• 제목/요약/키워드: Characteristic of deterioration

검색결과 194건 처리시간 0.031초

가지형 트리의 열화진단을 위한 방전통계량에 관한 연구 (A Study on Discharge Statistics Quantities for Deterioration Diagnosis of Branch-type Tree)

  • 신성권;김경민;김탁용;이덕진;박창옥;김재환
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 E
    • /
    • pp.2345-2348
    • /
    • 1999
  • Existing $\psi$-AEA-t (phase-AEA-time) characteristic in polymer materials for power cable is good in general deterioration characteristic according to time variation, but it is difficult to clearly distinguish from deterioration state and diagnosis of deterioration is not enough to some extent. This paper is interpreted AE discharge statistics quantities measuring phase-amplitude variation of acoustic emission characteristic obtained from treeing breakdown experiment. Besides it can know useful discharge statistics quantities (AE average inception phase/amplitude, AE average maximum phase/amplitude) about so many for diagnosis of treeing deterioration.

  • PDF

MPPF 커패시터의 전기적, 열적 열화시 소체의 화학적특성에 관한 연구 (A Study on Chemical Characteristic of Electrically and Thermally Treated MPPF Capacitor Elements)

  • 구교선;송현석;이동준;곽희로;송길목
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.227-230
    • /
    • 2001
  • This paper divides the factors of an accident into two parts, that are electrical deterioration and thermal deterioration, to analyze a characteristic of the factor of an accident which can break out in the capacitor of metal vaporized polypropylene film. For the purpose of creating capacitor which is caused by electric deterioration, we applied DC overvoltage, induced self-healing and breakdown from element. We applied gradual heat to get an element which is cause by thermal deterioration. The chemical structure of the shape and surface is analyzed by thermogravimetric analyzer (TGA), Scanning Electron Microscope (SEM) and Fourier Transform Infrared Spectrometer(FT-IR). As a result, the peak of methylene group came out, in case of electrical deterioration, as observing the self-healing point. However, the peak is disappeared in the heat treated element by 500[$^{\circ}C$], and the peak of carbonyl group which has C=O came out in case of thermal deterioration.

  • PDF

철근의 강종 및 직경 변화에 따른 부식특성에 관한 연구 (A Study on the Characteristics of Reinforcing Steel according to Specification and Diameter)

  • 임재원;지남용;윤상천;최진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2003년도 학술.기술논문 발표회
    • /
    • pp.53-58
    • /
    • 2003
  • Concrete structures move wholly with concrete and rebar, so they endure external force, but recently the embedded rebar in concrete has been corroded by environmental, physical and chemical factors, the embedded rebar corrosion influences concrete structure to deteriorate structure capacity. To revaluate effect to deterioration of concrete structure according to corrosion of rebar, the researcher mostly examined into corrosion rebar and complex relation of concrete. In that there are flexural strength deterioration of corrosion concrete structure and the bond strength of concrete. But It has not sufficiently studied about physical characteristic of corrosion rebar itself. In this study I will compare specification of rebar through corrosion experiment with corrosion ratio of rebar according to diameter and revaluate. And will investigate the effect to strength characteristic of rebar according to corrosion ratio.

  • PDF

철근의 강종 및 직경 변화에 따른 부식특성에 관한 연구 (A Study on the Characteristics of Reinforcing Steel according to Specification and Diameter)

  • 임재원;지남용;윤상천;최진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2003년도 학술.기술논문발표회
    • /
    • pp.53-58
    • /
    • 2003
  • Concrete structures move wholly with concrete and rebar, so they endure external force, but recently the embedded rebar in concrete has been corroded by environmental, physical and chemical factors. the embedded rebar corrosion influences concrete structure to deteriorate structure capacity. To revaluate effect to deterioration of concrete structure according to corrosion of rebar, the researcher mostly examined into corrosion rebar and complex relation of concrete. In that there are flexural strength deterioration of corrosion concrete structure and the bond strength of concrete. But It has not sufficiently studied about physical characteristic of corrosion rebar itself. In this study I will compare specification of rebar through corrosion experiment with corrosion ratio of rebar according to diameter and revaluate. And I will investigate the effect to strength characteristic of rebar according to corrosion ratio.

  • PDF

특정환경조건하에서의 콘크리트 내 이차광물생성과 그에 수반된 성능저하현상 (Secondary Mineral Formation and Concrete Deterioration Caused by Certain Environmental Conditions)

  • 이효민;황진연;진치섭;이진성;전쌍순
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.651-656
    • /
    • 2003
  • Durability of concrete is possibly related to externally-induced chemical attacks in addition to internally-induced deterioration. Externally-induced chemical attacks can be derived from various sources according to environmental conditions under which concrete structures are existing. The present study investigates the characteristic concrete deterioration and formation of secondary minerals by external chemical attacks under certain environmental condition. Petrographic microscope, SEM, EDAX, XRD analyses were conducted to identify secondary mineral formation and micro-structural analyses.

  • PDF

음향탐지를 이용한 트리잉의 열화진단을 위한 정량적 분석에 관한 연구 (A Study on Quantitative Analysis for Treeing Deterioration Diagnosis Using Acoustic Detection)

  • 이덕진;신성권;김재환
    • 조명전기설비학회논문지
    • /
    • 제13권4호
    • /
    • pp.68-74
    • /
    • 1999
  • 본 연구는 고분자재료에서 음향센서를 이용한 부분방전의 음향적 탐지를 행했다. 저밀도 폴리에틸렌에 대한 트리잉파괴 실험에서 음향센서로 얻어진 음향방출 특성의 시간순서대로 측정하여 통계처리를 행했다. 또한 5가지 특성량을 도입하고 $\psi$-AEA-n(위상-음향진폭-펄스수) 패턴을 분석한 결과, 보이드 시료의 AE평균개시진폭 $(\overline{AEA_{inc}})$과 AE 평균최대진폭$(\overline{AEA_{max}})$은 열화중기, AE펄스수, AE평균최대위상각$(\overline{\theta{max}})$은 열화말기를 진단하기 위해서 유용한 음향방출량임을 알 수 있다. 이들 음향방출량은 보이드 시료의 열화진단을 구별하는데 유용한 음향방출량임을 실험결과로부터 얻었다.

  • PDF

전자접촉기 열화에 따른 전기적 특성 분석 (Analysis of Electrical Characteristics Due to Deterioration of Electromagnetic Contactor)

  • 최순호
    • 한국전기전자재료학회논문지
    • /
    • 제32권5호
    • /
    • pp.407-412
    • /
    • 2019
  • In this paper, the changes in the electrical characteristics (arc energy, contact resistance, and bouncing phenomenon) due to the deterioration of the contact are analyzed. The results are generally consistent and can be analyzed for contact deterioration. The results of the experiment demonstrate that the arc energy is linearly related to the current when the contact samples and the voltage conditions are the same. The contact resistance varies due to multiple factors, but is generally within a certain range, and the contact deterioration can be determined. Contact stabilization can be detected by the decrease in the bouncing phenomenon due to deterioration (the change of the shape of the contact).

알루미나계 자기애자의 장기 피로특성에 관한 연구 (Study on Long-term Deterioration Properties of Porcelain Insulators with Aluminous System)

  • 한세원;조한구;이동일;최인혁
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.562-563
    • /
    • 2005
  • In case of aged porcelain, the failure in basic performance tests happened in cool-heat tests. Based on this characteristic, we studied the method predicting failure phenomena through more severe accelerated cool-heat ageing and accelerating thermal mechanical performance tests. Test results indicated that the thermal stress by temperature gradient was more severe parameter than thermal stress by quenching cycles within a category of standard or accelerating methods. And there is no the deterioration of statistic strength, but the deterioration of strength according to accelerating tests is serious.

  • PDF

ACSR 슬리브 개소에서의 송전선 재료특성 검토 (Material characteristic of ACSR due to eccentricity at sleeve point)

  • 강지원;홍동석;장태인;윤형희;이동일;최한열
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 제37회 하계학술대회 논문집 A
    • /
    • pp.309-310
    • /
    • 2006
  • The considerations for remaining life of ACSR (Aluminum Stranded Conductors Steel Reinforced) in transmission lines has become gradually important to hold reliability and stability of power supply. The remaining life of ACSR exposed to the atmosphere for a long period may rely on deterioration caused by environmental indices such as atmospheric corrosion, galvanic corrosion, crevice corrosion and fatigue corrosion. This paper deals with material characteristic of ACSR due to eccentricity at sleeve point. Test samples are ACSR 240[$mm^2$] conductors, which are real transmission lines. As a result, it is obvious that ACSR due to eccentricity may lead to mechanical deterioration.

  • PDF

FRF를 이용한 KTX 차륜 경년변화 분석 (Analysis KTX wheel aged deterioration using Frequency Response Function)

  • 윤차중;이성욱;조광우
    • 한국소음진동공학회:학술대회논문집
    • /
    • 한국소음진동공학회 2006년도 춘계학술대회논문집
    • /
    • pp.1453-1458
    • /
    • 2006
  • KTX Railway rolling stock wheel run its course to corrode, deteriorate and wear away through out the time. So it is natural that the performance and ability of wheel gets declined. The frequency characteristic analysis were accomplished to above trend and shock wave flow to wheels were examined. The result will be used to find Railway rolling stock wheel crack and maintenance method hereafter.

  • PDF