Influence of Temperature on Chloride Ion Diffusion of Concrete (콘크리트의 염화물이온 확산성상에 미치는 온도의 영향)

  • So, Hyoung-Seok;Choi, Seung-Hoon;Seo, Chung-Seok;Seo, Ki-Seog;So, Seung-Young
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.1
    • /
    • pp.71-78
    • /
    • 2014
  • The long term integrity of concrete cask is very important for spent nuclear fuel dry storage system. However, there are serious concerns about early deterioration of concrete cask from creaking and corrosion of reinforcing steel by chloride ion because the cask is usually located in seaside, expecially by combined deterioration such as chloride ion and heat, carbonation. This study is to investigate the relation between temperature and chloride ion diffusion of concrete. Immersion tests using 3.5% NaCl solution that were controlled in four level of temperature, i.e. 20, 40, 65, and $90^{\circ}C$, were conducted for four months. The chloride ion diffusion coefficient of concrete was predicted based on the results of profiles of Cl- ion concentration with the depth direction of concrete specimens using the method of potentiometric titration by $AgNO_3$. Test results indicate that the diffusion coefficient of chloride ion increases remarkably with increasing temperature, and there was a linear relation between the natural logarithm values of the diffusion coefficients and the reciprocal of the temperature from the Arrhenius plots. Activation energy of concrete in this study was about 46.6 (W/C = 40%), 41.7 (W/C = 50%), 30.7 (W/C = 60%) kJ/mol under a temperature of up to $90^{\circ}C$, and concrete with lower water-cement ratio has a tendency towards having higher temperature dependency.

The Analysis of Chloride Ion of Ground Water in the West Coast District of Jeollabuk-Do using Spatial Interpolation (공간보간법을 이용한 전라북도 서해안 지역의 지하수 염소이온 분석)

  • Lee, Geun-Sang;Im, Dong-Gil;Choi, Yun-Woong;Cho, Gi-Sung
    • Journal of Korean Society for Geospatial Information Science
    • /
    • v.19 no.4
    • /
    • pp.23-33
    • /
    • 2011
  • In this study, the data that examined the chloride ion concentration of ground water wells in the west coast of Jeollabukdo applying the GIS spatial estimation method were analyzed. In particular, through the designation of a validation point among ground water wells and then the analysis of error characteristics of the chloride ion concentration by each method of IDW (Inverse Distance Weight), Spline, and Kriging Interpolation method which is proper for estimating salt water intrusion was selected. The main conclusion from this study is as follows. First, as a result of analyzing the error characteristics of various spatial estimation methods by using the data from the chloride ion concentration of 485 ground water wells, the IDW method was found to be the most appropriate for estimating chloride ion concentration by salt water intrusion. Second, analyzing the average chloride ion concentration of the targeted regions has revealed that Gunsan-si with the record of $541mg/{\ell}$ did not meet water quality standards even for industrial use. Both Gimje-si and Gochang-gun satisfied drinking water quality standards and Buan-gun with $272mg/{\ell}$ was slightly below the standards for drinking water. Third, concerning the results of analysis according to administrative districts, as the areas adjacent to the west coast such as Daemyeong-dong, Joong-dong, Jangjae-dong and Guemam-dong in Gunsan-si are found to have very high chloride ion concentration, and both Hoehyeon-myeon and Daeya-myeon bounded by the Mankeong river did not meet water quality standards even for industrial use. From these facts, it is concluded that salt water intrusion has a great effect on Gunsan-si generally.

Chloride Ion Penetration Resistance of Slag-replaced Concrete and Cementless Slag Concrete by Marine Environmental Exposure (해양환경 폭로에 의한 슬래그 치환 콘크리트 및 슬래그 콘크리트의 염화물 이온 침투 저항성)

  • Lee, Bo-Kyeong;Kim, Gyu-Yong;Kim, Gyeong-Tae;Shin, Kyoung-Su;Nam, Jeong-Soo
    • Journal of the Korea Concrete Institute
    • /
    • v.29 no.3
    • /
    • pp.299-306
    • /
    • 2017
  • In this research, it was examined chloride ion penetration resistance of slag-replaced concrete and cementless slag concrete considering marine environmental exposure conditions of splash zone, tidal zone and immersion zone. In the design strength of grade 24 MPa, the specimens were tested to determine their compressive strength, scanning electron microscopy images and chloride migration coefficient. Further, chloride ion penetration depth and carbonation depth of specimens exposed to marine environment were measured. Experimental results confirm that chloride migration coefficient of specimens tended to decrease with increasing the replacement ratio of ground granulated blast-furnace slag in accelerated laboratory test. In addition, the specimens exposed to the tidal zone were found to be the greatest chloride ion penetration depth compared to splash zone and immersion zone. On the other hand, the chloride ion penetration depth of the specimens exposed to splash zone tended to increase with increasing the replacement ratio of ground granulated blast-furnace slag in contrast with the results for the tidal zone and immersion zone.

The Effect of Chloride on the Corrosion of Reinforced Concrete (염화물이 철근콘크리트의 부식에 미치는 영향)

  • Kim, Jeong-Sup;Shin, Yong-Seok;Lee, Sul;Kim, Kwang-Seok
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.9 no.2
    • /
    • pp.147-154
    • /
    • 2005
  • It is found that as contents of chloride ion and age increase, area of corrosion also increases. Inare increased to 1035 days from 730 days, slope of increase of corrosion area is greatest. Non-rust inhibitor specimens show corrosion area of 8~35 times more than rust inhibitor specimens and anticorrosive effects by application of rust inhibitor can be confirmed. When chloride ion is not contained, corrosion control effects of steel reinforcing according to increase of thickness are found, but specimens having chloride ion show no regular tend of thickness and corrosion due to complex problems such as reverse diffusion of chloride and test errors.

Aerosol Size Distribution and Composition at Kosan, Cheju Island : Measurements in April 1998 (제주도 고산에서의 에어로솔 입경분포별 조성: 1998년 4월 측정 연구)

  • 김용표;배귀남;지준호;진현철;문길주
    • Journal of Korean Society for Atmospheric Environment
    • /
    • v.15 no.5
    • /
    • pp.677-685
    • /
    • 1999
  • Aerosol mass size distributions were measured at Kosan, Cheju Island in April 1998 and their compositions were analyzed. Microorifice Uniform Deposit Impactor(MOUDI) was used to collect aerosols. Sulfate and ammonium ions were predominatly present at fine mode of the aerosols while nitrate, chloride, and metal ions were mostly at coarse mode. Based on the size distribution of nitrate, it is suggested that most nitrate were from gas to particle conversion on coarse particles. Non-sea salt(nss) fraction of sulfate accounted for more than 90% of total sulfate mass concentration. In general, ion concentrations in this study are lower than those measured at the same site from the previous studies. Ion balance and chloride ion levels indicates that there had been anthropogenic chloride emission sources near to the site during the measurements.

  • PDF

Effects of pH, Alkalinity, Chloride Ion on the Copper Pipe Corrosion (동관에서 pH, 알칼리도, 염소이온이 부식에 미치는 영향)

  • Jo, Kwan-Hyung;Kim, Sun-Il;Woo, Dal-Sik
    • Journal of Environmental Health Sciences
    • /
    • v.33 no.1 s.94
    • /
    • pp.43-48
    • /
    • 2007
  • This study investigated the effects of pH, alkalinity, and chlorine ion which are important water quality impact factors to the corrosion in the simulated distribution system where the copper pipe is affixed. The result shows that pitting index was increased as the alkalinity and chloride ion increase in the distilled water, but there was no relation to pH. Actually the uniform corrosion rate was decreased as the pH increase with the laboratory tap water. In conclusion, it is necessary to control the pH which stands above minimum 7.5 to prevent pitting corrosion in the copper pipe. Consequently, comprehensive research about the effect of lime soda($Ca(OH)_2$) which was used as a coagulation additive in the water treatment plant to pipe corrosion must be accomplished additionally.

Inhibition of Biological Perchlorate Reduction by Nitrate and Oxygen (질산염과 산소에 의한 생물학적 퍼클로레이트 환원의 저해)

  • Choi, Hyeok-Sun
    • Journal of Soil and Groundwater Environment
    • /
    • v.14 no.6
    • /
    • pp.29-34
    • /
    • 2009
  • In this study, a chloride ion probe as a direct measurement for perchlorate reduction was used to determine whether biological perchlorate reduction was inhibited by other electron acceptors ($O_2$ and ${NO_3}^-$) and to investigate competition of electron acceptors for using electron donors. Profiles of chloride production (= perchlorate reduction) in flasks containing perchlorate reducing populations were monitored by a chloride ion probe. Biological reduction of 2 mM perchlorate was inhibited by 2 mM nitrate that chloride production rate was decreased by 30% compared to perchlorate used as the only electron acceptor and chloride production rate was decreased by 70% when acetate was limited. Reduction of 2mM perchlorate was completely inhibited by oxygen at 7~8 mg/L, regardless of acetate excess / limitation.

Determination of Required Cover Depth of Concrete Exposed to Simultaneous Attack of Carbonation and Chloride Ion (중성화와 염소이온의 동시 복합환경에 노출된 콘크리트의 적정 피복두께의 결정)

  • 이창수;윤인석;이규동
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.11a
    • /
    • pp.90-93
    • /
    • 2003
  • The most common deteriorating processes of concrete structures in the world-wide are carbonation and chloride ion. In this paper, chloride profiles of carbonated concrete is predicted to considering two layer composite model, which is based on Fick's 2nd law. From the experimental result on combined deterioration of chloride and carbonation, it was examined that high chloride concentration was built up to 3-5㎜ over depth from carbonation depth. The analytical modeling of chloride diffusion, which was based on the Fick's 2nd law of diffusion, was suggested to depict the relative influence of the carbonation depth.

  • PDF

The Characteristics of Chloride Fixation in Non-Sintering Cement Matrix (비소성 시멘트 경화체내 염화물 고정화 특성)

  • Mun, Kyoung-Ju;Hyoung, Won-Kil;Park, Won-Chun;So, Seung-Young;Soh, Yang-Seob
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.725-728
    • /
    • 2006
  • This research investigates the characteristics of chloride fixation in non-sintering cement(NSC) matrix. NSC was manufactured by adding phosphogypsum and slack lime to granulated blast furnace slag as sulfate and alkali activators. As a result, the concentration of chloride ion in pore solution of NSC-solidified matrix is more low than that of OPC-solidified matrix containing the same chloride content in cement paste. Also, the concentration of chloride ion in pore solution of NSC-solidified matrix is similar with that of BSC-solidified matrix containing the same chloride content in cement paste.

  • PDF

A Study on the Strength Estimation Formular of the Precast Concrete Products Using the Chloride Ion Penetrating Test (염소이온투과시험을 이용한 콘크리트제품의 강도추정에 관한 연구)

  • 장문기;이정재
    • Proceedings of the Korean Society of Agricultural Engineers Conference
    • /
    • 1998.10a
    • /
    • pp.146-149
    • /
    • 1998
  • In this study, the chloride ion penetration test and the compressive strength test should be done simultaneously on the standard cylinder specimen. And from analyzing the data from those tests, a strength estimation equation with high credibility is to be developed.

  • PDF