플라이애쉬 수중불분리성 콘크리트의 내해수성에 관한 염화물 촉진 시험 (An Experimental Study of Chloride Acceleration on the Seawater Resistance of Fly Ash Antiwashout Underwater Concrete)

  • 권중현;김봉익
    • 한국해양공학회지
    • /
    • 제19권6호통권67호
    • /
    • pp.29-34
    • /
    • 2005
  • This paper describes the effect of fly ash replacement on seawater resistance of anti-washout underwater concrete, which was replaced cement by fly ash from $0\%$ to $50\%$. The experimental work was performed to find out the variations of length and weight of specimens, using a chloride acceleration test in $40\^{\circ}$C The results shaw that the admixture using fly ash on an anti-washcout underwater concrete in the sea environment makes it more durable for the attacks of chloride by seawater. Also, the length of specimens of anti-washout underwater concrete, at age 180 days, increased substantially, compared with normal concrete; however, the mixture in which cement was replaced $50\%$ of fly ash shows $93\%$ reduction of the expansion, compared with the normal anti "washout underwater concrete specimen.

염화물 확산 평가를 위한 전기적 실험법의 비교 연구 (Comparison Study on Electric Acceleration Test Method for Estimation of Chloride Diffusion Coefficient)

  • 최윤석;최성하;김명유;양은익;이성태
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.257-260
    • /
    • 2005
  • A general electric acceleration testing method for estimation of chloride diffusion coefficient is RCPT and CTH. Also, this testing methods have merit that reduce the testing time. In this paper, an experimental study is executed to investigate the effect of testing method on coefficient of chloride diffusion and it is compared with RCPT and CTH. According to this experiment results, W/C ratio and testing method influence chloride diffusion coefficient of concrete. As W/C ratio is increased, diffusion coefficient in concrete is also increased. Diffusion coefficient obtained by each testing method show the different values. However, there is no remarkable difference between the two testing method.

  • PDF

코팅재료의 도포 특성에 따른 전기적 촉진을 통한 염해 저항성 평가 (Evaluation of Chloride Resistance with Application Method of Coating Materials Using Electric Acceleration Test)

  • 김명유;양은익;연규석;주명기
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 추계 학술발표회 제17권2호
    • /
    • pp.551-554
    • /
    • 2005
  • The durability of concrete is decreased by various deterioration factors such as a crack, spalling, corrosion. Many repair and rehabilitation methods have been introduced to extend service life of RC structure. An application of coating material is one of repair and rehabilitation methods. However, there is a problem due to reduction of bonding strength and damage of coating material in the case of existed coating material. Thus, this paper is aim to investigate the chloride resistance according to application method of coating material which improve the existed problem. According to the results, it is showed that application of coating material reduces diffusion of chloride into concrete. In special, application of MMA polymer showed the best resistance for chloride attack. However, variation of application method and number of times has a minor effect on chloride diffusion.

  • PDF

콘크리트 구조물의 염해 내구성능 검토를 위한 현장 품질관리 시험법 검토 (Evaluation of Testing Method for Quality Control of Chloride Diffusivity in Concrete under chloride attack environment)

  • 김홍삼;정해문;안태송;김철호;전병섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2008년도 춘계 학술발표회 제20권1호
    • /
    • pp.973-976
    • /
    • 2008
  • 염해환경에 건설되는 콘크리트 구조물은 염소이온과 같은 유해이온이 외부로부터 콘크리트 중으로 침투, 확산하여 철근을 부식시킴으로써 구조물의 내구성을 크게 저하시키기 때문에 구조물의 내구성 평가 또는 설계시 중요한 고려사항이 된다. 현재 설계에서 사용되는 확산계수는 각 나라마다 제시된 근거가 다르므로, 직접 비교 검토하는 것이 곤란할 뿐만 아니라 동일 환경조건에서 동일 배합의 콘크리트에 대한 수명예측 결과가 크게 상이한 결과를 초래하게 된다. 본 연구는 염해환경하 콘크리트의 염해 내구성능 품질관리를 적용하기 위해서 현장에서 적용할 수 외국에서 규격화된 시험방법들을 비교 검토하고 이들 시험 방법 가운데 품질관리에 적합한 시험방법을 선정하여 재령별 확산 특성과 침지 시험 결과를 비교하여 분석하였다. 슬래그 미분말을 혼입한 콘크리트의 경우 침지시험(NT Build 443)과 촉진시험(NT Build 492)의 상관성을 분석한다면, 이들 토대로 콘크리트 배합의 품질관리 기준 확산계수를 도출할 수 있을 것으로 판단된다.

  • PDF

전기 영동법에 기초한 콘크리트의 급속 염소이온 확산 특성 평가 (Rapid Chloride Penetration Test for Concrete Based on the Electrochemical Method)

  • 오상균;박동천
    • 한국항해항만학회지
    • /
    • 제34권10호
    • /
    • pp.787-792
    • /
    • 2010
  • 콘크리트는 물시멘트비에 상응하는 공극을 가지게 되며, 공극을 통한 염소이온의 확산을 평가하기 위하여 해안가 폭로 및 해수 침지실험이 널리 사용된다. 이상의 실험은 경우에 따라서 다년간의 시간을 요하는 경우도 있어, 최근에는 전기 영동법에 기초한 급속 염소이온 확산시험을 실시하는 경우가 많으나, 그 값이 폭로 및 침지 시험에서 얻은 값과 상이한 경우가 많아 데이터의 실용성을 높이기 위하여 그 원인 규명이 절실한 실정이다. 본 연구에서는 평가 방법으로써 Nernst-Einstein의 식을 통한 염화물 이온 이동계수의 산정방법을 사용하였으며, NT BUILD 492법 및 해수 침지실험을 통한 확산 특성과 비교하여 값의 차이에 대하여 고찰하였다. 그 결과 실험인자의 변화가 염소이온 확산에 미치는 영향은 미비한 것으로 평가되어져 실험조건에서 발생하는 영향은 거의 없는 것으로 규명되었으며, NT BUILD 492법과도 거의 동일한 값이 구해졌다. 침지실험 결과와의 상이는 염소이온 확산에서 경계조건의 차이 및 염소이온의 시멘트 수화물과의 고정화에 의한 것으로 판단되어진다.

제설제 및 동결융해 환경하에서 콘크리트의 내구성 증진 방안에 관한 연구 (Improvement of Concrete Durability under Deicier and Freez-Thaw Environment)

  • 이병덕;윤병성
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 추계 학술발표회 제17권2호
    • /
    • pp.523-526
    • /
    • 2005
  • In order to traffic safety during winter season, snowfall and cold area has been spread the deicing chemicals, and the spraying amount is increasing every year. Use of deicing chemicals has been and will continue to be a major part of highway snow and ice control methods. Chloride-containing chemicals such as calcium chloride or rock salt are main deicers for the road. Extensive use of chloride deicers is, however, the source of substantial cost penalties due to their corrosive action and acceleration to deterioration concrete structures. Deterioration due to de-icer salt occurs in practice in concrete pavement, dike, barrier and similar structure. This paper reports the results of effect of de-icer salt on durability of concrete structure in winter. To protect concrete structure from damage by de-icer salt in winter, the exposure test was performed using three methods such as increase in design strength upto 32MPa application of granulated blast furnace slag powder, and concrete sealer. Of these, the method of increase in design strength upto 32MPa showed better durability for deterioration by de-icer salt.

  • PDF

적설한랭지역에서 콘크리트의 내구성 (Durable of Concrete in Snowfall and Cold Regions)

  • 이병덕;정해문;윤병성
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.221-224
    • /
    • 2005
  • In order to traffic safety during winter season, snowfall and cold area has been spread the deicing chemicals, and the spraying amount is increasing every year. Use of deicing chemicals has been and will continue to be a major part of highway snow and ice control methods. Chloride-containing chemicals such as calcium chloride or rock salt are main deicers for the road. Extensive use of chloride deicers is, however, the source of substantial cost penalties due to their corrosive action and acceleration to deterioration concrete structures. Deterioration due to de-icer salt occurs in practice in concrete pavement, dike, barrier and similar structure. This paper reports the results of effect of de-icer salt on durability of concrete structure in winter. To protect concrete structure from damage by de-icer salt in winter, the exposure test was performed using three methods such as increase in design strength upto 35MPa application of granulated blast furnace slag powder, and concrete sealer. Of these, the method of increase in design strength upto 35MPa showed better durability for deterioration by de-icer salt.

  • PDF

기능성 나노복합 무기질 활성탄계 표면 처리제를 적용한 콘크리트의 내구성능 평가에 관한 실험적 연구 (An experimental study on the durability evaluation of concrete applied functional nano composite inorganic activated carbon based coatings)

  • 양기영;장석재;백종명
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2006년도 추계학술대회 논문집
    • /
    • pp.1385-1390
    • /
    • 2006
  • Concrete structure can be deteriorated by ingress of moisture and aggressive agents. To maintain the sound performance of concrete structure during the service life, it needs to protect concrete from ingress of moisture and aggressive agents before arising deterioration of concrete. Protection of concrete is possible by surface treatment. In this study, durability of the functional nano composite inorganic activated carbon based coatings which can provide a barrier against the ingress of moisture or aggressive ions to concrete is discussed. For the durability evaluation of the coatings, fine void structure evaluation test, chloride penetration acceleration test, accelerated carbonation test, freezing and thawing test, and the accelerated test of chemical erosion are conducted. As the result of this study, the functional nano composite inorganic activated carbon based coatings which became one formed complex compound with adsorption and porosity on concrete surface, had an effect on the function of far infrared radiation, antimicrobial action, air cleaning, airing assurance, and the interception of moisture of deterioration factor, chloride ion, carbon dioxide, sulfate, and so on.

  • PDF

아초산계 방청제 도포에 의한 철근 부식 보수 시스템 공법 개발 (The Development of Repair System for RC Members with Damaged by Rebar Corrosion Using Inhibitor with High Nitrite Content)

  • 이한승;나정일;박순만
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.359-364
    • /
    • 2001
  • The purpose of this study is to develop the repair system for RC members with damaged by rebar corrosion using new corrosion inhibitor which was high nitrite content. In the experiments, the acceleration corrosion test of rebar was conducted using the specimen which was applied by various repair system. As a result, it was confirmed that the new repair system without concrete patching had high anti-corrosion property compared with other repair systems and was very effective as a spray type corrosion inhibitor in concrete containing chloride (0.1% of NaCl).

  • PDF

Hybrid형 폴리머 시멘트 슬러리로 도장한 철근의 부착강도와 부식저항성 (Bond Strength and Corrosion Resistance of Coated Reinforcing Bar Using Hybrid-Type Polymer Cement Slurry)

  • 조영국
    • 한국건축시공학회지
    • /
    • 제8권3호
    • /
    • pp.93-99
    • /
    • 2008
  • The purpose of this study is to evaluate the bond strength and corrosion resistance of coated reinforcing bar using hybrid-type polymer cement slurry(PCS). PCS coated steels, which is made from two types of polymer dispersions such as St/BA and EVA are prepared, and tested for bond strength and various corrosion resistances such as autoclaved cure, carbonation and H2SO4 solution. From the test results, the bond strength of PCS coated reinforcing bar using ordinary portland cement at 1-5, 2-1 and 4-5 of mixes is higher than that of uncoated regular steel. However, bond strength of almost PCS coated reinforcing bars using ultra rapid high strength cement is higher than that of epoxy coated bar, is also in ranges of 102% to 123% compared to that of uncoated regular steel. In autoclaved accelerating test, the ratio of corrosion of uncoated regular steel is increased with the increase in NaCl content, but the corrosion of PCS coated steel was very small. In the acceleration test for carbonation, increasing the amount of NaCl the corrosion of coated steel did not produce. The corrosion of uncoated regular steel is increased with the increase in the amount of NaCl. It can be seen that the NaCl following the acceleration test for carbonation can lower the corrosion resistance of concrete. As a result, the corrosion of steel largely is affected by the acceleration curing, chloride ion penetration and carbonation and shown more severe corrosion by applying complex factors. These corrosions of steel can be suppressed by the coating of PCS.