Physical Properties and Cytotoxicity of Dental Pit and Fissure Sealants Containing Cerium Oxide Nano Particles(CNPs) (세륨옥사이드나노입자(Cerium Oxide Nano Particles; CNPs)를 첨가한 치면열구전색재의 물리적 특성 및 세포독성)

  • Jeong, Mi-Ae;Kim, Dong-Ae
    • The Journal of the Korea Contents Association
    • /
    • v.22 no.3
    • /
    • pp.586-592
    • /
    • 2022
  • In this study cerium nano particles(CNPs) with 0-4.0 wt% was incorporated to the conventional dental pit and fissure sealant(ConciseTM) to produce new pit and fissure sealant the physical properties and cytotoxicity. The physical properties were measured for polymerizing depth the degree of water absorption and solubility. The cytotoxicity of cell viability was analyzed by MTT assay using immortalized human oral keratinocyte(IHOK). As a result of this preceding study the polymerizing depth was decreased by the increasing of the amount of CNPs. The solubility degree of the sealant added CNPs with 2.0 wt% showed was the lower and the water absorption showed no significantly difference with the control groups(p>0.05). The cytotoxicity test results showed high survival rates in all experimental groups. Therefore, pit and fissure sealant by the addition of CNPs excellent cell viability be produced without weaken the physical property of the cell viability fissure sealant containing CNPs does not weaken physical properties and has no cytotoxic effects biocompatibility. Considering its properties effect of CNPs, further studies are required for distribution technology application.

Changes in the amount of adhesion of Streptococcus mutans to pit and fissure sealant incorporating cerium oxide nano particles(CNPs) (세륨옥사이드나노입자(Cerium oxide nano particles: CNPs)를 함유한 치면열구전색재의 Streptococcus mutans 부착량 변화)

  • Lee, Seong-Sook;Park, Young-Min;Kim, Dong-Ae
    • Journal of Korean society of Dental Hygiene
    • /
    • v.20 no.4
    • /
    • pp.535-543
    • /
    • 2020
  • Objectives: The aim of this study was to investigated the surface roughness and change in the amount of adhesion of Streptococcus mutans to the commercial pit and fissure sealant containing cerium oxide nano particles(CNPs). Methods: The CNPs was incorporated into a commercial pit and fissure sealant at 0-4.0 wt%. Disk Specimens (ϕ 10 mm × 2 mm) were prepared by light polymerization the front and back for 40s. Average surface roughness was measured and Streptococcus mutans adhesion was observed under confocal laser scanning microscopy (CLSM) after 24 hour. Data were statistically analyzed by one-way ANOVA and Tukey HSDa post-hoc test. Results: Difference of the surface roughness(Ra) between groups was not statistically significant in both non CNPs group and CNPs group(p>0.05). In CNPs group, the amount of S. mutans adhesion was significantly different between control group and decreased in order of CNPs 4.0, CNPs 0.5, CNPs 1.0 and CNPs 2.0(p<0.05). Conclusions: Within the limitation of this study, these aspects of oral bacteria performances suggest potential usefulness of the CNPs incorporation, especially CNPs 1% and 2%, in pit and fissure sealant for inducing antibacterial effect.