Preparation of Fine Single-Crystalline Particles of Ferroxplana, $Ba_2Co_2Fe_{12}O_{22}$ from Crystallization of Glass (유리결정화에 의한 Ferroxplana $Ba_2Co_2Fe_{12}O_{22}$ 미세 단결정의 제조)

  • 김성재;김동호;이재동;김태옥
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.3
    • /
    • pp.236-242
    • /
    • 1993
  • As the fundamental research on preparation of fine single crystalline ferroxaplana by means of glass-crystallization methods using steel twin-roller, the properties of ferroxplana crystallized from glass were studied. Most of the specimens quenched by twin-roller at about 130$0^{\circ}C$ were glass phase, the crystallization of these glasses underwent multi-steps and ferroxplana phase was only stable in the temperature range of 88$0^{\circ}C$ to 95$0^{\circ}C$. Above 95$0^{\circ}C$ ferroxplana begines to be decomposed in glass. Ferroxplana had such magnetic properties as M8=29emu/g, MHC=166Oe, and Curie Temperature, Tc=610$\pm$5K.

  • PDF

Control of Pore Characteristics of Porous Glass in the $ZrO_2.SiO_2$ System Prepared by the Sol-Gel Method (졸-겔법으로 제조한 $ZrO_2.SiO_2$다공질유리의 세공제어)

  • 신대용;한상목
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.6
    • /
    • pp.485-491
    • /
    • 1993
  • Porous glass in the ZrO2.SiO2 system containning up to 30mol% zirconia were prepared by the sol-gel method from metal alkoxides and their pore characteristics with reaction parameters were investigated. The gels were made by hydrolyzing and condensation of the mixed metla alkoxides and were converted into the porous glass by heating up to $700^{\circ}C$. As a results, the mean pore radius became larger with increasing contents of HCl, H2O and hydrolysis temperature, and an alcohol with a large molecular weight for making the porous glass. In the case of 20ZrO2.80SiO2 porous glass with heated at $700^{\circ}C$, HCl and H2O content was 0.3mol and 4mol, the specific surface area was 284$m^2$/g, average mean pore radius was about 19.4$\AA$, porosity was 22.55% and pore characteristics depended on heating temperature.

  • PDF

Hardening and Hydroxyapatite Formation of Bioactive Cement Prepared from Calcium Phosphosilicate Glass

  • Kim, Cheol-Young;Park, Sang-Jong
    • The Korean Journal of Ceramics
    • /
    • v.1 no.3
    • /
    • pp.131-136
    • /
    • 1995
  • It has been reported that the biocement obtained by mixing $CaO-SiO_2-P_2O_5$ glass powders with ammonium phosphate solution has biocompatibility as will as high strength. The hardening mechanism and hydroxyapatite forming mechanism were discussed when $53.6%CaO_1,\; 38.1%SiO_2,\; 7.7P_2O_6,\; 0.6%CaF_2$(mole %) glass powder was reacted with ammonium phosphate solution and reacted in tris-buffer solution, respectively. High strength hardened biocement was obtained for the specimen with $CaNH_4PO_4\;H_2O$ crystal when the glass powder was mixed with ammonium phosphate solution, and hydroxyapatite crystal was rapidly formed only in the sample with $CaNH_4PO_4\;H_2O$ crystal when it was reacted in tris-buffer solution.

  • PDF

Ambient Pressure Dried Silica Aerogel Thin Film from Water Glass

  • Cha, Young-Chul;Yoon, Jong-Seol;Lee, Jun;Hwang, Hae-Jin;Moon, Ji-Woong
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.2
    • /
    • pp.87-89
    • /
    • 2008
  • A nano structured silica aerogel thin film was manufactured from inexpensive sodium silicate (water glass) using an ambient pressure drying method. High purity silicic sol was prepared by passing a water glass solution through an ion exchange resin, and the gel films were prepared on a modified glass substrate via dip coating. The dip coating conditions, such as coating time and solvent, were optimized. The optical and physical properties of the obtained silica aerogel thin film were characterized using a UV-visable spectrometer and a scanning electron microscope.

The Microwave Dielectric Properties on Glass Frit Addition of Low Temperature Co-fired Ceramic (Glass Frit 첨가에 따른 LTCC용 마이크로파 유전체의 유전 특성)

  • Yoon, Jung-Rag;Lee, Serk-Won;Lee, Heon-Young;Kim, Jee-Gyun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07b
    • /
    • pp.611-615
    • /
    • 2003
  • The crystalline and dielectric properties on $Al_2O_3$ filled glass frit ($CaO-Al_2O_3-SiO_2-MgO-B_2O_3$) with admixtures of $TiO_2$ have been investigated. The dielectric constant value of $7.5{\sim}7.8$, quality factor value of 700 were obtained for glass frit : $Al_2O_3$ (50 : 50 wt%) ceramics. As the amount of $TiO_2$ increased, temperature coefficient of dielectric constant were decreased.

  • PDF

A Study on Glass-Infiltrated Alumina and Spinel Composite I. Effect of Microstructure and Glass Content on Contant Damage and Strength (유리침윤 알루미나 및 스핀넬 복합체에 관한 연구 I. 미세구조 및 유리함량이 접촉손상 및 강동에 미치는 영향)

  • 정연길;최성철
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.7
    • /
    • pp.671-678
    • /
    • 1998
  • Hertzian indentation tests with sphere indenters were used to study the mechanical properties of glass-in-filtrated alumina and spinel composites and evaluated the effect of preform microstructure and evaluated the effect of preform microstructure and glass con-tents on contanct damage and strength. The spinel composite showed more brittle behavior than the alumina composite which is verified from indentation stress-strain curve cone cracks and quasi-plastic deformation developed at subsurface. Failure originated from either cone cracks(brittle mode) or deformation zone(quasi-plastic mode) above critical load for cracking(Pc) and yield ({{{{ {P }_{Y } }}) with the brittle mode more dominant in the spinels and the quasi-plastic mode more dominant in the aluminas. Even though brittle mode was dominant in the spinel composites the strength degradation from accumulation of damage above these critical loads was conspicuously small suggesting that the glass-infiltrated composites should be highly damage tolerant to the blunt contacts.

  • PDF

Effects of Processed Slag as Glassmaking Raw Material (on Soda-Lime Glass) (개질 고로 슬래그에 관한 연구 (유리 제조에 관한 연구))

  • 양중식
    • Journal of the Korean Ceramic Society
    • /
    • v.18 no.2
    • /
    • pp.112-118
    • /
    • 1981
  • A study was made on the processing of domestic blast furnace slag by flotation and chemical purification for the use of slag as a raw material in making soda lime glasses. Feasibility study has been made for the use of reprocessing slag as a source material for both coloring and chemical components (such as CaO, $Al_2O_3$, MgO and etc.) in the glass making process. Chemical composition of chemically purified slags ranges; $SiO_2$ 34.5~37.5, $Al_2O_3$, 16.2~14.1, $Fe_2O_3$ 0.33~0.14, CaO 34.5~38.8, MgO 4.0~5.2, NmO 0.16~0.39, $TiO_2$ 0.23~0.35, S 0.08~0.42, ignition loss 3.3~8.4 and others 0.48~0.51%. It was found that either amber or greenish color could be easily obtained with the addition of salg up to 24%, however the slag addition to glass batches much impaired the transmitancy of glass products, thus a glass made with 7% slag addition showed 82% in transmitancy value at 510 nm.

  • PDF

Preparationand Characteristics of ZnS-doped Borosilicate Glass(I) (ZnS 반도체 미립자 분산 Borosilicate Glass 제조 및 물성(I))

  • 이승한;박성수;박희찬;류봉기
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.5
    • /
    • pp.493-498
    • /
    • 1998
  • ZnS doped borosilicate glass for nonlinear optical application was prepared by melting and precipitation process. The optical band gap of the precipitated ZnS particles ranged from 3.83 to 3.96 eV compared with the bulk ZnS energy gap of 3.53 eV. This result was interpreted in terms of a quantum confinement effect due to small crystal size. ZnS partilcle size estimated by effective mass approximation ranged from about 39 to 83 $\AA$ It increased wtih the increase of heat tratment time and temperature.

  • PDF

Fabrication of Er-doped Sodium Borosilicate Glass Films Using Aerosol Flame Deposition Method (Aerosol Flame Deposition법을 이용한 Er-doped Sodium Borosilicate 유리박막 제작에 관한 연구)

  • 문종하;정형곤;이정우;박강희;박현수;김병훈
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.2
    • /
    • pp.117-121
    • /
    • 2000
  • Er-doped sodiumborosilicate glass films for waveguides amplifier were fabricated by Aerosol Flame Deposition(AFD) method. Al2O3 was added to sodium borosilicate glass films to suppress the formation of crystalline phase and control the refractive index. the formation of crystalline phase was suppressed above Al2O3 of 6 wt%. As the amount of Al2O3 increased from 2 to 12 wt% the refractive index of glass films increased lineary from 1.4595 up to 1.4710. After the core of 77SiO2-15B2O3-8Na2O+6 wt%Al2O3+8wt%Er2O3 was coated on the buffer layer of 77SiO2-15B2O3-8Na2O+6 wt%Al2O3, the core was etched by reactive ion etching. The absorption spectrum of 3 cm waveguide amplifier showed two peaks of 1530 and 1550 nm.

  • PDF

Joining Behavior of Ceramics to Metal by Using Lead-bismate Heavy Metal Glass Frit (중금속 창연산화납계 저온유리 분말을 이용한 세라믹스/금속의 접합거동)

  • Choi, Jin Sam
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.4
    • /
    • pp.312-316
    • /
    • 2014
  • The joining behavior of forsterite ceramics to SUS304 alloy using $8PbO-78Bi_2O_3-8B_2O_3-4ZnO-2SiO_2$ (wt%) system glass frit was investigated. The contact angle was smaller than $90^{\circ}$ at a temperature of $460^{\circ}C$. Redox reaction at the interface between forsterite and SUS304 was found to appear when the electrons in the metal part moved toward the glass part and the oxygen ions in glass moved to the metal side. The decrease of the surface tension due to the PbO solubility on the forsterite side contributed to the better wetting behavior at low temperature.