness. In addition, in vitro release profiles of sirolimus by changing top coating layer with different biodegradable polymers were investigated. Smooth surfaces with variable thickness could be fabricated by optimizing polymer concentration, flow rate, nozzle-tip distance, gas pressure, various solvents and ultrasonic power. Smooth surface could be generated by using volatile solvents (acetone, chloroform, and methylene chloride) or post-treating with solvent vapor. Coating thickness could be controlled by varying injection volume or polymer concentration, and higher concentration could reduce the coating time while obtaining the same thickness. The thickness measurement was the most effectively performed by a conventional cutting method among three different methods that were investigated in this study. Release profiles of sirolimus were effectively controlled by changing polymers for top layer. PLGA made the release rate 3 times faster than PDLLA and PLLA and all top layers prevented burst release at the initial phase of profiles. Our results will provide useful and informative knowledge for developing drug-eluting stents, especially coated with biodegradable polymers.

Fabrication and Pore Characteristics of Cu Foam by Slurry Coating Process

  • Park, Dahee;Jung, Eun-Mi;Yang, Sangsun;Yun, Jung-Yeul
    • Journal of Powder Materials
    • /
    • v.22 no.2
    • /
    • pp.87-92
    • /
    • 2015
  • Metallic porous materials have many interesting combinations of physical and geometrical properties with very low specific weight or high gas permeability. In this study, highly porous Cu foam is successfully fabricated by a slurry coating process. The Cu foam is fabricated specifically by changing the coating amount and the type of polyurethane foam used as a template. The processing parameters and pore characteristics are observed to identify the key parameters of the slurry coating process and the optimized morphological properties of the Cu foam. The pore characteristics of Cu foam are investigated by scanning electron micrographs and micro-CT analyzer, and air permeability of the Cu foam is measured by capillary flow porometer. We confirmed that the characteristics of Cu foam can be easily controlled in the slurry coating process by changing the microstructure, porosity, pore size, strut thickness, and the cell size. It can be considered that the fabricated Cu foams show tremendous promise for industrial application.

Studies on Rheological Properties of High Solid Coating Colors(Part 2) - Effect of Rheology Modifiers on High-Shear Viscosity and Dynamic Penetration Behavior - (고농도 도공액의 유동특성에 관한 연구(제2보) - 유동성 조절제가 고전단 점도 및 동적 침투특성에 미치는 영향 -)

  • Yoo, Sung-Jong;Cho, Byoung-Uk;Lee, Yong-Kyu
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.43 no.3
    • /
    • pp.121-127
    • /
    • 2011
  • This study used two types of rheology modifiers including an alkali-swellable emulsion (ASE) and an surface-adhesion emulsion (SAE) to elucidate their effects on high shear viscosity and dynamic penetration behavior among the flow properties of high solids coating. Since rheology under high shear and dynamic penetration behavior significantly affect the quality of coated paper in case of high solids coating, it is very important to examine the variations in rheology of high solids coating color by rheology modifier. It was found that the high solids coating color prepared with the SAE type showed superior dynamic penetration behavior and high shear viscosity than that with the ASE type rheology modifier.

The noble method for superhydrophobic thin film coating

  • Seo, Hyeon-Uk;Kim, Gwang-Dae;Jeong, Myeong-Geun;Kim, Dong-Un;Kim, Myeong-Ju;;Kim, Yeong-Dok;Im, Dong-Chan;Lee, Gyu-Hwan;Eom, Seong-Hyeon;Lee, Jae-Yeong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.496-496
    • /
    • 2011
  • A very simple and cost-effective method for fabrication of SiOx-incorporated diamond-like carbon (DLC) thin films at a preparation temperature of less than $200^{\circ}C$ was developed. Since DLC coating can be prepared not under vacuum but atmospheric conditions without any carrier gas flow, not only wafers but also powderic substrates can be used for DLC coating. Formation of DLC coating could result in appearance of superhydrophobic behaviors, which was sustained in a wide range of pH (1~14). DLC-coated surfaces selectively interacted with toluene in a toluene/water mixture. These results imply that our preparation method of the DLC coating can be useful in many application fields such as creating self-cleaning surfaces, and water and air purification filters.

  • PDF

Fiber network with superhydrophilic Si-DLC coating

  • Kim, Seong-Jin;Mun, Myeong-Un;Lee, Gwang-Ryeol;Kim, Ho-Yeong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.363-363
    • /
    • 2010
  • The high capillarity of a plastic fiber network having superhydrophilic Si-DLC coating is studied. Although the superhydrophilic surface maximize wetting ability on the flat surface, there remains a requirement for the more wettable surface for various applications such as air-filters or liquid-filters. In this research, the PET non-woven fabric surface was realized by superhydrophilic coating. PTE non-woven fabric network was chosen due to its micro-pore structure, cheap price, and productivity. Superhydrophobic fiber network was prepared with a coating of oxgyen plasma treated Si-DLC films using plasma-enhanced chemical vapor deposition (PECVD). We first fabricated superhydrophilic fabric structure by using a polyethylene terephthalate (PET) non-woven fabric (NWF) coated with a nanostructured films of the Si-incorporated diamond-like carbon (Si-DLC) followed by the plasma dry etching with oxygen. The Si-DLC with oxygen plasma etching becomes a superhydrophilic and the Si-DLC coating have several advantages of easy coating procedure at room temperature, strong mechanical performance, and long-lasting property in superhydrophilicity. It was found that the superhydrophobic fiber network shows better wicking ability through micro-pores and enables water to have much faster spreading speed than merely superhydrophilic surface. Here, capillarity on superhydrophilic fabric structure is investigated from the spreading pattern of water flowing on the vertical surface in a gravitational field. As water flows on vertical flat solid surface always fall down in gravitational direction (i.e. gravity dominant flow), while water flows on vertical superhydrophilic fabric surface showed the capillary dominant spreading.

  • PDF

Enhanced Wear Resistance of Cutting Tools Using Multilayer ta-C Coating (다층막 ta-C 코팅 적용을 통한 절삭공구의 내마모성 향상)

  • Kim, Do Hyun;Kang, Yong-Jin;Jang, Young-Jun;Kim, Jongkuk
    • Journal of the Korean institute of surface engineering
    • /
    • v.53 no.6
    • /
    • pp.360-368
    • /
    • 2020
  • Wear resistance of cutting tools is one of the most important requirements in terms of the durability of cutting tool itself as well as the machining accuracy of the workpiece. Generally, tungsten carbide ball end mills have been processed with hard coatings for high durability and wear resistance such as diamond coating and tetrahedral amorphous carbon(ta-C) coating. In this study, we developed multilayer ta-C coatings whose wear resistance is comparable to that of diamond coating. First, we prepared single layer ta-C coatings according to the substrate bias voltage and Ar gas flow, and the surface microstructure, raman characteristics, hardness and wear characteristics were evaluated. Then, considering the hardness and wear resistance of the single layer ta-C, we fabricated multilayer coatings consisting of hard and soft layers. As a result, it was confirmed that the wear resistance of the multilayer ta-C coating with hardness of 51 GPa, and elastic recovery rate of 85% improved to 97% compared to that of the diamond coated ball end mill.

Aerosol Deposition Nozzle Design for Uniform Flow Rate: Divergence Angle and Nozzle Length

  • Kim, Jae Young;Kim, Young Jin;Jeon, Jeong Eun;Jeon, Jun Woo;Choi, Beom Soo;Choi, Jeong Won;Hong, Sang Jeen
    • Journal of the Semiconductor & Display Technology
    • /
    • v.21 no.2
    • /
    • pp.38-44
    • /
    • 2022
  • Plasma density in semiconductor fabrication equipment becomes higher to achieve the improved the throughput of the process, but the increase of surface corrosion of the ceramic coated chamber wall has been observed by the increased plasma density. Plasma chamber wall coating with aerosol deposition prefer to be firm and uniform to prevent the potential creation of particle inside the chamber from the deformation of the coating materials, and the aerosol discharge nozzle is a good control factor for the deposited coating condition. In this paper, we investigated the design of the nozzle of the aerosol deposition to form a high-quality coating film. Computational fluid dynamics (CFD) study was employed to minimize boundary layer effect and shock wave. The degree of expansion, and design of simulation approach was applied to found out the relationship between the divergence angle and nozzle length as the key parameter for the nozzle design. We found that the trade-off tendency between divergence angle and nozzle length through simulation and quantitative analysis, and present the direction of nozzle design that can improve the uniformity of chamber wall coating.

Coater Die Design and Coating Quality Evaluation in the Machine Direction of Slot Coating Through Computer Simulation (컴퓨터 해석을 통한 Slot 코팅공정에서 운전방향의 코팅품질 평가 및 다이 설계)

  • Kim, T.H.;Lee, D.Y.;Sung, D.J.;Lyu, M.Y.
    • Elastomers and Composites
    • /
    • v.48 no.4
    • /
    • pp.282-287
    • /
    • 2013
  • Slot coating has been widely spread in photo resist coating on glass for flat display monitor. High quality of coating is required as high quality of image in display is needed. Coating quality in the slot coating is divided into nozzle direction quality and machine direction quality. Nozzle direction quality is related to flow uniformity inside the die whereas machine direction quality is related to die lip design and operational conditions. In this study coating uniformity in the machine direction of slot coating has been investigated through computer simulation. Die lip angle and die lip length were considered as outside die geometry and coating speed was considered as operational condition. Coating behavior has been analyzed and coating quality has been evaluated through computer simulation. Coating thickness decreased and coating uniformity increased as coating speed increased. However, the stability of meniscus formation was reduced and subsequently coating stability was reduced as coating speed increased. Coating thickness deviation decreased as die lip angle increased in down stream die. Coating thickness decreased and time to reaching steady state increased as increased die lip length in down stream die.

Development of two-component polyurethane metering system for in-mold coating (인몰드 코팅을 위한 2액형 폴리우레탄 공급장치 개발)

  • Seo, Bong-Hyun;Lee, Ho-Sang
    • Design & Manufacturing
    • /
    • v.10 no.2
    • /
    • pp.18-23
    • /
    • 2016
  • Injection molded thermoplastic parts may need to be coated to facilitate paint adhesion, or to satisfy other surface property requirements, such as appearance, durability, and weather resistance. In this paper, a two-component polyurethane metering system was developed for the simultaneous injection and surface coating of a plastic substrate. The system was composed of storage tanks, feed pumps, axial piston pumps, mixing head. The tank was designed to be double-jacket structured and fabricated for polyol and isocyanate, respectively. A temperature chamber was used to maintain the material temperature to be $80^{\circ}C$ during flowing from storage tank to mixing head. Inside the chamber, feed pump, low pressure filter, high pressure pump, high pressure filter, pressure sensor, flow meter were installed. A mixing head of L-type was used for homogeneous mixing of polyol and isocyanate. Inside the mixing head, a cartridge heater and a temperature sensor were installed to control the temperature of the materials. The flow rate of axial-piston pump was controlled by using closed-loop feedback control algorithm. The input flow-rates were compared with the measured values. The output error was 6.7% for open-loop control, whereas the error was below 2.2% for closed-loop control. In addition, the pressure generated through mixing-head nozzle increased with increasing flow rate. It was found that the pressure drop between metering pump and mixing-head nozzle was almost 10 bar.