• 제목/요약/키워드: Co-Based alloy

검색결과 248건 처리시간 0.033초

분말야금 및 주조형 니켈기 초내열합금 크리프 신뢰성의 초음파 모니터링 (Evaluation of Creep Reliability of Powder Metallurgy and Cast-type Ni-based Superalloy by Using Ultrasonic Wave)

  • 최찬양;송진헌;오세웅;김정석;권숙인;오승탁;현창용;변재원
    • 한국분말재료학회지
    • /
    • 제19권3호
    • /
    • pp.215-219
    • /
    • 2012
  • An attempt was made to evaluate creep reliability of two commercial Ni-based superalloys by using ultrasonic wave. The materials include fine-grained PM alloy fabricated by mechanical alloying and subsequent hot isostatic pressing, and IN738LC cast alloy with a grain size of a few cm. Microstructural parameters (fraction of creep cavity and size of ${\gamma}^{\prime}$ precipitates) and ultrasonic parameters (velocity, attenuation) were measured to try to find relationships between them. Ultrasonic velocity decreased with creep cavity formation in PM alloy. On the other hand, no distinct changing trend of ultrasonic velocity was observed for IN738LC alloy. Ultrasonic attenuation was found to have a linear correlation with the size of ${\gamma}^{\prime}$ precipitates and was suggested as a potential parameter for monitoring creep reliability of IN738LC alloy.

Fe-Si 전기강판 폐스크랩을 이용한 3원계 Fe-9.8Si-6.0Al 합금의 연자성 특성 (Soft Magnetic Property of Ternary Fe-9.8Si-6.0Al Alloy Using by Recycling Fe-Si Electrical Steel Sheet Scrap)

  • 홍원식;양형우;박지연;오철민;이우성;김승겸;한상조;심금택;김휘준
    • 마이크로전자및패키징학회지
    • /
    • 제24권1호
    • /
    • pp.1-8
    • /
    • 2017
  • Fe-9.8Si-6.0Al mother alloy was manufactured using by Fe-3.5Si recycled scrap and Si powder. And then, soft magnetic alloy powder of $D_{50}$ size and sphere type were prepared by gas atomization process. To obtain the soft magnetic powder of a high aspect ratio, in the first, we conducted the ball milling process for 8 hours. And heat treatment was performed under $650^{\circ}C$, 2 hours and $N_2$ atmosphere condition for reducing the residual stress of the powder. Based on these process, we made around $50{\mu}m$ diameter Fe-9.8Si-6.0Al powder, which morphology and shape was a similar to the commercial Fe-Si-Al powder. Finally, the soft magnetic sheets were prepared by tape casting process using by those powders. The permeability of the tape casting sheet was measured, and we confirmed the possibility of reusing to the soft magnetic materials of Fe-Si electric sheet scrap.

초음파 볼밀링 공정에 의한 용매 점도 특성에 따른 텅스텐계 합금 분쇄 거동 (Investigation on Size Distribution of Tungsten-based Alloy Particles with Solvent Viscosity During Ultrasonic Ball Milling Process)

  • 류근혁;소형섭;윤지석;김인호;이근재
    • 한국분말재료학회지
    • /
    • 제26권3호
    • /
    • pp.201-207
    • /
    • 2019
  • Tungsten heavy alloys (W-Ni-Fe) play an important role in various industries because of their excellent mechanical properties, such as the excellent hardness of tungsten, low thermal expansion, corrosion resistance of nickel, and ductility of iron. In tungsten heavy alloys, tungsten nanoparticles allow the relatively low-temperature molding of high-melting-point tungsten and can improve densification. In this study, to improve the densification of tungsten heavy alloy, nanoparticles are manufactured by ultrasonic milling of metal oxide. The physical properties of the metal oxide and the solvent viscosity are selected as the main parameters. When the density is low and the Mohs hardness is high, the particle size distribution is relatively high. When the density is high and the Mohs hardness is low, the particle size distribution is relatively low. Additionally, the average particle size tends to decrease with increasing viscosity. Metal oxides prepared by ultrasonic milling in high-viscosity solvent show an average particle size of less than 300 nm based on the dynamic light scattering and scanning electron microscopy analysis. The effects of the physical properties of the metal oxide and the solvent viscosity on the pulverization are analyzed experimentally.

Mechanical Properties and Microstructure of Aluminum Alloys with Dispersed Nanoscale Quasicrystalline Particles

  • Fujita, Masashi;Kimura, Hisamichi;Inoue, Akihisa
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.708-709
    • /
    • 2006
  • New Al-based alloys with very high ultimate tensile strength were developed in high Al concentration range of 91-95 at.% for Al-Fe-Cr-Ti-M (M: Co and Mo) systems and Al-Fe-Cr-Mo-Ti-Co system by the dispersion of nanoscale quasicrystalline particles in Al phase. The effect of adding elements, M was discussed in the viewpoint of stability of super-cooled liquid state and formation ability of quasicrystalline phase. The P/M Al-Fe-Cr-Ti-M alloys with dispersed nanoscale quasicrystalline particles exhibited ultimate tensile strength of 350MPa at 573K and 200MPa at 673K.

  • PDF

기체분무형 공정으로 제조된 Zr계 금속수소화물의 수소화반응 및 Ni-MH 2차전지 전극 특성에 관한 연구 (Hydrogneation and Electrochemical Characteristics of Gas-atomized Zr-based $AB_2$ Hydride for Ni-MH Secondary Battery)

  • 김진호;황광택;김병관;한정섭
    • 한국수소및신에너지학회논문집
    • /
    • 제20권6호
    • /
    • pp.505-511
    • /
    • 2009
  • The hydriding and electrochemical characteristics of Zr-based $AB_2$ alloy produced by gas atomization have been extensively examined. For the particle morphology of the as-cast and gas-atomized powders, it can be seen that the mechanically crushed powders are irregular, while the atomized powder particles are spherical. The increase of jet pressure of gas atomization process results in the decrease of hydrogen storage capacity and the slope of plateau pressure significantly increases. TEM and EDS studies showed the increase of jet pressure in the atomization process accelerated the phase separation within grain of the gas-atomized alloy, which brought about a poor hydrogenation property. However, the gas-atomized $AB_2$ alloy powders produced by jet pressure of 50 bar kept up the reversible $H_2$ storage capacity and discharge capacity similar to the mechanically crushed particles. In addition, the electrode of gas-atomized Zr-based $AB_2$ alloy of 50 bar showed improved cyclic stability over that of the cast and crushed particulate, which is attributed to the restriction of crack propagation by grain boundary and dislocation with ch/discharging cycling.

Magnetostrictive Properties of Polymer-Bonded Fe-Co Based Alloy Composites

  • S. M. Na;S. J. Suh;K. H. Shin;Lee, Y. S.;S. H. Lim
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 2002년도 동계연구발표회 논문개요집
    • /
    • pp.138-139
    • /
    • 2002
  • Polymer-bonded magnetostrictive composites have some distinct advantages over conventional type materials in being cost effective and suitable for high frequency applications due to high electrical resistivity. Composites of rare earth based alloys were reported to show good magnetostrictive characteristics both in static and dynamic conditions [1]. It was originally thought that the application of the polymer-bonding technique to transition metal alloys is straightforward. (omitted)

  • PDF

Pd 코팅된 Zr기 비정질 합금의 수소취성 및 표면특성 (Hydrogen Embrittlement and Surface Properties of Pd-coated Zr-based Amorphous Alloys)

  • 석송;이덕영;김기배
    • 한국수소및신에너지학회논문집
    • /
    • 제18권2호
    • /
    • pp.182-188
    • /
    • 2007
  • [ $Zr_{50}-Ni_{27}-Nb_{18}-Co_5$ ] amorphous alloys ribbon was prepared by a single-roller melt-spinning technique. In order to improve the hydrogen kinetics Pd-coating were carried out on each side of the amorphous ribbon. Pd prevents oxidation of Zr and catalyses the dissociation of molecular hydrogen to atomic hydrogen. In this work, the hydrogen embrittlement and surface properties on Zr-based amorphous alloys were investigated. The Zr-based amorphous alloys were characterized by X-ray diffractometry(XRD) and differential scanning calorimetry(DSC). The morphology of surface and roughness was observed by using scanning electron microscopy(SEM) and atomic force microscopy (AFM). A lattice parameter of both Pd and Zr-based amorphous alloy was increased after hydrogen permeation at 473 K. After hydrogen permeation at 473 K, some cracks were observed on the surface of Pd, which was the cause for the hydrogen embrittlement. The crystallization temperature of Zr-based amorphous alloy was decreased due to the permeated hydrogen.

도재용착용 Ni-Cr계 합금의 이트륨 첨가물이 도재전단결합강도에 미치는 영향 (Effect of yttrium additives on the shear bond strength of porcelain fused to Ni-Cr alloy for porcelain fused metal crown)

  • 우제승;노세라;노형록;임청하;이정환
    • 대한치과기공학회지
    • /
    • 제41권2호
    • /
    • pp.71-80
    • /
    • 2019
  • Purpose: In this study, to evaluate the effect of oxide changes on the shear bond strength according to the composition of Ni-Cr alloys for porcelain fused matal crown, T-4 alloys, Zeroy alloys and Zeroy-X alloys were selected. Methods: 20 specimens were fabricated using selected Ni-Cr alloys and porcelain powders. A Ni-Cr alloy having a diameter of 5 mm and a height of 25 mm was produced and the metal surface was polished. Porcelain powder was fired on the polished metal surface to a diameter of 5 mm and a height of 3 mm. The experiment group consisted of three groups, T-4(TNA), Zeroy(ZNA) and Zeroy-X(ZXA). The fabricated specimens were mounted on a jig of a universal testing machine(UTM) and fracture strength was measured by applying a shear force at a UTM crosshead speed of 0.5 mm/min. The fracture strength was calculated as the bond strength between the porcelain and the alloy. The surface of the fractured alloy was analyzed by X-ray diffraction(XRD) and scanning electron microscopy(SEM), and the components of the oxide were measured by energy dispersive X-ray spectroscopy(EDX) line profile method. Results: In SEM, XRD and EDX analysis, yttrium tended to increase the mechanical and chemical bonding forces. The shear bond strength of ZXA group containing yttrium showed the highest value at 27.53 MPa. Conclusion: Based on the results of this study, it is considered that the yttrium-added Ni-Cr alloy is clinically acceptable in porcelain shear bond strength.

베릴륨(Be)이 미 첨가된 치과도재소부용 Ni-Cr-Mo계 합금의 미세조직 및 기계적 성질 특성 (Microstructures and Mechanical Properties of Beryllium(Be)-free Ni-Cr-Mo based Alloys for Metal-Ceramic Crown)

  • 송경우;고은경;이정환;정종현;노학;한재익
    • 대한치과기공학회지
    • /
    • 제28권2호
    • /
    • pp.321-329
    • /
    • 2006
  • The popularity of Ni-Cr-Mo based metal alloys for metal-ceramic crown have increased recently because of low price, superior yield strength and rigidity. the use of these alloys give them the potential advantage of thinner copping with the required rigidity for long span bridges. The purpose of this study was to assess the microstructures and mechanical properties of Ni-Cr-Mo-(Si,Al,Nb,Zr,Ti.Cu,Mm) based Alloys not containing beryllium(Be) related toxic effects. The abtained results indicated that as-cast these specimen alloys showed compositional and microstructural differences, and mechanical properties values of Ni69Cr20Mo5Si2Al4 alloy among these specimen alloys was found to be superior to those of commercial Ni-Cr based alloy using in market place today.

  • PDF

고강도 Al-Zn기 다이캐스팅 합금개발에 관한 연구 I (A Study of the Development of a High-Strength Al-Zn Based Alloy for Die Casting I)

  • 신상수;염길용;김억수;임경묵
    • 대한금속재료학회지
    • /
    • 제48권10호
    • /
    • pp.936-941
    • /
    • 2010
  • Al-Zn based alloys are the most common types of wrought Al alloys. Although Al-Zn alloys have high strength, they cannot be applied to a conventional casting process. In this study, Al-Zn-based alloys applicable to a die casting process were developed successfully. The developed Al-45 wt% Zn-based alloys showed a fine equiaxed grain structure and high strength. A fine equiaxed grain having an average size of $25{\mu}m$ was obtained by the die casting process. The UTS and elongation of the new alloy are 475 MPa and ~3.5%, respectively. In addition, we elucidate the effect of a Zn addition on variations in different mechanical properties and the microstructure characteristics of (Al96.3-xZnxCu3Si0.4Fe0.3) x=20, 30, 40, and 45 wt% alloys fabricated by a die casting process.