Synthesis of Diamond Thin Film on WC-Co by RF PACVD (RF PACVD에 의한 초경합금상에 다이아몬드 박막의 합성)

  • Kim, Dae-Il;Lee, Sang-Hee;Park, Gu-Bum;Park, Sang-Hyun;Lee, Yong-Geun;Kim, Bo-Youl;Kim, Young-Bong;Lee, Duck-Chool
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.49 no.11
    • /
    • pp.596-602
    • /
    • 2000
  • Diamond thin films were synthesized on WC-Co substrate at various experimental parameters using 13.56MHz RF PACVD)radio frequency plasma-assisted chemical vapor deposition). In order to increased the nucleation density, the WC-Co substrate was polished with 3${\mu}m$ diamond paste. And the WC-Co substrate was preatreated in $HNO_3\;:\;H_2O$ = 1:1 and $O_2$ plasma. In $H_2-CH_4$ gas mixture, the crystallinity of thin film increased with decreasing $CH_4$ concentration at 800W discharge power and 20torr reaction pressure. In $H_2-CH_4-O_2$ gas mixture, the crystallinity of thin film increased with increasing $O_2$ concentration at 800W discharge power, 200torr reaction pressure and 4% $CH_4$ concentration.

  • PDF

Thickness-Driven Spin Reorientation Transition in Co/Pd(111) : In Situ SMOKE Three-Dimensional Vector Magnetometry

  • Lee, Jeong-Won;Kim, Sang-Koog;Kim, Jonggeol;Jeong, Jong-Ryul;Ahn, Jae-Seok;Shin, Sung-Chul
    • Journal of Magnetics
    • /
    • v.6 no.2
    • /
    • pp.53-56
    • /
    • 2001
  • We have developed a three-axis configurational in situ SMOKE apparatus by which three-dimensional vector magnetization reversal processes are studied for ultrathin Co films grown on a Pd (111) single crystal in the thickness range of spin reorientation transition. This study provides a better understanding of magnetization reversal motions with the knowledge of three components of the magnetization vector at the transition of an easy axis of magnetization from the film normal at 5 ML Co to in-plane at 6 ML Co (ML denotes monolayer). For a 5.25 ML Co, it was observed that a slightly canted magnetization vector from the film normal rotated in the film plane under an applied field direction parallel to the film normal.

  • PDF

Oil Film Thickness Measurement of Engine Bearing and Cam/tappet Contact in an Automotive Engine

  • Choi, Jae-Kwon;Min, Byung-Soon;Han, Dong-Chul
    • Tribology and Lubricants
    • /
    • v.11 no.5
    • /
    • pp.71-77
    • /
    • 1995
  • The capacitance technique was used to measure the minimum oil film thickness in engine bearing and the central oil film thickness between cam and tappet. This method is based on the measurement of total capacitance of oil film. For the measurement of the oil film thickness between cam and tappet, two surfaces were assumed to be flat and parallel within the Hertzian region and all the measured capacitance originated from this region. Shear rates from the measured minimum oil film thickness are over 10$^{6}$ sec$^{-1}$ in the greater part in both two cases. The minimum oil film thickness in engine bearing is larger than the surface roughness. Between cam and tappet it is mostly smaller than the surface roughness. In spite of the awkward restriction of the reliability of measured oil film thickness, it was known that the capacitance technique makes it possible to measure the oil film thickness in elastohydrodynamic and mixed lubrication regimes as well as in hydrodynamic regime. Therefore, it is also possible to classify the lubrication regimes based on the oil film thickness.

TAC Film as a Key Component for LCDs

  • Mori, Hiroyuki
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2005.07b
    • /
    • pp.1071-1074
    • /
    • 2005
  • TAC film is an indispensable optical component that protects the polarizing PVA (polyvinyl alcohol) film from being deteriorated and gives high durability, due to its unique features. The newly developed technology of controlling the birefringence of TAC film, together with the coating technology of a discotic material layer, enables excellent viewing angle characteristics and a cost-effective roll-to-roll polarizer manufacturing process.

  • PDF

Crystalline Qualities and Surface Morphologies of As-Grown $YBa_2Cu_3O_{7-x}$ Thin Films on MgO(100) Substrate by Reactive Coevaporation Method (반응성 동시 증착법에 의한 As-grown $YBa_2Cu_3O_{7-x}$ 박막의 결정 특성 및 표면형상에 관한 연구)

  • Jang, Ho-Yeon;Watanabe, Yasuhiro;Doshida, Yutaka;Shimizu, Kenji;Okamoto, Yoichi;Akibama, Ryozo;Song, Jin-Tae
    • Korean Journal of Materials Research
    • /
    • v.1 no.2
    • /
    • pp.93-98
    • /
    • 1991
  • The as-grown $YBa_2Cu_3O_{7-x}$ superconducting thin films on MgO(100) substrate have been prepared by a reactive coevaporation method. The superconducting transition temperature, surface morphology and crystalline quality were examined as a function of the substrate temperature ranging from $450^{\circ}C$ to $590^{\circ}C$. From the reflection high energy electron diffraction (RHEED) analysis, it was found the film consisted of almost amorphous phase with a halo pattern deposited at the substrate temperature of $450^{\circ}C$. The film deposited at the substrate temperature of $510^{\circ}C$ consisted of polycrystalline phase, showing a broad ring pattern. On the other hand, for the film deposited at $590^{\circ}C$, RHEED showed spotty pattern indicating that this film consisted of single crystal phase. It has rough film surface due to the surface outgrowth. The surface outgrowth increased as the substrate temperature increased from $510^{\circ}C$ to $590^{\circ}C$. the surface outgrowth may be due to the anisotropic growth rate. The highest transition temperature obtained in this study was $Tc_{zero}$ of 83K with $Tc_{onset}$ of 88K for the film deposited at $590^{\circ}C$ using activated RF oxygen plasma.

  • PDF

Characteristics of the ZnTe solar cell by the co-sputtering methods (Co-sputtering법으로 제작한 ZnTe 태양전지의 특성)

  • 장유진;김성우;최혁환;이명교;권태하
    • Journal of the Korea Institute of Information and Communication Engineering
    • /
    • v.8 no.2
    • /
    • pp.440-448
    • /
    • 2004
  • In this paper, to make a solar cell of II-Ⅵ ZnTe compound semiconductor, we studied for the property of the transparent electrode(AZO) and Buffer layer(ZnO), and for reducing the energyband gap of optical absorber layer which are most effective on its efficiency. The ZnTe thin film was used the optical absorber layer of solar cell. Zn and Te were deposited using the co-sputtering method. The thin film was sputtered RF power of Zn/50W and Te/30W, respectively and a substrate temperature of foot under Ar atmosphere of 10mTorr. The energy band gap of the thin film was 1.73ev Then the thin film was annealed at $400^{\circ}C$ for 10sec under a vacuum atmosphere. The energy band gap of 1.67eV was achieved and the film composition ratio of Zn and Te was 32% and 68%. At the best condition, the Solar Cell was manufactured and the efficiency of 6.85% (Voc: 0.69V, Jsc: 21.408㎃/$cm^2$, Fill factor (FF): 0.46) was achieved.

The Crystallization of Polycarbonate Film Using Methylene Chloride/1,3-Dioxolane as a Solution Casting Co-Solvent (Methylene Chloride/1,3-Dioxolane 혼합 용매에 의한 용액 가공 폴리카보네이트 필름의 결정화)

  • Kim, Whan-Ki;Kim, Jae-Hyun;Kim, Sung-Do;Han, Joon-Hee;Kang, Ho-Jong
    • Polymer(Korea)
    • /
    • v.32 no.5
    • /
    • pp.483-488
    • /
    • 2008
  • The effect of methylene chloride/1,3-dioxolane co-solvent on the crystallization in the optical polycarbonate film was investigated. Increasing 1,3-dioxolane content in co-solvent resulted in the crystallization due to the lowering of solvent evaporation rate during film drying process. The crystallization in PC film could be minimized by either controlling of solvent composition and increasing solvent drying temperature. It was found that the surface roughness of solution casting PC film was affected by both crystallization and solvent evaporation rate. This morphological effect by alternative solvent is ascribed to a large decrease in light transmissivity on the optical PC film.

Packaging technology of fresh-cut produce (신선편의식품 포장기술)

  • Kim, Ji Gang
    • Food Science and Industry
    • /
    • v.50 no.2
    • /
    • pp.12-26
    • /
    • 2017
  • Processing steps such as washing and cutting, involved in preparing fresh-cut produce causes tissue damage, leading to rapid quality deterioration. Major defects of fresh-cut produce are discoloration, softening, off-odor development, and microbial growth. Packaging of fresh-cut produce has been changed to reduce these quality problems. Flexible packaging film is widely used to pack fresh-cut produce. Vacuum packaging was the popular packaging method in the beginning of fresh-cut industry in Korea. Vacuum packaging creates high $CO_2$ and low $O_2$ levels to control browning of fresh-cut produce. However, these conditions induce some visual defects and off-odor development. Discoloration problem was also found when fresh-cut produce was packaged with conventional packaging film or plastic tray. Modified atmosphere (MA) packaging is effective for prolonging shelf-life of fresh-cut produce by decreasing $O_2$ and increasing $CO_2$ concentration in the package. Retail MA packaging using different oxygen transmission rate (OTR) film and micro-perforated film has started to be applied to fresh-cut produce in Korea. Proper MA package design that provides optimum range of $O_2$ and $CO_2$ partial pressures is one of the major challenges in the industry. An initial package flushing with $N_2$ or an low $O_2$/high $CO_2$ atmosphere is also used to more rapidly establish steady-state MA condition. Film OTR and $O_2$ flushing affects the fermentative volatile production, off-odor development, electrolyte leakage, discoloration, $CO_2$ injury, microbial population of fresh-cut produce. There is also a demand for convenient packaging to attract consumers. Rigid fresh-cut produce container for retail market has increased since the packaging provides excellent protection from physical damage during transport. Rigid tray used as actual serving vessel for the consumer is increasing in Korea. The tray with flexible lid to wrap or seal fresh-cut produce is more and more gaining popularity. Further practical technology to control quality change and microbial growth for each fresh-cut product has been studied since various fresh-cut items were required. The fresh-cut industry also focuses on searching for more convenient and environmentally friendly packaging.

Biaxial integrated optical film for VA mode LCD's made from in-situ photopolymerised reactive mesogens.

  • Kim, Kyeong-Hyeon;Lyu, Jae-Jin;Chung, Dong-Hoon;Verrall, M.;Slaney, K.;Perrett, T.;Parri, O.;Lee, Seung-Eun;Lee, Hee-Kyu
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2004.08a
    • /
    • pp.773-775
    • /
    • 2004
  • For high end, large area displays, all current LC modes require some degree of optical compensation to improve the front of screen viewing experience. Currently most optical films are laminated to the outside of the LCD cell, between the glass and polariser. In this paper we wish to show how it is possible to integrate the compensating optical film within a VA mode LCD cell. The paper will describe the process of making the biaxial film through the process of in-situ photopolymerisation of an aligned film of reactive mesogens in the cholesteric phase using polarised UV light. The film can be made on the colour filter array side of the LCD panel. In addition the process of fabricating a VA mode LCD containing this film will be described and the performance of this module will be presented

  • PDF

Antioxidant Packaging as Additional Measure to Augment CO2-enriched Modified Atmosphere Packaging for Preserving Infant Formula Powder

  • Jo, Min Gyeong;An, Duck Soon;Lee, Dong Sun
    • KOREAN JOURNAL OF PACKAGING SCIENCE & TECHNOLOGY
    • /
    • v.26 no.1
    • /
    • pp.19-23
    • /
    • 2020
  • Al-laminated packaging film incorporating ascorbic acid or tocopherol at inner food contact layer was tested in the potential to improve antioxidative preservation of powdered infant formula under CO2-enriched atmosphere. Product of 200 g was packaged with the packaging film containing 0.3% antioxidant in sealant layer of low density polyethylene and stored at 30℃ for 286 days with periodic measurement of package atmosphere and product's quality attributes. The CO2-flushed package resulted in shrinkage of tight contact between the product and the film not allowing gas sampling of package atmosphere after 140 days. Package of tocopherol-incorporated film allowed some ingress of oxygen after 112 days presumably due to its weakening of heat-seal area. The increased oxygen concentration in the tocopherol-added film package led to the concomitant increase of peroxide value, an index of lipid oxidation. On the other hand, packaging of ascorbic acid-added film pouch could suppress lipid oxidation marginally in consistent manner compared to control package without any antioxidant.